Hao Wang
Hao Wang has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
- Qiang Mao
Engineering Institute of Advanced Manufacturing and Modern Equipment Technology, Jiangsu University, Zhenjiang,Chin, Zhenjiang, 212013, CHINA
6 shared publications - Ze Jiang
Jiangsu University, Engineering Institute of Advanced Manufacturing and Modern Equipment Technology, China, Zhenjiang, ZhenJiang, JiangSu, 212013, CHINA
6 shared publications - Tianci Zhang
Jiangsu University, Zhenjiang, 212013, CHINA
5 shared publications - Chenyu Zhu
Engineering Institute of Advanced Manufacturing and Modern Equipment Technology, Jiangsu University, Jiangsu University, No. 301,Xuefu Road, Jingkou District, Zhenjiang, 212013, People's Republic of China, Zhenjiang, CHINA
4 shared publications - Xiaojing Xu
Institute of Advanced Manufacturing and Modern Equipment Technology, Jiangsu University, Zhenjiang, China
4 shared publications - Hao Chen
Jiangsu University, Engineering Institute of Advanced Manufacturing and Modern Equipment Technology, ZhenJiang, JiangSu, CHINA
3 shared publications
Latest Publications
- 16 January 2024
- Published by University of Queensland Library
Semisolid processing of aluminium alloys
The University of Queensland's institutional repository, UQ eSpace, aims to create global visibility and accessibility of UQ’s scholarly research.
- 16 January 2024
- Published by University of Queensland Library
Semisolid processing of aluminium alloys
The University of Queensland's institutional repository, UQ eSpace, aims to create global visibility and accessibility of UQ’s scholarly research.
- Open Access
- 1 December 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (12) , 1265g4
Effect of solid solution heat treatment following age hardening on microstructure and mechanical properties of 7000 series power aluminum alloy
In this paper, Al-11.1Zn-2.7Mg-1.7Cu-1.4Ti-0.2Zr alloy material was prepared by powder metallurgy to study the effect of the different solid-solution aging systems on the microstructure and mechanical properties of this 7000 series aluminum alloy. The microstructure of the alloy under the three different solid-solution processes S1, S2, and S3 were observed using an optical microscope, scanning electron microscope, and X-ray diffraction analysis. The mechanical properties were tested to determine the best solid-solution process. The results show that under the S2 solid-solution process, the alloy has the best mechanical properties, with a compressive strength of 646.7(±6.5) MPa and a fracture strain of 5.9(±0.06)%. The maximum hardness trends in the three solid-solution processes after aging are S2>S3>S1. The maximum hardness 220.7(±5.5 )HV occurs after S2 solid-solution and 121℃×18 h aging. Moreover, after S2 solid-solution treatment, the solid-solution degree is close to saturation, the solid-solution strengthening effect is the best, and dislocations contribute the most to the strength.
- 1 December 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (12) , 1265g4
Open AccessEffect of solid solution heat treatment following age hardening on microstructure and mechanical properties of 7000 series power aluminum alloy
In this paper, Al-11.1Zn-2.7Mg-1.7Cu-1.4Ti-0.2Zr alloy material was prepared by powder metallurgy to study the effect of the different solid-solution aging systems on the microstructure and mechanical properties of this 7000 series aluminum alloy. The microstructure of the alloy under the three different solid-solution processes S1, S2, and S3 were observed using an optical microscope, scanning electron microscope, and X-ray diffraction analysis. The mechanical properties were tested to determine the best solid-solution process. The results show that under the S2 solid-solution process, the alloy has the best mechanical properties, with a compressive strength of 646.7(±6.5) MPa and a fracture strain of 5.9(±0.06)%. The maximum hardness trends in the three solid-solution processes after aging are S2>S3>S1. The maximum hardness 220.7(±5.5 )HV occurs after S2 solid-solution and 121℃×18 h aging. Moreover, after S2 solid-solution treatment, the solid-solution degree is close to saturation, the solid-solution strengthening effect is the best, and dislocations contribute the most to the strength.
- 25 November 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (12) , 126597
Effect of SiCw volume fraction and cold pressure on microstructure and mechanical properties of aluminum matrix composites
The alloy powder and SiCw reinforcement were ball milled, cold-pressed, sintered, hot extruded and solution aged to obtain excellent mechanical properties such as hardness and compressive strength. The microstructure and properties of the material were characterized by metallographic microscope, scanning electron microscope (SEM), EDS, X-ray diffraction (XRD), HV-1000 microhardness and 7051 eddy current conductivity. The results show that the distribution of SiC whiskers in the mixed powder is relatively uniform, but there is still a small amount of agglomeration phenomenon in the sintered sample. The optimum cold pressure is 740 MPa. With the increase in SiCw content, the hardness, dislocation density and compressive strength of aluminum matrix composites are improved. The compressive strength of 5%SiCw reinforced aluminum matrix composite is 658.9 MPa and the elongation is 6.7%.
- 25 November 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (12) , 126597
Effect of SiCw volume fraction and cold pressure on microstructure and mechanical properties of aluminum matrix composites
The alloy powder and SiCw reinforcement were ball milled, cold-pressed, sintered, hot extruded and solution aged to obtain excellent mechanical properties such as hardness and compressive strength. The microstructure and properties of the material were characterized by metallographic microscope, scanning electron microscope (SEM), EDS, X-ray diffraction (XRD), HV-1000 microhardness and 7051 eddy current conductivity. The results show that the distribution of SiC whiskers in the mixed powder is relatively uniform, but there is still a small amount of agglomeration phenomenon in the sintered sample. The optimum cold pressure is 740 MPa. With the increase in SiCw content, the hardness, dislocation density and compressive strength of aluminum matrix composites are improved. The compressive strength of 5%SiCw reinforced aluminum matrix composite is 658.9 MPa and the elongation is 6.7%.
- 1 September 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (11) , 1165f4
Effect of SiCw volume fraction on microstructure and properties of SiCw/Al composite fabricated by hot isostatic pressing-hot pressing
- 1 September 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (11) , 1165f4
Effect of SiCw volume fraction on microstructure and properties of SiCw/Al composite fabricated by hot isostatic pressing-hot pressing
- 19 July 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (9) , 096582
Effect of surface boroaluminizing on thermal corrosion behavior of TC4 (Ti-6AL-4V) titanium alloy
- 19 July 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (9) , 096582
Effect of surface boroaluminizing on thermal corrosion behavior of TC4 (Ti-6AL-4V) titanium alloy
- 19 February 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (6) , 066504
Effect of multi-stage solution and aging process on microstructure and properties of Al–10.7Zn–2.8Mg–1.2Cu–0.2Zr aluminum alloy extrusion materials
Al-Zn-Mg-Cu extruded aluminum alloy was processed by multistage solid solution aging process to obtain excellent mechanical properties.Such as Strength, plasticity, corrosion resistance,and the microstructure and properties of the materials were characterized by metallographic microscope,XRD,hv-1000 microhardness tester and wdw-200 microcomputer controlled universal testing machine.The experimental results show that the aging temperature T7X-1 has lower strength but higher plasticity compared with T6.With the increase of the solid solution temperature, the strength showed a certain regularity, the maximum tensile strength of the alloy can reach 787.1 MPa.The multi-stage solid solution process can increase the dislocation density and improve the intergranular corrosion resistance of the alloy.And by comparison, the alloy in the solution treatment system (460 ℃×2 h+470 ℃×2 h+480 ℃×2 h and aging system(121 ℃×5 h+153 ℃×16 h) heat treatment state has a good comprehensive mechanical properties.
- 19 February 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (6) , 066504
Effect of multi-stage solution and aging process on microstructure and properties of Al–10.7Zn–2.8Mg–1.2Cu–0.2Zr aluminum alloy extrusion materials
Al-Zn-Mg-Cu extruded aluminum alloy was processed by multistage solid solution aging process to obtain excellent mechanical properties.Such as Strength, plasticity, corrosion resistance,and the microstructure and properties of the materials were characterized by metallographic microscope,XRD,hv-1000 microhardness tester and wdw-200 microcomputer controlled universal testing machine.The experimental results show that the aging temperature T7X-1 has lower strength but higher plasticity compared with T6.With the increase of the solid solution temperature, the strength showed a certain regularity, the maximum tensile strength of the alloy can reach 787.1 MPa.The multi-stage solid solution process can increase the dislocation density and improve the intergranular corrosion resistance of the alloy.And by comparison, the alloy in the solution treatment system (460 ℃×2 h+470 ℃×2 h+480 ℃×2 h and aging system(121 ℃×5 h+153 ℃×16 h) heat treatment state has a good comprehensive mechanical properties.
- 25 January 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (4) , 046551
Anisotropy of microstructure and properties of high strength hot-extruded processed aluminum alloy
- 25 January 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (4) , 046551
Anisotropy of microstructure and properties of high strength hot-extruded processed aluminum alloy
- 28 September 2018
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (1) , 016527
Effect of Zn/Mg and Cu/Mg on microstructure and properties of Al-xZn-3.0Mg-yCu-0.2Zr rolled aluminum alloy
Effect of Zn/Mg and Cu/Mg on microstructure and properties of Al-xZn-3.0Mg-yCu-0.2Zr rolled aluminum alloy was studied by XRD analysis, hardness and electric conductivity test, tensile test and intergranular corrosion experiments. The results show that for rolled aluminum alloy with compositon of Al-xZn-3.0Mg-yCu-0.2Zr, the increase of Zn/Mg and Cu/Mg values in the alloy can introduce dislocation into the alloy and promote recrystallization of the alloy. Increasing Zn to a certain extent has a strong hardening effect on the alloy, but when the Zn content rises above the solid solubility, the strength and toughness decrease. In addition, the increase of Zn is disadvantageous to the alloy's resistance to intergranular corrosion. The increase of the Cu/Mg value decreases the strength and the hardness, but the toughness is improved. In addition, the increase of Cu/Mg value will increase the resistance to intergranular corrosion of the alloy.
- 28 September 2018
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (1) , 016527
Effect of Zn/Mg and Cu/Mg on microstructure and properties of Al-xZn-3.0Mg-yCu-0.2Zr rolled aluminum alloy
Effect of Zn/Mg and Cu/Mg on microstructure and properties of Al-xZn-3.0Mg-yCu-0.2Zr rolled aluminum alloy was studied by XRD analysis, hardness and electric conductivity test, tensile test and intergranular corrosion experiments. The results show that for rolled aluminum alloy with compositon of Al-xZn-3.0Mg-yCu-0.2Zr, the increase of Zn/Mg and Cu/Mg values in the alloy can introduce dislocation into the alloy and promote recrystallization of the alloy. Increasing Zn to a certain extent has a strong hardening effect on the alloy, but when the Zn content rises above the solid solubility, the strength and toughness decrease. In addition, the increase of Zn is disadvantageous to the alloy's resistance to intergranular corrosion. The increase of the Cu/Mg value decreases the strength and the hardness, but the toughness is improved. In addition, the increase of Cu/Mg value will increase the resistance to intergranular corrosion of the alloy.