SYShenghua Yin

Shenghua Yin

*This is an algorithmically generated author record based on publicly available information.

Shenghua Yin has a total of 7 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Degradation Behavior of Concrete after Freeze-Thaw Cycles and Then Exposure to High Temperatures

    by Qifang Xie, Liujie Yang, Fangzheng Hu, Wenming Hao, Shenghua Yin, Lipeng Zhang

    Concrete behavior usually degrades due to freeze-thaw cycles, fire, or both. Existing studies on the degradation behavior of concrete due to exposure to high temperatures were primarily focused on unfrozen concrete. In this paper, the degradation behavior of damaged concrete, after different freeze-thaw cycles (25, 35, 45, and 55 cycles), exposure temperatures (20°C, 300°C, 400°C, and 500°C), and cooling methods (water-cooled and air-cooled), was tested with seventy-five prism specimens. The degradation behavior of the damaged concrete, such as surface characteristics, weight loss, compressive strength, peak strains, and elastic modulus, was studied and analyzed. Results show that (i) the surface color of the concrete does not change significantly throughout the test. As the number of freeze-thaw cycles and temperatures increase, the weight loss of the concrete specimens increases gradually. (ii) After freeze-thaw cycles, the relative strengths and elastic modulus of the concrete specimens significantly degrade compared with those of the unfrozen ones at same temperatures. (c) At elevated number of freeze-thaw cycles and exposure temperatures, the peak strain of the concrete increases gradually. (d) Cooling methods have different effects on the degradation of concrete under different number of freeze-thaw cycles. Finally, a uniaxial compression constitutive model for concrete after freeze-thaw cycles and then exposure to high temperatures was established and a good agreement was observed with test results.


  • Open Access

    Effects of High Temperatures on the Physical and Mechanical Properties of Carbonated Ordinary Concrete

    by Qifang Xie, Lipeng Zhang, Shenghua Yin, Baozhuang Zhang, Yaopeng Wu

    Fires are always known for seriously deteriorating concrete in structures, especially for those with certain carbonation due to long-time service. In this paper, 75 prism specimens were prepared and divided into four groups (three carbonated groups and one uncarbonated group). Specimens were tested under different temperatures (20, 300, 400, 500, 600, and 700°C), exposure times (3, 4, and 6 hours), and cooling methods (water and natural cooling). Surface characteristics, weight loss rate, and residual mechanical properties (strength, initial elastic modulus, peak, and ultimate compressive strains) of carbonated concrete specimens after elevated temperatures were investigated and compared with that of the uncarbonated ones. Results show that the weight loss rates of the carbonated concrete specimens are slightly lower than that of the uncarbonated ones and that the cracks are increased with raising of temperatures. Surface colors of carbonated concrete are significantly changed, but they are not sensitive to cooling methods. Surface cracks can be evidently observed on carbonated specimens when temperature reaches 400°C. Residual compressive strength and initial elastic modulus of carbonated concrete after natural cooling are generally larger than those cooled by water. The peak and ultimate compressive strains of both carbonated and uncarbonated concrete specimens increase after heating, but the values of the latter are greater than that of the former. Finally, the constitutive equation to predict the compressive behaviors of carbonated concrete after high temperatures was established and validated by tests.