Yoosung Ha
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Yoosung Ha has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
Hisashi Takamizawa
3 shared publications- Hisashi Takamizawa
The Oarai Center, Institute for Materials Research, Tohoku University, Oarai, Ibaraki 311-1313, Japan
3 shared publications Jinya Katsuyama
Japan Atomic Energy Agency , Shirakata 2-4 , Tokai-mura, Naka-gun, Ibaraki 319-1195, Japan
2 shared publications- Jinya Katsuyama
Nuclear Safety Research Center, Japan Atomic Energy Agency, 2-4 Shirakata, Tokai-mura, Naka-gun, Ibaraki 319-1195, Japan
2 shared publications - Tohru Tobita
Nuclear Safety Research Center, Japan Atomic Energy Agency , Shirakata 2-4, Tokai-mura, Naka-gun, Ibaraki-ken 319-1195, Japan
2 shared publications - Yutaka Nishiyama
Nuclear Safety Research Center, Japan Atomic Energy Agency, Tokai, Ibaraki 319-1195, Japan
2 shared publications
Latest Publications
- 11 August 2026
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 633
Evolution of solute clusters in heat-affected zones of reactor pressure vessel steel subjected to high neutron doses
- 11 August 2026
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 633
Evolution of solute clusters in heat-affected zones of reactor pressure vessel steel subjected to high neutron doses
- Open Access
- 28 April 2026
- Published by Elsevier in SSRN Electronic Journal
On-site assessment of yield and tensile strengths of NPP primary circuit structural components by instrumented indentation
This study is concerned with the evaluation of yield and tensile strengths of nuclear power plant (NPP) structural components by on-site measurement of instrumented indentation technique (IIT). Yield and tensile strengths were measured on the outer surface of Lemoniz NPP reactor pressure vessel (RPV) to primary piping joint segment employing IIT at ambient temperature. Tensile tests of specimens extracted from the joint were carried out at the reactor operating temperature. Through-thickness variation in yield and tensile strengths was assessed by the tensile tests and micro-hardness testing on joint axial cross section. The results of IIT were extrapolated to the reactor operating temperature by using strength-temperature correlations based on tabulated data of American Society of Mechanical Engineers (ASME), Boiler and Pressure Vessel Code (BPVC), Section II, Part D and compared to the tensile test results. A satisfactory agreement has been achieved, mainly for base materials. Larger deviation between surface IIT and bulk tensile test data has been observed for weldments. The through-thickness variation in yield and tensile strengths was within 5 %. It was concluded that surface IIT measurement carried out during reactor shut-down condition could estimate bulk equivalent yield and tensile strengths of RPV nozzle to primary piping joint materials at the reactor operating temperature by about 10 % deviation provided temperature extrapolation accurate enough would be applied.
- 28 April 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessOn-site assessment of yield and tensile strengths of NPP primary circuit structural components by instrumented indentation
This study is concerned with the evaluation of yield and tensile strengths of nuclear power plant (NPP) structural components by on-site measurement of instrumented indentation technique (IIT). Yield and tensile strengths were measured on the outer surface of Lemoniz NPP reactor pressure vessel (RPV) to primary piping joint segment employing IIT at ambient temperature. Tensile tests of specimens extracted from the joint were carried out at the reactor operating temperature. Through-thickness variation in yield and tensile strengths was assessed by the tensile tests and micro-hardness testing on joint axial cross section. The results of IIT were extrapolated to the reactor operating temperature by using strength-temperature correlations based on tabulated data of American Society of Mechanical Engineers (ASME), Boiler and Pressure Vessel Code (BPVC), Section II, Part D and compared to the tensile test results. A satisfactory agreement has been achieved, mainly for base materials. Larger deviation between surface IIT and bulk tensile test data has been observed for weldments. The through-thickness variation in yield and tensile strengths was within 5 %. It was concluded that surface IIT measurement carried out during reactor shut-down condition could estimate bulk equivalent yield and tensile strengths of RPV nozzle to primary piping joint materials at the reactor operating temperature by about 10 % deviation provided temperature extrapolation accurate enough would be applied.
- 19 January 2026
- Published by ASME International in Journal of Pressure Vessel Technology
- Vol. 148 (2)
Analysis of the Effect of Crack Curvature in Mini-C(T) Specimen on Fracture Toughness Evaluation
Accurate evaluation of the fracture toughness is essential to assess the structural integrity of reactor pressure vessels. The ASTM E1921 and JEAC4216 standardize the test method using a small-sized specimen, such as a miniature C(T) (mini-C(T)), to determine the reference temperature (T0) based on the master curve method. These standards prescribe the allowable crack curvature in the fracture toughness specimen. However, the allowable criterion of the crack curvature of both standards is different. The crack curvature of a mini-C(T) specimen may affect T0 determination due to variations in the plastic constraint. Herein, the effect of the crack curvature on the fracture toughness (KJc) evaluation or T0 determination using the mini-C(T) specimen was evaluated. Finite element analyses (FEAs), including the Weibull stress analysis, were performed to obtain quantitative information about the requirement of the crack curvature in ASTM E1921 and JEAC4216. FEA revealed that a specimen with a maximum allowable crack curvature decreased the plastic constraint, indicating a higher KJc value. The Weibull stress analysis revealed that the straightness criterion according to JEAC4216-2015 was reasonable for T0 determination. However, when all specimens with the maximum allowable crack curvature per ASTM E1921-21 were used for T0 determination, T0 was ∼10 °C lower than that of an ideal straight crack; this resulted in nonconservative T0 determination.
- 19 January 2026
- Published by ASME International in Journal of Pressure Vessel Technology
- Vol. 148 (2)
Analysis of the Effect of Crack Curvature in Mini-C(T) Specimen on Fracture Toughness Evaluation
Accurate evaluation of the fracture toughness is essential to assess the structural integrity of reactor pressure vessels. The ASTM E1921 and JEAC4216 standardize the test method using a small-sized specimen, such as a miniature C(T) (mini-C(T)), to determine the reference temperature (T0) based on the master curve method. These standards prescribe the allowable crack curvature in the fracture toughness specimen. However, the allowable criterion of the crack curvature of both standards is different. The crack curvature of a mini-C(T) specimen may affect T0 determination due to variations in the plastic constraint. Herein, the effect of the crack curvature on the fracture toughness (KJc) evaluation or T0 determination using the mini-C(T) specimen was evaluated. Finite element analyses (FEAs), including the Weibull stress analysis, were performed to obtain quantitative information about the requirement of the crack curvature in ASTM E1921 and JEAC4216. FEA revealed that a specimen with a maximum allowable crack curvature decreased the plastic constraint, indicating a higher KJc value. The Weibull stress analysis revealed that the straightness criterion according to JEAC4216-2015 was reasonable for T0 determination. However, when all specimens with the maximum allowable crack curvature per ASTM E1921-21 were used for T0 determination, T0 was ∼10 °C lower than that of an ideal straight crack; this resulted in nonconservative T0 determination.
- 2 December 2022
- Published by ASME International in Journal of Pressure Vessel Technology
- Vol. 145 (2)
Fracture Toughness Evaluation of the Heat-Affected Zone Under the Weld Overlay Cladding in Reactor Pressure Vessel Steel
The fracture toughness in the heat-affected zone (HAZ), which is located under the weld overlay cladding on the inner surface of the reactor pressure vessel (RPV), was evaluated by considering the inhomogeneous microstructures of the HAZ. In this regard, 0.4T-C(T) specimens and miniature C(T) (Mini-C(T)) specimens were manufactured to clarify the effect of the HAZ on fracture toughness. First, the fracture toughness was evaluated using 0.4T-C(T) specimens targeted on microstructural distribution due to the cladding bead location. The reference temperature (To) of HAZ at middle region of cladding bead was 12 °C higher than that at overlap cladding beads. Second, the fracture toughness was evaluated using Mini-C(T) specimens focused on the microstructural difference with distance from the boundary between the cladding and the base metal. The To value of the central position located at 3–7 mm from the boundary between the cladding and the base metal was higher than those of the other positions in HAZ. However, the To values of HAZ for both 0.4T-C(T) and Mini-C(T) specimens were significantly lower than that of the base metal at a quarter thickness by 40–60 °C. Compared with the literature data that indicated fracture toughness at the inner surface without overlay cladding and the base metal at a quarter thickness, this study concluded that the HAZ under the overlay cladding showed no detrimental effect on the conservatism of the structural integrity assessment of RPV steel.
- 2 December 2022
- Published by ASME International in Journal of Pressure Vessel Technology
- Vol. 145 (2)
Fracture Toughness Evaluation of the Heat-Affected Zone Under the Weld Overlay Cladding in Reactor Pressure Vessel Steel
The fracture toughness in the heat-affected zone (HAZ), which is located under the weld overlay cladding on the inner surface of the reactor pressure vessel (RPV), was evaluated by considering the inhomogeneous microstructures of the HAZ. In this regard, 0.4T-C(T) specimens and miniature C(T) (Mini-C(T)) specimens were manufactured to clarify the effect of the HAZ on fracture toughness. First, the fracture toughness was evaluated using 0.4T-C(T) specimens targeted on microstructural distribution due to the cladding bead location. The reference temperature (To) of HAZ at middle region of cladding bead was 12 °C higher than that at overlap cladding beads. Second, the fracture toughness was evaluated using Mini-C(T) specimens focused on the microstructural difference with distance from the boundary between the cladding and the base metal. The To value of the central position located at 3–7 mm from the boundary between the cladding and the base metal was higher than those of the other positions in HAZ. However, the To values of HAZ for both 0.4T-C(T) and Mini-C(T) specimens were significantly lower than that of the base metal at a quarter thickness by 40–60 °C. Compared with the literature data that indicated fracture toughness at the inner surface without overlay cladding and the base metal at a quarter thickness, this study concluded that the HAZ under the overlay cladding showed no detrimental effect on the conservatism of the structural integrity assessment of RPV steel.
- 1 December 2019
- Published by Elsevier in Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
- Vol. 461, 276-282
Ion-induced irradiation hardening of the weld heat-affected zone in low alloy steel
- 1 December 2019
- Published by Elsevier in Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
- Vol. 461, 276-282
Ion-induced irradiation hardening of the weld heat-affected zone in low alloy steel
- Open Access
Effect of Cold Rolling on Recrystallization Behavior of Al-Free and Al-Added 15Cr-ODS Ferritic Steels
The effect of cold rolling on the recrystallization behavior of Al-free and Al-added 15Cr-oxide dispersion strengthened (ODS) ferritic steels was investigated. The recrystallization of both steels are enhanced by cold rolling. The Al-free ODS steel with finer oxide particles is harder to recrystallize than Al-added ODS steel with coarser oxide particles. The effect of Al addition on the recrystallization behavior is evident. It is estimated that the recrystallization temperature of Al-free and Al-added 15Cr-ODS ferritic steel is 900 °C and 1250 °C with the annealing period of 1 h. In Al-free ODS steel, a small hardening was observed in the temperature range between 850 °C and 1200 °C, while no such phenomenon was observed in Al-added ODS steel, which is indicative of retardation of recovery by finely dispersed oxide particles. Oxide particle growth is mostly dependent on annealing temperature, while recrystallization and grain growth are controlled by not only the temperature, but the cold rolling ratio, which alters the multiple factors such as dislocation density, initial grain shape and oxide particle dispersion morphology. The cold rolling direction also influences the grain morphology and grain orientation in Al-added ODS steel, and the second rolling in a perpendicular direction to the first cold rolling direction induces the rotation of the grains from to . The recrystallization temperature is not significantly changed by the cold rolling direction. Recrystallization after cold rolling appears to increase the {111} grain orientation on the cold rolled specimen surface.
Open AccessEffect of Cold Rolling on Recrystallization Behavior of Al-Free and Al-Added 15Cr-ODS Ferritic Steels
The effect of cold rolling on the recrystallization behavior of Al-free and Al-added 15Cr-oxide dispersion strengthened (ODS) ferritic steels was investigated. The recrystallization of both steels are enhanced by cold rolling. The Al-free ODS steel with finer oxide particles is harder to recrystallize than Al-added ODS steel with coarser oxide particles. The effect of Al addition on the recrystallization behavior is evident. It is estimated that the recrystallization temperature of Al-free and Al-added 15Cr-ODS ferritic steel is 900 °C and 1250 °C with the annealing period of 1 h. In Al-free ODS steel, a small hardening was observed in the temperature range between 850 °C and 1200 °C, while no such phenomenon was observed in Al-added ODS steel, which is indicative of retardation of recovery by finely dispersed oxide particles. Oxide particle growth is mostly dependent on annealing temperature, while recrystallization and grain growth are controlled by not only the temperature, but the cold rolling ratio, which alters the multiple factors such as dislocation density, initial grain shape and oxide particle dispersion morphology. The cold rolling direction also influences the grain morphology and grain orientation in Al-added ODS steel, and the second rolling in a perpendicular direction to the first cold rolling direction induces the rotation of the grains from to . The recrystallization temperature is not significantly changed by the cold rolling direction. Recrystallization after cold rolling appears to increase the {111} grain orientation on the cold rolled specimen surface.
- 2 August 2018
- Published by ASME International in Journal of Pressure Vessel Technology
- Vol. 140 (5)
Applicability of Miniature Compact Tension Specimens for Fracture Toughness Evaluation of Highly Neutron Irradiated Reactor Pressure Vessel Steels
The applicability of miniature compact tension (Mini-C(T)) specimens to fracture toughness evaluation of neutron-irradiated reactor pressure vessel (RPV) steels was investigated. Three types of RPV steels neutron-irradiated to a high-fluence region were prepared and manufactured as Mini-C(T) specimens according to Japan Electric Association Code (JEAC) 4216-2015. Through careful selection of the test temperature by considering previously obtained mechanical properties data, valid fracture toughness, and reference temperature (To) was obtained with a relatively small number of specimens. Comparing the fracture toughness and To values determined using other larger specimens with those determined using the Mini-C(T) specimens, To values of both unirradiated and irradiated Mini-C(T) specimens were found to be the acceptable margin of error. The scatter of 1T-equivalent fracture toughness values of both unirradiated and irradiated materials obtained using Mini-C(T) specimens did not differ significantly from the values obtained using larger specimens. The correlation between the Charpy 41 J transition temperature (T41J) and the To values agreed very well with that of the data in the literature, regardless of specimen size and fracture toughness of the materials before irradiation. Based on these findings, it was concluded that Mini-C(T) specimens can be applied to fracture toughness evaluation of neutron-irradiated materials without significant specimen size dependence.
- 2 August 2018
- Published by ASME International in Journal of Pressure Vessel Technology
- Vol. 140 (5)
Applicability of Miniature Compact Tension Specimens for Fracture Toughness Evaluation of Highly Neutron Irradiated Reactor Pressure Vessel Steels
The applicability of miniature compact tension (Mini-C(T)) specimens to fracture toughness evaluation of neutron-irradiated reactor pressure vessel (RPV) steels was investigated. Three types of RPV steels neutron-irradiated to a high-fluence region were prepared and manufactured as Mini-C(T) specimens according to Japan Electric Association Code (JEAC) 4216-2015. Through careful selection of the test temperature by considering previously obtained mechanical properties data, valid fracture toughness, and reference temperature (To) was obtained with a relatively small number of specimens. Comparing the fracture toughness and To values determined using other larger specimens with those determined using the Mini-C(T) specimens, To values of both unirradiated and irradiated Mini-C(T) specimens were found to be the acceptable margin of error. The scatter of 1T-equivalent fracture toughness values of both unirradiated and irradiated materials obtained using Mini-C(T) specimens did not differ significantly from the values obtained using larger specimens. The correlation between the Charpy 41 J transition temperature (T41J) and the To values agreed very well with that of the data in the literature, regardless of specimen size and fracture toughness of the materials before irradiation. Based on these findings, it was concluded that Mini-C(T) specimens can be applied to fracture toughness evaluation of neutron-irradiated materials without significant specimen size dependence.