Victor Gostishchev
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Victor Gostishchev has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
E. Kh. Ri
2 shared publicationsS. N. Khimukhin
Institute of Materials Science, Khabarovsk Scientific Center, Far East Branch, Russian Academy of Sciences
2 shared publicationsA. V. Seredyuk
Pacific State University, Khabarovsk, Russia
1 shared publicationE. D. Kim
Pacific National University
1 shared publicationE. H. Ri
Pacific National University
1 shared publication- E. Kh. Ri
Pacific National University
1 shared publication
Latest Publications
- 1 January 2019
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 55 (1) , 32-36
High-Temperature Synthesis of Al–Zr–W Aluminum-Matrix Alloys
— This paper reports the preparation of Al–Zr–W aluminum-matrix alloys containing reinforcing inclusions of various phases. The alloys have been produced by the aluminothermic reduction of...
- 1 January 2019
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 55 (1) , 32-36
High-Temperature Synthesis of Al–Zr–W Aluminum-Matrix Alloys
— This paper reports the preparation of Al–Zr–W aluminum-matrix alloys containing reinforcing inclusions of various phases. The alloys have been produced by the aluminothermic reduction of...
- Open Access
Synthesis of Complex-Alloyed Nickel Aluminides from Oxide Compounds by Aluminothermic Method
This paper deals with the investigation of complex-alloyed nickel aluminides obtained from oxide compounds by aluminothermic reduction. The aim of the work was to study and develop the physicochemical basis for obtaining complex-alloyed nickel aluminides and their application for enhancing the properties of coatings made by electrospark deposition (ESD) on steel castings, as well as their use as grain refiners for tin bronze. The peculiarities of microstructure formation of master alloys based on the Al–TM (transition metal) system were studied using optical, electronic scanning microscopy and X-ray spectral microanalysis. There were regularities found in the formation of structural components of aluminum alloys (Ni–Al, Ni-Al-Cr, Ni-Al-Mo, Ni-Al-W, Ni-Al-Ti, Ni-Cr-Mo-W, Ni-Al-Cr-Mo-W-Ti, Ni-Al-Cr-V, Ni-Al-Cr-V-Mo) and changes in their microhardness, depending on the composition of the charge, which consisted of oxide compounds, and on the amount of reducing agent (aluminum powder). It is shown that all the alloys obtained are formed on the basis of the β phase (solid solution of alloying elements in nickel aluminide) and quasi-eutectic, consisting of the β′ phase and intermetallics of the alloying elements. The most effective alloys, in terms of increasing microhardness, were Al-Ni-Cr-Mo-W (7007 MPa) and Al-Ni-Cr-V-Mo (7914 MPa). The perspective is shown for applying the synthesized intermetallic master alloys as anode materials for producing coatings by electrospark deposition on steel of C1030 grade. The obtained coatings increase the heat resistance of steel samples by 7.5 times, while the coating from NiAl-Cr-Mo-W alloy remains practically nonoxidized under the selected test conditions. The use of NiAl intermetallics as a modifying additive (0.15 wt. %) in tin bronze allows increasing the microhardness of the α-solid solution by 1.9 times and the microhardness of the eutectic (α + β phase) by 2.7 times.
Open AccessSynthesis of Complex-Alloyed Nickel Aluminides from Oxide Compounds by Aluminothermic Method
This paper deals with the investigation of complex-alloyed nickel aluminides obtained from oxide compounds by aluminothermic reduction. The aim of the work was to study and develop the physicochemical basis for obtaining complex-alloyed nickel aluminides and their application for enhancing the properties of coatings made by electrospark deposition (ESD) on steel castings, as well as their use as grain refiners for tin bronze. The peculiarities of microstructure formation of master alloys based on the Al–TM (transition metal) system were studied using optical, electronic scanning microscopy and X-ray spectral microanalysis. There were regularities found in the formation of structural components of aluminum alloys (Ni–Al, Ni-Al-Cr, Ni-Al-Mo, Ni-Al-W, Ni-Al-Ti, Ni-Cr-Mo-W, Ni-Al-Cr-Mo-W-Ti, Ni-Al-Cr-V, Ni-Al-Cr-V-Mo) and changes in their microhardness, depending on the composition of the charge, which consisted of oxide compounds, and on the amount of reducing agent (aluminum powder). It is shown that all the alloys obtained are formed on the basis of the β phase (solid solution of alloying elements in nickel aluminide) and quasi-eutectic, consisting of the β′ phase and intermetallics of the alloying elements. The most effective alloys, in terms of increasing microhardness, were Al-Ni-Cr-Mo-W (7007 MPa) and Al-Ni-Cr-V-Mo (7914 MPa). The perspective is shown for applying the synthesized intermetallic master alloys as anode materials for producing coatings by electrospark deposition on steel of C1030 grade. The obtained coatings increase the heat resistance of steel samples by 7.5 times, while the coating from NiAl-Cr-Mo-W alloy remains practically nonoxidized under the selected test conditions. The use of NiAl intermetallics as a modifying additive (0.15 wt. %) in tin bronze allows increasing the microhardness of the α-solid solution by 1.9 times and the microhardness of the eutectic (α + β phase) by 2.7 times.
- 26 October 2017
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 79-84
Obtaining of complex-alloyed nickel aluminides and complex ligatures by metal oxides’ metallothermy
Modern heat-resistant nickel-aluminum based materials obtain high performance data due to the integrated introduction of alloying elements, including rare earth metals. Our article shows the results of obtaining of multicomponent ligatures and complex-alloyed nickel-aluminum alloys by aluminothermy of initial metal oxides with additives of special ligature containing cerium and lanthanum. Thermodynamic assessment of aluminothermic reactions of reduction of initial metal oxides is given. These reactions have their thermodynamic parameters in an environment favorable for the formation of refractory metal alloys. The melting process temperature enables the secondary production of alloys. Differential thermal analysis investigated the transformations in the aluminothermic systems: NiO – Al, Cr2O3 – Al, МоО3 – Al, WO3 – Al, TiO2 – Al, V2O3 – Al. Reduction of oxides becomes active after aluminum melting at the temperature of ~ 659 oC and proceeds by a heterogeneous mechanism, the beginning of which corresponds to the range of 800–1100 oC. We defined the charge composition, which ensures the maximum release of the metals in alloys (82–93 wt.%). During the alloy production, especially in the case of the synthesis of composite alloy based on the intermetallic system Ni – Al, aluminum excess (relative to the estimated) is introduced into the charge composition. X-ray phase and elemental analyses defined the composition of the obtained alloys. The microstructure was investigated. For example the ligature #1 is shown by several phases with different ratio of aluminium, chromium, molybdenum and tungsten. At the same time, the ligature #2 also contains titanium, vanadium, cerium and lanthanum in the form of reciprocal solid solutions. Aluminide alloys have a compositional structure: nickel-aluminum matrix distributed the inclusions of the alloying elements in solid solutions.Investigations were carried out using the equipment of the Center of Multiple Access “Applied Materials Science” (Pacific National University) with the financial support of the Ministry of Education and Science of the Russian Federation within the state tasks No. 11.7208.2017/7.8 and 11.3014.2017/4.6.
- 26 October 2017
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 79-84
Obtaining of complex-alloyed nickel aluminides and complex ligatures by metal oxides’ metallothermy
Modern heat-resistant nickel-aluminum based materials obtain high performance data due to the integrated introduction of alloying elements, including rare earth metals. Our article shows the results of obtaining of multicomponent ligatures and complex-alloyed nickel-aluminum alloys by aluminothermy of initial metal oxides with additives of special ligature containing cerium and lanthanum. Thermodynamic assessment of aluminothermic reactions of reduction of initial metal oxides is given. These reactions have their thermodynamic parameters in an environment favorable for the formation of refractory metal alloys. The melting process temperature enables the secondary production of alloys. Differential thermal analysis investigated the transformations in the aluminothermic systems: NiO – Al, Cr2O3 – Al, МоО3 – Al, WO3 – Al, TiO2 – Al, V2O3 – Al. Reduction of oxides becomes active after aluminum melting at the temperature of ~ 659 oC and proceeds by a heterogeneous mechanism, the beginning of which corresponds to the range of 800–1100 oC. We defined the charge composition, which ensures the maximum release of the metals in alloys (82–93 wt.%). During the alloy production, especially in the case of the synthesis of composite alloy based on the intermetallic system Ni – Al, aluminum excess (relative to the estimated) is introduced into the charge composition. X-ray phase and elemental analyses defined the composition of the obtained alloys. The microstructure was investigated. For example the ligature #1 is shown by several phases with different ratio of aluminium, chromium, molybdenum and tungsten. At the same time, the ligature #2 also contains titanium, vanadium, cerium and lanthanum in the form of reciprocal solid solutions. Aluminide alloys have a compositional structure: nickel-aluminum matrix distributed the inclusions of the alloying elements in solid solutions.Investigations were carried out using the equipment of the Center of Multiple Access “Applied Materials Science” (Pacific National University) with the financial support of the Ministry of Education and Science of the Russian Federation within the state tasks No. 11.7208.2017/7.8 and 11.3014.2017/4.6.
- 1 September 2015
- Published by Springer Nature in Metallurgist
- Vol. 59 (5-6) , 526-534
Preparation of Tin and Tungsten from Mineral Concentrates in Ionic Melts
- 1 September 2015
- Published by Springer Nature in Metallurgist
- Vol. 59 (5-6) , 526-534
Preparation of Tin and Tungsten from Mineral Concentrates in Ionic Melts
- 1 July 2015
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 56 (4) , 387-391
Physicochemical aspects of the fabrication of tungsten powder by the metallothermy of the scheelite concentrate in ionic melts
- 1 July 2015
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 56 (4) , 387-391
Physicochemical aspects of the fabrication of tungsten powder by the metallothermy of the scheelite concentrate in ionic melts
- Open Access
- 17 June 2015
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 1 (3) , 22-26-22
Physicochemical Aspects of Fabrication of the Tungsten Powder by Metallothermy of the Scheelite Concentrate in Ionic Melts
Изучены условия получения порошка вольфрама разложением шеелитового концентрата в среде солевых расплавов NaCl–Na2CO3, NaCl–Na2CO3–NaF, NaCl–Na2CO3–Na3AlF6 и восстановлением образующегося вольфрамата натрия алю- минием при температуре 1123–1273 К. Установлено, что выход порошка составляет ~93 мас.%, чистота вольфрама – 97 %. Определены гранулометрические характеристики порошков. Показано, что удельная поверхность порошков достигает величины 14,6·105 м–1.
- 17 June 2015
- Published by National University of Science and Technology MISiS in Izvestiya Vuzov. Tsvetnaya Metallurgiya (Proceedings of Higher Schools. Nonferrous Metallurgy)
- Vol. 1 (3) , 22-26-22
Open AccessPhysicochemical Aspects of Fabrication of the Tungsten Powder by Metallothermy of the Scheelite Concentrate in Ionic Melts
Изучены условия получения порошка вольфрама разложением шеелитового концентрата в среде солевых расплавов NaCl–Na2CO3, NaCl–Na2CO3–NaF, NaCl–Na2CO3–Na3AlF6 и восстановлением образующегося вольфрамата натрия алю- минием при температуре 1123–1273 К. Установлено, что выход порошка составляет ~93 мас.%, чистота вольфрама – 97 %. Определены гранулометрические характеристики порошков. Показано, что удельная поверхность порошков достигает величины 14,6·105 м–1.