JQJuanping Qu

Juanping Qu

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Juanping Qu has a total of 10 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Recovering Iron Concentrate from Low-Grade Siderite Tailings Based on the Process Mineralogy Characteristics

    by He Wan, Peng Yi, Saija Luukkanen, Juanping Qu, Chonghui Zhang, Shenghong Yang, Xianzhong Bu

    Refractory iron ore is often discarded as tailings. This causes a great waste of iron resources. In this paper, the flash roasting-magnetic separation process was designed by combining the magnetic separation process of magnetite and the process mineralogy of iron tailings. The flash suspension roasting effects with 3–4 s roasting time were evaluated by magnetic separation. The MLA results show that the tailings are ground to a fineness of P90 −75 μm, where the distribution of siderite and M/H in the −75 μm particle size is 85.37% and 92.75%, respectively. Moreover, M/H and siderite are mainly associated with muscovite and quartz. This indicates that regrinding for contiguous bodies of M/H and siderite is beneficial for improving the grade and recovery of iron concentrates. The results of the flash roasting-magnetic separation process show that a mixed iron concentrate containing 60.10% Fe with an iron recovery of 81.13% would be achieved after selective grinding and staged magnetic separation of the roasted ore. The result indicates that the flash suspension roasting effects with 3–4 s roasting time are achievable. The study provides an efficient approach for recovering refractory iron from tailings.


  • Open Access

    Adsorption Behaviors of Straight-Chain Alkanes on a Molybdenite [001]/[100] Surface: A Molecular Dynamics Study

    by He Wan, Peng Yi, Juanping Qu, Xianzhong Bu, Wei Yang, Hui Li

    Straight-chain alkanes (SCA) as collectors can effectively enhance the floatability of molybdenite. In a previous study, SCA were found to have an excellent adsorption effect on the molybdenite [001] surface (MS001), but they exhibited no adsorption behavior on the molybdenite [100] surface (MS100). However, other studies have shown that SCA could adsorb on MS100. In this paper, the underlying cause of this contradictory conclusion was identified by molecular dynamics simulation. The results show that SCA could adsorb both MS001 and MS100. However, at low SCA dosages, SCA have a strong interaction with MS001 but desorb quickly on MS100. This leads to the selective adsorption of SCA on MS001. As SCA’s concentration gradually increases, the selective adsorption behavior of SCA on MS001 will be disrupted. Excessive SCA concentration will lead to its adsorption at MS100.


  • Open Access

    A Novel Method for Improving Low-Temperature Flotation Performance of Nonpolar Oil in the Molybdenite Flotation

    by He Wan, Juanping Qu, Hui Li, Tingshu He, Xianzhong Bu, Wei Yang

    Nonpolar hydrocarbon oil (NHO) is one of the most extensively used collectors in the flotation of molybdenite due to its excellent selectivity. However, NHO has low sensibility at pulp temperature. At low temperatures (<283 K), although more kerosene is used, the recovery of molybdenite flotation is still lower than at room temperature. In this study, magnetizing treatment, which is an efficient, low-cost, innovative, and environmentally friendly emulsification method, was used to improve the flotation performance of NHO in low-temperature molybdenite flotation. The test results showed that, compared with unmagnetized kerosene (UMK), the optimum dosage of magnetized kerosene (MK) could be reduced by 11% at 298 K. At the same dosage of kerosene, the flotation recovery of MK was 3% higher than UMK at 278 K. The surface tension measurement results showed that the surface tension of MK rose periodically as the magnetic field intensity increased, and there was a maximum surface tension within each period. Further, the magnetic field intensity had the maximum flotation recovery of molybdenite at the maximum surface tension of MK. Combined with the analysis based on the Girifalco–Good theory and the static drop volume method of interfacial tension, the interfacial tension of kerosene–water was shown to decrease with the increase of the surface tension of kerosene. This finding indicates that the dispersibility of kerosene in pulp could be improved by reducing the size of oil droplets, thereby improving the molybdenite flotation recovery of kerosene at low-temperature pulp. It is helpful to improve the flotation recovery of molybdenite using NHO as a collector for low-temperature pulp (<283 K).


  • Open Access

    A New Concept on High-Calcium Flotation Wastewater Reuse

    by He Wan, Juanping Qu, Tingshu He, Xianzhong Bu, Wei Yang, Hui Li

    Calcium ions are a kind of unavoidable ions in water. It has the deleterious effect on molybdenite flotation. High-calcium flotation wastewater (HCFW) was reused for flotation circuits after the pretreatment removing Ca2+ in from HCFW. The high cost of wastewater treatment limits HCFW reuse. In this paper, an efficient, innovative, low-cost and environmental-friendly flotation wastewater reuse technology was introduced. XLM, as a composite collector for molybdenite, is a mixture of diesel oil (DO) and polycyclic aromatic hydrocarbons (PAHs). It could reduce the deleterious effects of Ca2+ on the flotation of molybdenite in HCFW. Therefore, this was used to replace the pretreatment removing Ca2+ in from high Ca2+ wastewater and saved the cost of wastewater treatment. When XLM consists of 4 wt % PAHs and 96 wt % DO, it has better adaptability than DO in the different Ca2+ concentration of flotation water. The contact angle measurements indicated that PAHs, as a synergistic component of a composite collector, could adsorb on the edges of molybdenite in the presence of Ca2+ by forming PAHs-Ca2+-MoO42− structure to increase the contact angle of fine molybdenite particle and reduce the deleterious effects of Ca2+ on the flotation of molybdenite. The industrial-scale test further that demonstrated XLM can improve the molybdenite roughing recovery and grade by 1.8% and 3.46% compared with DO as the collector in high Ca2+ flotation wastewater. It is feasible and effective to replace high-cost wastewater treatment for molybdenum plants.