Liuyang Han
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Liuyang Han has a total of 73 co-authors. Here are the top co-authors by number of shared publications:
- Haibin Zhou
Research Institute of Wood Industry, Chinese Academy of Forestry, Beijing 100091, China
6 shared publications - Guanglan Xi
National Center for Archaeology, Beijing 100013, China
5 shared publications - Xiangna Han
Key Laboratory of Archaeomaterials and Conservation, Ministry of Education, Institute of Cultural Heritage and History of Science and Technology, University of Science and Technology Beijing, Beijing 100083, China
4 shared publications - Yafang Yin
Research Institute of Wood Industry , Chinese Academy of Forestry , Beijing 100091 , China
4 shared publications Hong Guo
3 shared publications- Hong Guo
Key Laboratory of Archaeomaterials and Conservation, Ministry of Education, Institute of Cultural Heritage and History of Science & Technology, University of Science and Technology Beijing, Beijing 100083, China
3 shared publications
Latest Publications
- 22 October 2026
- Published by Elsevier in Journal of Cultural Heritage
- Vol. 82, 317-323
Non-destructive terahertz assessment of mechanical fragility in palm-leaf manuscripts using interpretable machine learning
- 22 October 2026
- Published by Elsevier in Journal of Cultural Heritage
- Vol. 82, 317-323
Non-destructive terahertz assessment of mechanical fragility in palm-leaf manuscripts using interpretable machine learning
- Open Access
- 14 July 2026
- Published by Elsevier in SSRN Electronic Journal
Non-Destructive Terahertz Assessment of Mechanical Fragility in Palm Leaf Manuscripts Using Interpretable Machine Learning
Conservation of palm leaf manuscripts (PLMs) requires tools that can estimate mechanical fragility without additional sampling once calibrated against reference mechanical data. This study develops a conservation-oriented workflow that integrates terahertz time-domain spectroscopy (THz-TDS), supervised regression, cross-validated model evaluation, and SHAP-based interpretability for quantitative prediction of tensile strength. A total of 223 independent palm-leaf specimens representing different deterioration states were measured by THz-TDS, and reference tensile-strength labels were obtained along the longitudinal fiber direction for model calibration. Absorption-coefficient spectra were modeled using partial least squares regression (PLSR), random forest (RF), and extreme gradient boosting (XGBoost), with predictive robustness evaluated through cross-validation and an independent test set. The optimized RF model achieved the best test-set performance (R² = 0.931, RMSE = 3.284 MPa, MAE = 2.807 MPa, MAPE = 14.078%). SHAP analysis revealed that absorption coefficients at 0.568 THz, 0.569 THz, and 0.205 THz were the most influential features, corresponding to spectral regions sensitive to moisture–cellulose interactions and microstructural degradation. The optimized RF model not only provided accurate tensile strength predictions but also effectively discriminated between PLMs of different preservation states, offering a rapid, in situ, and non-invasive alternative to destructive testing. This integrated approach provides a scientifically grounded tool for preventive conservation and targeted restoration, and has potential for broader application in the non-destructive mechanical assessment of other cellulose-based heritage materials.
- 14 July 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessNon-Destructive Terahertz Assessment of Mechanical Fragility in Palm Leaf Manuscripts Using Interpretable Machine Learning
Conservation of palm leaf manuscripts (PLMs) requires tools that can estimate mechanical fragility without additional sampling once calibrated against reference mechanical data. This study develops a conservation-oriented workflow that integrates terahertz time-domain spectroscopy (THz-TDS), supervised regression, cross-validated model evaluation, and SHAP-based interpretability for quantitative prediction of tensile strength. A total of 223 independent palm-leaf specimens representing different deterioration states were measured by THz-TDS, and reference tensile-strength labels were obtained along the longitudinal fiber direction for model calibration. Absorption-coefficient spectra were modeled using partial least squares regression (PLSR), random forest (RF), and extreme gradient boosting (XGBoost), with predictive robustness evaluated through cross-validation and an independent test set. The optimized RF model achieved the best test-set performance (R² = 0.931, RMSE = 3.284 MPa, MAE = 2.807 MPa, MAPE = 14.078%). SHAP analysis revealed that absorption coefficients at 0.568 THz, 0.569 THz, and 0.205 THz were the most influential features, corresponding to spectral regions sensitive to moisture–cellulose interactions and microstructural degradation. The optimized RF model not only provided accurate tensile strength predictions but also effectively discriminated between PLMs of different preservation states, offering a rapid, in situ, and non-invasive alternative to destructive testing. This integrated approach provides a scientifically grounded tool for preventive conservation and targeted restoration, and has potential for broader application in the non-destructive mechanical assessment of other cellulose-based heritage materials.
- Open Access
- 11 October 2025
- Published by Springer Nature in npj Heritage Science
- Vol. 13 (1) , 1-9
Synergistic ATRP-IL approach for improving the mechanical properties of fragile palm leaf manuscripts
- 11 October 2025
- Published by Springer Nature in npj Heritage Science
- Vol. 13 (1) , 1-9
Open AccessSynergistic ATRP-IL approach for improving the mechanical properties of fragile palm leaf manuscripts
- 23 September 2025
- Published by Elsevier in Journal of Cultural Heritage
- Vol. 76, 86-98
Multi-property prediction of waterlogged archaeological wood based on Wasserstein GAN-augmented tree models
- 23 September 2025
- Published by Elsevier in Journal of Cultural Heritage
- Vol. 76, 86-98
Multi-property prediction of waterlogged archaeological wood based on Wasserstein GAN-augmented tree models
- Open Access
Exploring the Possibility of Ionic Liquid as a Dimensional Stabilizer for Well-Preserved Waterlogged Archaeological Wood
Dehydration is the principal conservation process for waterlogged archaeological wood (WAW), with the aim of preventing shrinkage and cracking. For well-preserved WAW, shrinkage mainly takes place when the moisture content is below the fiber saturation point. Here, we conduct a new trial using ionic liquid as a dimensional stabilizer to maintain a stable swollen state of WAW. Molecular dynamics simulation (MD), shrinkage measurement, Fourier transform infrared spectroscopy (FTIR), and dynamic vapor sorption (DVS) were adopted to investigate the interactions and effects of 1-Butyl-3-methylimidazolium chloride ([Bmim][Cl]) on WAW (Dipterocarpaceae Dipterocarpus sp. with a maximum moisture content of 80.3%) in comparison with the conventional material polyethylene glycol (PEG). The results show that [Bmim][Cl] and its water mixtures have a comparable or slightly greater ability to swell amorphous cellulose than does water at room temperature, while crystalline cellulose is left intact. The samples treated with [Bmim][Cl] show less shrinkage than the PEG 300- and PEG 2000-treated samples at all tested concentrations after air-drying. The best dimension control was achieved by 40 wt% [Bmim][Cl], with volumetric shrinkage reduced from 5.03% to 0.47%. DVS analysis reveals that [Bmim][Cl] reduces moisture contents at moderate and low relative humidity (<80%) when the concentration is at or below 20 wt%, which suggests that good dimensional stability was not achieved by simply preserving the moisture content but possibly through the interaction of the ionic liquid with the wood polymers.
Open AccessExploring the Possibility of Ionic Liquid as a Dimensional Stabilizer for Well-Preserved Waterlogged Archaeological Wood
Dehydration is the principal conservation process for waterlogged archaeological wood (WAW), with the aim of preventing shrinkage and cracking. For well-preserved WAW, shrinkage mainly takes place when the moisture content is below the fiber saturation point. Here, we conduct a new trial using ionic liquid as a dimensional stabilizer to maintain a stable swollen state of WAW. Molecular dynamics simulation (MD), shrinkage measurement, Fourier transform infrared spectroscopy (FTIR), and dynamic vapor sorption (DVS) were adopted to investigate the interactions and effects of 1-Butyl-3-methylimidazolium chloride ([Bmim][Cl]) on WAW (Dipterocarpaceae Dipterocarpus sp. with a maximum moisture content of 80.3%) in comparison with the conventional material polyethylene glycol (PEG). The results show that [Bmim][Cl] and its water mixtures have a comparable or slightly greater ability to swell amorphous cellulose than does water at room temperature, while crystalline cellulose is left intact. The samples treated with [Bmim][Cl] show less shrinkage than the PEG 300- and PEG 2000-treated samples at all tested concentrations after air-drying. The best dimension control was achieved by 40 wt% [Bmim][Cl], with volumetric shrinkage reduced from 5.03% to 0.47%. DVS analysis reveals that [Bmim][Cl] reduces moisture contents at moderate and low relative humidity (<80%) when the concentration is at or below 20 wt%, which suggests that good dimensional stability was not achieved by simply preserving the moisture content but possibly through the interaction of the ionic liquid with the wood polymers.
- Open Access
- 5 August 2024
- Published by Springer Nature in Heritage Science
- Vol. 12 (1) , 1-12
The effect of traditional processing craft on the hygroscopicity of palm leaf manuscripts
Palm leaf manuscripts, which are crucial carriers of historical, religious, scientific, and artistic information in East and Southeast Asia, specifically encapsulate significant aspects of Buddhist culture and thus require comprehensive research and preservation efforts. The base material of palm leaf manuscripts is processed palm leaves, which are hygroscopic and profoundly affected by environmental humidity. Currently, there is a research gap regarding the impact of traditional processing crafts and natural aging on the hygroscopicity of palm leaf manuscripts. Utilizing dynamic water vapor sorption (DVS), the hygroscopic properties of palm leaves from various years were assessed before and after traditional processing in Yunnan Province, China. The results show that traditional processing slightly increases the equilibrium moisture content (EMC) in environments with 0 to 60% relative humidity (RH), but significantly lowers EMC in high humidity environments, with reductions up to 19.01%. Additionally, hysteresis doubled post-processing, indicating enhanced stability under fluctuating humidity conditions. Sorption models suggest that traditional processing increases the number of adsorption sites while reducing physical adsorption or capillary condensation. FT-IR (Fourier-transform infrared spectroscopy) analysis indicates that the relative contents of cellulose and hemicellulose were reduced by 39.90% and 3.97%, respectively. Degradation occurring in both the crystalline and amorphous regions of cellulose. After natural aging, the hygroscopicity of processed palm leaves improved across the entire humidity range of 0 to 95%, and there was a slight increase in hysteresis. This is due to the increase in both adsorption sites and physical adsorption capabilities. FT-IR results also indicate that the relative contents of cellulose and hemicellulose were decreased by 57.52% and 19.83% after nature aging, respectively. These findings confirm that traditional processing improves the writability and humidity resilience of the leaves, while natural aging enhances their overall hygroscopic properties. This research contributes to our understanding of how humidity damages palm leaf manuscripts. aids in determining optimal RH ranges for storage, and assesses the effectiveness of consolidation treatments in their long–term preservation.
- 5 August 2024
- Published by Springer Nature in Heritage Science
- Vol. 12 (1) , 1-12
Open AccessThe effect of traditional processing craft on the hygroscopicity of palm leaf manuscripts
Palm leaf manuscripts, which are crucial carriers of historical, religious, scientific, and artistic information in East and Southeast Asia, specifically encapsulate significant aspects of Buddhist culture and thus require comprehensive research and preservation efforts. The base material of palm leaf manuscripts is processed palm leaves, which are hygroscopic and profoundly affected by environmental humidity. Currently, there is a research gap regarding the impact of traditional processing crafts and natural aging on the hygroscopicity of palm leaf manuscripts. Utilizing dynamic water vapor sorption (DVS), the hygroscopic properties of palm leaves from various years were assessed before and after traditional processing in Yunnan Province, China. The results show that traditional processing slightly increases the equilibrium moisture content (EMC) in environments with 0 to 60% relative humidity (RH), but significantly lowers EMC in high humidity environments, with reductions up to 19.01%. Additionally, hysteresis doubled post-processing, indicating enhanced stability under fluctuating humidity conditions. Sorption models suggest that traditional processing increases the number of adsorption sites while reducing physical adsorption or capillary condensation. FT-IR (Fourier-transform infrared spectroscopy) analysis indicates that the relative contents of cellulose and hemicellulose were reduced by 39.90% and 3.97%, respectively. Degradation occurring in both the crystalline and amorphous regions of cellulose. After natural aging, the hygroscopicity of processed palm leaves improved across the entire humidity range of 0 to 95%, and there was a slight increase in hysteresis. This is due to the increase in both adsorption sites and physical adsorption capabilities. FT-IR results also indicate that the relative contents of cellulose and hemicellulose were decreased by 57.52% and 19.83% after nature aging, respectively. These findings confirm that traditional processing improves the writability and humidity resilience of the leaves, while natural aging enhances their overall hygroscopic properties. This research contributes to our understanding of how humidity damages palm leaf manuscripts. aids in determining optimal RH ranges for storage, and assesses the effectiveness of consolidation treatments in their long–term preservation.
- Open Access
Anti-Cracking TEOS-Based Hybrid Materials as Reinforcement Agents for Paper Relics
Tetraethoxysilane (TEOS) is the most commonly used silicon-based reinforcement agent for conserving art relics due to its cost-effectiveness and commercial maturity. However, the resulting silica gel phase is prone to developing cracks as the gel shrinks during the sol–gel process, potentially causing severe damage to the objects being treated. In this study, dodecyltrimethoxysilane (DTMS) was introduced into TEOS to minimize this shrinkage by adding elastic long chains to weaken the capillary forces. The gel formed from the DTMS/TEOS hybrid material was transparent and crack-free, featuring a dense microstructure without mesopores or micropores. It exhibited excellent thermal stability, with a glass transition temperature of up to 109.64 °C. Evaluation experiments were conducted on artificially aged, handmade bamboo paper. The TEOS-based hybrid material effectively combined with the paper fibers through the sol–gel process, polymerizing into a network structure that enveloped the paper surface or penetrated between the fibers. The surface of the treated paper displayed excellent hydrophobic properties, with no significant changes in appearance, color, or air permeability. The mechanical properties of the treated bamboo paper improved significantly, with longitudinal and transverse tensile strengths increasing by up to 36.63% and 44.25%, respectively. These research findings demonstrate the promising potential for the application of DTMS/TEOS hybrid materials in reinforcing paper relics.
Open AccessAnti-Cracking TEOS-Based Hybrid Materials as Reinforcement Agents for Paper Relics
Tetraethoxysilane (TEOS) is the most commonly used silicon-based reinforcement agent for conserving art relics due to its cost-effectiveness and commercial maturity. However, the resulting silica gel phase is prone to developing cracks as the gel shrinks during the sol–gel process, potentially causing severe damage to the objects being treated. In this study, dodecyltrimethoxysilane (DTMS) was introduced into TEOS to minimize this shrinkage by adding elastic long chains to weaken the capillary forces. The gel formed from the DTMS/TEOS hybrid material was transparent and crack-free, featuring a dense microstructure without mesopores or micropores. It exhibited excellent thermal stability, with a glass transition temperature of up to 109.64 °C. Evaluation experiments were conducted on artificially aged, handmade bamboo paper. The TEOS-based hybrid material effectively combined with the paper fibers through the sol–gel process, polymerizing into a network structure that enveloped the paper surface or penetrated between the fibers. The surface of the treated paper displayed excellent hydrophobic properties, with no significant changes in appearance, color, or air permeability. The mechanical properties of the treated bamboo paper improved significantly, with longitudinal and transverse tensile strengths increasing by up to 36.63% and 44.25%, respectively. These research findings demonstrate the promising potential for the application of DTMS/TEOS hybrid materials in reinforcing paper relics.
- Open Access
- 6 October 2023
- Published by Springer Nature in Heritage Science
- Vol. 11 (1) , 1-13
Prediction model of the hardness of waterlogged archaeological wood based on NIR spectroscopy
The significance of waterlogged archaeological wood (WAW) lies in its profound informational value, encompassing historical, cultural, artistic, and scientific aspects of human civilization, and therefore need to be properly studied and preserved. In this study, the utilization of near-infrared (NIR) spectroscopy is employed as a predictive tool for assessing the hardness value of WAW. Given the submerged burial conditions, waterlogged wooden heritage frequently undergo substantial degradation in their physical and mechanical properties. The mechanical properties of waterlogged wooden heritage are essential for evaluating their state of preservation and devising appropriate conservation and restoration strategies. However, conventional methods for testing mechanical properties are limited by factors such as the availability of adequate sample size and quantity, adherence to the “principle of minimum intervention,” and cost considerations. NIR spectroscopy is a non-destructive, rapid, sensitive, and low-cost analytical technique with great potential for application in this area. In this study, two large and significant ancient Chinese shipwrecks were investigated. One hundred ninety-seven samples were collected and analyzed using NIR spectroscopy and a portable C-type shore hardness testing method. A partial least squares (PLS) regression model was developed to predict the hardness of the WAW. The model was optimized and validated using different preprocessing methods and spectral ranges. The results indicate that the best models were obtained with first derivatives + multiple scattering corrections (MSC) and first derivatives + standard normal variate (SNV) preprocessing in the 1000–2100 nm spectral range, both with an R 2 c of 0.97, a root mean squared error of correction (RMSEC) of 2.39 and 2.40, and a standard error of correction (SEC) of 2.40 and 2.41. Furthermore, they exhibited an R 2 v of 0.89 and 0.87, a root mean squared error of cross-validation (RMSECV) of 4.43 and 4.67, a standard error of cross-validation (SECV) of 4.45 and 4.68, and RPD values of 3.02 and 2.88, respectively. A coefficient of determination of the established prediction model (R 2 p) of 0.89 with a relative standard deviation for prediction (RSD) of 6.9% < 10% was obtained using a sample from the prediction set to predict the established model inversely. These results demonstrate that NIR spectroscopy could enable a rapid, non-destructive, and accurate estimation of the hardness of WAW. Moreover, by carefully choosing appropriate preprocessing techniques and spectral ranges, the predictive capabilities and accuracy of the model can be further enhanced. This research also contributes to the development of a theoretical framework and a methodological approach for future studies in this field. Furthermore, the data obtained from this study are crucial for determining effective preservation strategies for waterlogged archaeological wood.
- 6 October 2023
- Published by Springer Nature in Heritage Science
- Vol. 11 (1) , 1-13
Open AccessPrediction model of the hardness of waterlogged archaeological wood based on NIR spectroscopy
The significance of waterlogged archaeological wood (WAW) lies in its profound informational value, encompassing historical, cultural, artistic, and scientific aspects of human civilization, and therefore need to be properly studied and preserved. In this study, the utilization of near-infrared (NIR) spectroscopy is employed as a predictive tool for assessing the hardness value of WAW. Given the submerged burial conditions, waterlogged wooden heritage frequently undergo substantial degradation in their physical and mechanical properties. The mechanical properties of waterlogged wooden heritage are essential for evaluating their state of preservation and devising appropriate conservation and restoration strategies. However, conventional methods for testing mechanical properties are limited by factors such as the availability of adequate sample size and quantity, adherence to the “principle of minimum intervention,” and cost considerations. NIR spectroscopy is a non-destructive, rapid, sensitive, and low-cost analytical technique with great potential for application in this area. In this study, two large and significant ancient Chinese shipwrecks were investigated. One hundred ninety-seven samples were collected and analyzed using NIR spectroscopy and a portable C-type shore hardness testing method. A partial least squares (PLS) regression model was developed to predict the hardness of the WAW. The model was optimized and validated using different preprocessing methods and spectral ranges. The results indicate that the best models were obtained with first derivatives + multiple scattering corrections (MSC) and first derivatives + standard normal variate (SNV) preprocessing in the 1000–2100 nm spectral range, both with an R 2 c of 0.97, a root mean squared error of correction (RMSEC) of 2.39 and 2.40, and a standard error of correction (SEC) of 2.40 and 2.41. Furthermore, they exhibited an R 2 v of 0.89 and 0.87, a root mean squared error of cross-validation (RMSECV) of 4.43 and 4.67, a standard error of cross-validation (SECV) of 4.45 and 4.68, and RPD values of 3.02 and 2.88, respectively. A coefficient of determination of the established prediction model (R 2 p) of 0.89 with a relative standard deviation for prediction (RSD) of 6.9% < 10% was obtained using a sample from the prediction set to predict the established model inversely. These results demonstrate that NIR spectroscopy could enable a rapid, non-destructive, and accurate estimation of the hardness of WAW. Moreover, by carefully choosing appropriate preprocessing techniques and spectral ranges, the predictive capabilities and accuracy of the model can be further enhanced. This research also contributes to the development of a theoretical framework and a methodological approach for future studies in this field. Furthermore, the data obtained from this study are crucial for determining effective preservation strategies for waterlogged archaeological wood.
- Open Access
Size Effect on Hygroscopicity of Waterlogged Archaeological Wood by Simultaneous Dynamic Vapour Sorption
Hygroscopicity is one of the most important properties of wood and plays a decisive role in its dimensional stability. In this context, conservation plans for waterlogged archaeological wood (WAW) and relevant waterlogged artefacts must be created. The size of the sample required for a moisture sorption assessment may affect the results for (and thus the perception of) the hygroscopicity of a testing artefact. Herein, to investigate the effects of the sample size on the hygroscopicity of WAW as measured via dynamic vapour sorption (DVS), typical WAW and recent (i.e., sound) wood are processed into four differently sized samples, ranging in thickness from 200 mesh to millimetre. The equilibrium moisture contents (EMCs) of the wood samples are simultaneously measured using simultaneous DVS. The sorption isotherms show that the EMC values of the recent wood at each relative humidity increase as the sample size decreases, with the superfine powder sample achieving the highest EMC of all of the recent samples. Although the WAW has a higher EMC than that of recent wood, the effect of the size of the WAW sample on its hygroscopic properties is surprisingly not as pronounced as that for the recent wood. In addition, the hysteresis between the samples of different sizes of the archaeological wood is significantly smaller than that for the reference samples. Furthermore, regarding the standard deviations of the parameters obtained from the Guggenheim Anderson de Boer and Hailwood–Horrobin models, the values for WAW are all much smaller than those for the reference wood. This further verifies the disappearance of the size effect of the hygroscopicity for WAW.
Open AccessSize Effect on Hygroscopicity of Waterlogged Archaeological Wood by Simultaneous Dynamic Vapour Sorption
Hygroscopicity is one of the most important properties of wood and plays a decisive role in its dimensional stability. In this context, conservation plans for waterlogged archaeological wood (WAW) and relevant waterlogged artefacts must be created. The size of the sample required for a moisture sorption assessment may affect the results for (and thus the perception of) the hygroscopicity of a testing artefact. Herein, to investigate the effects of the sample size on the hygroscopicity of WAW as measured via dynamic vapour sorption (DVS), typical WAW and recent (i.e., sound) wood are processed into four differently sized samples, ranging in thickness from 200 mesh to millimetre. The equilibrium moisture contents (EMCs) of the wood samples are simultaneously measured using simultaneous DVS. The sorption isotherms show that the EMC values of the recent wood at each relative humidity increase as the sample size decreases, with the superfine powder sample achieving the highest EMC of all of the recent samples. Although the WAW has a higher EMC than that of recent wood, the effect of the size of the WAW sample on its hygroscopic properties is surprisingly not as pronounced as that for the recent wood. In addition, the hysteresis between the samples of different sizes of the archaeological wood is significantly smaller than that for the reference samples. Furthermore, regarding the standard deviations of the parameters obtained from the Guggenheim Anderson de Boer and Hailwood–Horrobin models, the values for WAW are all much smaller than those for the reference wood. This further verifies the disappearance of the size effect of the hygroscopicity for WAW.
- Open Access
Influence of Natural Aging on the Moisture Sorption Behaviour of Wooden Structural Components
A greater understanding of moisture sorption behaviour of aged wooden structural components, which has a close relationship with dimensional stability, is required to effectively evaluate and preserve historical artefacts. This study focused on the effects of aging on Baotou beam samples from a Chinese historical wooden building. An analysis of the sorption isotherms and hysteresis loops of a naturally aged, decayed sample (AOS), an aged sound sample (AIS), and a reference sample (RS), using classical sorption isotherm models revealed that the moisture sorption behaviour of samples from the same growth ring in a Baotou beam can differ significantly. AOS showed higher hygroscopicity than AIS, and both these samples were more hygroscopic than RS. Furthermore, the mono/multilayer moisture contents of AOS were always higher than those of AIS and RS. In addition, Fourier transform infrared, second-derivative infrared, and two-dimensional correlation infrared spectroscopy were used to investigate chemical changes in the samples. The relative hemicellulose and lignin contents of the samples changed significantly with wood aging. Furthermore, AOS exhibited the highest calcium oxalate content, which may be associated with fungal infections. Overall, these results provide valuable insights into the effects of aging on wood samples and the dimensional stability of timber structures, which could inform future research on methods for the preservation or restoration of aging timber structures.
Open AccessInfluence of Natural Aging on the Moisture Sorption Behaviour of Wooden Structural Components
A greater understanding of moisture sorption behaviour of aged wooden structural components, which has a close relationship with dimensional stability, is required to effectively evaluate and preserve historical artefacts. This study focused on the effects of aging on Baotou beam samples from a Chinese historical wooden building. An analysis of the sorption isotherms and hysteresis loops of a naturally aged, decayed sample (AOS), an aged sound sample (AIS), and a reference sample (RS), using classical sorption isotherm models revealed that the moisture sorption behaviour of samples from the same growth ring in a Baotou beam can differ significantly. AOS showed higher hygroscopicity than AIS, and both these samples were more hygroscopic than RS. Furthermore, the mono/multilayer moisture contents of AOS were always higher than those of AIS and RS. In addition, Fourier transform infrared, second-derivative infrared, and two-dimensional correlation infrared spectroscopy were used to investigate chemical changes in the samples. The relative hemicellulose and lignin contents of the samples changed significantly with wood aging. Furthermore, AOS exhibited the highest calcium oxalate content, which may be associated with fungal infections. Overall, these results provide valuable insights into the effects of aging on wood samples and the dimensional stability of timber structures, which could inform future research on methods for the preservation or restoration of aging timber structures.