MSMaximilian Sieber

Maximilian Sieber

*This is an algorithmically generated author record based on publicly available information.

Maximilian Sieber has a total of 9 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Characterisation Method of the Passivation Mechanisms during the pre-discharge Stage of Plasma Electrolytic Oxidation Indicating the Mode of Action of Fluorides in PEO of Magnesium

    by Frank Simchen, Maximilian Sieber, Thomas Mehner, Thomas Lampke

    Plasma electrolytic oxidation (PEO) is a method to obtain protective coatings on metallic light-weight construction materials. Here, the workpiece receives a strong anodic polarisation in a suitable aqueous electrolyte, which leads to the formation of a passive layer and a gaseous shell. Afterwards, plasma electrolytic discharges appear on the substrate surface and convert it into a ceramic layer. The properties of the passive layer are influenced by the selected substrate/electrolyte combination and are essential for the PEO process-initiation and characteristics. In this work, a new method for the systematic investigation of the substrate/electrolyte interactions during the pre-discharge stage is presented. The procedure is carried out by a polarisation experiment and allows for a quantitative characterisation of the passivation behavior, based on a small electrolyte volume. The method is used to investigate a literature-known electrical conduction mechanism on passive films formed on magnesium, by cross-comparison between different Mg and Al materials. In addition, the influence of phosphate, glycerol, and fluoride on the passivation behaviour of the Mg alloy AZ31 in an alkaline environment is considered and quantified. The results provide an explanatory approach for the positive influence of toxic fluorides within the electrolyte on the morphology of PEO layers on magnesium.


  • Top Cited Papers
    Open Access

    Introduction to Plasma Electrolytic Oxidation—An Overview of the Process and Applications

    by Frank Simchen, Maximilian Sieber, Alexander Kopp, Thomas Lampke

    Plasma electrolytic oxidation (PEO), also called micro-arc oxidation (MAO), is an innovative method in producing oxide-ceramic coatings on metals, such as aluminum, titanium, magnesium, zirconium, etc. The process is characterized by discharges, which develop in a strong electric field, in a system consisting of the substrate, the oxide layer, a gas envelope, and the electrolyte. The electric breakdown in this system establishes a plasma state, in which, under anodic polarization, the substrate material is locally converted to a compound consisting of the substrate material itself (including alloying elements) and oxygen in addition to the electrolyte components. The review presents the process kinetics according to the existing models of the discharge phenomena, as well as the influence of the process parameters on the process, and thus, on the resulting coating properties, e.g., morphology and composition.


  • Open Access

    Evaluation of volatile corrosion inhibitors in the presence of condensation water by electrochemical methods

    by M Sieber, S Lautner, F Faßbender

    Volatile corrosion inhibitors (VCI) are a means of temporary corrosion protection based on the release of inhibitors from films, papers, diffusers or oil to the gaseous phase. By adsorption on a metal surface, the inhibitors prevent degradation of the primary oxide layer and impede corrosion. Thus, VCI provide corrosion protection for high-quality goods and semi-finished parts made from metals during transportation and storage. The application of oil on the metal surface for corrosion protection and its removal can be avoided. Due to rapid volatilization of the VCI after unpacking, no costly cleaning of parts prior to further use is required. In a new approach for evaluation of the protective effect of VCI, a metallic sample is exposed in a small chamber filled with air alongside a VCI-containing product. The air is humidified and the sample is cooled down under dewpoint, which leads to condensation of humidity and represents corrosive stress. The state of the metallic surface under the condensed water film is characterized by electrochemical methods. The present work demonstrates the evaluation of the anticorrosive effect of various VCI-films on mild steel. In summary, the application-oriented test allows for quick and quantified evaluation of VCI-containing products with a tabletop device.

  • Open Access

    Plasma Electrolytic Oxidation of High-Strength Aluminium Alloys—Substrate Effect on Wear and Corrosion Performance

    by Maximilian Sieber, Frank Simchen, Roy Morgenstern, Ingolf Scharf, Thomas Lampke

    With the progress in materials science and production technology and the establishment of light-weight design in many fields of the industry, the application of light metals no longer requires only mechanical strength, but also a significant protection of the material against wear and corrosion. Hard and wear-resistant oxide coatings on aluminium are produced by plasma electrolytic oxidation (PEO). During PEO, a conversion of the aluminium substrate to a ceramic oxide takes place. While the role of strength-giving alloying elements like Cu, Mg/Si, Zn, and Zn/Cu on the PEO process has selectively been subject of investigation in the past, the significance of the alloy composition for the service properties of the coatings is still unknown. Therefore, the performance of PEO coatings produced on the widely used commercial high-strength alloys AlCu4Mg1 (EN AW-2024), AlMgSi1 (EN AW-6082), and AlZn5.5MgCu (EN AW-7075) is examined with regard to their behaviour in the rubber-wheel test according to ASTM G65 and the current density-potential behaviour of the substrates with undamaged and worn coatings in dilute NaCl solution. To give a reference to the unalloyed material the testings were carried out also on Al 99.5 (EN AW-1050) which was treated in an adjusted PEO process. Although differences in the conversion of intermetallic phases during PEO and the phase composition of the coatings on the various substrates are determined, the service properties are hardly depending on the alloying elements of the investigated aluminium materials. The wear rates in the rubber-wheel test are low for all the alloyed samples. The current density-potential curves show a decrease of the corrosion current density by approximately one order of magnitude compared to the bare substrate. Eventually, previous wear of the coatings does not deteriorate the corrosion behaviour. PEO layers on technically pure aluminum can resist the testing regimes if they are prepared in an electrolyte with an elevated silicate content and without additional hydroxide ions, during a longer process time.