Marie Collin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Marie Collin has a total of 93 co-authors. Here are the top co-authors by number of shared publications:
- Torben Gädt
Chair for the Chemistry of Construction Materials, TUM School of Natural Sciences, Technical University of Munich, Garching, Germany
8 shared publications Kirk Ellison
Electric Power Research Institute Charlotte North Carolina USA
6 shared publicationsDale P. Prentice
Laboratory for the Chemistry of Construction Materials (LC2) Department of Civil and Environmental Engineering University of California Los Angeles California USA
5 shared publications- Dante Simonetti
University of California, Los Angeles
4 shared publications - Gaurav Sant
University of California, Los Angeles
4 shared publications - Maxime Fournier
CEA, DEN, DE2D, Univ. Montpellier, Marcoule, France
4 shared publications
Latest Publications
- Open Access
- 16 September 2026
- Published by Elsevier in Cement and Concrete Research
- Vol. 210
Comparing polycarboxylate and -phosphate ethers as stabilizers for C-S-H based cement accelerators
- 16 September 2026
- Published by Elsevier in Cement and Concrete Research
- Vol. 210
Open AccessComparing polycarboxylate and -phosphate ethers as stabilizers for C-S-H based cement accelerators
- 3 April 2026
- Published by Agence Bibliographique de l'Enseignement Supérieur
Géochimie en milieu nanoporeux : application aux verres nucléaires
Ce travail de thèse s’intéresse aux interactions entre la solution et la pellicule d’altération, appelée gel, qui se forme lors de la lixiviation des verres borosilicatés d’intérêt nucléaire, et plus spécifiquement dans ce travail, sur le verre à six oxydes ISG. Afin de mieux comprendre les mécanismes de formation du gel, ainsi que ses propriétés de passivation, une étude combinant analyses expérimentales et simulations de dynamique moléculaire (DM) est réalisée.Dans un premier temps, l’étude se focalise sur la structure du verre sain dans le but de mieux appréhender les processus de lixiviation. Pour ce faire, des analyses par spectroscopie RMN sont réalisées. Les résultats sont comparés à ceux obtenus par DM afin de valider la simulation. Cette dernière permet alors une exploration complète de l’ordre à courte et moyenne distances. Elle montre en outre une distribution homogène des formateurs de réseau et l’absence de zones enrichies en bore. Ce dernier, que l’on sait fortement soluble, a tendance à fragmenter le réseau silicaté, affectant de ce fait sa réactivité.Les processus de formation du gel sont ensuite étudiés expérimentalement, dans des conditions favorisant la passivation (90 °C, pH 7, solution saturée en silice). Nous mettons en évidence un fort effet des éléments exogènes en solution, notamment les alcalins faiblement hydratés tels que le potassium et le césium. Ces derniers entrainent ainsi une chute marquée de l’altération du verre. Afin de comprendre cet effet, les gels formés en présence de différents alcalins sont caractérisés. Les analyses montrent un départ congruent du bore et du sodium, et une incorporation du potassium et du césium de la solution qui prennent le rôle de compensateur de charge des unités [AlO4]- assuré par le calcium dans les gels formés en milieux sans alcalin ou contenant des alcalins fortement hydraté comme le lithium ou le sodium. Les différents gels présentent des degrés d’hydratation variés, en accord avec les résultats de simulation de DM de la diffusion de l’eau dans une silice nanoporeuse en milieu alcalin. Ces simulations montrent que la combinaison d’effets stériques (taille des alcalins) et physico-chimiques (énergie d’hydratation) entraine une diminution de la quantité d’eau dans les porosités contenant des ions potassium ou césium.Par ailleurs, les différents gels obtenus dans les conditions d’altération précitées sont fortement polymérisés, indiquant une réorganisation du réseau silicaté à la suite du départ des éléments facilement hydrolysables comme le bore. Cette réorganisation a lieu sans hydrolyse complète des tétraèdres de silicium, ce qui invalide dans ce cas le modèle de formation des gels par dissolution congruente/précipitation. La spéciation de l’eau au sein du gel, obtenue en combinant ATG et RMN du proton, permet de plus de déterminer quantitativement la répartition des atomes d’oxygène au sein du gel (atomes d’oxygène pontants, non pontants ou H2O).Ces données sont alors utilisées pour l’interprétation d’expériences de traçage en milieu enrichi en eau marquée en 18O d’échantillons pré-altérés. Ces expériences, menées à différentes températures, mettent en évidence pour la première fois une réorganisation continue du réseau du gel, avec une diminution au cours du temps de l’accessibilité des espèces mobiles (H2O et hydroxyles) au verre sain du fait de la maturation de la porosité au sein du gel. Nous déterminons différentes diffusivités pour l’eau en fonction de la topologie du gel et proposons l’hypothèse que cette atténuation progressive de la réactivité du réseau soit à l’origine du caractère passivant du gel.
- 3 April 2026
- Published by Agence Bibliographique de l'Enseignement Supérieur
Géochimie en milieu nanoporeux : application aux verres nucléaires
Ce travail de thèse s’intéresse aux interactions entre la solution et la pellicule d’altération, appelée gel, qui se forme lors de la lixiviation des verres borosilicatés d’intérêt nucléaire, et plus spécifiquement dans ce travail, sur le verre à six oxydes ISG. Afin de mieux comprendre les mécanismes de formation du gel, ainsi que ses propriétés de passivation, une étude combinant analyses expérimentales et simulations de dynamique moléculaire (DM) est réalisée.Dans un premier temps, l’étude se focalise sur la structure du verre sain dans le but de mieux appréhender les processus de lixiviation. Pour ce faire, des analyses par spectroscopie RMN sont réalisées. Les résultats sont comparés à ceux obtenus par DM afin de valider la simulation. Cette dernière permet alors une exploration complète de l’ordre à courte et moyenne distances. Elle montre en outre une distribution homogène des formateurs de réseau et l’absence de zones enrichies en bore. Ce dernier, que l’on sait fortement soluble, a tendance à fragmenter le réseau silicaté, affectant de ce fait sa réactivité.Les processus de formation du gel sont ensuite étudiés expérimentalement, dans des conditions favorisant la passivation (90 °C, pH 7, solution saturée en silice). Nous mettons en évidence un fort effet des éléments exogènes en solution, notamment les alcalins faiblement hydratés tels que le potassium et le césium. Ces derniers entrainent ainsi une chute marquée de l’altération du verre. Afin de comprendre cet effet, les gels formés en présence de différents alcalins sont caractérisés. Les analyses montrent un départ congruent du bore et du sodium, et une incorporation du potassium et du césium de la solution qui prennent le rôle de compensateur de charge des unités [AlO4]- assuré par le calcium dans les gels formés en milieux sans alcalin ou contenant des alcalins fortement hydraté comme le lithium ou le sodium. Les différents gels présentent des degrés d’hydratation variés, en accord avec les résultats de simulation de DM de la diffusion de l’eau dans une silice nanoporeuse en milieu alcalin. Ces simulations montrent que la combinaison d’effets stériques (taille des alcalins) et physico-chimiques (énergie d’hydratation) entraine une diminution de la quantité d’eau dans les porosités contenant des ions potassium ou césium.Par ailleurs, les différents gels obtenus dans les conditions d’altération précitées sont fortement polymérisés, indiquant une réorganisation du réseau silicaté à la suite du départ des éléments facilement hydrolysables comme le bore. Cette réorganisation a lieu sans hydrolyse complète des tétraèdres de silicium, ce qui invalide dans ce cas le modèle de formation des gels par dissolution congruente/précipitation. La spéciation de l’eau au sein du gel, obtenue en combinant ATG et RMN du proton, permet de plus de déterminer quantitativement la répartition des atomes d’oxygène au sein du gel (atomes d’oxygène pontants, non pontants ou H2O).Ces données sont alors utilisées pour l’interprétation d’expériences de traçage en milieu enrichi en eau marquée en 18O d’échantillons pré-altérés. Ces expériences, menées à différentes températures, mettent en évidence pour la première fois une réorganisation continue du réseau du gel, avec une diminution au cours du temps de l’accessibilité des espèces mobiles (H2O et hydroxyles) au verre sain du fait de la maturation de la porosité au sein du gel. Nous déterminons différentes diffusivités pour l’eau en fonction de la topologie du gel et proposons l’hypothèse que cette atténuation progressive de la réactivité du réseau soit à l’origine du caractère passivant du gel.
- 27 February 2026
- Published by Elsevier in Journal of Membrane Science
- Vol. 747
Unveiling Structure–Performance relationships in nanofiltration membranes via mechanistic sensitivity analysis
- 27 February 2026
- Published by Elsevier in Journal of Membrane Science
- Vol. 747
Unveiling Structure–Performance relationships in nanofiltration membranes via mechanistic sensitivity analysis
- Open Access
- 23 January 2026
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (1)
Mechanistic insights into the anion‐driven suppression of the initial cement reaction of tricalcium aluminate
The hydration process of ordinary Portland cement (OPC) involves intricate interactions among ions in the pore solution, dissolving clinker phases, and precipitating hydrates. Tricalcium aluminate () shows the highest reactivity of the cement clinker phases during the initial hydration stages of OPC. The kinetic control of this reaction is of fundamental importance. In commercial OPC, cement producers add calcium sulfates to suppress the initial reactivity of . Dissolution suppression strongly depends on the chemical nature of the added anion. This study explores the early hydration behavior of in the presence of three sodium salts (NaCl, , and ) using in situ isothermal calorimetry and in situ X‐ray diffraction. Among the sodium salts studied, phosphate exhibits the strongest inhibition of early hydration, followed by sulfate and chloride. The experimental data are combined with two theoretical methods: thermodynamic modeling and molecular dynamics simulations. The molecular dynamics simulation implies the very fast formation of a hydroxyapatite‐like surface layer on the surface. It also yields the interfacial tensions of the salt‐containing systems, which corresponds to the experimentally observed order. Time‐dependent thermodynamic modeling of the hydrating systems provides insights into the equilibrium phase composition. This work can provide pathways for further studies bridging experimental in situ methods and theoretical approaches such as all‐atom molecular simulations and thermodynamic modeling.
- 23 January 2026
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 109 (1)
Open AccessMechanistic insights into the anion‐driven suppression of the initial cement reaction of tricalcium aluminate
The hydration process of ordinary Portland cement (OPC) involves intricate interactions among ions in the pore solution, dissolving clinker phases, and precipitating hydrates. Tricalcium aluminate () shows the highest reactivity of the cement clinker phases during the initial hydration stages of OPC. The kinetic control of this reaction is of fundamental importance. In commercial OPC, cement producers add calcium sulfates to suppress the initial reactivity of . Dissolution suppression strongly depends on the chemical nature of the added anion. This study explores the early hydration behavior of in the presence of three sodium salts (NaCl, , and ) using in situ isothermal calorimetry and in situ X‐ray diffraction. Among the sodium salts studied, phosphate exhibits the strongest inhibition of early hydration, followed by sulfate and chloride. The experimental data are combined with two theoretical methods: thermodynamic modeling and molecular dynamics simulations. The molecular dynamics simulation implies the very fast formation of a hydroxyapatite‐like surface layer on the surface. It also yields the interfacial tensions of the salt‐containing systems, which corresponds to the experimentally observed order. Time‐dependent thermodynamic modeling of the hydrating systems provides insights into the equilibrium phase composition. This work can provide pathways for further studies bridging experimental in situ methods and theoretical approaches such as all‐atom molecular simulations and thermodynamic modeling.
- Open Access
- 26 June 2025
- Published by Elsevier in Cement and Concrete Research
- Vol. 197
Citric, tartaric, and succinic acid effects on C3S dissolution and the nucleation kinetics of C-S-H and portlandite
- 26 June 2025
- Published by Elsevier in Cement and Concrete Research
- Vol. 197
Open AccessCitric, tartaric, and succinic acid effects on C3S dissolution and the nucleation kinetics of C-S-H and portlandite
- Open Access
- 25 April 2025
- Published by Wiley in Chemistry – A European Journal
- Vol. 31 (27) , e202500207
Influence of Polymeric Dispersants on the Dissolution Rate of Tricalcium Silicate and the Nucleation of Calcium‐Silicate‐Hydrate and Portlandite
Polycarboxylate ether (PCE) and polyphosphate ether (PPE) dispersants (also known as superplasticizers) are indispensable components of modern concrete mix designs. They reduce the yield stress of cement suspensions and thereby facilitate the reduction of the water‐to‐cement ratio. However, PCEs and PPEs also cause retardation of the cement hydration as a secondary effect, which causes delayed concrete strength development. It is proposed that the retardation is caused by the polymer influence on the tricalcium silicate dissolution rate and the crystallization of the hydration products (e.g., calcium hydroxide Ca(OH) and calcium‐silicate‐hydrate or C‐S‐H). This study examines the effect of four different polymeric superplasticizers with carboxylate and phosphate groups on the reaction kinetics of the pure cement phase tricalcium silicate (in cement shorthand ). Our results confirm the strong retarding effect of the polymers on the hydration reaction of the paste. Based on model experiments, we studied the polymer influence on the dissolution of and the nucleation of the hydration products. We observed no dissolution‐inhibiting effect of the polymers at the chosen concentrations and undersaturation. However, such an inhibiting effect may occur at solution conditions closer to the saturation limit. Titrimetric analyses indicate that all polymers suppress the nucleation of portlandite and C‐S‐H, with a higher polymer charge density leading to a more pronounced inhibition.
- 25 April 2025
- Published by Wiley in Chemistry – A European Journal
- Vol. 31 (27) , e202500207
Open AccessInfluence of Polymeric Dispersants on the Dissolution Rate of Tricalcium Silicate and the Nucleation of Calcium‐Silicate‐Hydrate and Portlandite
Polycarboxylate ether (PCE) and polyphosphate ether (PPE) dispersants (also known as superplasticizers) are indispensable components of modern concrete mix designs. They reduce the yield stress of cement suspensions and thereby facilitate the reduction of the water‐to‐cement ratio. However, PCEs and PPEs also cause retardation of the cement hydration as a secondary effect, which causes delayed concrete strength development. It is proposed that the retardation is caused by the polymer influence on the tricalcium silicate dissolution rate and the crystallization of the hydration products (e.g., calcium hydroxide Ca(OH) and calcium‐silicate‐hydrate or C‐S‐H). This study examines the effect of four different polymeric superplasticizers with carboxylate and phosphate groups on the reaction kinetics of the pure cement phase tricalcium silicate (in cement shorthand ). Our results confirm the strong retarding effect of the polymers on the hydration reaction of the paste. Based on model experiments, we studied the polymer influence on the dissolution of and the nucleation of the hydration products. We observed no dissolution‐inhibiting effect of the polymers at the chosen concentrations and undersaturation. However, such an inhibiting effect may occur at solution conditions closer to the saturation limit. Titrimetric analyses indicate that all polymers suppress the nucleation of portlandite and C‐S‐H, with a higher polymer charge density leading to a more pronounced inhibition.
- Open Access
- 7 November 2024
- Published by American Chemical Society (ACS) in ChemRxiv
Calcium Aluminate Cement Hydration Under the Influence of Mineral Acids
In technical mortars and refractory concrete, the reactivity of calcium aluminate cement (CAC) is typically controlled by retarders and accelerators. This study examines the retarding impact of five strong acids (HCl, HNO3, HClO4, H2SO4, and H3PO4) on CAC hydration (1) in dilute suspensions at a water-to-solid (w/s) ratio of 100, and (2) in pastes at a w/s of 0.3. Doing so, we identified several factors that affect the dissolution and hydration of CAC. In dilute suspensions, in-situ monitoring of the pH and conductivity reveals that the acids delay the initial dissolution of monocalcium aluminate (CA). The inhibition time depends exponentially on the proton concentration, and linearly on the available CA surface area, which is partially explained by the preferential formation of Al(OH)3 suggested by thermodynamic modeling. Notably, the acids’ efficiency varies at equimolar proton dosages. For H3PO4, we explain the outstanding inhibition efficiency by the joint formation of hydroxylapatite and Al(OH)3. For the other acids, the dissolution inhibition power follows an anion-specific sequence sulfate > chloride > nitrate > perchlorate, which aligns with the Hofmeister series and suggests a stabilization of calcium ion solvation by the anion. Isothermal calorimetry experiments performed on pastes show that the retardation order of these acids (H3PO4 > HClO4 > HNO3 > H2SO4 > HCl) differs from that observed at w/s of 100. Phosphoric acid still displays exceptional retardation properties suggesting a unique mechanism of action most likely related to early hydroxylapatite and Al(OH)3 formation. For the other acids, Al(OH)3 and anion-containing AFm phases formation may explain the differences in retardation maximum.
- 7 November 2024
- Published by American Chemical Society (ACS) in ChemRxiv
Open AccessCalcium Aluminate Cement Hydration Under the Influence of Mineral Acids
In technical mortars and refractory concrete, the reactivity of calcium aluminate cement (CAC) is typically controlled by retarders and accelerators. This study examines the retarding impact of five strong acids (HCl, HNO3, HClO4, H2SO4, and H3PO4) on CAC hydration (1) in dilute suspensions at a water-to-solid (w/s) ratio of 100, and (2) in pastes at a w/s of 0.3. Doing so, we identified several factors that affect the dissolution and hydration of CAC. In dilute suspensions, in-situ monitoring of the pH and conductivity reveals that the acids delay the initial dissolution of monocalcium aluminate (CA). The inhibition time depends exponentially on the proton concentration, and linearly on the available CA surface area, which is partially explained by the preferential formation of Al(OH)3 suggested by thermodynamic modeling. Notably, the acids’ efficiency varies at equimolar proton dosages. For H3PO4, we explain the outstanding inhibition efficiency by the joint formation of hydroxylapatite and Al(OH)3. For the other acids, the dissolution inhibition power follows an anion-specific sequence sulfate > chloride > nitrate > perchlorate, which aligns with the Hofmeister series and suggests a stabilization of calcium ion solvation by the anion. Isothermal calorimetry experiments performed on pastes show that the retardation order of these acids (H3PO4 > HClO4 > HNO3 > H2SO4 > HCl) differs from that observed at w/s of 100. Phosphoric acid still displays exceptional retardation properties suggesting a unique mechanism of action most likely related to early hydroxylapatite and Al(OH)3 formation. For the other acids, Al(OH)3 and anion-containing AFm phases formation may explain the differences in retardation maximum.
- Open Access
- 10 October 2024
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 12 (43) , 15762-15787
ZeroCAL: Eliminating Carbon Dioxide Emissions from Limestone’s Decomposition to Decarbonize Cement Production
Limestone (calcite, CaCO3) is an abundant and cost-effective source of calcium oxide (CaO) for cement and lime production. However, the thermochemical decomposition of limestone (∼800 °C, 1 bar) to produce lime (CaO) results in substantial carbon dioxide (CO2(g)) emissions and energy use, i.e., ∼1 tonne [t] of CO2 and ∼1.4 MWh per t of CaO produced. Here, we describe a new pathway to use CaCO3 as a Ca source to make hydrated lime (portlandite, Ca(OH)2) at ambient conditions (p, T)-while nearly eliminating process CO2(g) emissions (as low as 1.5 mol. % of the CO2 in the precursor CaCO3, equivalent to 9 kg of CO2(g) per t of Ca(OH)2)-within an aqueous flow-electrolysis/pH-swing process that coproduces hydrogen (H2(g)) and oxygen (O2(g)). Because Ca(OH)2 is a zero-carbon precursor for cement and lime production, this approach represents a significant advancement in the production of zero-carbon cement. The Zero CArbon Lime (ZeroCAL) process includes dissolution, separation/recovery, and electrolysis stages according to the following steps: (Step 1) chelator (e.g., ethylenediaminetetraacetic acid, EDTA)-promoted dissolution of CaCO3 and complexation of Ca2+ under basic (>pH 9) conditions, (Step 2a) Ca enrichment and separation using nanofiltration (NF), which allows separation of the Ca-EDTA complex from the accompanying bicarbonate (HCO3 -) species, (Step 2b) acidity-promoted decomplexation of Ca from EDTA, which allows near-complete chelator recovery and the formation of a Ca-enriched stream, and (Step 3) rapid precipitation of Ca(OH)2 from the Ca-enriched stream using electrolytically produced alkalinity. These reactions can be conducted in a seawater matrix yielding coproducts including hydrochloric acid (HCl) and sodium bicarbonate (NaHCO3), resulting from electrolysis and limestone dissolution, respectively. Careful analysis of the reaction stoichiometries and energy balances indicates that approximately 1.35 t of CaCO3, 1.09 t of water, 0.79 t of sodium chloride (NaCl), and ∼2 MWh of electrical energy are required to produce 1 t of Ca(OH)2, with significant opportunity for process intensification. This approach has major implications for decarbonizing cement production within a paradigm that emphasizes the use of existing cement plants and electrification of industrial operations, while also creating approaches for alkalinity production that enable cost-effective and scalable CO2 mineralization via Ca(OH)2 carbonation.
- 10 October 2024
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 12 (43) , 15762-15787
Open AccessZeroCAL: Eliminating Carbon Dioxide Emissions from Limestone’s Decomposition to Decarbonize Cement Production
Limestone (calcite, CaCO3) is an abundant and cost-effective source of calcium oxide (CaO) for cement and lime production. However, the thermochemical decomposition of limestone (∼800 °C, 1 bar) to produce lime (CaO) results in substantial carbon dioxide (CO2(g)) emissions and energy use, i.e., ∼1 tonne [t] of CO2 and ∼1.4 MWh per t of CaO produced. Here, we describe a new pathway to use CaCO3 as a Ca source to make hydrated lime (portlandite, Ca(OH)2) at ambient conditions (p, T)-while nearly eliminating process CO2(g) emissions (as low as 1.5 mol. % of the CO2 in the precursor CaCO3, equivalent to 9 kg of CO2(g) per t of Ca(OH)2)-within an aqueous flow-electrolysis/pH-swing process that coproduces hydrogen (H2(g)) and oxygen (O2(g)). Because Ca(OH)2 is a zero-carbon precursor for cement and lime production, this approach represents a significant advancement in the production of zero-carbon cement. The Zero CArbon Lime (ZeroCAL) process includes dissolution, separation/recovery, and electrolysis stages according to the following steps: (Step 1) chelator (e.g., ethylenediaminetetraacetic acid, EDTA)-promoted dissolution of CaCO3 and complexation of Ca2+ under basic (>pH 9) conditions, (Step 2a) Ca enrichment and separation using nanofiltration (NF), which allows separation of the Ca-EDTA complex from the accompanying bicarbonate (HCO3 -) species, (Step 2b) acidity-promoted decomplexation of Ca from EDTA, which allows near-complete chelator recovery and the formation of a Ca-enriched stream, and (Step 3) rapid precipitation of Ca(OH)2 from the Ca-enriched stream using electrolytically produced alkalinity. These reactions can be conducted in a seawater matrix yielding coproducts including hydrochloric acid (HCl) and sodium bicarbonate (NaHCO3), resulting from electrolysis and limestone dissolution, respectively. Careful analysis of the reaction stoichiometries and energy balances indicates that approximately 1.35 t of CaCO3, 1.09 t of water, 0.79 t of sodium chloride (NaCl), and ∼2 MWh of electrical energy are required to produce 1 t of Ca(OH)2, with significant opportunity for process intensification. This approach has major implications for decarbonizing cement production within a paradigm that emphasizes the use of existing cement plants and electrification of industrial operations, while also creating approaches for alkalinity production that enable cost-effective and scalable CO2 mineralization via Ca(OH)2 carbonation.
- Open Access
- 24 September 2024
- Published by American Chemical Society (ACS) in ChemRxiv
Citric, Tartaric, and Succinic Acid Effects on C3S Dissolution and the Nucleation Kinetics of C-S-H and Portlandite
Functional additives like carboxylic acids modify the hydration mechanism of Portland cement and are commonly used as set retarders. These retarders can affect the clinker phase dissolution and the crystallization of hydrate phases. However, their specific effects are not fully understood. This study focuses on understanding the role of citric, tartaric, and succinic acid in the dissolution of tricalcium silicate (C3S) and the crystallization of C-S-H and portlandite. The results reveal that these acids accelerate C3S dissolution, while their sodium salts exhibit minimal effects at high undersaturation. At low undersaturation, citrate reduces the dissolution rate by 50%, and tartrate can fully suppress dissolution in the model experiment. Potentiometric titration studies reveal that the additives inhibit the nucleation and crystal growth of C-S-H and portlandite by stabilizing prenucleation clusters. In summary, the additives’ relative impact on dissolution and crystallization suggests that the retarding effect of citric and tartaric acid is predominantly caused by the inhibition of nucleation and crystal growth.
- 24 September 2024
- Published by American Chemical Society (ACS) in ChemRxiv
Open AccessCitric, Tartaric, and Succinic Acid Effects on C3S Dissolution and the Nucleation Kinetics of C-S-H and Portlandite
Functional additives like carboxylic acids modify the hydration mechanism of Portland cement and are commonly used as set retarders. These retarders can affect the clinker phase dissolution and the crystallization of hydrate phases. However, their specific effects are not fully understood. This study focuses on understanding the role of citric, tartaric, and succinic acid in the dissolution of tricalcium silicate (C3S) and the crystallization of C-S-H and portlandite. The results reveal that these acids accelerate C3S dissolution, while their sodium salts exhibit minimal effects at high undersaturation. At low undersaturation, citrate reduces the dissolution rate by 50%, and tartrate can fully suppress dissolution in the model experiment. Potentiometric titration studies reveal that the additives inhibit the nucleation and crystal growth of C-S-H and portlandite by stabilizing prenucleation clusters. In summary, the additives’ relative impact on dissolution and crystallization suggests that the retarding effect of citric and tartaric acid is predominantly caused by the inhibition of nucleation and crystal growth.