Duoqiang Zhao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Duoqiang Zhao has a total of 9 co-authors. Here are the top co-authors by number of shared publications:
- Yongming Chen
School of Metallurgy and Environment, Central South University, Changsha, China
3 shared publications - Chaobo Tang
School of Metallurgy and Environment, Central South University, Changsha 410083, China
2 shared publications - Jing He
School of Metallurgy and Environment, Central South University, Changsha 410083, China
2 shared publications - Shenghai Yang
School of Metallurgy and Environment, Central South University, Changsha 410083, China
2 shared publications - Yafei Jie
School of Metallurgy and Environment, Central South University, Changsha 410083, China
2 shared publications - Hao Li
School of Metallurgy and Environment, Central South University, Changsha 410083, China
1 shared publication
Latest Publications
- Open Access
Oxidizing Roasting Behavior and Leaching Performance for the Recovery of Spent LiFePO4 Batteries
In this study, the effects of oxidizing roasting process on the liberation of cathode materials from Al foil under different conditions were investigated systematically. The mineralogical characteristics of the cathode materials before and after thermal treatment were extensively characterized using scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS), X-ray diffraction (XRD) as well as Fourier transform infrared (FT-IR) spectroscopy and X-ray photoelectron spectroscopy (XPS). The results indicated that the increase in roasting temperature, oxygen concentration, and air flow rate enhanced the liberation of cathode materials. The cathode materials were gradually oxidized to Li3Fe2(PO4)3 and Fe2O3. Further, the carbon and fluorine content in the cathode materials decreased slowly during the thermal treatment, while the Al content increased. When the roasting temperature exceeded the melting point of Al, the Al foils were ablated and the cathode materials adhered to the Al foils again, resulting in difficulty in separation. The cathode materials leaching performance test results demonstrated that the oxidation of cathode materials had a negative effect on the leaching of Fe in sulfuric acid leaching system.
Open AccessOxidizing Roasting Behavior and Leaching Performance for the Recovery of Spent LiFePO4 Batteries
In this study, the effects of oxidizing roasting process on the liberation of cathode materials from Al foil under different conditions were investigated systematically. The mineralogical characteristics of the cathode materials before and after thermal treatment were extensively characterized using scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS), X-ray diffraction (XRD) as well as Fourier transform infrared (FT-IR) spectroscopy and X-ray photoelectron spectroscopy (XPS). The results indicated that the increase in roasting temperature, oxygen concentration, and air flow rate enhanced the liberation of cathode materials. The cathode materials were gradually oxidized to Li3Fe2(PO4)3 and Fe2O3. Further, the carbon and fluorine content in the cathode materials decreased slowly during the thermal treatment, while the Al content increased. When the roasting temperature exceeded the melting point of Al, the Al foils were ablated and the cathode materials adhered to the Al foils again, resulting in difficulty in separation. The cathode materials leaching performance test results demonstrated that the oxidation of cathode materials had a negative effect on the leaching of Fe in sulfuric acid leaching system.
- Open Access
Hydrometallurgical Process for Zinc Recovery from C.Z.O. Generated by the Steelmaking Industry with Ammonia–Ammonium Chloride Solution
In this research, some experimental steps were investigated to recover zinc contained in crude zinc oxide (C.Z.O.). In the first stage, the C.Z.O. was treated in NH3–NH4Cl–H2O solution to dissolve the metals. The optimized leaching conditions in batch experiments were obtained: agitation speed 250 rpm, concentration of ammonia and ammonium chloride 2.5 mol/L and 5 mol/L, respectively, time 30min, temperature 40 °C, and L/S = 6 mL/g. The extraction percentage of zinc was over 81% under the optimized leaching conditions. The kinetic study indicates that zinc extraction from the C.Z.O particles was very rapid. In the second stage, the solution from the leaching process was purified by adding zinc dust to the solution. The Cu, Cd, Pb, Sb, and As could be reduced to levels of 0.03, 0.09, 0.87, 0.22, and 0.12 mg/L after the purification process. Finally, the electrowinning process was used to recover dissolved Zn from the final solution. The zinc content in the electrowon zinc was more than 99.99%.
Open AccessHydrometallurgical Process for Zinc Recovery from C.Z.O. Generated by the Steelmaking Industry with Ammonia–Ammonium Chloride Solution
In this research, some experimental steps were investigated to recover zinc contained in crude zinc oxide (C.Z.O.). In the first stage, the C.Z.O. was treated in NH3–NH4Cl–H2O solution to dissolve the metals. The optimized leaching conditions in batch experiments were obtained: agitation speed 250 rpm, concentration of ammonia and ammonium chloride 2.5 mol/L and 5 mol/L, respectively, time 30min, temperature 40 °C, and L/S = 6 mL/g. The extraction percentage of zinc was over 81% under the optimized leaching conditions. The kinetic study indicates that zinc extraction from the C.Z.O particles was very rapid. In the second stage, the solution from the leaching process was purified by adding zinc dust to the solution. The Cu, Cd, Pb, Sb, and As could be reduced to levels of 0.03, 0.09, 0.87, 0.22, and 0.12 mg/L after the purification process. Finally, the electrowinning process was used to recover dissolved Zn from the final solution. The zinc content in the electrowon zinc was more than 99.99%.
- Open Access
Leaching Kinetics of Hemimorphite in Ammonium Chloride Solution
The leaching kinetics of hemimorphite (Zn4Si2O7(OH)2·H2O) in ammonium chloride solution was presented in detail. Effects of stirring speed (150–350 rpm), leaching temperature (75–108 °C), particle size of hemimorphite (45–150 μm), and the concentration of ammonium chloride (3.5–5.5 mol/L) on the zinc extraction rate were studied. The zinc extraction rate enhanced slightly with the increase in stirring speed, but increased significantly with an increase in the leaching temperature and ammonium chloride concentration. Zinc extraction was enhanced significantly in the first 60 min with decreasing particle size, but had little effect on the leaching process after 60 min. Scanning electron microscopy (SEM) analysis showed that some silica gel formed in the leaching process was not separated from the hemimorphite surface, but covered some of the active particle surface. The Elovich equation successfully described the leaching kinetics of hemimorphite in ammonium chloride solution with an apparent activation energy of 405.14 kJ/mol at temperatures of 75–90 °C and 239.61 kJ/mol at temperatures of 95–108 °C, which is characteristic for a chemically-controlled process. Silica gel is generated at temperatures of 75–90 °C and decomposed into silica at temperatures of 95–108 °C.
Open AccessLeaching Kinetics of Hemimorphite in Ammonium Chloride Solution
The leaching kinetics of hemimorphite (Zn4Si2O7(OH)2·H2O) in ammonium chloride solution was presented in detail. Effects of stirring speed (150–350 rpm), leaching temperature (75–108 °C), particle size of hemimorphite (45–150 μm), and the concentration of ammonium chloride (3.5–5.5 mol/L) on the zinc extraction rate were studied. The zinc extraction rate enhanced slightly with the increase in stirring speed, but increased significantly with an increase in the leaching temperature and ammonium chloride concentration. Zinc extraction was enhanced significantly in the first 60 min with decreasing particle size, but had little effect on the leaching process after 60 min. Scanning electron microscopy (SEM) analysis showed that some silica gel formed in the leaching process was not separated from the hemimorphite surface, but covered some of the active particle surface. The Elovich equation successfully described the leaching kinetics of hemimorphite in ammonium chloride solution with an apparent activation energy of 405.14 kJ/mol at temperatures of 75–90 °C and 239.61 kJ/mol at temperatures of 95–108 °C, which is characteristic for a chemically-controlled process. Silica gel is generated at temperatures of 75–90 °C and decomposed into silica at temperatures of 95–108 °C.