Ángeles Colaccio
Research Subjects
Research Interests
Ángeles Colaccio has a total of 5 co-authors. Here are the top co-authors by number of shared publications:
- Alicia Esther Ares
Programa de Materiales y Fisicoquímica (ProMyF), Instituto de Materiales de Misiones (IMAM), Facultad de Ciencias Exactas, Químicas y Naturales (FCEQyN), Universidad Nacional de Misiones (UNaM), 1552 Félix de Azara Street, Posadas 3300, Misiones, Argentina
2 shared publications - Carlos Enrique Schvezov
Instituto de Materiales de Misiones (IMAM), CONICET-UNaM, Posadas 3300, Misiones, Argentina
2 shared publications - María Laura Vera
Instituto de Materiales de Misiones (IMAM), CONICET-UNaM, Posadas 3300, Misiones, Argentina
2 shared publications - Mario Roberto Rosenberger
Materials, Modeling and Metrology Program, Faculty of Sciences, University of Misiones, 1552 Azara Street, 3300 Posadas, Argentina
1 shared publication - Mario Roberto Rosenberger
Instituto de Materiales de Misiones (IMAM), CONICET-UNaM, Posadas 3300, Misiones, Argentina
1 shared publication
Latest Publications
- Open Access
Influence of the Electrolyte Concentration on the Smooth TiO2 Anodic Coatings on Ti-6Al-4V
To obtain smooth TiO2 coatings for building a new design of Ti-6Al-4V heart valve, the anodic oxidation technique in pre-spark conditions was evaluated. TiO2 coating is necessary for its recognized biocompatibility and corrosion resistance. A required feature on surfaces in contact with blood is a low level of roughness (Ra ≤ 50 nm) that does not favor the formation of blood clots. The present paper compares the coatings obtained by anodic oxidation of the Ti-6Al-4V alloy using H2SO4 at different concentrations (0.1–4 M) as electrolyte and applying different voltages (from 20 to 70 V). Color and morphological analysis of coatings are performed using optical and scanning microscopy. The crystalline phases were analyzed by glancing X-ray diffraction. By varying the applied voltage, different interference colors coatings were obtained. The differences in morphologies of the coatings caused by changes in acid concentration are more evident at high voltages, limiting the oxidation conditions for the desired application. Anatase phase was detected from 70 V for 1 M H2SO4. An increase in the concentration of H2SO4 decreases the voltage at which the transformation of amorphous to crystalline coatings occurs; i.e., with 4 M H2SO4, the anatase phase appears at 60 V.
Open AccessInfluence of the Electrolyte Concentration on the Smooth TiO2 Anodic Coatings on Ti-6Al-4V
To obtain smooth TiO2 coatings for building a new design of Ti-6Al-4V heart valve, the anodic oxidation technique in pre-spark conditions was evaluated. TiO2 coating is necessary for its recognized biocompatibility and corrosion resistance. A required feature on surfaces in contact with blood is a low level of roughness (Ra ≤ 50 nm) that does not favor the formation of blood clots. The present paper compares the coatings obtained by anodic oxidation of the Ti-6Al-4V alloy using H2SO4 at different concentrations (0.1–4 M) as electrolyte and applying different voltages (from 20 to 70 V). Color and morphological analysis of coatings are performed using optical and scanning microscopy. The crystalline phases were analyzed by glancing X-ray diffraction. By varying the applied voltage, different interference colors coatings were obtained. The differences in morphologies of the coatings caused by changes in acid concentration are more evident at high voltages, limiting the oxidation conditions for the desired application. Anatase phase was detected from 70 V for 1 M H2SO4. An increase in the concentration of H2SO4 decreases the voltage at which the transformation of amorphous to crystalline coatings occurs; i.e., with 4 M H2SO4, the anatase phase appears at 60 V.
- Open Access
- 2 March 2017
- Published by MDPI AG in Preprints.org
Influence of the Electrolyte Concentration on the Smooth TiO2 Anodic Coatings on Ti-6Al-4V
To obtain smooth coatings of TiO2 for building a new design of Ti-6Al-4V heart valve, the anodic oxidation technique in pre-spark conditions was evaluated. TiO2 coating is necessary for its recognize biocompatibility and corrosion resistance. A required feature on surfaces in contact with blood is a low level of roughness (Ra ≤ 50 nm) that not favor the formation of blood clots. The present paper compares the coatings obtained by anodic oxidation of the Ti-6Al-4V alloy using H2SO4 at different concentrations (0.1 M to 4 M) as electrolyte and applying different voltages (from 20 V to 70 V). Color and morphological analysis of coatings are performed using optical and scanning microscopy. The crystalline phases were analyzed by glancing X-ray diffraction. By varying the applied voltage different interference colors coatings were obtained. The differences in morphologies of the coatings, due to the change in concentration, are more evident at high voltages limiting the oxidation conditions for the desired application. Anatase phase was detected from 70 V for 1 M H2SO4. An increase in the concentration of H2SO4 decreases the voltage at which the transformation of amorphous to crystalline coatings occurs, i.e. with 4 M H2SO4 the anatase phase appears at 60 V.
- 2 March 2017
- Published by MDPI AG in Preprints.org
Open AccessInfluence of the Electrolyte Concentration on the Smooth TiO2 Anodic Coatings on Ti-6Al-4V
To obtain smooth coatings of TiO2 for building a new design of Ti-6Al-4V heart valve, the anodic oxidation technique in pre-spark conditions was evaluated. TiO2 coating is necessary for its recognize biocompatibility and corrosion resistance. A required feature on surfaces in contact with blood is a low level of roughness (Ra ≤ 50 nm) that not favor the formation of blood clots. The present paper compares the coatings obtained by anodic oxidation of the Ti-6Al-4V alloy using H2SO4 at different concentrations (0.1 M to 4 M) as electrolyte and applying different voltages (from 20 V to 70 V). Color and morphological analysis of coatings are performed using optical and scanning microscopy. The crystalline phases were analyzed by glancing X-ray diffraction. By varying the applied voltage different interference colors coatings were obtained. The differences in morphologies of the coatings, due to the change in concentration, are more evident at high voltages limiting the oxidation conditions for the desired application. Anatase phase was detected from 70 V for 1 M H2SO4. An increase in the concentration of H2SO4 decreases the voltage at which the transformation of amorphous to crystalline coatings occurs, i.e. with 4 M H2SO4 the anatase phase appears at 60 V.