Cristiane Reis Martins
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Cristiane Reis Martins has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- Alexandre Oka Thomaz Cordeiro
Universidade Federal de Sao Paulo, Brasil
2 shared publications - Julia Baruque-Ramos
Universidade de São Paulo
2 shared publications - Lais Kohan
Centre for Textile Science and Technology (2C2T), University of Minho
2 shared publications Alexandre Oka Thomaz Cordeiro
Universidade Federal de Sao Paulo, Brasil
1 shared publication- Christiane de Arruda Rodrigues
Federal University of São Paulo
1 shared publication - Daniela Santoro Rosa
Center for Engineering, Modeling, and Applied Social Sciences (CECS), Federal University of ABC (UFABC), Santo André, Brazil
1 shared publication
Latest Publications
- Open Access
- 1 January 2025
- Published by FapUNIFESP (SciELO) in Polímeros
- Vol. 35 (3)
Sustainable styrene-butadiene composites with sisal fiber and rubber waste from footwear
This study examines the impact of three surface treatment methods on sisal fibers used as reinforcement in styrene-butadiene rubber (SBR) composites: washing with water, alkaline treatment (mercerization), and silanization, with each composite containing 5 wt% of fibers. The preparation process involved using an internal mixer and rubber mixing mill to shape the composites, followed by vulcanization in an automated system press. The effectiveness of the treatments was evaluated using scanning electron microscopy, along with tensile tests, rheometer analysis, and measurements of hardness and density. The treatments enhanced fiber modification by increasing surface roughness through the grafting of silanol groups, thereby improving their interaction with the elastomeric matrix. Notably, composites reinforced with silanized fibers exhibited the highest performance and interaction among the various treatment methods, showing a higher modulus at 100%. Alkaline and silanization treatments reduced vulcanization time. Sisal fibers combined with SBR waste can promote sustainability in the footwear industry.
- 1 January 2025
- Published by FapUNIFESP (SciELO) in Polímeros
- Vol. 35 (3)
Open AccessSustainable styrene-butadiene composites with sisal fiber and rubber waste from footwear
This study examines the impact of three surface treatment methods on sisal fibers used as reinforcement in styrene-butadiene rubber (SBR) composites: washing with water, alkaline treatment (mercerization), and silanization, with each composite containing 5 wt% of fibers. The preparation process involved using an internal mixer and rubber mixing mill to shape the composites, followed by vulcanization in an automated system press. The effectiveness of the treatments was evaluated using scanning electron microscopy, along with tensile tests, rheometer analysis, and measurements of hardness and density. The treatments enhanced fiber modification by increasing surface roughness through the grafting of silanol groups, thereby improving their interaction with the elastomeric matrix. Notably, composites reinforced with silanized fibers exhibited the highest performance and interaction among the various treatment methods, showing a higher modulus at 100%. Alkaline and silanization treatments reduced vulcanization time. Sisal fibers combined with SBR waste can promote sustainability in the footwear industry.
- Open Access
- 9 April 2022
- Published by Springer Nature in Materials Circular Economy
- Vol. 4 (1) , 1-10
Cotton Weaving Waste Incorporation in PVC Composites
The largest amount of solid waste from the textile industries is mainly derived from fabric manufacturing until the cutting stage: hard fibers (spinning waste), beaming and soft fibers (weaving yarn waste), and off-cuts (cutting process). This research aimed to (i) conduct an exploratory interview with a large Brazilian cotton textile manufacturer to identify its main solid waste and corresponding destinations; and (ii) produce and evaluate PVC composites reinforced with cotton textile residues from the weaving process. Cotton fibrous reinforcements in the proportion of 2.5% (w/w) presented the best results of tensile strength and elongation concerning the others. Briquette residue (2.5%) had better dispersion in the matrix and slightly higher tensile strength when compared to other residues. The composites presented different visual aspects, and their use in fashion products with sustainable appeal could be a viable alternative. Therefore, additional tests should be performed to ensure the appropriate mechanical properties for applications in this and other areas.
- 9 April 2022
- Published by Springer Nature in Materials Circular Economy
- Vol. 4 (1) , 1-10
Open AccessCotton Weaving Waste Incorporation in PVC Composites
The largest amount of solid waste from the textile industries is mainly derived from fabric manufacturing until the cutting stage: hard fibers (spinning waste), beaming and soft fibers (weaving yarn waste), and off-cuts (cutting process). This research aimed to (i) conduct an exploratory interview with a large Brazilian cotton textile manufacturer to identify its main solid waste and corresponding destinations; and (ii) produce and evaluate PVC composites reinforced with cotton textile residues from the weaving process. Cotton fibrous reinforcements in the proportion of 2.5% (w/w) presented the best results of tensile strength and elongation concerning the others. Briquette residue (2.5%) had better dispersion in the matrix and slightly higher tensile strength when compared to other residues. The composites presented different visual aspects, and their use in fashion products with sustainable appeal could be a viable alternative. Therefore, additional tests should be performed to ensure the appropriate mechanical properties for applications in this and other areas.
- 2 March 2022
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 282
Microstructure and corrosion behavior of as-quenched CuAl-based alloys
- 2 March 2022
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 282
Microstructure and corrosion behavior of as-quenched CuAl-based alloys
- 30 May 2020
- Published by Springer Nature in Journal of Solid State Electrochemistry
- Vol. 24 (8) , 1877-1888
Characterization of nanotubular oxide layer grown on Ti14wt.%Nb alloy by anodization and its performance in photoelectrocatalytic process
- 30 May 2020
- Published by Springer Nature in Journal of Solid State Electrochemistry
- Vol. 24 (8) , 1877-1888
Characterization of nanotubular oxide layer grown on Ti14wt.%Nb alloy by anodization and its performance in photoelectrocatalytic process
- Open Access
- 1 January 2020
- Published by FapUNIFESP (SciELO) in Polímeros
- Vol. 30 (4)
The incorporation of untreated and alkali-treated banana fiber in SEBS composites
In this work, banana fiber was used as reinforcement for the preparation of a thermoplastic elastomer composite (TPE). Few studies are exploring the natural fiber incorporation on TPEs, with no one using banana fiber. The fiber was extracted from banana pseudostem and modified with an alkaline solution. The untreated and treated banana fibers were incorporated in 2%, 5%, and 10% in SEBS. The mixture was performed in a thermokinetic mixer (K-Mixer) and plates prepared by compression molding. The composites were characterized by Scanning Electron Microscopic (SEM), tensile testing, mechanical dynamical analysis (DMA). It can be observed that the samples with untreated fibers presented a higher tensile strength, except for the incorporation of 5% of BF. Young's modulus increase as the fiber's incorporation grows, indicating greater rigidity of the composite. It was found that the chemically treated banana fiber composites, e.g., TPE/TBF5 and TPE/TBF10, shows a 15.4% and 22.2% higher elongation.
- 1 January 2020
- Published by FapUNIFESP (SciELO) in Polímeros
- Vol. 30 (4)
Open AccessThe incorporation of untreated and alkali-treated banana fiber in SEBS composites
In this work, banana fiber was used as reinforcement for the preparation of a thermoplastic elastomer composite (TPE). Few studies are exploring the natural fiber incorporation on TPEs, with no one using banana fiber. The fiber was extracted from banana pseudostem and modified with an alkaline solution. The untreated and treated banana fibers were incorporated in 2%, 5%, and 10% in SEBS. The mixture was performed in a thermokinetic mixer (K-Mixer) and plates prepared by compression molding. The composites were characterized by Scanning Electron Microscopic (SEM), tensile testing, mechanical dynamical analysis (DMA). It can be observed that the samples with untreated fibers presented a higher tensile strength, except for the incorporation of 5% of BF. Young's modulus increase as the fiber's incorporation grows, indicating greater rigidity of the composite. It was found that the chemically treated banana fiber composites, e.g., TPE/TBF5 and TPE/TBF10, shows a 15.4% and 22.2% higher elongation.
- 22 July 2019
- Published by Springer Nature in SN Applied Sciences
- Vol. 1 (8) , 1-10
Panorama of natural fibers applied in Brazilian footwear: materials and market
- 22 July 2019
- Published by Springer Nature in SN Applied Sciences
- Vol. 1 (8) , 1-10
Panorama of natural fibers applied in Brazilian footwear: materials and market