Huaguan Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Huaguan Li has a total of 50 co-authors. Here are the top co-authors by number of shared publications:
- Jie Tao
College of Materials Science and Technology Nanjing University of Aeronautics and Astronautics Nanjing People's Republic of China
5 shared publications - Xunzhong Guo
College of Material Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 211100, China
3 shared publications - Wei-Jie Fei
School of Materials Science and Engineering, Nanjing Institute of Technology, Nanjing, Jiangsu, CHINA
2 shared publications - Albert Sedlmaier
Data M Sheet Metal Solutions GmbH
1 shared publication - Ali Abd El-Aty
Seoul National University
1 shared publication - Chao Pan
Nanjing University of Aeronautics and Astronautics
1 shared publication
Latest Publications
- 6 December 2024
- Published by Springer Nature in Applied Composite Materials
- Vol. 32 (2) , 625-637
The Influence of Trigger Angle Structure on the Energy Absorption Capabilities of Aluminum Alloy/Thermoplastic Reinforced Polypropylene Hybrid Tubes
- 6 December 2024
- Published by Springer Nature in Applied Composite Materials
- Vol. 32 (2) , 625-637
The Influence of Trigger Angle Structure on the Energy Absorption Capabilities of Aluminum Alloy/Thermoplastic Reinforced Polypropylene Hybrid Tubes
- 24 August 2022
- Published by Springer Nature
- p. 1-28
Introduction and State of the Art of Flexible Forming Technologies
- 24 August 2022
- Published by Springer Nature
- p. 1-28
Introduction and State of the Art of Flexible Forming Technologies
- 24 August 2022
- Published by Springer Nature
- p. 227-266
Tube 3D Quench Forming Technology
- Open Access
Evolution Behaviors and Reduction Mechanism of Curing Residual Stresses in GLARE Laminates under a Hot-Pressing Condition
Nowadays, variable preparation, forming and processing methods of fiber metal laminates are constantly developing to meet the requirements of different application fields, hence the characteristics and evolution of residual stresses under different manufacturing conditions deserve more attention. In this work, the evolution behaviors of curing residual stresses in GLARE under a hot-pressing condition were studied, and the residual stress reduction mechanism was also explained. Results suggested the FE prediction models of the entire cure process, verified by the fiber Bragg grating (FBG) sensors, were more precise than the traditional elastic model. Moreover, the stress evolution during the cure process mainly occurred in the cooling stage, in which the different coefficient of thermal expansion (CTE) of aluminum and GFRP played a major role. Meanwhile, curing shrinkage stress in the GFRP layer during the holding stage at curing temperature obviously influenced the final stress level. The residual stresses in GFRP layers differed by 9.6 MPa under a hot-pressing and autoclave condition, in which the convection heat transfer condition played a major role as it caused lower thermal stress in the holding stage and a smaller temperature gradient in the cooling stage. Considering this, a lower cooling rate could be a feasible way to obtain GLARE with lower residual stress under a hot-pressing condition.
Open AccessEvolution Behaviors and Reduction Mechanism of Curing Residual Stresses in GLARE Laminates under a Hot-Pressing Condition
Nowadays, variable preparation, forming and processing methods of fiber metal laminates are constantly developing to meet the requirements of different application fields, hence the characteristics and evolution of residual stresses under different manufacturing conditions deserve more attention. In this work, the evolution behaviors of curing residual stresses in GLARE under a hot-pressing condition were studied, and the residual stress reduction mechanism was also explained. Results suggested the FE prediction models of the entire cure process, verified by the fiber Bragg grating (FBG) sensors, were more precise than the traditional elastic model. Moreover, the stress evolution during the cure process mainly occurred in the cooling stage, in which the different coefficient of thermal expansion (CTE) of aluminum and GFRP played a major role. Meanwhile, curing shrinkage stress in the GFRP layer during the holding stage at curing temperature obviously influenced the final stress level. The residual stresses in GFRP layers differed by 9.6 MPa under a hot-pressing and autoclave condition, in which the convection heat transfer condition played a major role as it caused lower thermal stress in the holding stage and a smaller temperature gradient in the cooling stage. Considering this, a lower cooling rate could be a feasible way to obtain GLARE with lower residual stress under a hot-pressing condition.
- Open Access
Low-Velocity Impact Resistance of Al/Gf/PP Laminates with Different Interface Performance
The weak interface performance between metal and composite (IPMC) makes the composite materials susceptible to impact load. Aluminum/glass fiber/polypropylene (Al/Gf/PP) laminates were manufactured with the aluminum alloy sheets modified by nitrogen plasma surface treatment and the phosphoric acid anodizing method, respectively. FEM models of Al/Gf/PP laminates under low-velocity impact were established in ABAQUS/Explicit based on the generated data including the model I and II interlaminar fracture toughness. Low-velocity impact tests were performed to investigate the impact resistance of Al/Gf/PP laminates including load traces, failure mechanism, and energy absorption. The results showed that delamination was the main failure mode of two kinds of laminates under the impact energy of 20 J and 30 J. When the impact energy was between 40 J and 50 J, there were metal cracks on the rear surface of the plasma pretreated specimens, which possessed higher energy absorption and impact resistance, although the integrity of the laminates could not be preserved. Since the residual compressive stress was generated during the cooling process, the laminates were more susceptible to stretching rather than delamination. For impact energy (60 J) causing the through-the-thickness crack of two kinds of laminates, plasma pretreated specimens exhibited higher SEA values close to 9 Jm2/kg due to better IPMC. Combined with the FEM simulation results, the interface played a role in stress transmission and specimens with better IPMC enabled the laminates to absorb more energy.
Open AccessLow-Velocity Impact Resistance of Al/Gf/PP Laminates with Different Interface Performance
The weak interface performance between metal and composite (IPMC) makes the composite materials susceptible to impact load. Aluminum/glass fiber/polypropylene (Al/Gf/PP) laminates were manufactured with the aluminum alloy sheets modified by nitrogen plasma surface treatment and the phosphoric acid anodizing method, respectively. FEM models of Al/Gf/PP laminates under low-velocity impact were established in ABAQUS/Explicit based on the generated data including the model I and II interlaminar fracture toughness. Low-velocity impact tests were performed to investigate the impact resistance of Al/Gf/PP laminates including load traces, failure mechanism, and energy absorption. The results showed that delamination was the main failure mode of two kinds of laminates under the impact energy of 20 J and 30 J. When the impact energy was between 40 J and 50 J, there were metal cracks on the rear surface of the plasma pretreated specimens, which possessed higher energy absorption and impact resistance, although the integrity of the laminates could not be preserved. Since the residual compressive stress was generated during the cooling process, the laminates were more susceptible to stretching rather than delamination. For impact energy (60 J) causing the through-the-thickness crack of two kinds of laminates, plasma pretreated specimens exhibited higher SEA values close to 9 Jm2/kg due to better IPMC. Combined with the FEM simulation results, the interface played a role in stress transmission and specimens with better IPMC enabled the laminates to absorb more energy.
- 20 September 2021
- Published by Wiley in Polymer Composites
- Vol. 42 (12) , 6523-6533
Residual stress variation and deformation of shot peened glass fiber reinforced composites/aluminum–lithium laminates under thermal shock and thermal fatigue
This paper aims to reveal the deformation mechanism of glass fiber reinforced composites (GFRP)/aluminum–lithium (Al–Li) laminates under thermal shock or fatigue and verify reliability of shot peen forming for the composites. In this study, residual stresses in laminate after shot peening was analyzed using finite element model, and the simulation results were verified by experiments. It was found that the shot peened laminates, compared with pure metal panel, similarly exhibited compressive stress at the two external metal surfaces and tensile stress in GFRP layer. The residual stresses changed discontinuously at the metal/fiber and 0°/90° fiber interface owing to the different modulus. Moreover, stresses generated during curing process significantly affected the final deformation after shot peening. Residual stresses altered in each layer with the increase of temperature from 0 to 100°C, which caused the arc height of the laminate decreased. However, the arc height increased to initial dimensions when the temperature dropped to 0°C. Thermal shock process was proved that it hardly influenced the sample geometry. The stress relaxation behaviors were found in long‐term thermal fatigue. 1100 cycles from −55 to 100°C, which lasted 4 h in every cycle, resulted in 5% decrease of the arc height. The deformation problem should be further concentrated on for components made of GFRP/Al–Li laminates and processed by shot peen forming technology.
- 20 September 2021
- Published by Wiley in Polymer Composites
- Vol. 42 (12) , 6523-6533
Residual stress variation and deformation of shot peened glass fiber reinforced composites/aluminum–lithium laminates under thermal shock and thermal fatigue
This paper aims to reveal the deformation mechanism of glass fiber reinforced composites (GFRP)/aluminum–lithium (Al–Li) laminates under thermal shock or fatigue and verify reliability of shot peen forming for the composites. In this study, residual stresses in laminate after shot peening was analyzed using finite element model, and the simulation results were verified by experiments. It was found that the shot peened laminates, compared with pure metal panel, similarly exhibited compressive stress at the two external metal surfaces and tensile stress in GFRP layer. The residual stresses changed discontinuously at the metal/fiber and 0°/90° fiber interface owing to the different modulus. Moreover, stresses generated during curing process significantly affected the final deformation after shot peening. Residual stresses altered in each layer with the increase of temperature from 0 to 100°C, which caused the arc height of the laminate decreased. However, the arc height increased to initial dimensions when the temperature dropped to 0°C. Thermal shock process was proved that it hardly influenced the sample geometry. The stress relaxation behaviors were found in long‐term thermal fatigue. 1100 cycles from −55 to 100°C, which lasted 4 h in every cycle, resulted in 5% decrease of the arc height. The deformation problem should be further concentrated on for components made of GFRP/Al–Li laminates and processed by shot peen forming technology.
- Open Access
- 1 April 2020
- Published by IOP Publishing in Materials Research Express
- Vol. 7 (4) , 046509
Effect of pre-deformation and artificial aging on fatigue life of 2198 Al-Li alloy
The effects of pre-deformation and artificial aging on fatigue life of 2198 Al-Li alloy were explored to further reveal its fatigue behavior and improve the damage tolerance. Fatigue life was investigated on 2198-T3 alloy after pre-deformation and aging treatments. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were used to study the fracture morphology, precipitation behavior, fatigue crack initiation and propagation. Results indicated that T1 (Al2CuLi) phase dominated the strengthening of 2198-T3 alloy after the further aging. Pre-deformation increased the number of dislocations in the matrix, which provided favorable position for nucleation of T1. The precipitation of θ′ (Al2Cu) and δ′ (Al3Li) were inhibited. Also, the formation and coarsening of precipitate-free zone (PFZ) were effectively avoided in this condition. Dislocation density in the 2198 Al-Li alloy matrix increased with the amount of pre-deformation, leading to an increase in micro-crack defects on the surface and inside alloy. As a result, decreased fatigue life and an increased crack growth rate of the alloy were observed. Overall, 2198 Al-Li alloy had the best fatigue life and damage tolerance enhancement after it underwent 3% pre-deformation and was aged at 155 °C for 15 h.
- 1 April 2020
- Published by IOP Publishing in Materials Research Express
- Vol. 7 (4) , 046509
Open AccessEffect of pre-deformation and artificial aging on fatigue life of 2198 Al-Li alloy
The effects of pre-deformation and artificial aging on fatigue life of 2198 Al-Li alloy were explored to further reveal its fatigue behavior and improve the damage tolerance. Fatigue life was investigated on 2198-T3 alloy after pre-deformation and aging treatments. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were used to study the fracture morphology, precipitation behavior, fatigue crack initiation and propagation. Results indicated that T1 (Al2CuLi) phase dominated the strengthening of 2198-T3 alloy after the further aging. Pre-deformation increased the number of dislocations in the matrix, which provided favorable position for nucleation of T1. The precipitation of θ′ (Al2Cu) and δ′ (Al3Li) were inhibited. Also, the formation and coarsening of precipitate-free zone (PFZ) were effectively avoided in this condition. Dislocation density in the 2198 Al-Li alloy matrix increased with the amount of pre-deformation, leading to an increase in micro-crack defects on the surface and inside alloy. As a result, decreased fatigue life and an increased crack growth rate of the alloy were observed. Overall, 2198 Al-Li alloy had the best fatigue life and damage tolerance enhancement after it underwent 3% pre-deformation and was aged at 155 °C for 15 h.
- 24 May 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (8) , 0865b2
Spring-back and failure characteristics of roll bending of GLARE laminates
- 24 May 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (8) , 0865b2
Spring-back and failure characteristics of roll bending of GLARE laminates
- 25 March 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (7) , 076527
Flow behaviors of 22MnB5 steel at a high temperature
Flow behaviors of 22MnB5 ultra-high strength steel (UHSS) at different temperatures and strain rates were investigated using uniaxial tension tests. The variables of the Arrhenius model, which involved n, Q, α, and lnA, was calculated using a fifth order polynomial fitting method. At a strain of 0.1, the values of n, Q, α, and lnA were respectively 8.24579, 177.7588 kJmol-1, 0.00618 MPa-1, and 25.77352 s-1. The results indicate that the change in rheological stress was inversely proportional to the change in temperature but was positively correlated with the change in strain rate. The new model reproduced the flow behaviors of this novel UHSS sheet well for a wide range of strain rates and temperature conditions.
- 25 March 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (7) , 076527
Flow behaviors of 22MnB5 steel at a high temperature
Flow behaviors of 22MnB5 ultra-high strength steel (UHSS) at different temperatures and strain rates were investigated using uniaxial tension tests. The variables of the Arrhenius model, which involved n, Q, α, and lnA, was calculated using a fifth order polynomial fitting method. At a strain of 0.1, the values of n, Q, α, and lnA were respectively 8.24579, 177.7588 kJmol-1, 0.00618 MPa-1, and 25.77352 s-1. The results indicate that the change in rheological stress was inversely proportional to the change in temperature but was positively correlated with the change in strain rate. The new model reproduced the flow behaviors of this novel UHSS sheet well for a wide range of strain rates and temperature conditions.
- 24 January 2018
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 96 (1-4) , 587-596
The feasibility research on shot-peen forming of the novel fiber metal laminates based on aluminum-lithium alloy
- 24 January 2018
- Published by Springer Nature in The International Journal of Advanced Manufacturing Technology
- Vol. 96 (1-4) , 587-596
The feasibility research on shot-peen forming of the novel fiber metal laminates based on aluminum-lithium alloy