Nailu Chen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Nailu Chen has a total of 35 co-authors. Here are the top co-authors by number of shared publications:
Yonghua Rong
15 shared publicationsXunwei Zuo
12 shared publicationsYu Liu
School of Materials Science and Engineering, Shanghai University of Engineering Science, Shanghai, People’s Republic of China
8 shared publicationsJianfeng Wan
5 shared publicationsShengwei Qin
School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai, People’s Republic of China
5 shared publicationsHongqing Zheng
4 shared publications
Latest Publications
- 20 September 2026
- Published by Elsevier in International Journal of Mechanical Sciences
- Vol. 328
Mechanistic role of carbides in quenching-partitioning-tempering steel fracture
- 20 September 2026
- Published by Elsevier in International Journal of Mechanical Sciences
- Vol. 328
Mechanistic role of carbides in quenching-partitioning-tempering steel fracture
- Open Access
- 2 August 2026
- Published by Elsevier in Materials & Design
- Vol. 269
Quenching-partitioning-tempering (Q-P-T) steels: Microstructural design, interface-mediated deformation, and mechanical-property synergy
- 2 August 2026
- Published by Elsevier in Materials & Design
- Vol. 269
Open AccessQuenching-partitioning-tempering (Q-P-T) steels: Microstructural design, interface-mediated deformation, and mechanical-property synergy
- Open Access
- 11 September 2025
- Published by National Academy of Sciences in Proceedings of the National Academy of Sciences of the United States of America
- Vol. 122 (37)
Toughness enhancement by massive dislocation absorption at the crack front
Low-cost yet high-performance structural materials have been invariantly sought for modern engineering applications. However, due to the localized stress concentration induced by a high Peierls-Nabarro stress and limited dislocation mobility, increasing material strength usually comes at the expense of ductility and toughness, resulting in a trade-off between strength–ductility/strength–toughness. Here, we report an anomalous phenomenon of dislocation absorption at the crack front, which is unlike typically observed dislocation emission at the crack tip, in a heterogeneous “plain” steel consisting of tempered lath martensite embedded with stable carbon-enriched retained austenite. The continuous absorption of dislocations emitted from the tempered martensite into the tough austenite significantly alleviates the localized stress concentration, and as such retards crack propagation in the tempered martensite matrix. This allows the plain high-carbon low-alloyed steel subjected to simple quenching–partitioning–tempering processes to achieve remarkable properties comprising a multiplication of strength and elongation over 50 GPa·% with an exceptionally high fracture toughness over 130 MPa·m 1/2 . The toughening strategy based on this mechanism provides a promising route for developing cost-effective plain steels with ultrahigh strength, ductility, and toughness that is a persistent pursuit in the steel industry.
- 11 September 2025
- Published by National Academy of Sciences in Proceedings of the National Academy of Sciences of the United States of America
- Vol. 122 (37)
Open AccessToughness enhancement by massive dislocation absorption at the crack front
Low-cost yet high-performance structural materials have been invariantly sought for modern engineering applications. However, due to the localized stress concentration induced by a high Peierls-Nabarro stress and limited dislocation mobility, increasing material strength usually comes at the expense of ductility and toughness, resulting in a trade-off between strength–ductility/strength–toughness. Here, we report an anomalous phenomenon of dislocation absorption at the crack front, which is unlike typically observed dislocation emission at the crack tip, in a heterogeneous “plain” steel consisting of tempered lath martensite embedded with stable carbon-enriched retained austenite. The continuous absorption of dislocations emitted from the tempered martensite into the tough austenite significantly alleviates the localized stress concentration, and as such retards crack propagation in the tempered martensite matrix. This allows the plain high-carbon low-alloyed steel subjected to simple quenching–partitioning–tempering processes to achieve remarkable properties comprising a multiplication of strength and elongation over 50 GPa·% with an exceptionally high fracture toughness over 130 MPa·m 1/2 . The toughening strategy based on this mechanism provides a promising route for developing cost-effective plain steels with ultrahigh strength, ductility, and toughness that is a persistent pursuit in the steel industry.
- 23 March 2022
- Published by Elsevier in Journal of Materials Science & Technology
- Vol. 124, 116-120
Universality of quenching-partitioning-tempering local equilibrium model
- 23 March 2022
- Published by Elsevier in Journal of Materials Science & Technology
- Vol. 124, 116-120
Universality of quenching-partitioning-tempering local equilibrium model
- 1 June 2021
- Published by Elsevier in Science Bulletin
- Vol. 66 (11) , 1058-1062
Dislocations across interphase enable plain steel with high strength-ductility
- 1 June 2021
- Published by Elsevier in Science Bulletin
- Vol. 66 (11) , 1058-1062
Dislocations across interphase enable plain steel with high strength-ductility
- Open Access
- 2 January 2020
- Published by Taylor & Francis in Heat Treatment and Surface Engineering
- Vol. 2 (1) , 9-15
The process design of water quenching based on finite element simulation and its applications
Quenching is a widely used process in heat treatment enterprises. Clean and cheap water quenching instead of high pollution and high cost of oil quenching or polymer aqueous solution quenching will become a trend in these enterprises. However, since the cracking problem of alloy steel parts induced by water quenching with high cooling rate has not been solved, the oil and polymer aqueous solution with low cooling rate are still widely used in various countries in the world. Water–air alternative timed quenching’ process and differential time grading quenching process proposed by us have been successfully applied to treat various large-size alloy steel parts in China. In this review paper, we will introduce the face issues in the design of these two kinds of processes based on finite element simulation (FES): (1) Main factor affecting accurate prediction of quenching stress; (2) The method to determine the optimizing process. Two engineering examples are selected to clarify how to solve the cracking issues of alloy steel part by FES.
- 2 January 2020
- Published by Taylor & Francis in Heat Treatment and Surface Engineering
- Vol. 2 (1) , 9-15
Open AccessThe process design of water quenching based on finite element simulation and its applications
Quenching is a widely used process in heat treatment enterprises. Clean and cheap water quenching instead of high pollution and high cost of oil quenching or polymer aqueous solution quenching will become a trend in these enterprises. However, since the cracking problem of alloy steel parts induced by water quenching with high cooling rate has not been solved, the oil and polymer aqueous solution with low cooling rate are still widely used in various countries in the world. Water–air alternative timed quenching’ process and differential time grading quenching process proposed by us have been successfully applied to treat various large-size alloy steel parts in China. In this review paper, we will introduce the face issues in the design of these two kinds of processes based on finite element simulation (FES): (1) Main factor affecting accurate prediction of quenching stress; (2) The method to determine the optimizing process. Two engineering examples are selected to clarify how to solve the cracking issues of alloy steel part by FES.
- Open Access
- 5 March 2019
- Published by Taylor & Francis in Heat Treatment and Surface Engineering
- Vol. 1 (1-2) , 57-62
High hardness-toughness and wear resistance of white cast iron treated by a multicycle quenching-partitioning-tempering process
Based on a multicycle quenching-partitioning-tempering process, a novel process is proposed to treat Fe–2.4C–12.0Cr (mass %) white cast iron balls. It is a destabilizing heat treatment following multicycle quenching and sub-critical treatment (De-MQ-Sct) process. Such a complex process may be simply performed by alternate water quenching and air cooling. For comparison, the white cast iron balls also were treated by conventional normalization (NOR) process and oil-quenching process. The partitioning of carbon from martensite to retained austenite during the De-MQ-Sct process promotes the interaction between carbide precipitation and martensitic transformation. While this interaction is a unique effect only produced by multicycle quenching linking destabilizing and sub-critical treatments, which leads to more, and finer, secondary carbides and more carbon-enriched austenite in De-MQ-Sct sample than those in a NOR or oil-quenching sample. The average hardness of 60 HRC and impact toughness of 12.6 J/cm2 are obtained in De-MQ-Sct white cast iron balls, which are much higher than those in a NOR and oil-quenching ones. The wear behavior measured by pin-on-disk wear tests indicate that the weight loss of De-MQ-Sct sample is only about one-third of the NOR sample and one half of the oil-quenching sample. Microstructural characterization reveals that high hardness-toughness and wear resistance of the De-MQ-Sct balls are mainly attributed to the large quantities of fine secondary carbides and stable carbon-enriched retained austenite.
- 5 March 2019
- Published by Taylor & Francis in Heat Treatment and Surface Engineering
- Vol. 1 (1-2) , 57-62
Open AccessHigh hardness-toughness and wear resistance of white cast iron treated by a multicycle quenching-partitioning-tempering process
Based on a multicycle quenching-partitioning-tempering process, a novel process is proposed to treat Fe–2.4C–12.0Cr (mass %) white cast iron balls. It is a destabilizing heat treatment following multicycle quenching and sub-critical treatment (De-MQ-Sct) process. Such a complex process may be simply performed by alternate water quenching and air cooling. For comparison, the white cast iron balls also were treated by conventional normalization (NOR) process and oil-quenching process. The partitioning of carbon from martensite to retained austenite during the De-MQ-Sct process promotes the interaction between carbide precipitation and martensitic transformation. While this interaction is a unique effect only produced by multicycle quenching linking destabilizing and sub-critical treatments, which leads to more, and finer, secondary carbides and more carbon-enriched austenite in De-MQ-Sct sample than those in a NOR or oil-quenching sample. The average hardness of 60 HRC and impact toughness of 12.6 J/cm2 are obtained in De-MQ-Sct white cast iron balls, which are much higher than those in a NOR and oil-quenching ones. The wear behavior measured by pin-on-disk wear tests indicate that the weight loss of De-MQ-Sct sample is only about one-third of the NOR sample and one half of the oil-quenching sample. Microstructural characterization reveals that high hardness-toughness and wear resistance of the De-MQ-Sct balls are mainly attributed to the large quantities of fine secondary carbides and stable carbon-enriched retained austenite.
- Open Access
- 5 March 2019
- Published by Taylor & Francis in Heat Treatment and Surface Engineering
- Vol. 1 (1-2) , 2-10
The twice softening of martensitic matrix in Q–P–T steels and its effect on ductility
When a Si-containing steel is subjected to quenching-partitioning-tempering (Q–P–T) process, it will become a martensitic steel with considerable volume of retained austenite, which is attributed to the partitioning of carbon from martensite to retained austenite leading to carbon-depletion in martensitic matrix and carbon-enrichment in the retained austenite. The softening of the martensitic matrix caused by carbon-depletion markedly enhances its deformation ability and raises the ductility of Q–P–T steels. During deformation dislocation absorption by retained austenite (DARA) effect will occur, that is, the dislocations in martensitic matrix will move into nearby retained austenite through the martensite-austenite interface and be absorbed by the retained austenite. This second softening of the martensitic matrix also enhances its deformation ability and effectively raises the ductility. The effect of DARA on ductility during deformation is more effective than the transformation-induced plasticity (TRIP) effect caused by martensitic transformation of retained austenite, because during the TRIP effect the twin-type martensite produced by strain-induced martensitic transformation of retained austenite is very detrimental to ductility.
- 5 March 2019
- Published by Taylor & Francis in Heat Treatment and Surface Engineering
- Vol. 1 (1-2) , 2-10
Open AccessThe twice softening of martensitic matrix in Q–P–T steels and its effect on ductility
When a Si-containing steel is subjected to quenching-partitioning-tempering (Q–P–T) process, it will become a martensitic steel with considerable volume of retained austenite, which is attributed to the partitioning of carbon from martensite to retained austenite leading to carbon-depletion in martensitic matrix and carbon-enrichment in the retained austenite. The softening of the martensitic matrix caused by carbon-depletion markedly enhances its deformation ability and raises the ductility of Q–P–T steels. During deformation dislocation absorption by retained austenite (DARA) effect will occur, that is, the dislocations in martensitic matrix will move into nearby retained austenite through the martensite-austenite interface and be absorbed by the retained austenite. This second softening of the martensitic matrix also enhances its deformation ability and effectively raises the ductility. The effect of DARA on ductility during deformation is more effective than the transformation-induced plasticity (TRIP) effect caused by martensitic transformation of retained austenite, because during the TRIP effect the twin-type martensite produced by strain-induced martensitic transformation of retained austenite is very detrimental to ductility.