SASaya Ajito

Saya Ajito

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Saya Ajito has a total of 56 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Hydrogen absorption and desorption properties of Mn-based Mn–Al alloy investigated using synchrotron radiation x-ray diffraction technique

    by Reina Utsumi, Saya Ajito, Shigeyuki Takagi, Yuki Nakahira, Hiroyuki Saitoh, Tetsu Watanuki, Toyoto Sato, Eiji Akiyama, Shin-Ichi Orimo

  • Open Access

    Hydrogen Embrittlement of Hole-Expanded TRIP-aided Martensitic Steel Sheet

    by Zisong Guo, Tomohiko Hojo, Hiroyuki Saitoh, Ayumi Shiro, Takahisa Shobu, Ryo Yasuda, Saya Ajito, Motomichi Koyama, Eiji Akiyama, Fumio Yuse, et al.

    The effects of stress, plastic strain, and hydrogen on hydrogen embrittlement fracture of hole-expanded transformation-induced plasticity-aided martensitic steel were investigated. The hydrogen embrittlement properties were evaluated by means of cathodic hydrogen charging to the hole-expanded specimen. The residual stress and plastic strain distributions in the hole-expanded specimens were analyzed using finite element analysis. The hydrogen content was measured using a thermal desorption spectrometer. Hydrogen embrittlement cracking occurred approximately 3 mm from the hole edge in the radial direction. As the crack propagated, it diverged in the circumferential direction. The fracture morphology primarily consisted of a mixture of intergranular and quasi-cleavage fractures. The tensile stress in the circumferential direction at the position where the hydrogen embrittlement crack was initiated was the highest, and the tensile stress in the radial direction and hydrostatic stress were also high. The hydrogen content in the vicinity of the hole edge of the hole-expanded specimen was the highest owing to the large amount of plastic strain applied by hole punching and hole expanding whereas the hydrogen content at the positions where the hydrogen embrittlement crack was propagated was not very high. Thus, the highest tensile stress in the circumferential direction is the controlling factor in the location of the crack initiation site and the direction of the initial crack and its growth during the initial phase. The high hydrostatic stress that causes hydrogen accumulation could also assist the crack initiation.


  • Video Imaging of Microscopic Hydrogen Diffusion at Grain Boundaries of Pure Ni

    by Hiroshi Kakinuma, Motomichi Koyama, Rama Srinivas Varanasi, Saya Ajito, Eiji Akiyama

    Corrosion-induced hydrogen entry into a metal is thought to cause hydrogen embrittlement. The hydrogen atoms diffuse in the metal and localize at the hydrogen trapping site, inducing the loss of ductility. The hydrogen diffusion behavior is known to depend on the microstructure. 1-3) For example, in the case of pure Ni, random grain boundaries (GBs) are the preferential hydrogen diffusion path. 2,3) It has also been shown that the hydrogen flux depends on the free volume of the random GBs. 3) On the other hand, the geometrical structure of the Σ3 GB is almost the same as that of grain interior; thus, preferential hydrogen diffusion is not expected to occur. However, the hydrogen flux may depend on the coherency of the Σ3 GB, because there are incoherent Σ3 GBs with large free volume. In this study, it was attempted to elucidate the coherency-dependent hydrogen diffusion at Σ3 GBs. A hydrogenochromic sensor, 4-6) polyaniline, was polymerized on one side of a pure Ni foil. Polyaniline is known to react with hydrogen atoms in metals, changing its color from blue to yellow. 4,5) Therefore, the hydrogen distribution in the metal can be analyzed based on the color distribution of the polyaniline layer. A Ni foil (99.9%) with a thickness of 115 µm was electrochemically polished in a mixed solution of perchloric acid and acetic acid. The final thickness of the foil was approximately 90 µm. A polyaniline layer was formed on one side of the foil. The other side of the foil was polarized at constant current density of −10 A m −2 in 1 M NaOH. During hydrogen charging, the color of the polyaniline layer was observed using an inverted optical microscope. The preferential hydrogen diffusion path in the Ni foil was random GBs with a misorientation angle of more than 15°. Furthermore, hydrogen diffusion was enhanced in the incoherent portion of Σ3 GBs; the hydrogen diffusion behavior at the coherent portion of Σ3 GBs was almost the same as that in grain interior. The visualization of the hydrogen diffusion behavior in the Ni foil using a polyaniline layer clarified that the hydrogen diffusion at Σ3 GBs depends on the coherency, and the enhanced hydrogen diffusion occurs at the micro- and nano-scale incoherent portion. References: 1) H. Kakinuma, S. Ajito, M. Koyama, E. Akiyama, Microscopic visualization of hydrogen diffusion in UNS S32750 super duplex stainless steel: Roles of crystal structure and grain size, Int. J. Hydrog. Energy , 59 , 866-873 (2024). 2) H. Kakinuma, M. Koyama, R.S. Varanasi, S. Ajito, E. Akiyama, Semi-quantitative characterisation of coherency-dependent hydrogen diffusion at Σ3 grain boundaries in pure Ni, Mater. Res. Lett. , 1-8 (2025). 3) H. Kakinuma, S. Ajito, T. Hojo, M. Koyama, E. Akiyama, In situ visualization of misorientation-dependent hydrogen diffusion at grain boundaries of pure polycrystalline Ni using a hydrogen video imaging system, Acta Mater. , 263 , 119536 (2024). 4) H. Kakinuma, S. Ajito, T. Hojo, M. Koyama, E. Akiyama, Real-time Visualization of Hydrogen Distribution in Metals Using Polyaniline: An Ultrasensitive Hydrogenochromic Sensor, Adv. Mater. Inter. , 9 , 2101984 (2022). 5) H. Kakinuma, S. Ajito, T. Hojo, M. Koyama, S. Hiromoto, E. Akiyama, Simultaneous observations of the corrosion behavior of an Fe sheet and the associated hydrogen distribution therein employing a hydrogenochromic sensor, Corros. Sci. , 206 , 110534 (2022). 6) H. Kakinuma, S. Ajito, T. Hojo, M. Koyama, S. Hiromoto, E. Akiyama, In situ 2D Mapping of Hydrogen Entry into an Fe Sheet under a Droplet of NaCl Solution Using a Hydrogenochromic Sensor, Int. J. Hydrog. Energy , 47 , 38468 (2022).


  • Open Access

    In situ 2D visualization of hydrogen entry into Zn-coated steels in NaCl solutions: Roles of Zn dissolution and potential distribution

    by Hiroshi Kakinuma, Saya Ajito, Koki Okumura, Makoto Akahoshi, Yu Takabatake, Tomohiko Omura, Motomichi Koyama, Eiji Akiyama


  • Open Access

    Stress and Plastic Strain Partitioning Behaviors and Those Contributions to Martensitic Transformation of Retained Austenite in Medium Manganese and Transformation-Induced Plasticity-Aided Bainitic Ferrite Steels

    by Tomohiko Hojo, Motomichi Koyama, Bakuya Kumai, Yutao Zhou, Yuki Shibayama, Ayumi Shiro, Takahisa Shobu, Hiroyuki Saitoh, Saya Ajito, Eiji Akiyama

    Stress and plastic strain distributions and those partitioning behaviors of ferrite and retained austenite were investigated in the medium manganese (Mn) and the transformation-induced plasticity-aided bainitic ferrite (TBF) steels, and the martensitic transformation behaviors of retained austenite during Lüders elongation and work hardening were analyzed using synchrotron X-ray diffraction at SPring-8. The stress and plastic strain of retained austenite and volume fraction of retained austenite were remarkably changed during Lüders deformation in the medium Mn steel, implying that the medium Mn steel possessed inhomogeneous deformation at the parallel part of the tensile specimen. On the other hand, the distributions of the stress, plastic strain and volume fraction of retained austenite were homogeneous and the homogeneous deformation occurred at the parallel part of the tensile specimen at the plastic deformation regime with work hardening in the medium Mn and TBF steels. The martensitic transformation of retained austenite at Lüders deformation in the medium Mn steel was possessed owing to the application of high stress and preferential deformation at retained austenite, resulting in a significant increase in the plastic deformation and reduction of stress in the retained austenite. The martensitic transformation of retained austenite at the plastic deformation regime with work hardening was induced by the high dislocation density and newly applied plastic deformation in retained austenite in the medium Mn steel whereas the TBF steel possessed gradual transformation of retained austenite which is applied high tensile stress and moderate plastic deformation.


  • Real-Time 2D Mapping of Hydrogen Entry and pH Distribution inside a NaCl Droplet on an Fe Sheet Using a Hydrogenochromic Sensor

    by Hiroshi Kakinuma, Sachiko Hiromoto, Tomohiko Hojo, Saya Ajito, Motomichi Koyama, Eiji Akiyama

    Atmospheric corrosion on a steel is known to promote hydrogen entry into the steel. However, the mechanism of corrosion-induced hydrogen entry is still unclear, because it is difficult to detect the small amount of hydrogen entered steels due to corrosion. In previous literature, electrochemical hydrogen permeation tests with Devanathan-Stachurski cells have been conducted to detect corrosion-induced hydrogen entry. While the electrochemical hydrogen permeation tests can measure the corrosion-induced hydrogen permeation current with high sensitivity and high time resolution, the hydrogen distribution in the steels cannot be measured. It has been challenging to analyze the two-dimensional information of corrosion-induced hydrogen entry. In this study, a hydrogenochromic sensor consisting of the polyaniline (PANI) and Ni layers was used to visualize the hydrogen distribution in an Fe sheet under corrosion conditions. A PANI layer polymerized on a metal surface reacts with atomic state hydrogen in the metal, resulting in the color change from blue or purple to yellow or transparent.1,2 The intermediate Ni layer between the metal surface and the PANI layer works as a catalysis of the hydrogenation reaction of the PANI layer.1 Therefore, the small amounts of hydrogen that entered the metals can be visualized using the hydrogenochromic sensor consisting of the Ni and PANI layers.3 –6 In this study, the Ni layer was plated on one side of an Fe sheet by current-static polarization at –30 A m–2 for 180 s in the Watts bath at 333 K. In addition, the PANI layer was electrically polymerized on the Ni layer at a constant voltage of 1 V for 200 s in a 0.5 M H2SO4-0.5 M aniline solution. A droplet of 0.1 M NaCl containing thymol blue was placed on the other side of the specimen (bare Fe surface). The color of thymol blue is known to be changed by the increase in pH from neutral to alkaline. Thus, the hydrogen entry behavior and pH change in the droplet were analyzed simultaneously by observing the droplet and hydrogenochromic sensor with digital cameras. Large crystallographic pits occurred in the initial stage of corrosion, but hydrogen entry was hardly promoted by the crystallographic pits. Subsequently, a rust-formed area was observed. Because the hydrogen entry proceeded under the rust-formed area, acidification was thought to occur under the rust-formed area, causing the hydrogen evolution reaction. The pH on the non-corroded area was alkaline, suggesting that alkalization proceeded on the non-corroded area due to the oxygen reduction reaction. The edges of the rust-formed area were close to the alkalized area, resulting in the thickening of rust at the edges. After the disappearance of the droplet due to drying, hydrogen entry almost ceased. However, hydrogen entry was confirmed under the thick rust layer formed at the edge of the rust-formed area. It was found that hydrogen entry is likely to proceed under the thick rust layer, which contains concentrated NaCl solution, even after the disappearance of the droplet. References: 1) H. Kakinuma, S. Ajito, T. Hojo, M. Koyama, E. Akiyama, Real-time Visualization of Hydrogen Distribution in Metals Using Polyaniline: An Ultrasensitive Hydrogenochromic Sensor, Adv. Mater. Inter., 9, 2101984 (2022). 2) H. Kakinuma, S. Ajito, T. Hojo, M. Koyama, S. Hiromoto, E. Akiyama, Simultaneous Observations of the Corrosion Behavior of an Fe Sheet and the Assosciated Hydrogen Distribution therein Employing a Hydrogenochromic Sensor, Corros. Sci., 206, 110534 (2022). 3) H. Kakinuma, S. Ajito, T. Hojo, M. Koyama, S. Hiromoto, E. Akiyama, In situ 2D Mapping of Hydrogen Entry into an Fe Sheet under a Droplet of NaCl Solution Using a Hydrogenochromic Sensor, Int. J. Hydrog. Energy, 47, 38468 (2022). 4) H. Kakinuma, S. Ajito, T. Hojo, M. Koyama, E. Akiyama, In situ visualization of misorientation-dependent hydrogen diffusion at grain boundaries of pure polycrystalline Ni using a hydrogen video imaging system, Acta Mater., 263, 119536 (2024). 5) H. Kakinuma, S. Ajito, M. Koyama, E. Akiyama, Microscopic visualization of hydrogen diffusion in UNS S32750 super duplex stainless steel: Roles of crystal structure and grain size, Int. J. Hydrog. Energy, 59, 866-873 (2024). 6) H. Kakinuma, S. Hiromoto, T. Hojo, S. Ajito, M. Koyama, E. Akiyama, Mechanism of Local Hydrogen Entry into Fe sheets Induced by Atmospheric Corrosion: Significance of Potential, pH, and Rust Layer Thickness, Corros. Sci., 112043 (2024).

  • Open Access

    Grain boundary nanochemistry and intergranular corrosion of Fe-0.01wt.%P alloy: Roles of elemental segregations and misorientation

    by Saya Ajito, Kazuya Tojima, Hiroshi Kakinuma, Kohei Ikeda, Yongjie Zhang, Tomohiko Hojo, Goro Miyamoto, Motomichi Koyama, Tadashi Furuhara, Eiji Akiyama


  • Open Access

    Visualization of Microscopic Hydrogen Diffusion in Polycrystalline Pure Ni Using an Ir Complex

    by Saya Ajito, Hiroshi Kakinuma, Motomichi Koyama, Eiji Akiyama

    金属材料の水素脆化機構を明らかにするために,金属組織に依存した微視的な水素分布をその場検出する技術が求められている.本研究では,多結晶純ニッケル箔中の水素拡散の微視的な分布を,イリジウム錯体膜を用いて可視化することに成功した.ニッケル箔中の水素流束は,ランダム粒界で大きく,粒内や対応粒界では小さいことがわかった.