Hua-Feng Fei
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Hua-Feng Fei has a total of 65 co-authors. Here are the top co-authors by number of shared publications:
Bin Huang
Institute of Chemistry, Chinese Academy of Sciences
14 shared publicationsZhijie Zhang
Institute of Chemistry, Chinese Academy of Sciences
12 shared publications- Benjamin M. Yavitt
University of Cincinnati
8 shared publications Yan Zhao
Key Laboratory of Science and Technology on High‐tech Polymer Materials Institute of Chemistry, Chinese Academy of Sciences Beijing People's Republic of China
8 shared publications- James J. Watkins
Conte Center for Polymer Research, Department of Polymer Science and Engineering, University of Massachusetts, Amherst, Massachusetts 01003, USA
7 shared publications Yan Yu
Key Laboratory of Science and Technology on High‐Tech Polymer Materials, Institute of Chemistry Chinese Academy of Sciences Beijing China
7 shared publications
Latest Publications
- 30 September 2026
- Published by American Chemical Society (ACS) in Chemistry of Materials
- Vol. 38 (19) , 10308-10318
High-Damping Elastomers Enabled by Precise Regulation of Polyborosiloxane Relaxation Behaviors
Viscoelastic polymer materials exhibiting high damping capacity within a specified frequency–temperature range effectively dissipate mechanical energy as heat, thereby mitigating damage induced by vibrations and impact loads. However, developing a convenient method for precisely designing damping materials with tunable energy dissipation properties across a desired frequency–temperature range remains challenging. Herein, we present a strategy for fabricating high-damping polyborosiloxane (PBS) elastomers (PBSEs) with tunable damping performance across a specified frequency–temperature range. This is achieved by precisely modulating the PBS relaxation behavior─specifically, through systematic variation of both the B–O bond content and the molecular weight of the PDMS diol precursors. We found that the resultant PBSEs exhibit controllable high-damping performance across an ultrawide frequency range (tan δ > 0.3, 10–3 to 102 Hz) and temperature range (tan δ = 0.5–0.6, −20 to 150 °C). Moreover, PBSEs exhibit excellent impact-protective performance compared with commercial materials and attenuate impact force by more than 95%. This unique design concept will provide a convenient approach to developing advanced damping materials.
- 30 September 2026
- Published by American Chemical Society (ACS) in Chemistry of Materials
- Vol. 38 (19) , 10308-10318
High-Damping Elastomers Enabled by Precise Regulation of Polyborosiloxane Relaxation Behaviors
Viscoelastic polymer materials exhibiting high damping capacity within a specified frequency–temperature range effectively dissipate mechanical energy as heat, thereby mitigating damage induced by vibrations and impact loads. However, developing a convenient method for precisely designing damping materials with tunable energy dissipation properties across a desired frequency–temperature range remains challenging. Herein, we present a strategy for fabricating high-damping polyborosiloxane (PBS) elastomers (PBSEs) with tunable damping performance across a specified frequency–temperature range. This is achieved by precisely modulating the PBS relaxation behavior─specifically, through systematic variation of both the B–O bond content and the molecular weight of the PDMS diol precursors. We found that the resultant PBSEs exhibit controllable high-damping performance across an ultrawide frequency range (tan δ > 0.3, 10–3 to 102 Hz) and temperature range (tan δ = 0.5–0.6, −20 to 150 °C). Moreover, PBSEs exhibit excellent impact-protective performance compared with commercial materials and attenuate impact force by more than 95%. This unique design concept will provide a convenient approach to developing advanced damping materials.
- 30 July 2026
- Published by Elsevier in Journal of Power Sources
- Vol. 692
Regulating solvation structure and interfacial chemistry in gel polymer electrolytes for stable lithium metal batteries
- 30 July 2026
- Published by Elsevier in Journal of Power Sources
- Vol. 692
Regulating solvation structure and interfacial chemistry in gel polymer electrolytes for stable lithium metal batteries
- 21 January 2026
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 143 (14)
Optimized Sol–Gel Synthesis of Elastic Silicone Resins With Balanced Thermal Stability and Mechanical Properties
Silicone rubber exhibits greater elasticity but poorer thermal stability than silicone resins, owing to its lower crosslinking density. Thus, this study introduces phenyltrimethoxysilane (PhTMS) into hydroxyl‐terminated polydimethylsiloxane (OH‐PDMS) through a sol–gel co‐hydrolysis and condensation approach, yielding elastic silicone resins (ESR) that combine the elasticity of silicone rubber with the thermal stability of silicone resins. The effects of PhTMS content and OH‐PDMS chain length on overall performance were systematically studied. The optimized ESR (5–300‐ESR‐v) showed a markedly higher T d5 (5% weight loss temperature) (389°C in air, 452°C in N 2 ) than OH‐PDMS‐v (350°C in air, 400°C in N 2 ), alongside superior mechanical performance and adhesive strength. Compared with traditional silicone resins, the resulting ESR are solvent‐free, low‐viscosity, and curable at room temperature, achieving an optimal balance of thermal stability, strength, and toughness. This makes them promising candidates for heat‐resistant materials.
- 21 January 2026
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 143 (14)
Optimized Sol–Gel Synthesis of Elastic Silicone Resins With Balanced Thermal Stability and Mechanical Properties
Silicone rubber exhibits greater elasticity but poorer thermal stability than silicone resins, owing to its lower crosslinking density. Thus, this study introduces phenyltrimethoxysilane (PhTMS) into hydroxyl‐terminated polydimethylsiloxane (OH‐PDMS) through a sol–gel co‐hydrolysis and condensation approach, yielding elastic silicone resins (ESR) that combine the elasticity of silicone rubber with the thermal stability of silicone resins. The effects of PhTMS content and OH‐PDMS chain length on overall performance were systematically studied. The optimized ESR (5–300‐ESR‐v) showed a markedly higher T d5 (5% weight loss temperature) (389°C in air, 452°C in N 2 ) than OH‐PDMS‐v (350°C in air, 400°C in N 2 ), alongside superior mechanical performance and adhesive strength. Compared with traditional silicone resins, the resulting ESR are solvent‐free, low‐viscosity, and curable at room temperature, achieving an optimal balance of thermal stability, strength, and toughness. This makes them promising candidates for heat‐resistant materials.
- Open Access
- 23 July 2025
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 13 (34) , 28100-28110
Viscoelasticity-controllable dynamic borate polydimethylsiloxane networks for enhancing energy dissipation of elastomers
A novel strategy has been developed to precisely enhance the energy dissipation performance of the PDMS double-network elastomers by modulating the viscoelastic properties of the dynamic borate PDMS network.
- 23 July 2025
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 13 (34) , 28100-28110
Open AccessViscoelasticity-controllable dynamic borate polydimethylsiloxane networks for enhancing energy dissipation of elastomers
A novel strategy has been developed to precisely enhance the energy dissipation performance of the PDMS double-network elastomers by modulating the viscoelastic properties of the dynamic borate PDMS network.
- Open Access
- 13 March 2025
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 10 (11) , 11516-11524
Lightweight Flexible and Efficient Electromagnetic Shielding Composites Based on Silver-Coated Glass Microspheres
Composites consisting of silicone rubber and conductive fillers are extensively utilized in electronic devices due to their high performance in the field of electromagnetic interference (EMI) shielding. Traditional electromagnetic shielding polymer composites often use metal fillers such as silver, which suffer from drawbacks such as high costs and increased density. This study details the synthesis of silver-coated glass microspheres (Ag@GMs) via an ethylene glycol activation method, followed by their application in the formulation of lightweight, flexible, and effective EMI shielding silicone rubber composites. The deposition of a silver coating on the surface of the glass microspheres promotes the constitution of three-dimensional conductive networks, achieving a maximum density of 1.83 g/cm3 and an electrical conductivity of 204.63 S/cm. At the core-shell interface of the silver-coated glass microspheres, interface polarization loss and the internal reflection of electromagnetic waves are significantly enhanced, resulting in the electromagnetic shielding efficiency of up to 120 dB. Moreover, the composite exhibits excellent bending resistance and aging stability, indicating its promising potential for EMI protection in wearable, smart, and precision electronic applications.
- 13 March 2025
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 10 (11) , 11516-11524
Open AccessLightweight Flexible and Efficient Electromagnetic Shielding Composites Based on Silver-Coated Glass Microspheres
Composites consisting of silicone rubber and conductive fillers are extensively utilized in electronic devices due to their high performance in the field of electromagnetic interference (EMI) shielding. Traditional electromagnetic shielding polymer composites often use metal fillers such as silver, which suffer from drawbacks such as high costs and increased density. This study details the synthesis of silver-coated glass microspheres (Ag@GMs) via an ethylene glycol activation method, followed by their application in the formulation of lightweight, flexible, and effective EMI shielding silicone rubber composites. The deposition of a silver coating on the surface of the glass microspheres promotes the constitution of three-dimensional conductive networks, achieving a maximum density of 1.83 g/cm3 and an electrical conductivity of 204.63 S/cm. At the core-shell interface of the silver-coated glass microspheres, interface polarization loss and the internal reflection of electromagnetic waves are significantly enhanced, resulting in the electromagnetic shielding efficiency of up to 120 dB. Moreover, the composite exhibits excellent bending resistance and aging stability, indicating its promising potential for EMI protection in wearable, smart, and precision electronic applications.
- 30 December 2024
- Published by American Chemical Society (ACS) in ACS Nano
- Vol. 19 (2) , 1884-1910
Opportunities in Bottlebrush Block Copolymers for Advanced Materials
Bottlebrush block copolymers (BBCPs) are a unique class of materials that contain a backbone with densely grafted and chemically distinct polymeric side chains. The nonlinear architecture of BBCPs provides numerous degrees of freedom in their preparation, including control over key parameters such as grafting density, side chain length, block arrangement, and overall molecular weight. This uniquely branched structure provides BBCPs with several important distinctions from their linear counterparts, including sterically induced side chain and backbone conformations, rapid and large self-assembled nanostructures, and reduced or eliminated entanglement effects (assuming sufficient grafting density and that the molecular weight of the side chains is below their respective entanglement molecular weight). These distinctions allow access to large domain sizes, very rapid assembly, and the ability to preferentially add additives and/or precursors to one domain, thereby enabling the efficient fabrication of a wide range of advanced materials and devices. BBCPs have been utilized to create finely controlled and well-ordered nanostructures for use in applications, such as photonic crystals, drug delivery systems, energy conversion, energy storage devices, and key components in surface coatings. To further deploy BBCPs as templates for the formation of precise nanostructures, having a thorough understanding of their synthesis, self-assembly, and templating is necessary. To explore and understand the self-assembly and subsequent applications of BBCPs, this review emphasizes the physics of self-assembly for BBCPs (including architectural, rheological, and thermodynamic considerations) and structure-property relationships between BBCPs and their resulting nanostructures. Lastly, we provide an overview of current research trends using BBCPs in energy storage, energy conversion, photonic, 3D printing, and drug delivery applications. We aim to provide researchers with the fundamentals of BBCP self-assembly in their use as nanostructured materials to continue their development of advanced materials.
- 30 December 2024
- Published by American Chemical Society (ACS) in ACS Nano
- Vol. 19 (2) , 1884-1910
Opportunities in Bottlebrush Block Copolymers for Advanced Materials
Bottlebrush block copolymers (BBCPs) are a unique class of materials that contain a backbone with densely grafted and chemically distinct polymeric side chains. The nonlinear architecture of BBCPs provides numerous degrees of freedom in their preparation, including control over key parameters such as grafting density, side chain length, block arrangement, and overall molecular weight. This uniquely branched structure provides BBCPs with several important distinctions from their linear counterparts, including sterically induced side chain and backbone conformations, rapid and large self-assembled nanostructures, and reduced or eliminated entanglement effects (assuming sufficient grafting density and that the molecular weight of the side chains is below their respective entanglement molecular weight). These distinctions allow access to large domain sizes, very rapid assembly, and the ability to preferentially add additives and/or precursors to one domain, thereby enabling the efficient fabrication of a wide range of advanced materials and devices. BBCPs have been utilized to create finely controlled and well-ordered nanostructures for use in applications, such as photonic crystals, drug delivery systems, energy conversion, energy storage devices, and key components in surface coatings. To further deploy BBCPs as templates for the formation of precise nanostructures, having a thorough understanding of their synthesis, self-assembly, and templating is necessary. To explore and understand the self-assembly and subsequent applications of BBCPs, this review emphasizes the physics of self-assembly for BBCPs (including architectural, rheological, and thermodynamic considerations) and structure-property relationships between BBCPs and their resulting nanostructures. Lastly, we provide an overview of current research trends using BBCPs in energy storage, energy conversion, photonic, 3D printing, and drug delivery applications. We aim to provide researchers with the fundamentals of BBCP self-assembly in their use as nanostructured materials to continue their development of advanced materials.
- 13 November 2024
- Published by Royal Society of Chemistry (RSC) in Green Chemistry
- Vol. 27 (1) , 155-162
DIPEA-induced Si–H activation of siloxane for hydrosilylation polymerization via metal-free photocatalysis
Although metal-free hydrosilylation of siloxanes is essential for the industrial preparation of organosilicon compounds due to its unique advantages, such as the avoidance of the use and residue of precious metals, efficient metal-free silicon hydrogenation reactions are still rare. Herein, we report a straightforward visible light-driven metal-free hydrosilylation reaction based on siloxanes and silicon vinyl groups, catalyzed by the synergistic effect of the organic photooxidation catalyst 2,4,6-tris(diphenylamino)-5-fluoroisophthalonitrile and the base N,N′-diisopropylethylamine, which undergo electron transfer and selectively induce Si–H activation during catalysis. After optimization, the silicon vinyl conversion rate in the hydrosilylation reaction exceeded 99% without using any traditional hydrogen atom transfer reagents. Mechanistic studies based on experimental data and theoretical calculations revealed that the reaction proceeds through a free radical reaction and is thermodynamically feasible. The proposed methodology efficiently affords linear polymer formation via a stepwise growth approach. Furthermore, it can crosslink commercial high-molecular-weight polyvinyl silicone oil with disiloxane, realizing the gelation of the material.
- 13 November 2024
- Published by Royal Society of Chemistry (RSC) in Green Chemistry
- Vol. 27 (1) , 155-162
DIPEA-induced Si–H activation of siloxane for hydrosilylation polymerization via metal-free photocatalysis
Although metal-free hydrosilylation of siloxanes is essential for the industrial preparation of organosilicon compounds due to its unique advantages, such as the avoidance of the use and residue of precious metals, efficient metal-free silicon hydrogenation reactions are still rare. Herein, we report a straightforward visible light-driven metal-free hydrosilylation reaction based on siloxanes and silicon vinyl groups, catalyzed by the synergistic effect of the organic photooxidation catalyst 2,4,6-tris(diphenylamino)-5-fluoroisophthalonitrile and the base N,N′-diisopropylethylamine, which undergo electron transfer and selectively induce Si–H activation during catalysis. After optimization, the silicon vinyl conversion rate in the hydrosilylation reaction exceeded 99% without using any traditional hydrogen atom transfer reagents. Mechanistic studies based on experimental data and theoretical calculations revealed that the reaction proceeds through a free radical reaction and is thermodynamically feasible. The proposed methodology efficiently affords linear polymer formation via a stepwise growth approach. Furthermore, it can crosslink commercial high-molecular-weight polyvinyl silicone oil with disiloxane, realizing the gelation of the material.
- 18 July 2024
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 6 (15) , 8918-8928
Ternary Siloxane Copolymers Based Tough Elastomer under Ultralow Temperatures Condition
- 18 July 2024
- Published by American Chemical Society (ACS) in ACS Applied Polymer Materials
- Vol. 6 (15) , 8918-8928
Ternary Siloxane Copolymers Based Tough Elastomer under Ultralow Temperatures Condition
- 3 January 2024
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 141 (13)
Kinetics and thermal properties of polydiethylsiloxane initiated by potassium trimethylsilanolate
This work reports the kinetics of anionic ring‐opening polymerization of hexaethylcyclotrisiloxane (D3Et) with potassium trimethylsilanolate as initiator and diglyme and N,N‐dimethylformamide (DMF) as promoters. The polymerization rate of D3Et is influenced by the nature of promoters and the reaction temperatures. With the use of DMF as a promoter, the polymerization activation energy is 107.89 kJ/mol, and the polymerization rate constant at 110°C is 0.08466 min−1 with [P]/[I] = 3.0. Gel permeation chromatography and 29Si NMR spectra showed that the intermolecular redistribution occurred during the late stage of polymerization, which facilitated the synthesis of high‐molecular‐weight polydiethylsiloxane (PDES). Differential scanning calorimetry analysis showed that PDES exhibited a glass transition temperature of −142°C and complex crystallization phenomena. Thermogravimetric analysis illustrated that the PDES that was prepared using this method had good thermal stability with onset decomposition temperatures of 483 and 452°C under nitrogen and air conditions, respectively. This work presents innovative approaches for achieving a more energy‐efficient synthesis of PDES to meet the demands of industrial‐scale production.
- 3 January 2024
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 141 (13)
Kinetics and thermal properties of polydiethylsiloxane initiated by potassium trimethylsilanolate
This work reports the kinetics of anionic ring‐opening polymerization of hexaethylcyclotrisiloxane (D3Et) with potassium trimethylsilanolate as initiator and diglyme and N,N‐dimethylformamide (DMF) as promoters. The polymerization rate of D3Et is influenced by the nature of promoters and the reaction temperatures. With the use of DMF as a promoter, the polymerization activation energy is 107.89 kJ/mol, and the polymerization rate constant at 110°C is 0.08466 min−1 with [P]/[I] = 3.0. Gel permeation chromatography and 29Si NMR spectra showed that the intermolecular redistribution occurred during the late stage of polymerization, which facilitated the synthesis of high‐molecular‐weight polydiethylsiloxane (PDES). Differential scanning calorimetry analysis showed that PDES exhibited a glass transition temperature of −142°C and complex crystallization phenomena. Thermogravimetric analysis illustrated that the PDES that was prepared using this method had good thermal stability with onset decomposition temperatures of 483 and 452°C under nitrogen and air conditions, respectively. This work presents innovative approaches for achieving a more energy‐efficient synthesis of PDES to meet the demands of industrial‐scale production.
- 27 November 2023
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 141 (8)
Effects of metal oxides on the dielectric and mechanical properties of silicone rubber composites
Polysiloxane dielectric elastomers have garnered a considerable deal of attention over the last decade due to their potential as electroactive soft materials. However, the intrinsic low dielectric constant of polysiloxanes has proven a serious limitation in their practical use. In this work, we controlled the dielectric properties of silicone rubber composites by changing the type and content of oxide fillers. The silicone‐based dielectric elastomers with a high dielectric constant (5.21@1 kHz), low modulus (1.62 MPa), and high elongation (1100%) were successfully obtained. The effects of different types of metal oxides on the dielectric properties and mechanical properties of the prepared composites are further explored. Due to their excellent comprehensive features, these types of materials are expected to be applied in capacitive sensors, actuators, generators, and beyond.
- 27 November 2023
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 141 (8)
Effects of metal oxides on the dielectric and mechanical properties of silicone rubber composites
Polysiloxane dielectric elastomers have garnered a considerable deal of attention over the last decade due to their potential as electroactive soft materials. However, the intrinsic low dielectric constant of polysiloxanes has proven a serious limitation in their practical use. In this work, we controlled the dielectric properties of silicone rubber composites by changing the type and content of oxide fillers. The silicone‐based dielectric elastomers with a high dielectric constant (5.21@1 kHz), low modulus (1.62 MPa), and high elongation (1100%) were successfully obtained. The effects of different types of metal oxides on the dielectric properties and mechanical properties of the prepared composites are further explored. Due to their excellent comprehensive features, these types of materials are expected to be applied in capacitive sensors, actuators, generators, and beyond.