Jayashree Samantray
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Jayashree Samantray has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
- Amit Anand
Indian Institute of Technology Bhubaneswar
4 shared publications Barsha Dash
3 shared publicationsMalay K. Ghosh
CSIR-Institute of Minerals and Materials Technology, Bhubaneswar 751013, India
2 shared publications- Malay Kumar Ghosh
Hydro & Electrometallurgy Department, CSIR-Institute of Minerals and Materials Technology, Bhubaneswar, India
2 shared publications Ajay K. Behera
Sambalpur University
1 shared publicationAjaya Kumar Behera
1 shared publication
Latest Publications
- 1 August 2025
- Published by Springer Nature in Mining, Metallurgy & Exploration
- Vol. 42 (5) , 3133-3143
Bio Waste Application for Potassium Extraction from Nepheline Syenite
- 1 August 2025
- Published by Springer Nature in Mining, Metallurgy & Exploration
- Vol. 42 (5) , 3133-3143
Bio Waste Application for Potassium Extraction from Nepheline Syenite
- 23 February 2022
- Published by Elsevier in Minerals Engineering
- Vol. 179
Silicate minerals - Potential source of potash - A review
- 23 February 2022
- Published by Elsevier in Minerals Engineering
- Vol. 179
Silicate minerals - Potential source of potash - A review
- 16 June 2020
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 5 (25) , 14990-14998
Sustainable Process for the Extraction of Potassium from Feldspar Using Eggshell Powder
To recover potassium from feldspar, a biowaste, i.e., eggshell, was used. The chief composition of eggshells is calcite. As it is a rich source of Ca, hence it is used with HCl to produce calcium chloride. Feldspar is an aluminosilicate mineral that bears potassium in the interstitial sites. To unlock the potassium from the interstitial sites, it was roasted with calcium chloride prepared by mixing eggshell and hydrochloric acid. At the roasting temperature, CaCl2 melts and penetrates into the aluminosilicate matrix to replace K with Ca. Potassium ion released from the silicate matrix combines with chloride ions to form potassium chloride, which solubilized in water during the leaching process of the roasted feldspar. For elucidation of the mechanism of the roasting process, the shrinking core model was applied to the roast–leach data, and diffusion through the product layer was inferred as the rate-determining step. The order of the roasting process was found to be 2.158 and activation energy calculated to be 155.3 kJ/mol. Apart from potassium, sodium and excess calcium also got co-leached. To recover potassium from the leach liquor selectively, sodium perchlorate was added to precipitate potassium as KClO4. Further, potassium perchlorate was thermally decomposed to give fertilizer grade potassium chloride (purity: 99.81%).
- 16 June 2020
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 5 (25) , 14990-14998
Sustainable Process for the Extraction of Potassium from Feldspar Using Eggshell Powder
To recover potassium from feldspar, a biowaste, i.e., eggshell, was used. The chief composition of eggshells is calcite. As it is a rich source of Ca, hence it is used with HCl to produce calcium chloride. Feldspar is an aluminosilicate mineral that bears potassium in the interstitial sites. To unlock the potassium from the interstitial sites, it was roasted with calcium chloride prepared by mixing eggshell and hydrochloric acid. At the roasting temperature, CaCl2 melts and penetrates into the aluminosilicate matrix to replace K with Ca. Potassium ion released from the silicate matrix combines with chloride ions to form potassium chloride, which solubilized in water during the leaching process of the roasted feldspar. For elucidation of the mechanism of the roasting process, the shrinking core model was applied to the roast–leach data, and diffusion through the product layer was inferred as the rate-determining step. The order of the roasting process was found to be 2.158 and activation energy calculated to be 155.3 kJ/mol. Apart from potassium, sodium and excess calcium also got co-leached. To recover potassium from the leach liquor selectively, sodium perchlorate was added to precipitate potassium as KClO4. Further, potassium perchlorate was thermally decomposed to give fertilizer grade potassium chloride (purity: 99.81%).
- 25 March 2020
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 73 (4) , 1081-1091
Leaching of Rare Earth Elements from the Residue Generated by the Lixiviation of Waste Phosphor with Sulphuric Acid
- 25 March 2020
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 73 (4) , 1081-1091
Leaching of Rare Earth Elements from the Residue Generated by the Lixiviation of Waste Phosphor with Sulphuric Acid
- 7 June 2019
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 72 (10) , 2613-2622
Production of Potassium Chloride from K-Feldspar Through Roast–Leach–Solvent Extraction Route
- 7 June 2019
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 72 (10) , 2613-2622
Production of Potassium Chloride from K-Feldspar Through Roast–Leach–Solvent Extraction Route