YaChao Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
YaChao Wang has a total of 74 co-authors. Here are the top co-authors by number of shared publications:
JiangPing Zhao
School of Resources Engineering Xi'an University of Architecture & Technology 710055 Xi'an Shaanxi China
19 shared publications- Jiangping Zhao
School of Resources Engineering, Xi’an University of Architecture and Technology, Xi’an 710055, China
6 shared publications Fan Li
School of Resources Engineering, Xi’an University of Architecture & Technology, Xi’an 710055, China
5 shared publications- Weidong Dai
Institute for Hygiene of Ordnance Industry, Xi’an 710065, China
4 shared publications Jun Deng
School of Safety Science and Engineering Xi'an University of Science and Technology Xi'an China
3 shared publicationsKang Yu
School of Resources Engineering Xi'an University of Architecture and Technology Xi'an China
3 shared publications
Latest Publications
- Open Access
Fire Growth Behavior and Predictive Modeling of 3D-Printed Triply Periodic Minimal Surface (TPMS) Porous PLA Structures
Triply periodic minimal surfaces (TPMSs) are increasingly used in thermal management systems due to their high surface area and interconnected porous architecture. However, how TPMS geometry influences fire growth remains poorly understood. Herein, Gyroid, Diamond, and Schwarz-P PLA structures were fabricated through additive manufacturing, and their fire behavior was characterized via cone calorimetry. Univariate experiments demonstrate that flame propagation is primarily governed by cell structure, rather than porosity or specific surface area. The orthogonal array L9(33), covering three factors of wall thickness, cell size and cell type (Gyroid, Diamond, and Schwarz-P), indicates that their effects on the flame growth index (FGI) rank as: cell size > unit cell > thickness. Meanwhile, a multivariate regression model was developed to predict the FGI of TPMS porous PLA, exhibiting high prediction accuracy (R2 = 0.95) and low residual standard deviation. These results provide quantitative insights into the correlation between TPMS geometric features and fire growth, which facilitates the design of safer porous structures for thermal management applications.
Open AccessFire Growth Behavior and Predictive Modeling of 3D-Printed Triply Periodic Minimal Surface (TPMS) Porous PLA Structures
Triply periodic minimal surfaces (TPMSs) are increasingly used in thermal management systems due to their high surface area and interconnected porous architecture. However, how TPMS geometry influences fire growth remains poorly understood. Herein, Gyroid, Diamond, and Schwarz-P PLA structures were fabricated through additive manufacturing, and their fire behavior was characterized via cone calorimetry. Univariate experiments demonstrate that flame propagation is primarily governed by cell structure, rather than porosity or specific surface area. The orthogonal array L9(33), covering three factors of wall thickness, cell size and cell type (Gyroid, Diamond, and Schwarz-P), indicates that their effects on the flame growth index (FGI) rank as: cell size > unit cell > thickness. Meanwhile, a multivariate regression model was developed to predict the FGI of TPMS porous PLA, exhibiting high prediction accuracy (R2 = 0.95) and low residual standard deviation. These results provide quantitative insights into the correlation between TPMS geometric features and fire growth, which facilitates the design of safer porous structures for thermal management applications.
- Open Access
Chitosan Oligosaccharide@Melamine Polyphosphate Modified Polylactic Acid with Enhanced Flame Retardancy
A novel material, chitosan oligosaccharide@melamine polyphosphate (CMP), with enhanced flame-retardant and hydrophobic properties, was synthesized by cross-linking melamine polyphosphate (MPP) with chitosan oligosaccharide. Compared with MPP, the CMP overcomes its inherent drawbacks when used as a flame retardant in polylactic acid (PLA) composites, namely the high loading demand and unsatisfactory interfacial compatibility with the polymer matrix. The results demonstrated that the peak heat release rate (p-HRR) dropped significantly in comparison to pure PLA, from 304.69 kW·m−2 to 210.39 kW·m−2, while the fire performance index (FPI) increased from 0.1 to 0.48 s·m−2·kW−1. Furthermore, the fire growth index (FGI) decreased from 1.51 kW·m−2·s−1 to 1.03 kW·m−2·s−1. Additionally, the CMP demonstrated enhanced thermal stability, making the pyrolysis activation energy Eα increase from 135.04 to 191.97 kJ/mol during 308~416 °C by pyrolysis kinetics. Compared to composite PLA incorporating pristine MPP, the CMP-modified counterpart exhibits superior mechanical properties and significantly enhanced hydrophobicity, evidenced by a maximum water contact angle reaching 93.96°. It provides a strategy for adapting phosphorus-based flame retardants for PLA, thereby broadening their applicability across diverse scenarios.
Open AccessChitosan Oligosaccharide@Melamine Polyphosphate Modified Polylactic Acid with Enhanced Flame Retardancy
A novel material, chitosan oligosaccharide@melamine polyphosphate (CMP), with enhanced flame-retardant and hydrophobic properties, was synthesized by cross-linking melamine polyphosphate (MPP) with chitosan oligosaccharide. Compared with MPP, the CMP overcomes its inherent drawbacks when used as a flame retardant in polylactic acid (PLA) composites, namely the high loading demand and unsatisfactory interfacial compatibility with the polymer matrix. The results demonstrated that the peak heat release rate (p-HRR) dropped significantly in comparison to pure PLA, from 304.69 kW·m−2 to 210.39 kW·m−2, while the fire performance index (FPI) increased from 0.1 to 0.48 s·m−2·kW−1. Furthermore, the fire growth index (FGI) decreased from 1.51 kW·m−2·s−1 to 1.03 kW·m−2·s−1. Additionally, the CMP demonstrated enhanced thermal stability, making the pyrolysis activation energy Eα increase from 135.04 to 191.97 kJ/mol during 308~416 °C by pyrolysis kinetics. Compared to composite PLA incorporating pristine MPP, the CMP-modified counterpart exhibits superior mechanical properties and significantly enhanced hydrophobicity, evidenced by a maximum water contact angle reaching 93.96°. It provides a strategy for adapting phosphorus-based flame retardants for PLA, thereby broadening their applicability across diverse scenarios.
- 25 May 2026
- Published by Springer Nature in Fire Technology
- Vol. 62 (4) , 88
Semi-quantitative Fire Risk Assessment for High-Density Historic Districts Based on Improved Fire Risk Index
- 25 May 2026
- Published by Springer Nature in Fire Technology
- Vol. 62 (4) , 88
Semi-quantitative Fire Risk Assessment for High-Density Historic Districts Based on Improved Fire Risk Index
- Open Access
- 12 January 2026
- Published by Lukasiewicz Research Network - Poznan Technology Institute in Drewno. Prace Naukowe, Doniesienia, Komunikaty = Wood. Research Papers, Reports, Announcements
- Vol. 69 (217)
Microscopic damage mechanism of Chinese fir subjected to environmental aging consisting of ultraviolet irradiation, thermal-humidity cycling, and salt fog
As a cornerstone structural material in Chinese architectural heritage, understanding the long-term durability of Chinese fir (Cunninghamia lanceolata) is critical for its preservation. This study comparatively investigates the degradation of Chinese fir under three accelerated aging protocols simulating key environmental threats: ultraviolet (UV) weathering, thermal-humidity cycling, and salt fog. The results revealed distinct degradation mechanisms with significant implications for heritage diagnostics. Salt fog exposure induced the most severe degradation, causing a 63.9% loss in bending strength through comprehensive chemical attacks. UV weathering led to significant surface photodegradation and microcracking, while thermal-humidity cycling caused a 46.5% reduction in bending strength, primarily due to physical stresses. Crucially, a strong, universal correlation was established between cellulose crystallinity (CrI) and the mechanical properties (tensile, R = 0.874; compressive, R = 0.902; bending, R = 0.941) across all aging conditions. This identifies CrI as a robust and minimally invasive indicator for assessing the mechanical integrity of historic timbers. Furthermore, the degradation kinetics under each stressor followed highly predictable linear trends (R² > 0.89), providing a quantitative basis for developing targeted conservation strategies and more accurate service life prediction models for timber heritage structures.
- 12 January 2026
- Published by Lukasiewicz Research Network - Poznan Technology Institute in Drewno. Prace Naukowe, Doniesienia, Komunikaty = Wood. Research Papers, Reports, Announcements
- Vol. 69 (217)
Open AccessMicroscopic damage mechanism of Chinese fir subjected to environmental aging consisting of ultraviolet irradiation, thermal-humidity cycling, and salt fog
As a cornerstone structural material in Chinese architectural heritage, understanding the long-term durability of Chinese fir (Cunninghamia lanceolata) is critical for its preservation. This study comparatively investigates the degradation of Chinese fir under three accelerated aging protocols simulating key environmental threats: ultraviolet (UV) weathering, thermal-humidity cycling, and salt fog. The results revealed distinct degradation mechanisms with significant implications for heritage diagnostics. Salt fog exposure induced the most severe degradation, causing a 63.9% loss in bending strength through comprehensive chemical attacks. UV weathering led to significant surface photodegradation and microcracking, while thermal-humidity cycling caused a 46.5% reduction in bending strength, primarily due to physical stresses. Crucially, a strong, universal correlation was established between cellulose crystallinity (CrI) and the mechanical properties (tensile, R = 0.874; compressive, R = 0.902; bending, R = 0.941) across all aging conditions. This identifies CrI as a robust and minimally invasive indicator for assessing the mechanical integrity of historic timbers. Furthermore, the degradation kinetics under each stressor followed highly predictable linear trends (R² > 0.89), providing a quantitative basis for developing targeted conservation strategies and more accurate service life prediction models for timber heritage structures.
- 9 January 2026
- Published by Elsevier in Materialia
- Vol. 45
Mechanisms of fire resistance deterioration in chinese fir induced by environmental aging
- 9 January 2026
- Published by Elsevier in Materialia
- Vol. 45
Mechanisms of fire resistance deterioration in chinese fir induced by environmental aging
- 5 September 2025
- Published by American Chemical Society (ACS) in Langmuir
- Vol. 41 (36) , 24995-25014
Mesoporous Heat-Trapping and Smoke-Adsorbing Fe-MOFs Improve Fire Safety and Compression Resistance of Rigid Polyurethane Foam
The use of highly flammable materials such as foams, resins, and plastics has led to an increase in the frequency and severity of urban fires worldwide. To address this issue, this study developed a high-specific-surface-area mesoporous metal-organic framework (Fe-MOFs) with heat trapping and smoke adsorption. The Fe-MOFs, zinc tailings (ZTs), piperazine pyrophosphate (PAPP), and sodium lignosulfonate (LS) were used to modify rigid polyurethane foam (RPUF). Cone calorimeter combustion experiments showed that Fe-MOFs significantly reduced the heat release and smoke emission of RPUF through heat trapping and smoke adsorption. Compared to pure RPUF, the peak heat release rate (p-HRR) and total heat release rate (THR) of Fe-2 decreased by 64.5% and 68.6%, respectively, and the total smoke production (TSP) of Fe-5 decreased by 55.6%. Vertical combustion experiments showed that all RPUF achieved UL-94 V-0 rating. Thermogravimetric analysis, pyrolysis kinetics, and thermogravimetry-infrared indicated that Fe-MOFs protected RPUF during the main decomposition stage (301-446 °C) and enhanced its thermal stability by accelerating the decomposition of PAPP and LS. Residual carbon analysis revealed that the appropriate amount of Fe-MOFs helped form the solid, dense, continuous, and stable carbon layer. This carbon layer hindered flame and heat transfer and limited heat and smoke release. Physical property tests showed that Fe-MOFs affected the foaming process of RPUF. This led to increased density and compressive strength of RPUF. Compared to pure RPUF, the compressive strength of Fe-2 increased from 0.147 to 0.281 MPa. These results indicated that Fe-MOFs help to enhance the performance of RPUF. This study provides an efficient solution for the recovery of solid waste and the development of fire-resistant polymer composites.
- 5 September 2025
- Published by American Chemical Society (ACS) in Langmuir
- Vol. 41 (36) , 24995-25014
Mesoporous Heat-Trapping and Smoke-Adsorbing Fe-MOFs Improve Fire Safety and Compression Resistance of Rigid Polyurethane Foam
The use of highly flammable materials such as foams, resins, and plastics has led to an increase in the frequency and severity of urban fires worldwide. To address this issue, this study developed a high-specific-surface-area mesoporous metal-organic framework (Fe-MOFs) with heat trapping and smoke adsorption. The Fe-MOFs, zinc tailings (ZTs), piperazine pyrophosphate (PAPP), and sodium lignosulfonate (LS) were used to modify rigid polyurethane foam (RPUF). Cone calorimeter combustion experiments showed that Fe-MOFs significantly reduced the heat release and smoke emission of RPUF through heat trapping and smoke adsorption. Compared to pure RPUF, the peak heat release rate (p-HRR) and total heat release rate (THR) of Fe-2 decreased by 64.5% and 68.6%, respectively, and the total smoke production (TSP) of Fe-5 decreased by 55.6%. Vertical combustion experiments showed that all RPUF achieved UL-94 V-0 rating. Thermogravimetric analysis, pyrolysis kinetics, and thermogravimetry-infrared indicated that Fe-MOFs protected RPUF during the main decomposition stage (301-446 °C) and enhanced its thermal stability by accelerating the decomposition of PAPP and LS. Residual carbon analysis revealed that the appropriate amount of Fe-MOFs helped form the solid, dense, continuous, and stable carbon layer. This carbon layer hindered flame and heat transfer and limited heat and smoke release. Physical property tests showed that Fe-MOFs affected the foaming process of RPUF. This led to increased density and compressive strength of RPUF. Compared to pure RPUF, the compressive strength of Fe-2 increased from 0.147 to 0.281 MPa. These results indicated that Fe-MOFs help to enhance the performance of RPUF. This study provides an efficient solution for the recovery of solid waste and the development of fire-resistant polymer composites.
- 18 August 2025
- Published by Elsevier in International Journal of Biological Macromolecules
- Vol. 322 (Pt 3) , 146922
Synthesis of metal coordination polymers based amino trimethylene phosphonic acid and zinc phytate to improve the flame retardancy of polylactic acid
- 18 August 2025
- Published by Elsevier in International Journal of Biological Macromolecules
- Vol. 322 (Pt 3) , 146922
Synthesis of metal coordination polymers based amino trimethylene phosphonic acid and zinc phytate to improve the flame retardancy of polylactic acid
- Open Access
Enhanced Flame Retardancy of Silica Fume-Based Geopolymer Composite Coatings Through In Situ-Formed Boron Phosphate from Doped Zinc Phytate and Boric Acid
Silica fume-based geopolymer composite coatings, an approach to using metallurgical solid waste, exert flame retardancy with ecological, halogen-free, and environmentally friendly advantages, but their fire resistance needs to be improved further. Herein, a silica fume-based geopolymer composite flame-retardant coating was designed by doping boric acid (BA), zinc phytate (ZnPA), and melamine (MEL). The results of a cone calorimeter demonstrated that appropriate ZnPA and BA significantly enhanced its flame retardancy, evidenced by the peak heat release rate (p-HRR) decreasing from 268.78 to 118.72 kW·m−2, the fire performance index (FPI) increasing from 0.59 to 2.83 s·m2·kW−1, and the flame retardancy index increasing from 1.00 to 8.48, respectively. Meanwhile, the in situ-formed boron phosphate (BPO4) facilitated the residual resilience of the fire-barrier layer. Furthermore, the pyrolysis kinetics indicated that the three-level chemical reactions governed the pyrolysis of the coatings. BPO4 made the pyrolysis Eα climb from 94.28 (P5) to 127.08 (B3) kJ·mol−1 with temperatures of 731–940 °C, corresponding to improved thermal stability. Consequently, this study explored the synergistic flame-retardant mechanism of silica fume-based geopolymer coatings doped with ZnPA, BA, and MEL, providing an efficient strategy for the high-value-added recycling utilization of silica fume.
Open AccessEnhanced Flame Retardancy of Silica Fume-Based Geopolymer Composite Coatings Through In Situ-Formed Boron Phosphate from Doped Zinc Phytate and Boric Acid
Silica fume-based geopolymer composite coatings, an approach to using metallurgical solid waste, exert flame retardancy with ecological, halogen-free, and environmentally friendly advantages, but their fire resistance needs to be improved further. Herein, a silica fume-based geopolymer composite flame-retardant coating was designed by doping boric acid (BA), zinc phytate (ZnPA), and melamine (MEL). The results of a cone calorimeter demonstrated that appropriate ZnPA and BA significantly enhanced its flame retardancy, evidenced by the peak heat release rate (p-HRR) decreasing from 268.78 to 118.72 kW·m−2, the fire performance index (FPI) increasing from 0.59 to 2.83 s·m2·kW−1, and the flame retardancy index increasing from 1.00 to 8.48, respectively. Meanwhile, the in situ-formed boron phosphate (BPO4) facilitated the residual resilience of the fire-barrier layer. Furthermore, the pyrolysis kinetics indicated that the three-level chemical reactions governed the pyrolysis of the coatings. BPO4 made the pyrolysis Eα climb from 94.28 (P5) to 127.08 (B3) kJ·mol−1 with temperatures of 731–940 °C, corresponding to improved thermal stability. Consequently, this study explored the synergistic flame-retardant mechanism of silica fume-based geopolymer coatings doped with ZnPA, BA, and MEL, providing an efficient strategy for the high-value-added recycling utilization of silica fume.
- Open Access
- 17 June 2025
- Published by MDPI AG in Preprints.org
Enhanced Flame Retardancy of Silica Fume-Based Geopolymer Composite Coatings Through In-Situ Formed Boron Phosphate from Doped Zinc Phytate and Boric Acid
Silica fume-based geopolymer composite coating, an approach for utilization of metallurgical solid waste, exerts flame retardancy with ecology, halogen-free and environmentally friendly advantage, but its fire resistance needs to be improved further. Herein, the silica fume-based geopolymer composite flame-retardant coating is benignly designed by doping boric acid (BA), zinc phytate (ZnPA), and melamine (MEL). The results of cone calorimeter demonstrate that appropriate ZnPA and BA significantly enhance its flame retardancy, evidenced by that the peak heat release rate (p-HRR) decreases from 268.78 to 118.72 kW·m-2, the flame performance index (FPI) increases from 0.59 to 2.83 s·m2·kW-1, and the fire resistance index increases from 1.00 to 8.48, respectively. Meanwhile, the in-situ formed boron phosphate (BPO4) facilitates the residual resilience of the fire-barrier layer. Furthermore, the pyrolysis kinetics indicate that the three-level chemical reaction model governs the pyrolysis of coatings. BPO4 makes the pyrolysis Eα climb from 94.28 (P5) to 127.08 (B3) kJ·mol-1 during 731-940°C, corresponding to the improved thermal stability. Consequently, it explores the synergistic flame-retardant mechanism of silica fume-based geopolymer coatings doped with ZnPA, BA, and MEL, providing an efficient strategy for high value-added recycling utilization of silica fume.
- 17 June 2025
- Published by MDPI AG in Preprints.org
Open AccessEnhanced Flame Retardancy of Silica Fume-Based Geopolymer Composite Coatings Through In-Situ Formed Boron Phosphate from Doped Zinc Phytate and Boric Acid
Silica fume-based geopolymer composite coating, an approach for utilization of metallurgical solid waste, exerts flame retardancy with ecology, halogen-free and environmentally friendly advantage, but its fire resistance needs to be improved further. Herein, the silica fume-based geopolymer composite flame-retardant coating is benignly designed by doping boric acid (BA), zinc phytate (ZnPA), and melamine (MEL). The results of cone calorimeter demonstrate that appropriate ZnPA and BA significantly enhance its flame retardancy, evidenced by that the peak heat release rate (p-HRR) decreases from 268.78 to 118.72 kW·m-2, the flame performance index (FPI) increases from 0.59 to 2.83 s·m2·kW-1, and the fire resistance index increases from 1.00 to 8.48, respectively. Meanwhile, the in-situ formed boron phosphate (BPO4) facilitates the residual resilience of the fire-barrier layer. Furthermore, the pyrolysis kinetics indicate that the three-level chemical reaction model governs the pyrolysis of coatings. BPO4 makes the pyrolysis Eα climb from 94.28 (P5) to 127.08 (B3) kJ·mol-1 during 731-940°C, corresponding to the improved thermal stability. Consequently, it explores the synergistic flame-retardant mechanism of silica fume-based geopolymer coatings doped with ZnPA, BA, and MEL, providing an efficient strategy for high value-added recycling utilization of silica fume.