Yanzhen Bo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yanzhen Bo has a total of 4 co-authors. Here are the top co-authors by number of shared publications:
- Biao Ma
Chang’an University
1 shared publication - Kun Wei
School of Highway, Chang’an University, Xi’an, Shaanxi 710064, People’s Republic of China
1 shared publication - Xueyan Zhou
Key Laboratory for Special Area Highway Engineering of Ministry of Education, Chang’an University, Xi’an 710064, China
1 shared publication - Zhanping You
Michigan Technological Univ
1 shared publication
Latest Publications
- Open Access
- 23 May 2017
- Published by MDPI AG in Applied Sciences
- Vol. 7 (6) , 523
Analysis of Preparation and Properties on Shape Memory Hydrogenated Epoxy Resin Used for Asphalt Mixtures
The objective of this investigation is to prepare the shape memory hydrogenated epoxy resin used for asphalt mixtures (SM-HEP-AM) and study its properties. The shape memory hydrogenated epoxy resin (SM-HEP) is prepared using hydrogenated bisphenol A epoxy resin (AL-3040), polypropylene glycol diglycidylether diacrylate (JH-230), and isophorone diamine (IPDA). The formulations of the SM-HEP-AM are obtained by the linearly fitted method. The thermo-mechanical property, molecular structure, and shape-memory performance of the SM-HEP-AM are studied. The glass-transition temperature (Tg) is determined using the differential scanning calorimeter (DSC). The results proved that the Tg level increased when the JH-230 content decreased. The thermo-mechanical property of the SM-HEP-AM is measured by dynamical mechanical analysis (DMA). The storage modulus of the SM-HEP-AM decreased with the increase in the JH-230 content. The above phenomena are attributed to the change in the JH-230 content. The shape memory performance results of the SM-HEP-AM indicate that specimen deformation can completely recover after only several minutes at Tg + 10 °C and Tg + 20 °C. The shape recovery time of the SM-HEP-AM increases with increased JH-230 content, and the change between the shape recovery time and JH-230 content gradually decreased as the temperature increased. The deformation recovery performance of asphalt mixture with and without the SM-HEP-AM (Tg = 40 °C) was tested by the deformation recovery test. This was used to prove that the SM-HEP-AM helps to improve the deformation recovery performance of the asphalt mixture.
- 23 May 2017
- Published by MDPI AG in Applied Sciences
- Vol. 7 (6) , 523
Open AccessAnalysis of Preparation and Properties on Shape Memory Hydrogenated Epoxy Resin Used for Asphalt Mixtures
The objective of this investigation is to prepare the shape memory hydrogenated epoxy resin used for asphalt mixtures (SM-HEP-AM) and study its properties. The shape memory hydrogenated epoxy resin (SM-HEP) is prepared using hydrogenated bisphenol A epoxy resin (AL-3040), polypropylene glycol diglycidylether diacrylate (JH-230), and isophorone diamine (IPDA). The formulations of the SM-HEP-AM are obtained by the linearly fitted method. The thermo-mechanical property, molecular structure, and shape-memory performance of the SM-HEP-AM are studied. The glass-transition temperature (Tg) is determined using the differential scanning calorimeter (DSC). The results proved that the Tg level increased when the JH-230 content decreased. The thermo-mechanical property of the SM-HEP-AM is measured by dynamical mechanical analysis (DMA). The storage modulus of the SM-HEP-AM decreased with the increase in the JH-230 content. The above phenomena are attributed to the change in the JH-230 content. The shape memory performance results of the SM-HEP-AM indicate that specimen deformation can completely recover after only several minutes at Tg + 10 °C and Tg + 20 °C. The shape recovery time of the SM-HEP-AM increases with increased JH-230 content, and the change between the shape recovery time and JH-230 content gradually decreased as the temperature increased. The deformation recovery performance of asphalt mixture with and without the SM-HEP-AM (Tg = 40 °C) was tested by the deformation recovery test. This was used to prove that the SM-HEP-AM helps to improve the deformation recovery performance of the asphalt mixture.