Hui-Yun Bor
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Hui-Yun Bor has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Sheng-Long Lee
Department of Mechanical Engineering, National Central University, Taoyuan, Taiwan
3 shared publications - Chao-Nan Wei
Chung-Shan Institute of Science and Technology, Taoyuan 32546, Taiwan
1 shared publication - Chih-Ting Wu
Department of Vehicle Engineering , Army Academy R.O.C. , Zhongli , Taoyuan City , Taiwan, R.O.C.
1 shared publication - Jing-Chie Lin
Institute of Material Science and Engineering, National Central University, Jhong-Li District, Tao-Yuan City 32001, Taiwan
1 shared publication - Jo-Kuang Nieh
Materials and Electro-Optics Research Division, National Chung-Shan Institute of Science and Technology, Taoyuan 320-338, Taiwan
1 shared publication - Kung-Hui Liu
Institute of Material Science and Engineering, National Central University, Jhongli 32001, Taiwan
1 shared publication
Latest Publications
- Open Access
Effects of Mn, Zn Additions and Cooling Rate on Mechanical and Corrosion Properties of Al-4.6Mg Casting Alloys
The mechanical properties of the Al-Mg alloy can be enhanced by adding metallic elements, but a continuous distribution of precipitates at grain boundaries leads to intergranular corrosion during sensitization treatment. In the present work, Mn, Zn additions, water cooling and furnace cooling were executed to investigate their effects on the mechanical and corrosion properties of the Al-4.6Mg alloy. Our results show that adding Mn to Al-4.6Mg alloys may produce grain refinement and dispersion strengthening, increasing tensile strength and hardness. The presence of Mn did not affect the corrosion resistance of Al-Mg alloys. Adding Zn to the Al-4.6Mg alloy increased tensile strength and hardness, but decreased corrosion resistance. Combined, the addition of Mn and Zn to the Al-4.6Mg alloy exhibited the highest tensile strength and hardness, but seriously reduced corrosion resistance. Furnace cooling substituted for water quenching could avoid intergranular corrosion, but slightly decreased the tensile strength and hardness by 7.0% and 6.8%, respectively.
Open AccessEffects of Mn, Zn Additions and Cooling Rate on Mechanical and Corrosion Properties of Al-4.6Mg Casting Alloys
The mechanical properties of the Al-Mg alloy can be enhanced by adding metallic elements, but a continuous distribution of precipitates at grain boundaries leads to intergranular corrosion during sensitization treatment. In the present work, Mn, Zn additions, water cooling and furnace cooling were executed to investigate their effects on the mechanical and corrosion properties of the Al-4.6Mg alloy. Our results show that adding Mn to Al-4.6Mg alloys may produce grain refinement and dispersion strengthening, increasing tensile strength and hardness. The presence of Mn did not affect the corrosion resistance of Al-Mg alloys. Adding Zn to the Al-4.6Mg alloy increased tensile strength and hardness, but decreased corrosion resistance. Combined, the addition of Mn and Zn to the Al-4.6Mg alloy exhibited the highest tensile strength and hardness, but seriously reduced corrosion resistance. Furnace cooling substituted for water quenching could avoid intergranular corrosion, but slightly decreased the tensile strength and hardness by 7.0% and 6.8%, respectively.
- Open Access
Electrical and Physical Characteristics of WO3/Ag/WO3 Sandwich Structure Fabricated with Magnetic-Control Sputtering Metrology †
In this work, three layers of transparent conductive films of WO3/Ag/WO3 (WAW) were deposited on a glass substrate by radio frequency (RF) magnetron sputtering. The thicknesses of WO3 (around 50~60 nm) and Ag (10~20 nm) films were mainly the changeable factors to achieve the optimal transparent conductivity attempting to replace the indium tin oxide (ITO) in cost consideration. The prepared films were cardinally subjected to physical and electrical characteristic analyses by means of X-ray diffraction analysis (XRD), field-emission scanning electron microscope (FE-SEM), and Keithley 4200 semiconductor parameter analyzer. The experimental results show as the thickness of the Ag layer increases from 10 nm to 20 nm, the resistance becomes smaller. While the thickness of the WO3 layer increases from 50 nm to 60 nm, its electrical resistance becomes larger.
Open AccessElectrical and Physical Characteristics of WO3/Ag/WO3 Sandwich Structure Fabricated with Magnetic-Control Sputtering Metrology †
In this work, three layers of transparent conductive films of WO3/Ag/WO3 (WAW) were deposited on a glass substrate by radio frequency (RF) magnetron sputtering. The thicknesses of WO3 (around 50~60 nm) and Ag (10~20 nm) films were mainly the changeable factors to achieve the optimal transparent conductivity attempting to replace the indium tin oxide (ITO) in cost consideration. The prepared films were cardinally subjected to physical and electrical characteristic analyses by means of X-ray diffraction analysis (XRD), field-emission scanning electron microscope (FE-SEM), and Keithley 4200 semiconductor parameter analyzer. The experimental results show as the thickness of the Ag layer increases from 10 nm to 20 nm, the resistance becomes smaller. While the thickness of the WO3 layer increases from 50 nm to 60 nm, its electrical resistance becomes larger.
- Open Access
Effect of Trace Be and Sc Additions on the Mechanical Properties of A357 Alloys
The effect of the addition of Be and Sc on the microstructure and mechanical properties of A357 alloy were systematically investigated. The results show that the addition of small amounts of Be and Sc could change the acicular structure of iron-bearing intermetallic compounds to harmless compact Al-Fe-Si and Sc-Fe iron-bearing intermetallic compounds. Compact iron-bearing intermetallic compounds could improve fluidity, causing a reduction in interdendritic shrinkage during solidification. The addition of 0.05 wt % Be enhanced the quality index of the A357 alloy by 11% and increased the notch-yield ratio of fracture toughness by 4.5%. In contrast, the addition of 0.05 wt % Sc increased the quality index and the notch to yield ratio of fracture toughness up to 17% and 9%, respectively. Therefore, the microstructure and mechanical properties of the A357 alloy could be improved by substituting Be with Sc.
Open AccessEffect of Trace Be and Sc Additions on the Mechanical Properties of A357 Alloys
The effect of the addition of Be and Sc on the microstructure and mechanical properties of A357 alloy were systematically investigated. The results show that the addition of small amounts of Be and Sc could change the acicular structure of iron-bearing intermetallic compounds to harmless compact Al-Fe-Si and Sc-Fe iron-bearing intermetallic compounds. Compact iron-bearing intermetallic compounds could improve fluidity, causing a reduction in interdendritic shrinkage during solidification. The addition of 0.05 wt % Be enhanced the quality index of the A357 alloy by 11% and increased the notch-yield ratio of fracture toughness by 4.5%. In contrast, the addition of 0.05 wt % Sc increased the quality index and the notch to yield ratio of fracture toughness up to 17% and 9%, respectively. Therefore, the microstructure and mechanical properties of the A357 alloy could be improved by substituting Be with Sc.
- 7 February 2013
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 44 (6) , 2831-2838
Effect of Natural Aging and Cold Working on Microstructures and Mechanical Properties of Al-4.6Cu-0.5Mg-0.5Ag alloy
- 7 February 2013
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 44 (6) , 2831-2838
Effect of Natural Aging and Cold Working on Microstructures and Mechanical Properties of Al-4.6Cu-0.5Mg-0.5Ag alloy