Jianxin Lin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Jianxin Lin has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Guang Ran
College of Energy Xiamen University Xiamen China
4 shared publications - Chao Ye
College of Energy, Xiamen University, Xiamen 361102, China
3 shared publications - Penghui Lei
College of Energy, Xiamen University, Xiamen 361102, China
3 shared publications - Ning Li
College of Energy, Xiamen University, Xiamen 361102, China
2 shared publications - Qiang Shen
College of Energy, Xiamen University, Xiamen 361102, China
2 shared publications - Chenwei Liu
College of Energy, Xiamen University, Xiamen 361102, Fujian Province, China
1 shared publication
Latest Publications
- Open Access
Microstructure Analysis of Neutron Absorber Al/B4C Metal Matrix Composites
The microstructure of Al/B4C metal matrix composites (MMCs) used as neutron absorbers in both dry storage casks and wet storage pools of spent nuclear fuel was analyzed by SEM and TEM. A polishing method of a focused Ga+ ion beam was used to obtain an ideal sample surface with very low roughness, which was used to statistically analyze the distribution characteristics and size factor of B4C particles in the aluminum matrix. The area of B4C particles mainly ranged from 0 to 0.5 μm2, which was the proportion of 64.29%, 86.99% and 76.86% of total statistical results for the Al-15%B4C, Al-25%B4C and Al-30%B4C MMCs, respectively. The average area of B4C particles in the Al-15%B4C, Al-25%B4C and Al-30%B4C MMCs were about 1.396, 0.528 and 1.183 μm2, respectively. The nanoscale precipitates were analyzed by the element mappings in scanning transmission electron microscopy (STEM) mode and electron energy loss spectroscopy (EELS) mode, which included elliptic alloy precipitates with elemental Cu, Cr, Fe and Si, except for Al, and B4C nanoparticles with polygonal shape. The interface characteristics showed that the (021) crystal plane of B4C particle and (111) crystal plane of aluminum matrix grew together. The lattice misfit was about 1.68% for (111)Al//(021)B4C. The corrosion properties and corresponding mechanism of Al/B4C MMCs were investigated in an aqueous solution with 5000 ppm boric acid at 100 °C and atmospheric pressure, which showed that the mass increment rate was first decreased with increasing corrosion time and then increased.
Open AccessMicrostructure Analysis of Neutron Absorber Al/B4C Metal Matrix Composites
The microstructure of Al/B4C metal matrix composites (MMCs) used as neutron absorbers in both dry storage casks and wet storage pools of spent nuclear fuel was analyzed by SEM and TEM. A polishing method of a focused Ga+ ion beam was used to obtain an ideal sample surface with very low roughness, which was used to statistically analyze the distribution characteristics and size factor of B4C particles in the aluminum matrix. The area of B4C particles mainly ranged from 0 to 0.5 μm2, which was the proportion of 64.29%, 86.99% and 76.86% of total statistical results for the Al-15%B4C, Al-25%B4C and Al-30%B4C MMCs, respectively. The average area of B4C particles in the Al-15%B4C, Al-25%B4C and Al-30%B4C MMCs were about 1.396, 0.528 and 1.183 μm2, respectively. The nanoscale precipitates were analyzed by the element mappings in scanning transmission electron microscopy (STEM) mode and electron energy loss spectroscopy (EELS) mode, which included elliptic alloy precipitates with elemental Cu, Cr, Fe and Si, except for Al, and B4C nanoparticles with polygonal shape. The interface characteristics showed that the (021) crystal plane of B4C particle and (111) crystal plane of aluminum matrix grew together. The lattice misfit was about 1.68% for (111)Al//(021)B4C. The corrosion properties and corresponding mechanism of Al/B4C MMCs were investigated in an aqueous solution with 5000 ppm boric acid at 100 °C and atmospheric pressure, which showed that the mass increment rate was first decreased with increasing corrosion time and then increased.
- Open Access
Recrystallization-Induced Surface Cracks of Carbon Ions Irradiated 6H-SiC after Annealing
Single crystal 6H-SiC wafers with 4° off-axis [0001] orientation were irradiated with carbon ions and then annealed at 900 °C for different time periods. The microstructure and surface morphology of these samples were investigated by grazing incidence X-ray diffraction (GIXRD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). Ion irradiation induced SiC amorphization, but the surface was smooth and did not have special structures. During the annealing process, the amorphous SiC was recrystallized to form columnar crystals that had a large amount of twin structures. The longer the annealing time was, the greater the amount of recrystallized SiC would be. The recrystallization volume fraction was accorded with the law of the Johnson–Mehl–Avrami equation. The surface morphology consisted of tiny pieces with an average width of approximately 30 nm in the annealed SiC. The volume shrinkage of irradiated SiC layer and the anisotropy of newly born crystals during annealing process produced internal stress and then induced not only a large number of dislocation walls in the non-irradiated layer but also the initiation and propagation of the cracks. The direction of dislocation walls was perpendicular to the growth direction of the columnar crystal. The longer the annealing time was, the larger the length and width of the formed crack would be. A quantitative model of the crack growth was provided to calculate the length and width of the cracks at a given annealing time.
Open AccessRecrystallization-Induced Surface Cracks of Carbon Ions Irradiated 6H-SiC after Annealing
Single crystal 6H-SiC wafers with 4° off-axis [0001] orientation were irradiated with carbon ions and then annealed at 900 °C for different time periods. The microstructure and surface morphology of these samples were investigated by grazing incidence X-ray diffraction (GIXRD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). Ion irradiation induced SiC amorphization, but the surface was smooth and did not have special structures. During the annealing process, the amorphous SiC was recrystallized to form columnar crystals that had a large amount of twin structures. The longer the annealing time was, the greater the amount of recrystallized SiC would be. The recrystallization volume fraction was accorded with the law of the Johnson–Mehl–Avrami equation. The surface morphology consisted of tiny pieces with an average width of approximately 30 nm in the annealed SiC. The volume shrinkage of irradiated SiC layer and the anisotropy of newly born crystals during annealing process produced internal stress and then induced not only a large number of dislocation walls in the non-irradiated layer but also the initiation and propagation of the cracks. The direction of dislocation walls was perpendicular to the growth direction of the columnar crystal. The longer the annealing time was, the larger the length and width of the formed crack would be. A quantitative model of the crack growth was provided to calculate the length and width of the cracks at a given annealing time.
- Open Access
In Situ TEM Study of Microstructure Evolution of Zr-Nb-Fe Alloy Irradiated by 800 keV Kr2+ Ions
The microstructure evolution of Zr-1.1Nb-1.51Fe-0.26Cu-0.72Ni zirconium alloy, irradiated by 800 keV Kr2+ ions at 585 K using the IVEM-Tandem Facility at Argonne National Laboratory, was observed by in situ transmission electron microscopy. A number of β-Nb precipitates with a body-centered cubic (BCC) structure were distributed in the as-received zirconium alloy with micrometer-size grains. Kr2+ ion irradiation induced the growth of β-Nb precipitates, which could be attributed to the segregation of the dissolved niobium atoms in the zirconium lattice and the migration to the existing precipitates. The size of precipitates was increased with increasing Kr2+ ion fluence. During Kr2+ iron irradiation, the zirconium crystals without Nb precipitates tended to transform to the nanocrystals, which was not observed in the zirconium crystals with Nb nanoparticles. The existing Nb nanoparticles were the key factor that constrained the nanocrystallization of zirconium crystals. The thickness of the formed Zr-nanocrystal layer was about 300 nm, which was consistent with the depth of Kr2+ iron irradiation. The mechanism of the precipitate growth and the formation of zirconium nanocrystal was analyzed and discussed.
Open AccessIn Situ TEM Study of Microstructure Evolution of Zr-Nb-Fe Alloy Irradiated by 800 keV Kr2+ Ions
The microstructure evolution of Zr-1.1Nb-1.51Fe-0.26Cu-0.72Ni zirconium alloy, irradiated by 800 keV Kr2+ ions at 585 K using the IVEM-Tandem Facility at Argonne National Laboratory, was observed by in situ transmission electron microscopy. A number of β-Nb precipitates with a body-centered cubic (BCC) structure were distributed in the as-received zirconium alloy with micrometer-size grains. Kr2+ ion irradiation induced the growth of β-Nb precipitates, which could be attributed to the segregation of the dissolved niobium atoms in the zirconium lattice and the migration to the existing precipitates. The size of precipitates was increased with increasing Kr2+ ion fluence. During Kr2+ iron irradiation, the zirconium crystals without Nb precipitates tended to transform to the nanocrystals, which was not observed in the zirconium crystals with Nb nanoparticles. The existing Nb nanoparticles were the key factor that constrained the nanocrystallization of zirconium crystals. The thickness of the formed Zr-nanocrystal layer was about 300 nm, which was consistent with the depth of Kr2+ iron irradiation. The mechanism of the precipitate growth and the formation of zirconium nanocrystal was analyzed and discussed.
- Open Access
Microstructural Evolution of Dy2O3-TiO2 Powder Mixtures during Ball Milling and Post-Milled Annealing
The microstructural evolution of Dy2O3-TiO2 powder mixtures during ball milling and post-milled annealing was investigated using XRD, SEM, TEM, and DSC. At high ball-milling rotation speeds, the mixtures were fined, homogenized, nanocrystallized, and later completely amorphized, and the transformation of Dy2O3 from the cubic to the monoclinic crystal structure was observed. The amorphous transformation resulted from monoclinic Dy2O3, not from cubic Dy2O3. However, at low ball-milling rotation speeds, the mixtures were only fined and homogenized. An intermediate phase with a similar crystal structure to that of cubic Dy2TiO5 was detected in the amorphous mixtures annealed from 800 to 1000 °C, which was a metastable phase that transformed to orthorhombic Dy2TiO5 when the annealing temperature was above 1050 °C. However, at the same annealing temperatures, pyrochlore Dy2Ti2O7 initially formed and subsequently reacted with the remaining Dy2O3 to form orthorhombic Dy2TiO5 in the homogenous mixtures. The evolutionary mechanism of powder mixtures during ball milling and subsequent annealing was analyzed.
Open AccessMicrostructural Evolution of Dy2O3-TiO2 Powder Mixtures during Ball Milling and Post-Milled Annealing
The microstructural evolution of Dy2O3-TiO2 powder mixtures during ball milling and post-milled annealing was investigated using XRD, SEM, TEM, and DSC. At high ball-milling rotation speeds, the mixtures were fined, homogenized, nanocrystallized, and later completely amorphized, and the transformation of Dy2O3 from the cubic to the monoclinic crystal structure was observed. The amorphous transformation resulted from monoclinic Dy2O3, not from cubic Dy2O3. However, at low ball-milling rotation speeds, the mixtures were only fined and homogenized. An intermediate phase with a similar crystal structure to that of cubic Dy2TiO5 was detected in the amorphous mixtures annealed from 800 to 1000 °C, which was a metastable phase that transformed to orthorhombic Dy2TiO5 when the annealing temperature was above 1050 °C. However, at the same annealing temperatures, pyrochlore Dy2Ti2O7 initially formed and subsequently reacted with the remaining Dy2O3 to form orthorhombic Dy2TiO5 in the homogenous mixtures. The evolutionary mechanism of powder mixtures during ball milling and subsequent annealing was analyzed.