JSJiuqiang Song

Jiuqiang Song

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Jiuqiang Song has a total of 13 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    A Novel Acetylene-Functional/Silicon-Containing Benzoxazine Resin: Preparation, Curing Kinetics and Thermal Properties

    by Qilin Mei, Honghua Wang, Danliao Tong, Jiuqiang Song, Zhixiong Huang

    Benzoxazine resin has been paid more attention in the fields of aviation, electronics, automobiles and new energy industries because of its excellent comprehensive performance. Further application is limited, however, by shortcomings such as high brittleness and high curing temperature. Furthermore, higher thermal stability is imperiously demanded in special areas. Incorporating both an acetylene group and silicon into the benzoxazine monomer is a promising possible solution to improve the curing processability, thermal properties and toughness of benzoxazine. In this paper, an acetylene-functional/silicon-containing benzoxazine monomer was prepared by two-step synthesis, and acetylene-functional benzoxazine was also prepared as a comparison. FTIR and 1H NMR confirmed the molecular structure of acetylene-functional/silicon-containing benzoxazine. Differential scanning calorimetry (DSC) analysis showed that the initial and peak degradation temperatures of acetylene-functional/silicon-containing benzoxazine were decreased by 21 °C and 18 °C compared with acetylene-functional benzoxazine, respectively. The apparent activation energy of the curing reaction of acetylene-functional/silicon-containing benzoxazine was 83.1 kJ/mol, which was slightly lower than acetylene-functional benzoxazine (84.7 kJ/mol). TGA results showed that the acetylene-functional/silicon-containing benzoxazine had a higher thermal stability than acetylene-functional benzoxazine. The temperatures of 5% weight loss of acetylene-functional/silicon-containing benzoxazine were 380 °C in nitrogen and 485 °C in air, and the char yield at 1000 °C was 80% in nitrogen and 21% in air, respectively. The results of mechanical properties showed that the impact strength of acetylene-functional/silicon-containing benzoxazine was higher than acetylene-functional benzoxazine by 35.4%. The tensile and flexural strengths of acetylene-functional/silicon-containing benzoxazine were slightly higher than that of acetylene-functional benzoxazine.


  • Open Access

    Effects of Zirconium Silicide on the Vulcanization, Mechanical and Ablation Resistance Properties of Ceramifiable Silicone Rubber Composites

    by Jiuqiang Song, Zhixiong Huang, Yan Qin, Honghua Wang, Minxian Shi

    Ceramifiable silicone rubber composites play important roles in the field of thermal protection systems (TPS) for rocket motor cases due to their advantages. Ceramifiable silicone rubber composites filled with different contents of ZrSi2 were prepared in this paper. The fffects of ZrSi2 on the vulcanization, mechanical and ablation resistance properties of the composites were also investigated. The results showed that the introduction of ZrSi2 decreased the vulcanization time of silicone rubber. FTIR spectra showed that ZrSi2 did not participate in reactions of the functional groups of silicone rubber. With the increasing content of ZrSi2, the tensile strength increased first and then decreased. The elongation at break decreased and the permanent deformation increased gradually. The thermal conductivity of the composite increased from 0.553 W/(m·K) to 0.694 W/(m·K) as the content of the ZrSi2 increased from 0 to 40 phr. In addition, the thermal conductivity of the composite decreased with the increase of temperature. Moreover, thermal analysis showed that the addition of ZrSi2 increased the initial decomposition temperature of the composite, but had little effect on the peak decomposition temperature in nitrogen. However, the thermal decomposition temperature of the composite in air was lower than that in nitrogen. The addition of ZrSi2 decreased the linear and mass ablation rate, which improved the ablative resistance of the composite. With the ZrSi2 content of 30 phr, the linear and mass ablation rate were 0.041 mm/s and 0.029 g/s, decreasing by 57.5% and 46.3% compared with the composite without ZrSi2, respectively. Consequently, the ceramifiable silicone rubber composite filled with ZrSi2 is very promising for TPS.


  • Open Access

    Thermal Decomposition and Ceramifying Process of Ceramifiable Silicone Rubber Composite with Hydrated Zinc Borate

    by Jiuqiang Song, Zhixiong Huang, Yan Qin, Xinyi Li

    The ceramifiable silicone rubber composite was prepared using hydrated zinc borate and kaolin as ceramifiable fillers. Effects of the hydrated zinc borate content and the combustion temperature on the properties of the ceramifiable silicone rubber composite were investigated. Thermal decomposition and ceramifying processes of the composite in a muffle furnace under air were also studied. The results showed that the density and the hardness of the composites increased as the content of the hydrated zinc borate increased from 0 to 30 phr. The tensile strength and elongation at break decreased. In addition, hydrated zinc borate decreased the decomposition temperature of the composite, whereas the residue weight under air atmosphere was increased. In the process of decomposition and oxidation of the ceramifiable silicone rubber composite in air, B2O3 was generated by the decomposition of zinc borate and participated in the formation of the residue network structure, which decreased the temperature of the ceramifying transition. The new phases, zinc aluminate (ZnO·Al2O3) and aluminum-rich mullite (9Al2O3·2SiO2), appeared after high-temperature thermochemical reactions. Microscopy images revealed that different structures were formed at different temperatures. The network structure of the ceramic residue became increasingly compact, and the compressive strength increased from 0.31 to 1.82 MPa with the increase of temperature from 800 to 1400 °C, which had a better protective effect on heat transfer and mass loss. The weight loss and the linear shrinkage of the ceramic residue was 37.6% and 21.9%, respectively, with the 30 phr content of hydrated zinc borate. The bending strength was improved from 0.11 to 11.58 MPa, and the compressive strength also increased from 0.03 to 1.14 MPa.


  • Open Access

    Ceramifiable and mechanical properties of silicone rubber foam composite with frit and high silica glass fiber

    by J Q Song, Z X Huang, Y Qin, G Y Yang, X Wang

    In this paper, ceramifiable silicone rubber foam composite was prepared by silicone rubber, fumed SiO2, talc, frit, high silica glass fiber, foaming and vulcanizing agents. Thermal property, micromorphology, phase transformation and compressive strength of pyrolysis residues at different temperatures were discussed. Thermogravimetric analysis (TGA) results indicated that the amount of ceramic residues increased from 34.5% to 41.1% at 1000 °C with the increase of frit content, whereas T5 and Tmax decreased by 43°C and 103°C, respectively. SEM images showed that pore size became well-distributed by adding frits to the silicone rubber. And after pyrolysis at 1000°C, bridged structure was formed well, which made the structure of residues be coherent and integrated. XRD tests indicated that new crystalline phase, MgSiO3, was appeared at above 1000°C. The effect of frit on compressive strength of composite at room temperature was little, but there was a great improvement after being treated at high temperature, especially at 1000°C.