Hitesh K. Trivedi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Hitesh K. Trivedi has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Armen Kvryan
Micron School of Materials Science & Engineering, Boise State University, Boise, ID, USA
1 shared publication - Chinpei Wang
Cummins Technical Center, R&T Cummins, Inc. Advanced Materials Evaluation Laboratories Columbus, IN 47201
1 shared publication - Corey M. Efaw
Micron School of Materials Science & Engineering, Boise State University, Boise, ID 83725-2090, USA
1 shared publication - Elton Graugnard
Boise State University
1 shared publication - Farshid Sadeghi
School of Mechanical Engineering, Purdue University
1 shared publication Justin K. Mason
Air Force Research Laboratory (AFRL)
1 shared publication
Latest Publications
- Open Access
- 15 September 2021
- Published by ASME International in Journal of Tribology
- Vol. 143 (12)
Effects of Grain Refinement on Rolling Contact Fatigue in Bearing Contacts
This paper presents a finite element model (FEM) to investigate the effect of prior austenite grain refinement on rolling contact fatigue (RCF). RCF life was determined using continuum damage mechanics (CDM), which simulated material deterioration as a function of cycle. Continuum damage mechanics calculations in this investigation considered the subsurface shear (orthogonal) reversal to be responsible for RCF failure. To establish the CDM critical parameters—resistance stress (σr) and damage rate exponent (m)—torsion stress-life data from open literature of three different grain sizes for the same material was used. It was observed from the torsion S-N (stress-life) data that the resistance stress exhibits a linear relationship with grain diameter. As grain diameter was refined, the resistance stress was found to increase. The damage rate exponent (m) displayed no relation to grain diameter; hence, the average value from the three torsion S-N curves was used in this investigation. In order to assess the effect of grain refinement on RCF life, a series of unique material microstructures were constructed using the Voronoi tessellation process at eight mean grain diameters. Finite element (FE) simulations were devised at three contact pressures, typical of heavily loaded lubricated contacts, and the RCF life was determined for each set of microstructures of a given mean grain diameter. The RCF results at the eight grain diameters indicate that fatigue performance is improved exponentially with finer grain diameter. The observed life improvements from the RCF simulations resulting from grain refinement exhibit good corroboration with existing experimental results found in open literature. A single predictive fatigue life equation was constructed from this investigation’s RCF simulations to evaluate the stochastic RCF performance, given grain diameter and contact pressure, of non-conformal contacts.
- 15 September 2021
- Published by ASME International in Journal of Tribology
- Vol. 143 (12)
Open AccessEffects of Grain Refinement on Rolling Contact Fatigue in Bearing Contacts
This paper presents a finite element model (FEM) to investigate the effect of prior austenite grain refinement on rolling contact fatigue (RCF). RCF life was determined using continuum damage mechanics (CDM), which simulated material deterioration as a function of cycle. Continuum damage mechanics calculations in this investigation considered the subsurface shear (orthogonal) reversal to be responsible for RCF failure. To establish the CDM critical parameters—resistance stress (σr) and damage rate exponent (m)—torsion stress-life data from open literature of three different grain sizes for the same material was used. It was observed from the torsion S-N (stress-life) data that the resistance stress exhibits a linear relationship with grain diameter. As grain diameter was refined, the resistance stress was found to increase. The damage rate exponent (m) displayed no relation to grain diameter; hence, the average value from the three torsion S-N curves was used in this investigation. In order to assess the effect of grain refinement on RCF life, a series of unique material microstructures were constructed using the Voronoi tessellation process at eight mean grain diameters. Finite element (FE) simulations were devised at three contact pressures, typical of heavily loaded lubricated contacts, and the RCF life was determined for each set of microstructures of a given mean grain diameter. The RCF results at the eight grain diameters indicate that fatigue performance is improved exponentially with finer grain diameter. The observed life improvements from the RCF simulations resulting from grain refinement exhibit good corroboration with existing experimental results found in open literature. A single predictive fatigue life equation was constructed from this investigation’s RCF simulations to evaluate the stochastic RCF performance, given grain diameter and contact pressure, of non-conformal contacts.
- Open Access
Corrosion Initiation and Propagation on Carburized Martensitic Stainless Steel Surfaces Studied via Advanced Scanning Probe Microscopy
Historically, high carbon steels have been used in mechanical applications because their high surface hardness contributes to excellent wear performance. However, in aggressive environments, current bearing steels exhibit insufficient corrosion resistance. Martensitic stainless steels are attractive for bearing applications due to their high corrosion resistance and ability to be surface hardened via carburizing heat treatments. Here three different carburizing heat treatments were applied to UNS S42670: a high-temperature temper (HTT), a low-temperature temper (LTT), and carbo-nitriding (CN). Magnetic force microscopy showed differences in magnetic domains between the matrix and carbides, while scanning Kelvin probe force microscopy (SKPFM) revealed a 90–200 mV Volta potential difference between the two phases. Corrosion progression was monitored on the nanoscale via SKPFM and in situ atomic force microscopy (AFM), revealing different corrosion modes among heat treatments that predicted bulk corrosion behavior in electrochemical testing. HTT outperforms LTT and CN in wear testing and thus is recommended for non-corrosive aerospace applications, whereas CN is recommended for corrosion-prone applications as it exhibits exceptional corrosion resistance. The results reported here support the use of scanning probe microscopy for predicting bulk corrosion behavior by measuring nanoscale surface differences in properties between carbides and the surrounding matrix.
Open AccessCorrosion Initiation and Propagation on Carburized Martensitic Stainless Steel Surfaces Studied via Advanced Scanning Probe Microscopy
Historically, high carbon steels have been used in mechanical applications because their high surface hardness contributes to excellent wear performance. However, in aggressive environments, current bearing steels exhibit insufficient corrosion resistance. Martensitic stainless steels are attractive for bearing applications due to their high corrosion resistance and ability to be surface hardened via carburizing heat treatments. Here three different carburizing heat treatments were applied to UNS S42670: a high-temperature temper (HTT), a low-temperature temper (LTT), and carbo-nitriding (CN). Magnetic force microscopy showed differences in magnetic domains between the matrix and carbides, while scanning Kelvin probe force microscopy (SKPFM) revealed a 90–200 mV Volta potential difference between the two phases. Corrosion progression was monitored on the nanoscale via SKPFM and in situ atomic force microscopy (AFM), revealing different corrosion modes among heat treatments that predicted bulk corrosion behavior in electrochemical testing. HTT outperforms LTT and CN in wear testing and thus is recommended for non-corrosive aerospace applications, whereas CN is recommended for corrosion-prone applications as it exhibits exceptional corrosion resistance. The results reported here support the use of scanning probe microscopy for predicting bulk corrosion behavior by measuring nanoscale surface differences in properties between carbides and the surrounding matrix.
- 23 March 2017
- Published by Springer Nature in Journal of Failure Analysis and Prevention
- Vol. 17 (3) , 426-439
Spall Propagation Characteristics of Refurbished VIM–VAR AISI M50 Angular Contact Bearings
- 23 March 2017
- Published by Springer Nature in Journal of Failure Analysis and Prevention
- Vol. 17 (3) , 426-439
Spall Propagation Characteristics of Refurbished VIM–VAR AISI M50 Angular Contact Bearings
- 3 March 2016
- Published by Taylor & Francis in Tribology Transactions
- Vol. 59 (2) , 363-374
Effect of Silicon Nitride Ball on Adhesive Wear of Martensitic Stainless Steel Pyrowear 675 and AISI M-50 Races with Type II Ester Oil
Advanced bearing materials for future military and commercial gas turbines are required to operate at high speeds, high temperature, and higher thrust loads. At elevated operating conditions, the bearing and gear materials must be able to operate with ultrathin oil films without suffering detrimental effects of adhesive wear. The development of materials with rolling-element fatigue and corrosion resistance properties without deterioration in adhesive wear attributes is a significant challenge. To meet those performance requirements, the forerunner, martensitic stainless steel Pyrowear 675 (AMS 5930), has been in development for aerospace bearing and gear applications. This article addresses the adhesive wear performance of three variants of Pyrowear 675 with silicon nitride ball material simulating a hybrid bearing evaluated using a WAM8 machine. Baseline testing was conducted using conventional bearing steel AISI M-50. Adhesive wear testing was conducted at a temperature of 200°C and at different contact slips (15, 30, 50, and 70%) and entraining velocities (1.3 to 10.2 m/s). Posttest specimens were analyzed by scanning electron microscopy (SEM) and auger electron spectroscopy (AES). All the hybrid material pairs demonstrated very good adhesive wear performance compared to the baseline AISI M-50–AISI M-50 pair.
- 3 March 2016
- Published by Taylor & Francis in Tribology Transactions
- Vol. 59 (2) , 363-374
Effect of Silicon Nitride Ball on Adhesive Wear of Martensitic Stainless Steel Pyrowear 675 and AISI M-50 Races with Type II Ester Oil
Advanced bearing materials for future military and commercial gas turbines are required to operate at high speeds, high temperature, and higher thrust loads. At elevated operating conditions, the bearing and gear materials must be able to operate with ultrathin oil films without suffering detrimental effects of adhesive wear. The development of materials with rolling-element fatigue and corrosion resistance properties without deterioration in adhesive wear attributes is a significant challenge. To meet those performance requirements, the forerunner, martensitic stainless steel Pyrowear 675 (AMS 5930), has been in development for aerospace bearing and gear applications. This article addresses the adhesive wear performance of three variants of Pyrowear 675 with silicon nitride ball material simulating a hybrid bearing evaluated using a WAM8 machine. Baseline testing was conducted using conventional bearing steel AISI M-50. Adhesive wear testing was conducted at a temperature of 200°C and at different contact slips (15, 30, 50, and 70%) and entraining velocities (1.3 to 10.2 m/s). Posttest specimens were analyzed by scanning electron microscopy (SEM) and auger electron spectroscopy (AES). All the hybrid material pairs demonstrated very good adhesive wear performance compared to the baseline AISI M-50–AISI M-50 pair.