Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Chao-Wei Tang has a total of 44 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    The Development and Application Status of Advanced Cement-Based Materials

    by Chao-Wei Tang

    Cement-based materials exhibit excellent properties, such as plasticity, castability, high compressive strength, fire resistance, durability, and cost-effectiveness


  • Open Access

    A Case Study of Using Numerical Analysis to Assess the Slope Stability of National Freeways in Northern Taiwan

    by Hao-Wei Chiu, Yi-Hao Tsai, Chao-Wei Tang, Chih-Yu Chu, Shong-Loong Chen

    Taiwan is located at a junction of tectonic plates, which results in frequent earthquakes. Its terrain is mostly hilly, and its rainfall ranks among the highest in the world. Each of these elements affects the stability of slopes in various regions of Taiwan. Several slopes along Taiwan’s Freeway 1 and 5 have experienced landslides and rockfalls. It is imperative that the slope stability of these national freeways be analyzed to avoid future slope collapses brought on by precipitation or other outside factors. Thus, three sites on Taiwan’s Freeway 1 and 5 were chosen for numerical slope stability analysis in this study. PLAXIS 2D CE (Version: 24.02.00.1144) finite element software was used in this study to simulate and analyze the safety of freeway slope protection projects. Displacements induced by normal and high groundwater levels were discussed. Moreover, a pseudo-static study of slope displacements under seismic conditions was performed. According to the results of the numerical study, the force operating on the slope was centered on the sliding surface when the groundwater level was normal, and it extended to the top when the groundwater level was high. By comparison, under seismic conditions, the force acting on the slope extended to the whole slope. Furthermore, the slope safety factor of Site 1 was greater than the design specification value in three different scenarios. This confirms that the slope protection project at Site 1 is effective.


  • Open Access

    A Case Study of Using Numerical Analysis to Assess Slope Stability of National Highways in Northern Taiwan

    by Hao-Wei Chiu, Yi-Hao Tsai, Chao-Wei Tang, Chih-Yu Chu, Shong-Long Chen

    Because of its location at the meeting point of the Eurasian Plate and the Philippine Sea Plate, Taiwan experiences earthquakes frequently. Mountains and hills make up the majority of the landscape, and Taiwan has some of the highest precipitation levels in the world. The stability of slopes in different parts of Taiwan is influenced by all of these factors. The study's instances are the National Freeway 1 and 5 slopes, where several landslide and rockfall incidents have occurred. This study used PLAXIS 2D CE finite element software to simulate and analyze the safety of highway slope protection projects. Displacements induced by normal and high groundwater levels were discussed. Moreover, a pseudo-static study of slope displacements under seismic conditions was performed. According to the results of the numerical study, the force operating on the slope was centered on the sliding surface when the groundwater level was normal, and it extended to the top when the groundwater level was high. By comparison, under seismic conditions, the force acting on the slope extended to the whole slope.

  • Open Access

    Applying Microbial-Induced Calcium Carbonate Precipitation Technology to Improve the Bond Strength of Lightweight Aggregate Concrete after High-Temperature Damage

    by How-Ji Chen, Yung-Hsiang Lo, Chao-Wei Tang, Han-Wen Chang

    High temperatures and external force can easily lead to a decline in the bond strength of reinforced concrete components. Microbial-induced calcium carbonate precipitation (MICP) technology has considerable potential for repairing concrete. Given this, this study utilized MICP technology to improve the bond strength of heat- and pull-damaged lightweight aggregate concrete (LWAC). The specimens of a control group (Group A) and two experimental groups (Group B and Group C) were prepared. The experimental group was prepared using lightweight aggregates (LWAs) that had been immersed in a nutrient solution and a bacterial solution. The control group was prepared using LWAs that were not immersed in a nutrient solution or bacterial solution. These specimens healed themselves in different ways after exposure to high temperatures (300 °C and 500 °C) and pull-out damage. Groups A and B adopted the same self-healing method; that is, their specimens were placed in a computer-controlled incubator at 40 °C. Group C used different self-healing methods. The specimens in this group were soaked in a mixed solution of urea and calcium acetate at 40 °C for two days and then taken out and placed in an incubator at 40 °C for two days. A cycle took four days until the expected self-healing age was reached. After being exposed to 300 °C and self-healed for 90 days, the residual bond strengths of the secondary pull-out tests in Groups A, B, and C were 20.63, 22.13, and 25.69 MPa, respectively. Moreover, compared with Group A, the relative bond strength ratios of the secondary pull-out tests in Groups B and C increased by 5.8% and 20.3%, respectively. This demonstrates that MICP technology could effectively improve the bond strength of LWAC after high-temperature and pull-out damage.


  • Open Access

    Applying MICP Technology to Improve the Bond Strength of LWAC after High-Temperature Damage

    by How-Ji Chen, Yung-Hsiang Lo, Chao-Wei Tang, Han-Wen Chang

    This study aimed to use biomineralization technology to improve the bond strength of fiber-reinforced lightweight aggregate concrete (LWAC) after exposure to temperatures of 300 °C and 500 °C. The specimens of a control group (Group A) and two experimental groups (Group B and Group C) were prepared. These specimens healed themselves in different ways after exposure to high temperatures and pull-out tests. The self-healing method of Group A involved placing the specimen into an incubator. The self-healing method of Group B was the same as that of Group A. The self-healing method of Group C involved immersing the specimen in a mixed solution of urea and calcium acetate for two days, then taking it out and placing it in an incubator for two days. A cycle of four days was undertaken until the desired age was reached. After the specimens were healed to the planned age, the first and secondary pull-out tests and repair compound identification were carried out. After exposure to a temperature of 300 °C and self-healing for 90 days, compared with the specimens in Group A, the relative bond strength ratios of the secondary pull-out tests of the specimens in Group C increased by 20.3%. This indicates that biomineralization can effectively improve the bond strength of LWAC after high-temperature damage.

  • Open Access

    The Evaluation of the Effectiveness of Biomineralization Technology in Improving the Strength of Damaged Fiber-Reinforced LWAC

    by How-Ji Chen, Tsung-Kai Chen, Chao-Wei Tang, Han-Wen Chang

    Concrete cracks and local damage can affect the bond performance between concrete and steel bars, thereby reducing the durability of reinforced concrete structures. Compared with general concrete crack repair methods, biomineralization repair not only has effective bonding capabilities but is also particularly environmentally friendly. Therefore, this study aimed to apply biomineralization technology to repair damaged fiber-reinforced lightweight aggregate concrete (LWAC). Two groups of LWAC specimens were prepared. The experimental group used lightweight aggregates (LWAs) containing bacterial spores and nutrient sources, while the control group used LWAs without bacterial spores and nutrient sources. These specimens were first subjected to compression tests and pull-out tests, respectively, and thus were damaged. After the damaged specimen healed itself in different ways for 28 days, secondary compression and pull-out tests were conducted. The self-healing method of the control group involved placing the specimens in an incubator. The experimental group was divided into experimental group I and experimental group II according to the self-healing method. The self-healing method of experimental group I was the same as that of the control group. The self-healing method of experimental group II involved soaking the specimen in a mixed solution of urea and calcium acetate for two days, and then taking it out and placing it in an incubator for two days, with a cycle of four days. The test results show that in terms of the relative bond strength ratio, the experimental group II increased by 17.9% compared with the control group. Moreover, the precipitate formed at the cracks in the sample was confirmed to be calcium carbonate with the EDS and XRD analysis results, which improved the compressive strength and bond strength after self-healing. This indicates that the biomineralization self-healing method used in experimental group II is more effective.


  • Open Access

    Evaluation of the Effectiveness of Biomineralization Technology in Repairing the Strength of Damaged Fiber-Reinforced LWAC

    by How-Ji Chen, Tsung-Kai Chen, Chao-Wei Tang, Han-Wen Chang

    Concrete cracks and local damage can affect the bond performance between concrete and steel bars, thereby reducing the durability of reinforced concrete structures. Compared with general concrete crack repair methods, biomineralization repair not only has effective bonding capabilities but is also particularly environmentally friendly. In view of this, this study aimed to apply biomineralization technology to repair damaged fiber-reinforced lightweight aggregate concrete (LWAC). Two groups of LWAC specimens were prepared. The control group used lightweight aggregates (LWAs) without bacterial spores and nutrient sources, and the experimental group used LWAs containing bacterial spores and nutrient sources. These specimens were first subjected to compression tests and pull-out tests, respectively, and thus were damaged. After the damaged specimen healed itself in different ways for 28 days, secondary compression and pull-out tests were conducted. The self-healing method of the control group involved placing the specimens in an incubator. The experimental group was further divided into experimental group I and experimental group II. The self-healing method of experimental group I was the same as that of the control group. The self-healing method of experimental group II involved soaking the specimen in a mixed solution of urea and calcium acetate for two days, and then taking it out and placing it in an incubator for two days, with a cycle of four days. The test results showed that, compared with the control group specimens, the relative bond strength ratio of the experimental group II specimens increased by 17.9%. Moreover, the EDS and XRD analysis results confirmed that the precipitate formed at the crack was calcium carbonate, which improved the compressive strength and bond strength after self-healing. This indicates that the biomineralization maintenance method used in experimental group II is more effective.


  • Open Access

    An Extended Special Issue on Advances in High-Performance Fiber-Reinforced Concrete

    by Chao-Wei Tang

    Adding fiber to cement concrete can improve the shortcomings of concrete, such as low tensile properties and low ductility, and improve its resistance to permeability and impact


  • Open Access

    Evaluation of the Superiority of Lightweight-Aggregate-Concrete Prestressed Box Girders in Terms of Durability and Prestress Loss

    by How-Ji Chen, Cheng-Chang Kuo, Chao-Wei Tang

    This case study aimed to compare the differences in the durability and prestress loss between normal-weight-concrete (NC) and lightweight-aggregate-concrete (LWC) prestressed box girders, which were constructed at the same time in the same area, so as to verify the superiority of using synthetic lightweight aggregate (LWA) made from reservoir sediments in prestressed bridges. For the NCs and LWCs used in the prestressed box girders, the basic mechanical properties (compressive strength, flexural strength, splitting tensile strength, and elastic modulus) were tested, as well as the durability properties (chloride ion penetration resistance and rapid chloride permeability). Then, through the prestress-monitoring system, the prestress losses of the two groups of prestressed box girders were tracked. The results of the durability test confirmed that LWC can inhibit the penetration of air, water, and chloride ions by strengthening the interfacial transition zone between the aggregate and the cement paste, thereby improving its durability. Moreover, the magnetic-flux prestress loss of the NC prestressed box girder reached 8.1%. In contrast, the magnetic-flux prestress losses on both sides of the LWC prestressed box girder were 4.6% and 4.9%, respectively. This verified that, under the same environmental conditions, the use of LWC produced less of a prestress loss than the use of NC.


  • Open Access

    Application of Biomineralization Technology in the Stabilization of Electric Arc Furnace Reducing Slag

    by How-Ji Chen, You-Ren Lin, Chao-Wei Tang, Yi-Chun Hung

    The unstable substances in steel slag are the main substances that affect its stability, which limits the large-scale resource utilization of steel slag. Most of the current methods for stabilizing electric arc furnace (EAF) slag are time-consuming and cannot be completely stabilized. In view of this, this study aimed to explore the feasibility of microbial-induced calcium carbonate precipitation (MICP) technology for stabilizing EAF reducing slag, and this was to be achieved by using the reaction between carbonate ions and free calcium oxide (f-CaO) in reducing slag to form a more stable calcium carbonate to achieve the purpose of stabilization. The test results showed that, when the EAF reducing slag aggregates (ERSAs) were immersed in a Sporosarcina pasteurii bacteria solution or water, the f-CaO contained in it would react such that stabilization was achieved. The titration test results showed that the f-CaO content of the ERSAs immersed in the bacterial solution and water decreased. The expansion test results of the ERSAs that were subjected to hydration showed that the seven-day expansion of ERSAs after biomineralization could meet the Taiwan regulation requirement of an expansion rate less than 0.5%. The thermogravimetric analysis showed that both the experimental group and the control group might contain calcium carbonate compounds. The results of the X-ray diffraction analysis showed that the CaCO3 content in the ERSAs that were immersed in the bacterial solution was significantly higher than those that were immersed in water. Moreover, the compressive strength test results of concrete prepared with ERSAs showed that the compressive strength of the control group concrete began to decline after 28 days. In contrast, the experimental group concrete had a good stabilization effect, and there was no decline in compressive strength until 180 days. At 240 days, the surface cracks of the experimental group were particularly small, while the surface of the control group showed obvious cracks. These results confirmed that a mineralization reaction with S. pasteurii bacteria could be used as a stabilization technology for ERSAs.