ASAli Sadooghi

Ali Sadooghi

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Ali Sadooghi has a total of 41 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Experimental Study of Mechanical and Impact Behavior of Novel Fiber‐Reinforced Honeycomb Composites

    by Farzad Rahmani, Ali Sadooghi, Seyed Jalal Hashemi, Sahar Jafari

    In this study, composite honeycomb structures were fabricated using unsaturated polyester resin reinforced with carbon and glass fibers. Honeycomb structures are widely used in lightweight engineering applications due to their high strength‐to‐weight ratio and excellent energy absorption capability. The main objective of this research was to investigate the effect of reinforcement fiber type and architecture on the mechanical behavior of composite honeycomb structures under different loading conditions. Specimens with identical geometries and different reinforcement configurations were manufactured using a controlled molding process. Compressive, flexural, and impact tests were carried out to evaluate the structural performance of the samples. The results indicated that carbon woven reinforced honeycomb structures exhibited the highest mechanical performance, achieving maximum compressive and flexural failure forces of approximately 6090 and 1517 N, respectively. Glass woven reinforced samples showed greater deformation capability and more progressive energy absorption, particularly under impact loading. In contrast, chopped‐strand reinforced structures demonstrated reduced load‐carrying capacity due to fiber discontinuity. Overall, woven reinforcement architectures provided superior strength, structural stability, and impact resistance. Scanning electron microscopy (SEM) was employed to investigate fracture surfaces and failure mechanisms.


  • Open Access

    Advancing Mechanical Properties of Polypropylene Matrix Composites: Analysis of Diverse Reinforcing Fillers

    by Ali Sadooghi, Seyed Jalal Hashemi, Vahid Zal, Farzad Rahmani, Kaveh Rahmani, Mahdi Bodaghi

    Currently, much research is being conducted on increasing the strength of thermoplastic polymers using various additives. Polypropylene (PP) is widely used in the automotive industry and electrical equipment. In this paper, using various reinforcing particles/fibers, including calcium carbonate, CaCO3, (at 20%, 25%, and 30% weight percentages), 20% talc, and 20% barite particles, as well as 30% glass fibers (GFs) (with varying L/D ratios, 200, 250, and 300) were integrated. First, PP and additives were mixed homogeneously by an extrusion process, and then test samples were made by high‐pressure injection of the extruded product into the mold. Various tests, including tensile, impact, and melt flow index (MFI) tests, were conducted to investigate the effect of additives on the properties of composites produced by plastic injection molding. SEM analysis was used to examine the fracture cross‐section of the samples and the distribution of additives. Results revealed significant outcomes across multiple tests: the addition of reinforcing particles led to a reduction in yield strain while creating notable variations in yield strength. Charpy impact tests demonstrated varied energy absorption, with the highest observed in the 30% GF sample (with L/D ratio of 350). Furthermore, the incorporation of reinforcing particles and fibers increased the heat deflection temperature, with the 30% GF sample exhibiting the highest value. Additionally, reinforcements effectively mitigated shrinkage, with significant reductions noted in samples containing talc and GF. The PP sample displayed a shrinkage rate of 19.1%. This figure significantly decreased to 1.42% and 0.26% for the samples reinforced by talc and GF [L/D = 350]. Furthermore, the introduction of GFs resulted in a decreased MFI, while other particles exhibited minimal impact.


  • Open Access

    Enhancing Compressive and Crush Performance of 3D‐Printed ABS Thin‐Walled Tubes Through Glass Fiber Reinforcement and Polyurethane Foam Infusion

    by Ali Sadooghi, Seyed Jalal Hashemi, Sadegh Mirzamohammadi, Farzad Rahmani, Kaveh Rahmani

    This study introduces a novel approach to enhancing the mechanical performance of 3D‐printed acrylonitrile butadiene styrene (ABS) thin‐walled circular tubes by incorporating varying percentages of glass fibers and filling them with different types of polyurethane (PU) foam. Leveraging fused filament fabrication (FFF), the tubes were reinforced with glass fibers (0%, 5%, 10%, and 15%) and injected with soft, semisoft, and rigid PU foams to assess their impact on compressive strength and crush behavior. The experimental results revealed significant improvements in both failure force and energy absorption with the addition of glass fibers and PU foam. Notably, increasing the glass fiber content to 10% transformed brittle failure into a more ductile behavior, while the inclusion of PU foam further elevated the structural strength. The optimal configuration, comprising 10% glass fiber and rigid PU foam, achieved a remarkable compressive force of 3232.61 N and crushing resistance of 755.52 N. Conversely, the weakest performance was observed in samples with 15% glass fiber and no PU foam, underscoring the critical balance between reinforcement and material composition. Crucially, SEM analysis provided insights into the microstructural behavior of the samples, revealing strong bonding between the glass fibers and ABS matrix, as well as between the PU foam and tube walls. The SEM images also highlighted the transition from brittle to ductile failure modes, particularly in samples with optimal glass fiber content. This research demonstrates that the strategic combination of glass fibers and PU foams, coupled with detailed microstructural analysis, can significantly enhance the structural integrity of 3D‐printed components. These findings pave the way for the development of lightweight, high‐strength materials suitable for demanding applications in aerospace, automotive, and structural engineering.


  • Determining the Drucker-Prager Cap model constants using experimental, numerical and optimization for compacted Mg powders at different strain rates

    by K Rahmani, H Bakhtiari, H Malekmohammadi, A Sadooghi, F Khakbaz

    This article investigates an inverse approach to determine the coefficients of the Drucker-Prager model for magnesium powder. The approach involves conducting finite element simulations of the powder compression process within LS-DYNA software, employing the Drucker-Prager material model. The goal is to minimize the disparity between force-displacement outcomes derived from simulations and experimental data using a surrogate optimization method. Experimental data were obtained through a uniaxial compression test and served as a basis for adjusting the Cap model coefficients. A random selection of coefficients was made using the Latin cube method and simulations were performed based on the initial coefficients. The optimization was then performed using the particle swarm algorithm over 20 iterations. The optimized coefficients were validated against experimental data, demonstrating close agreement. By utilizing the extracted coefficients, the relative density of the samples was calculated at three different compaction speeds, i.e., 15.5 m s−1 (using a Hopkinson bar), 8 m s−1 (using a drop weight), and 1 mm min−1 (using an Instron machine). The analysis revealed the highest relative density and stress in the densified sample via the Hopkinson bar method, reaching 99.83% and 1.1 GPa, respectively.


  • Experimental Study of Polyester/Fiberglass/Stainless Steel Fiber Metal Laminates Mechanical Properties

    by Vahid Zal, Ali Sadooghi, Seyed Jalal Hashemi, Kaveh Rahmani, Amir H. Roohi, Hamid Khodayari, Jafar Babazadeh


  • Study on wear, corrosion and fatigue properties of dual metallic bearings coated with nickel and aluminum particles

    by Zahra Esfahani, Ali Sadooghi, Kaveh Rahmani, Seyed Jalal Hashemi

    One of the solutions for improving the mechanical properties is coating them with particles, which is carried out by various methods. In this study, dual metallic copper/steel bearings were investigated so that, one of them was an uncoated (S0) and three coated samples, nickel micro-particles (S1), nickel/aluminum micro-particles (S2), and nickel/aluminum nano-particles (S3) were produced. The samples were subjected to mechanical tests including micro hardness, wear, and scratch, and then their corrosion rate and fatigue life were evaluated. The results showed that creating a nano-sized coating on the sample improved their properties compared to the micro-sized and uncoated samples. The highest micro hardness was obtained for sample S3, which was equal to 103.6 HV, 18% higher than sample S0. The lowest wear and corrosion rates were also obtained for sample S3, which were equal to 0.38 mg m−1 and 3.14 mm year−1, respectively. Also, sample S3 had lowest delamination amount in the scratch test equal to 0.17 mm and most number of cycles until failure, 242 thousand cycles, in the fatigue test which was 76% more than the number of cycles spent on sample S0. Additionally, the microstructure of the corroded and worn surfaces of samples were examined by SEM imaging.


  • Open Access

    Investigation of structural, mechanical, and corrosion properties of steel 316L reinforcement by hBN and TiC particles

    by Amir H Roohi, Amirhossein Mirsadeghi, Ali Sadooghi

    The powder metallurgy process is commonly used to produce nanocomposite samples so that, their properties depend on the process parameters and the weight fraction of reinforcements. In the current study, producing metal matrix nanocomposite with steel 316L as a matrix and mixing of hBN/TiC nanoparticles as a reinforcement is conducted. The total weight percentages of reinforcements are 6% wt and 8% wt (i.e. with an equal proportion for each nanoparticle). The powders were mixed for 10 h and then compacted at different pressures (300 MPa and 400 MPa) by cold isostatic pressure (CIP) conditions. The compacted powders were sintered at different temperatures (1350 °C and 1450 °C), and times (2 h and 4 h) in the furnace. The microstructural analysis of nanocomposite was performed by SEM, XRD, EDX, DTA, and also FT-IR tests. The results showed that by increasing the weight fraction of nanoparticles the microhardness and wear rate improved and, on the contrary, the flexural strength and corrosion rate decreased. The optimum result for the microhardness and wear rate were achieved when the sample contains 8% wt nanoparticles, compacted at 400 MPa and sintered at 1350 °C for 4 h. As well, the highest flexural strength and corrosion rate belong to the sample compacted and sintered at 400 MPa, 1450 °C for 2 h.