V. V. Yashin
V. V. Yashin has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- I. A. Latushkin5 shared publications
E. V. Aryshensky
4 shared publications- D. A. Stozharov2 shared publications
E. V. Aryshenskii
Korolev Samara National Research University, Samara, Russia
2 shared publications- Sergey V. Konovalov
Siberian State Industrial University
2 shared publications A. A. Ragazin
AO Arkonik SMZ, Samara, Russia
1 shared publication
Latest Publications
- 30 November 2022
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 75-80
Understanding the recrystallization kinetics in aluminium alloy billets with poorly developed cast structure
- 30 November 2022
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 75-80
Understanding the recrystallization kinetics in aluminium alloy billets with poorly developed cast structure
- 1 October 2021
- Published by Pleiades Publishing Ltd in Physics of Metals and Metallography
- Vol. 122 (10) , 960-968
Effect of Scandium on the Microstructure of the Al–Cu–Mn–Mg–Hf–Nb Alloy
The effect of scandium additives on the microstructure and mechanical properties of the Al–Cu–Mn–Mg–Nb–Hf alloy has been investigated. The phase composition of the alloy has been calculated using Thermo-Calc software. The trial ingots of the alloy with and without scandium have been cast to be subjected to homogenization, annealing for supersaturated solid solution decomposition, rolling in the laboratory mill, and recrystallization annealing. The samples have been studied by optical and electron microscopy (transmission microscope) at each stage. The phase composition of the scandium-free alloy has been shown to contain Al12Mn, Al2CuMg4, and Al20Cu2Mn3 secondary particles from 10 to 200 nm in size. The scandium-bearing alloy contains Al3(ScxHf1 – x) particles. The mass fraction of this phase after homogenization is 0.5%, and it increases to 1.9% at an annealing temperature of 300°C. These particles ensure the recrystallization-free deformation at 380–400°C and the softening by recovery. High-temperature annealing (540°C) initiates static recrystallization resulting in the formation of a microstructure with a relative average grain diameter of 8 μm. In the case of a scandium-free alloy, the number of blocking particles is insufficient to suppress boundary migration upon annealing, and the grain size remains over 26 μm under the same treatment conditions.
- 1 October 2021
- Published by Pleiades Publishing Ltd in Physics of Metals and Metallography
- Vol. 122 (10) , 960-968
Effect of Scandium on the Microstructure of the Al–Cu–Mn–Mg–Hf–Nb Alloy
The effect of scandium additives on the microstructure and mechanical properties of the Al–Cu–Mn–Mg–Nb–Hf alloy has been investigated. The phase composition of the alloy has been calculated using Thermo-Calc software. The trial ingots of the alloy with and without scandium have been cast to be subjected to homogenization, annealing for supersaturated solid solution decomposition, rolling in the laboratory mill, and recrystallization annealing. The samples have been studied by optical and electron microscopy (transmission microscope) at each stage. The phase composition of the scandium-free alloy has been shown to contain Al12Mn, Al2CuMg4, and Al20Cu2Mn3 secondary particles from 10 to 200 nm in size. The scandium-bearing alloy contains Al3(ScxHf1 – x) particles. The mass fraction of this phase after homogenization is 0.5%, and it increases to 1.9% at an annealing temperature of 300°C. These particles ensure the recrystallization-free deformation at 380–400°C and the softening by recovery. High-temperature annealing (540°C) initiates static recrystallization resulting in the formation of a microstructure with a relative average grain diameter of 8 μm. In the case of a scandium-free alloy, the number of blocking particles is insufficient to suppress boundary migration upon annealing, and the grain size remains over 26 μm under the same treatment conditions.
- 29 January 2021
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 58-64
Study of recrystallization kinetics of aluminium alloy 1565ch with low degree of cast structure conditioning
The present study addresses recrystallization process in Al – Mg 1565ch system alloy samples (Russian classification). The samples are taken from cast ingot, produced by continuous casting in DC mold and homogenized based on standard commercial mode. Then the samples were heated to 350–500 oC and rolled in lab mill with different process schedules to cover the entire range of temperature and strain rates, applied in rolling. After rolling the samples were annealed at 350, 400 and 450 oC, their resultant microstructure was examined by optic microscope. The rate of new grains nucleation, their growth speed, analytical notations, describing recrystallization kinetics, were obtained within the frames of the study to be applied during this alloy recrystallization modelling; the main alloy-specific recrystallization features were identified and compared with alloy АА5182 (classification of American Aluminum Association). It is demonstrated, that 1565ch recrystallization has a number of specific features in case of as-cast structure deformation with low strain levels (ε = 0.14÷0.56): first, high rate of new grains nucleation; second, low grain growth speed to the extent of complete process blocking. Optimal recrystallization temperature is identified as 400 oC, at this temperature the process is over 75% complete, the temperature drop (350 oC) causes incubation period extension, while recrystallization subsides at recrystallized structure volume of about 30%, in case of temperature rise (450 oC) the structure is saturated with fine new grains nuclei, probably, emerging during heating, but due to high intensity of recovery and polygonization, recrystallization driving force drops to zero, the process stops with mixed structure and max recrystallized grains volume of 20%. This research was funded through a grant by the Russian Science Foundation, Project 18-79-10099.
- 29 January 2021
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 58-64
Study of recrystallization kinetics of aluminium alloy 1565ch with low degree of cast structure conditioning
The present study addresses recrystallization process in Al – Mg 1565ch system alloy samples (Russian classification). The samples are taken from cast ingot, produced by continuous casting in DC mold and homogenized based on standard commercial mode. Then the samples were heated to 350–500 oC and rolled in lab mill with different process schedules to cover the entire range of temperature and strain rates, applied in rolling. After rolling the samples were annealed at 350, 400 and 450 oC, their resultant microstructure was examined by optic microscope. The rate of new grains nucleation, their growth speed, analytical notations, describing recrystallization kinetics, were obtained within the frames of the study to be applied during this alloy recrystallization modelling; the main alloy-specific recrystallization features were identified and compared with alloy АА5182 (classification of American Aluminum Association). It is demonstrated, that 1565ch recrystallization has a number of specific features in case of as-cast structure deformation with low strain levels (ε = 0.14÷0.56): first, high rate of new grains nucleation; second, low grain growth speed to the extent of complete process blocking. Optimal recrystallization temperature is identified as 400 oC, at this temperature the process is over 75% complete, the temperature drop (350 oC) causes incubation period extension, while recrystallization subsides at recrystallized structure volume of about 30%, in case of temperature rise (450 oC) the structure is saturated with fine new grains nuclei, probably, emerging during heating, but due to high intensity of recovery and polygonization, recrystallization driving force drops to zero, the process stops with mixed structure and max recrystallized grains volume of 20%. This research was funded through a grant by the Russian Science Foundation, Project 18-79-10099.
- 25 November 2020
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 84-90
Effect of hafnium transition metal additives on the microstructure of 01570 aluminum alloy
- 25 November 2020
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 84-90
Effect of hafnium transition metal additives on the microstructure of 01570 aluminum alloy
- 25 November 2020
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 77-84
Study of kinetics of the supersaturated solid solution decomposition in alloys of the Al – Mg system with transition elements addition
The objective of the study is to determine kinetics of L12 structure type particles precipitation in Al – Mg system aluminum alloys, containing scandium and zirconium. The article addresses microstructure evolution of scandium containing alloys, including two-component alloy and Al – Mg system alloys, containing multiple components, i.e., 1565ch alloy (Al – Mg – Mn – Zn – Zr system) and 01570 alloy (Al – Mg – Mn – Sc – Zr system). The samples were produced by casting in water chilled copper permanent mold. Analysis of the samples, representing various alloys, including 99.95% pure aluminum, confirmed quantitative data of solutes effect on electrical resistance. The optimal homogenization modes, enabling max alloying components dissolution in aluminum matrix, were established for the studied alloys. After that the samples were subjected to heterogenization annealing in the temperature range from 250 oC to 450 oC, with soaking time ranging from 1 to 106 s. C-curves of supersaturated solid solution decomposition were plotted based on correlation of samples electrical resistance in max saturated solution and after annealing under different modes; it was demonstrated, that decomposition curves of the alloys, containing 0.2 and more scandium, have two peaks, at 300 oC and at 425 oC. The obtained data are approximated by power functions (min determination coefficient R2 is 0.97), which are helpful for such alloys thermomechanical treatment modelling. It is demonstrated, that during cast samples heat treatment at the temperature above 350 oC decomposition of alloys, containing 0.2% and more scandium, is associated with secondary crystallization, and decomposition product distribution is fan-shaped, confirming the theory of discontinuous decomposition, observed by other researchers in similar alloys. The size of L12 structure particles, generated during discontinuous decomposition, ranged from 50 to 270 nm, which is significantly different from the optimal values of 40–50 nm.The study was supported by a grant from the Russian Science Foundation, project 18-79-10099.
- 25 November 2020
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 77-84
Study of kinetics of the supersaturated solid solution decomposition in alloys of the Al – Mg system with transition elements addition
The objective of the study is to determine kinetics of L12 structure type particles precipitation in Al – Mg system aluminum alloys, containing scandium and zirconium. The article addresses microstructure evolution of scandium containing alloys, including two-component alloy and Al – Mg system alloys, containing multiple components, i.e., 1565ch alloy (Al – Mg – Mn – Zn – Zr system) and 01570 alloy (Al – Mg – Mn – Sc – Zr system). The samples were produced by casting in water chilled copper permanent mold. Analysis of the samples, representing various alloys, including 99.95% pure aluminum, confirmed quantitative data of solutes effect on electrical resistance. The optimal homogenization modes, enabling max alloying components dissolution in aluminum matrix, were established for the studied alloys. After that the samples were subjected to heterogenization annealing in the temperature range from 250 oC to 450 oC, with soaking time ranging from 1 to 106 s. C-curves of supersaturated solid solution decomposition were plotted based on correlation of samples electrical resistance in max saturated solution and after annealing under different modes; it was demonstrated, that decomposition curves of the alloys, containing 0.2 and more scandium, have two peaks, at 300 oC and at 425 oC. The obtained data are approximated by power functions (min determination coefficient R2 is 0.97), which are helpful for such alloys thermomechanical treatment modelling. It is demonstrated, that during cast samples heat treatment at the temperature above 350 oC decomposition of alloys, containing 0.2% and more scandium, is associated with secondary crystallization, and decomposition product distribution is fan-shaped, confirming the theory of discontinuous decomposition, observed by other researchers in similar alloys. The size of L12 structure particles, generated during discontinuous decomposition, ranged from 50 to 270 nm, which is significantly different from the optimal values of 40–50 nm.The study was supported by a grant from the Russian Science Foundation, project 18-79-10099.
- 1 September 2019
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 61 (5-6) , 300-304
A Study of Texture Component Distribution Over the Cross Section of an Aluminum Alloy 8011 Billet with Hot Rolling in a Four-Stand Continuous Group
- 1 September 2019
- Published by Springer Nature in Metal Science and Heat Treatment
- Vol. 61 (5-6) , 300-304
A Study of Texture Component Distribution Over the Cross Section of an Aluminum Alloy 8011 Billet with Hot Rolling in a Four-Stand Continuous Group
- 29 March 2019
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 64-69
Rheological behavior of 01570 and AA5182 wrought aluminum alloys under hot deformation conditions
The rheological properties under hot deformation of 01570 alloy containing scandium and zirconium micro-additives were studied in comparison with alloy AA5182. Hot deformation was performed by uniaxial compression on Gleeble 3800 thermomechanical processes physical simulator at the temperature range of 350–450 oС and strain rates of 0.001–10 s–1. Alloy samples were selected from ingots obtained under industrial conditions and subjected to standard homogenization. It is demonstrated, that alloys flow stresses increase with rate increase and deformation temperature decrease reflecting changes of Zener-Hollomon parameter, describing the temperature-rate deformation mode. At low Zener-Hollomon parameter values, two studied alloys have close flow stress values; at high parameter values 01570 alloy, micro-alloyed with scandium and zirconium, has higher strain resistance compared to AA5182 alloy. This effect is explained by the presence of fine Al3 (Sc, Zr) intermetallic compounds particles in 01570 alloy, causing dispersion hardening, as well as a higher magnesium content in this alloy. Obtained analytical expressions allow calculating the steady-state flow stresses of the alloys at specified temperature — rate parameters of hot deformation. These expressions application can be recommended for slab rolling practice calculation, being especially true 01570 type alloys, requiring strictly regulated temperature conditions during processing. A computer simulation of 01570 alloy reverse rolling was performed using the obtained analytical expressions with account for this alloy flow stress values. It is shown that the calculated and actual values of the torque on all passes of the reversing rolling coincide with the accuracy sufficient for engineering purposes.
- 29 March 2019
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 64-69
Rheological behavior of 01570 and AA5182 wrought aluminum alloys under hot deformation conditions
The rheological properties under hot deformation of 01570 alloy containing scandium and zirconium micro-additives were studied in comparison with alloy AA5182. Hot deformation was performed by uniaxial compression on Gleeble 3800 thermomechanical processes physical simulator at the temperature range of 350–450 oС and strain rates of 0.001–10 s–1. Alloy samples were selected from ingots obtained under industrial conditions and subjected to standard homogenization. It is demonstrated, that alloys flow stresses increase with rate increase and deformation temperature decrease reflecting changes of Zener-Hollomon parameter, describing the temperature-rate deformation mode. At low Zener-Hollomon parameter values, two studied alloys have close flow stress values; at high parameter values 01570 alloy, micro-alloyed with scandium and zirconium, has higher strain resistance compared to AA5182 alloy. This effect is explained by the presence of fine Al3 (Sc, Zr) intermetallic compounds particles in 01570 alloy, causing dispersion hardening, as well as a higher magnesium content in this alloy. Obtained analytical expressions allow calculating the steady-state flow stresses of the alloys at specified temperature — rate parameters of hot deformation. These expressions application can be recommended for slab rolling practice calculation, being especially true 01570 type alloys, requiring strictly regulated temperature conditions during processing. A computer simulation of 01570 alloy reverse rolling was performed using the obtained analytical expressions with account for this alloy flow stress values. It is shown that the calculated and actual values of the torque on all passes of the reversing rolling coincide with the accuracy sufficient for engineering purposes.
- 28 February 2019
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 56-61
How microalloying of the AlMg5 alloy with transition metals (Sc, Zr, Nb) impacts the structure of a cast billet
The work conducted as part of this research focused on understanding how microalloying of the AlMg5 alloy with the transition metals of Zr, Sc and Nb can impact the grain structure of a cast billet. A complete factorial experiment was carried out during which different concentrations of the above elements were applied – from 0.1 to 0.3 %. The experiment provided a quantitative analysis of the inoculation effect produced by each of the studied transition metals. An induction furnace was used to produce ingots, which were chill cast. Metallographic specimens were prepared for each casting and analysed for microstructure with a 100:1 magnification optical microscope. The results of the microstructural analysis indicate a strong inoculation effect produced by zirconium and scandium and a low effect when niobium is used for grain refinement. The authors were able to obtain ingots with a grain structure with the maximum grain size being 23 μm versus the initial dendritic structure of a cast ingot (with the interdendritic distance of 153 μm) produced under the same conditions but not inoculated with transition metals. A curve was built showing how the grain size is governed by the total amount of rare earth elements, i. e. Zr, Sc and Nb. With the help of regression analysis the authors came up with an analytical expression for the above relationship.This research was funded by the Russian Science Foundation, Project 18-79-10099.
- 28 February 2019
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 56-61
How microalloying of the AlMg5 alloy with transition metals (Sc, Zr, Nb) impacts the structure of a cast billet
The work conducted as part of this research focused on understanding how microalloying of the AlMg5 alloy with the transition metals of Zr, Sc and Nb can impact the grain structure of a cast billet. A complete factorial experiment was carried out during which different concentrations of the above elements were applied – from 0.1 to 0.3 %. The experiment provided a quantitative analysis of the inoculation effect produced by each of the studied transition metals. An induction furnace was used to produce ingots, which were chill cast. Metallographic specimens were prepared for each casting and analysed for microstructure with a 100:1 magnification optical microscope. The results of the microstructural analysis indicate a strong inoculation effect produced by zirconium and scandium and a low effect when niobium is used for grain refinement. The authors were able to obtain ingots with a grain structure with the maximum grain size being 23 μm versus the initial dendritic structure of a cast ingot (with the interdendritic distance of 153 μm) produced under the same conditions but not inoculated with transition metals. A curve was built showing how the grain size is governed by the total amount of rare earth elements, i. e. Zr, Sc and Nb. With the help of regression analysis the authors came up with an analytical expression for the above relationship.This research was funded by the Russian Science Foundation, Project 18-79-10099.