Magdy Ahmed Mahmoud Ibrahim
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Magdy Ahmed Mahmoud Ibrahim has a total of 74 co-authors. Here are the top co-authors by number of shared publications:
Nobl F. El Boraei
11 shared publicationsIbrahim H. Elshamy
Chemistry Department, Faculty of Science, Ain Shams University, Abbassia, Egypt
9 shared publications- Manal A. El Sayed
Department of Chemistry, College of Science, Qassim University, Buraidah 51452, Saudi Arabia
5 shared publications - Inam M. A. Omar
Department of Chemistry, College of Science, Taibah University, Al Madinah Al Munawara 30002, Saudi Arabia
4 shared publications - Shimaa Abdel Halim
Department of Chemistry, Faculty of Education, Ain Shams University, Roxy, Cairo 11711, Egypt
4 shared publications - Aziza. S. El-Tabei
Egyptian Petroleum Research Institute, Nasr City, Cairo 11727, Egypt
3 shared publications
Latest Publications
- Open Access
- 18 November 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1)
Quantitative strengthening and corrosion correlation for partial and full substitution of nickel by nitrogen on AISI 316 stainless steel via VIM
Nickel stabilization of the austenitic phase in stainless steels faces economic and supply-chain pressures, motivating partial or near-complete nickel substitution through nitrogen alloying as an alternative alloy-design strategy. This study systematically evaluates partial (0.24 N, 6.56 wt% Ni retained) and near-complete (0.52 N, 0.01 wt% Ni) nitrogen substitution in AISI 316 stainless steel, produced via vacuum induction furnace (VIM) under controlled-nitrogen-pressure melting at 18 and 32 bar, respectively. Nitrogen addition refined austenite grain size by 53.4% (from 29 to 13.5 μm) and increased dislocation density from 0.13 × 10 14 to 1.97 × 10 14 m −2 , with the 0.52N alloy developing a duplex (γ + α) microstructure. A phase-resolved strengthening model decomposed yield strength contributions into grain refinement, solid-solution, and dislocation mechanisms, achieving good agreement with experimental results. Nitrogen shifted corrosion potential positively, reduced corrosion current density from 9.1 to 2.4 µA cm −2 , and EIS analysis showed the passive film’s charge-transfer resistance rising from 121.5 to 193.5 kΩ cm 2 with a corresponding fall in effective capacitance, while the electrical-equivalent film thickness recalculated from these parameters increases only modestly, from 0.10 to 0.12 nm. Dilatometry revealed a thermal instability window (780–840 °C) unique to the 0.52N alloy, consistent with thermally activated phase evolution within its γ + α duplex microstructure. The 0.24N alloy provides the most balanced combination of strength, ductility, corrosion resistance, and thermal stability among the investigated conditions, while the 0.52N alloy provides the highest strength but also exhibits greater phase complexity and a thermal-instability window; therefore, both alloys require application-specific validation of processing, weldability/forming behaviour, and long-term service performance before industrial deployment.
- 18 November 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1)
Open AccessQuantitative strengthening and corrosion correlation for partial and full substitution of nickel by nitrogen on AISI 316 stainless steel via VIM
Nickel stabilization of the austenitic phase in stainless steels faces economic and supply-chain pressures, motivating partial or near-complete nickel substitution through nitrogen alloying as an alternative alloy-design strategy. This study systematically evaluates partial (0.24 N, 6.56 wt% Ni retained) and near-complete (0.52 N, 0.01 wt% Ni) nitrogen substitution in AISI 316 stainless steel, produced via vacuum induction furnace (VIM) under controlled-nitrogen-pressure melting at 18 and 32 bar, respectively. Nitrogen addition refined austenite grain size by 53.4% (from 29 to 13.5 μm) and increased dislocation density from 0.13 × 10 14 to 1.97 × 10 14 m −2 , with the 0.52N alloy developing a duplex (γ + α) microstructure. A phase-resolved strengthening model decomposed yield strength contributions into grain refinement, solid-solution, and dislocation mechanisms, achieving good agreement with experimental results. Nitrogen shifted corrosion potential positively, reduced corrosion current density from 9.1 to 2.4 µA cm −2 , and EIS analysis showed the passive film’s charge-transfer resistance rising from 121.5 to 193.5 kΩ cm 2 with a corresponding fall in effective capacitance, while the electrical-equivalent film thickness recalculated from these parameters increases only modestly, from 0.10 to 0.12 nm. Dilatometry revealed a thermal instability window (780–840 °C) unique to the 0.52N alloy, consistent with thermally activated phase evolution within its γ + α duplex microstructure. The 0.24N alloy provides the most balanced combination of strength, ductility, corrosion resistance, and thermal stability among the investigated conditions, while the 0.52N alloy provides the highest strength but also exhibits greater phase complexity and a thermal-instability window; therefore, both alloys require application-specific validation of processing, weldability/forming behaviour, and long-term service performance before industrial deployment.
- Open Access
- 19 July 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1)
Structure-activity relationship of pyrazole-based corrosion inhibitors for carbon steel in HCl: combined experimental and theoretical study
The corrosion inhibition performance of two newly synthesized pyrazole-based derivatives, P6 (bis-pyrazole) and P8 (pyrazolyl-thiadiazine), toward carbon steel in 1.0 M HCl was systematically investigated using combined experimental and theoretical approaches. Electrochemical and gravimetric results revealed high inhibition efficiencies exceeding 95% at 5 × 10⁻⁴ M, with P6 exhibiting superior performance. This enhanced performance is attributed to its stronger adsorption affinity and more stable interaction with the steel surface. Polarization measurements revealed predominantly anodic inhibition behavior, although both anodic and cathodic reactions were affected, while impedance analysis confirmed the formation of a protective adsorbed film. Surface characterization (SEM, EDX, and AFM) further supported the development of a compact and homogeneous protective layer. Thermodynamic analysis suggested a mixed adsorption mechanism involving electrostatic and chemical interactions. Computational studies (DFT and Monte Carlo simulations) corroborated the experimental findings, demonstrating strong adsorption on the Fe (110) surface.
- 19 July 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1)
Open AccessStructure-activity relationship of pyrazole-based corrosion inhibitors for carbon steel in HCl: combined experimental and theoretical study
The corrosion inhibition performance of two newly synthesized pyrazole-based derivatives, P6 (bis-pyrazole) and P8 (pyrazolyl-thiadiazine), toward carbon steel in 1.0 M HCl was systematically investigated using combined experimental and theoretical approaches. Electrochemical and gravimetric results revealed high inhibition efficiencies exceeding 95% at 5 × 10⁻⁴ M, with P6 exhibiting superior performance. This enhanced performance is attributed to its stronger adsorption affinity and more stable interaction with the steel surface. Polarization measurements revealed predominantly anodic inhibition behavior, although both anodic and cathodic reactions were affected, while impedance analysis confirmed the formation of a protective adsorbed film. Surface characterization (SEM, EDX, and AFM) further supported the development of a compact and homogeneous protective layer. Thermodynamic analysis suggested a mixed adsorption mechanism involving electrostatic and chemical interactions. Computational studies (DFT and Monte Carlo simulations) corroborated the experimental findings, demonstrating strong adsorption on the Fe (110) surface.
- Open Access
- 5 June 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1) , 17837
Unraveling the corrosion-mitigating action of cyclobenzaprine hydrochloride on carbon steel in acidic media: integrated experimental and multiscale molecular perspectives
Using a combination of computational and experimental methods, the corrosion protection effectiveness provided by cyclobenzaprine (CBA) for carbon steel (CS) in a 1.0 M hydrochloric acid solution was systematically examined. The corrosion protection efficiency and electrochemical behavior of CS with and without different concentrations of CBA were assessed using gravimetric measurements, polarization studies, impedance measurements, and the evaluation of the open circuit potential. The addition of CBA resulted in a notable decrease in double-layer capacitance (C dl ) and an increase in charge transfer resistance (R ct ), a considerable increase in the relaxation time constant (τ), as well as a considerable decrease in corrosion rate and corrosion current density, according to gravimetric and electrochemical data. The formation of a surface-bound shielding layer on the CS was demonstrated by surface characterization using SEM/EDS, AFM analysis, wettability assessment via contact angle evaluation, and UV–visible spectroscopic examination. At 192 μmol L −1 , the most effective corrosion protection of ~ 96% was achieved. The results showed that CBA functioned as an effective mixed-type inhibitor. Predominant physical adsorption was indicated by the corrosion inhibition efficiency, which improved with higher inhibitor dosage but decreased as the temperature rose. The thermodynamic and kinetic analyses showed spontaneous adsorption, following the Langmuir isotherm. The electronic characteristics and active adsorption centers of CBA were elucidated through density functional theory calculations, Fukui function examination, and natural bond orbital investigation. Additionally, the significance of π–electron systems and heteroatoms in surface interactions was emphasized.
- 5 June 2026
- Published by Springer Nature in Scientific Reports
- Vol. 16 (1) , 17837
Open AccessUnraveling the corrosion-mitigating action of cyclobenzaprine hydrochloride on carbon steel in acidic media: integrated experimental and multiscale molecular perspectives
Using a combination of computational and experimental methods, the corrosion protection effectiveness provided by cyclobenzaprine (CBA) for carbon steel (CS) in a 1.0 M hydrochloric acid solution was systematically examined. The corrosion protection efficiency and electrochemical behavior of CS with and without different concentrations of CBA were assessed using gravimetric measurements, polarization studies, impedance measurements, and the evaluation of the open circuit potential. The addition of CBA resulted in a notable decrease in double-layer capacitance (C dl ) and an increase in charge transfer resistance (R ct ), a considerable increase in the relaxation time constant (τ), as well as a considerable decrease in corrosion rate and corrosion current density, according to gravimetric and electrochemical data. The formation of a surface-bound shielding layer on the CS was demonstrated by surface characterization using SEM/EDS, AFM analysis, wettability assessment via contact angle evaluation, and UV–visible spectroscopic examination. At 192 μmol L −1 , the most effective corrosion protection of ~ 96% was achieved. The results showed that CBA functioned as an effective mixed-type inhibitor. Predominant physical adsorption was indicated by the corrosion inhibition efficiency, which improved with higher inhibitor dosage but decreased as the temperature rose. The thermodynamic and kinetic analyses showed spontaneous adsorption, following the Langmuir isotherm. The electronic characteristics and active adsorption centers of CBA were elucidated through density functional theory calculations, Fukui function examination, and natural bond orbital investigation. Additionally, the significance of π–electron systems and heteroatoms in surface interactions was emphasized.
- Open Access
- 7 May 2026
- Published by Elsevier in SSRN Electronic Journal
A defect-mediated correlation between mechanical strength and passivation in nitrogen-modified AISI 316 stainless steel
Two modified austenitic stainless steels have been developed through partial and full replacement of nickel by nitrogen beside AISI316 as a reference. Grain size is refined from 60 to 16 µm, and the dislocation density increases from 1.0 × 1015 to 2.8 × 1015 m−2. A physically based additive model decouples grain-boundary, solid-solution, and dislocation strengthening, predicting yield strengths of 473, 728, and 1025 MPa, which deviate from the measured values (485, 703, 950 MPa) by –12 to +75 MPa. Simultaneously, the polarization resistance doubles and the passive-film thickness increases from 1.7 to 10.0 nm. The observed trends indicate a defect-mediated coupling between mechanical strengthening and passivation, offering semi-quantitative design guidance for low-nickel, high-strength corrosion-resistant steels.
- 7 May 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessA defect-mediated correlation between mechanical strength and passivation in nitrogen-modified AISI 316 stainless steel
Two modified austenitic stainless steels have been developed through partial and full replacement of nickel by nitrogen beside AISI316 as a reference. Grain size is refined from 60 to 16 µm, and the dislocation density increases from 1.0 × 1015 to 2.8 × 1015 m−2. A physically based additive model decouples grain-boundary, solid-solution, and dislocation strengthening, predicting yield strengths of 473, 728, and 1025 MPa, which deviate from the measured values (485, 703, 950 MPa) by –12 to +75 MPa. Simultaneously, the polarization resistance doubles and the passive-film thickness increases from 1.7 to 10.0 nm. The observed trends indicate a defect-mediated coupling between mechanical strengthening and passivation, offering semi-quantitative design guidance for low-nickel, high-strength corrosion-resistant steels.
- Open Access
Quaternium-22 as a High-Performance Corrosion Inhibitor for Carbon Steel in Acidic Media: Experimental and Theoretical Insights
This work provides an integrated experimental and computational evaluation of the cationic surfactant Quaternium-22 (Q-22) as a potentially eco-compatible corrosion inhibitor for carbon steel (CS) in 1 M hydrochloric acid. Gravimetric analysis and electrochemical techniques, including electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization (PDP), were employed over a temperature range of 20–50 °C. Q-22 exhibited mixed-type inhibition behavior, with efficiency rising to 97% at an optimal concentration of 277 μmol L−1. Performance was concentration-dependent but diminished with increasing temperature, indicating partial inhibitor desorption at elevated temperatures. Thermodynamic evaluation confirmed a spontaneous adsorption process consistent with the Langmuir isotherm, involving a combined physisorption and chemisorption mechanism. Surface characterization via scanning electron microscopy (SEM), atomic force microscopy (AFM), contact angle (CA) measurement, and X-ray photoelectron spectroscopy (XPS) confirmed the formation of a coherent, hydrophobic inhibitor layer that substantially reduced surface roughness and corrosion damage. Theoretical investigations using density functional theory (DFT), natural bond orbital (NBO) analysis, and molecular dynamics (MD) simulations revealed strong adsorption energies and favorable electronic properties consistent with the inhibitor’s high experimental efficacy. Overall, the results demonstrate that Q-22 is a highly effective, eco-compatible corrosion inhibitor for CS in acidic environments, operating through a stable adsorptive film-forming mechanism.
Open AccessQuaternium-22 as a High-Performance Corrosion Inhibitor for Carbon Steel in Acidic Media: Experimental and Theoretical Insights
This work provides an integrated experimental and computational evaluation of the cationic surfactant Quaternium-22 (Q-22) as a potentially eco-compatible corrosion inhibitor for carbon steel (CS) in 1 M hydrochloric acid. Gravimetric analysis and electrochemical techniques, including electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization (PDP), were employed over a temperature range of 20–50 °C. Q-22 exhibited mixed-type inhibition behavior, with efficiency rising to 97% at an optimal concentration of 277 μmol L−1. Performance was concentration-dependent but diminished with increasing temperature, indicating partial inhibitor desorption at elevated temperatures. Thermodynamic evaluation confirmed a spontaneous adsorption process consistent with the Langmuir isotherm, involving a combined physisorption and chemisorption mechanism. Surface characterization via scanning electron microscopy (SEM), atomic force microscopy (AFM), contact angle (CA) measurement, and X-ray photoelectron spectroscopy (XPS) confirmed the formation of a coherent, hydrophobic inhibitor layer that substantially reduced surface roughness and corrosion damage. Theoretical investigations using density functional theory (DFT), natural bond orbital (NBO) analysis, and molecular dynamics (MD) simulations revealed strong adsorption energies and favorable electronic properties consistent with the inhibitor’s high experimental efficacy. Overall, the results demonstrate that Q-22 is a highly effective, eco-compatible corrosion inhibitor for CS in acidic environments, operating through a stable adsorptive film-forming mechanism.
- Open Access
- 27 February 2026
- Published by MDPI AG in Preprints.org
Quaternium-22 as a High-Performance Corrosion Inhibitor for Carbon Steel in Acidic Media: Experimental and Theoretical Insights
This work provides an integrated experimental and computational assessment of the cationic surfactant Quaternium-22 (Q-22) as a potentially eco-compatible corrosion inhibitor for carbon steel (CS) in 1 M hydrochloric acid. Gravimetric analysis and electrochemical techniques: electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization (PDP) were employed over a 20–50 °C temperature range. Q-22 exhibited mixed-type inhibition behavior, with efficiency rising to 97% at an optimal concentration of 277 μmol L⁻¹. Performance was concentration-dependent but diminished with increasing temperature, indicating partial inhibitor desorption at elevated temperatures. Thermodynamic evaluation confirmed a spontaneous adsorption process aligned with the Langmuir isotherm, involving a mixed physisorption and chemisorption mechanism. Surface characterization via scanning electron microscopy (SEM), atomic force microscopy (AFM), contact angle (CA) measurement, and X-ray photoelectron spectroscopy (XPS) verified the formation of a coherent, hydrophobic inhibitor layer that substantially reduced surface roughness and corrosion damage. Theoretical validation using density functional theory (DFT), natural bond orbital (NBO) analysis, and molecular dynamics (MD) simulations revealed strong adsorption energetics and favorable electronic properties consistent with the inhibitor’s high experimental efficacy. The collective findings establish Q-22 as a potent, eco-compatible corrosion inhibitor for CS in acidic environments, operating through a robust adsorptive film-forming mechanism.
- 27 February 2026
- Published by MDPI AG in Preprints.org
Open AccessQuaternium-22 as a High-Performance Corrosion Inhibitor for Carbon Steel in Acidic Media: Experimental and Theoretical Insights
This work provides an integrated experimental and computational assessment of the cationic surfactant Quaternium-22 (Q-22) as a potentially eco-compatible corrosion inhibitor for carbon steel (CS) in 1 M hydrochloric acid. Gravimetric analysis and electrochemical techniques: electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization (PDP) were employed over a 20–50 °C temperature range. Q-22 exhibited mixed-type inhibition behavior, with efficiency rising to 97% at an optimal concentration of 277 μmol L⁻¹. Performance was concentration-dependent but diminished with increasing temperature, indicating partial inhibitor desorption at elevated temperatures. Thermodynamic evaluation confirmed a spontaneous adsorption process aligned with the Langmuir isotherm, involving a mixed physisorption and chemisorption mechanism. Surface characterization via scanning electron microscopy (SEM), atomic force microscopy (AFM), contact angle (CA) measurement, and X-ray photoelectron spectroscopy (XPS) verified the formation of a coherent, hydrophobic inhibitor layer that substantially reduced surface roughness and corrosion damage. Theoretical validation using density functional theory (DFT), natural bond orbital (NBO) analysis, and molecular dynamics (MD) simulations revealed strong adsorption energetics and favorable electronic properties consistent with the inhibitor’s high experimental efficacy. The collective findings establish Q-22 as a potent, eco-compatible corrosion inhibitor for CS in acidic environments, operating through a robust adsorptive film-forming mechanism.
- Open Access
Electrochemical Stability of Passive Films on β-TiZrNbTa Alloys in Seawater-Based Electrolytes: Influence of Fluoride, pH, and Scan Rate
The corrosion behavior and passive-film stability of a β-TiZrNbTa (β-TZNT) alloy were investigated in artificial seawater (ASW), focusing on the effects of pH, temperature, immersion time, fluoride ion concentration, and potential scan rate. In addition to electrochemical methods such as open-circuit potential (OCP), potentiodynamic polarization (PDP), and electrochemical impedance spectroscopy (EIS), scanning electron microscopy (SEM) and X-ray diffraction (XRD) were employed for surface characterization. The establishment of a stable and efficient passive layer enriched in Zr-, Nb-, and Ta-oxides was responsible for the β-TZNT alloy’s superior corrosion resistance in fluoride-free ASW when compared to commercially pure titanium. Reduced passive-film resistance resulted from corrosion kinetics being greatly accelerated by decreasing the pH and increasing the temperature. The presence of fluoride ions strongly affected the passivity of the alloy due to the chemical dissolution of TiO2 through the formation of soluble fluoride complexes, resulting in an increase in the corrosion current densities by more than one order of magnitude. A bilayer passive structure with a compact inner barrier layer and a porous outer layer was identified by EIS analysis. The stability of this structure gradually decreased with increasing fluoride concentration and acidity. Over time, passive-film degradation was dominant in fluoride-free seawater, whereas prolonged exposure in fluoride-containing media promoted partial re-passivation. Overall, these results highlight the potential and limitations of the β-TZNT alloy for marine and offshore applications by offering new mechanistic insights into the synergistic effects of fluoride ions and environmental factors on corrosion performance.
Open AccessElectrochemical Stability of Passive Films on β-TiZrNbTa Alloys in Seawater-Based Electrolytes: Influence of Fluoride, pH, and Scan Rate
The corrosion behavior and passive-film stability of a β-TiZrNbTa (β-TZNT) alloy were investigated in artificial seawater (ASW), focusing on the effects of pH, temperature, immersion time, fluoride ion concentration, and potential scan rate. In addition to electrochemical methods such as open-circuit potential (OCP), potentiodynamic polarization (PDP), and electrochemical impedance spectroscopy (EIS), scanning electron microscopy (SEM) and X-ray diffraction (XRD) were employed for surface characterization. The establishment of a stable and efficient passive layer enriched in Zr-, Nb-, and Ta-oxides was responsible for the β-TZNT alloy’s superior corrosion resistance in fluoride-free ASW when compared to commercially pure titanium. Reduced passive-film resistance resulted from corrosion kinetics being greatly accelerated by decreasing the pH and increasing the temperature. The presence of fluoride ions strongly affected the passivity of the alloy due to the chemical dissolution of TiO2 through the formation of soluble fluoride complexes, resulting in an increase in the corrosion current densities by more than one order of magnitude. A bilayer passive structure with a compact inner barrier layer and a porous outer layer was identified by EIS analysis. The stability of this structure gradually decreased with increasing fluoride concentration and acidity. Over time, passive-film degradation was dominant in fluoride-free seawater, whereas prolonged exposure in fluoride-containing media promoted partial re-passivation. Overall, these results highlight the potential and limitations of the β-TZNT alloy for marine and offshore applications by offering new mechanistic insights into the synergistic effects of fluoride ions and environmental factors on corrosion performance.
- Open Access
- 7 January 2026
- Published by MDPI AG in Preprints.org
Electrochemical Stability of Passive Films on β-TiZrTaNb Alloy in Seawater-Based Electrolytes: Influence of Fluoride, pH, and Scan Rate
The corrosion behavior and passive-film stability of a β-TiZrNbTa (β-TZNT) alloy were thoroughly examined in artificial seawater (ASW), with a focus on the effects of pH, temperature, immersion time, fluoride ion concentration, and potential scan rate. In addi-tion to electrochemical methods such as open-circuit potential (OCP), potentiodynamic polarization (PDP), and electrochemical impedance spectroscopy (EIS), scanning elec-tron microscopy (SEM) and X-ray diffraction (XRD) were used for surface characteriza-tion. The establishment of a stable and efficient passive layer enriched with Zr-, Nb-, and Ta-oxides was responsible for the β-TZNT alloy's superior corrosion resistance in fluo-ride-free ASW when compared to commercially pure titanium. Reduced passive-film re-sistance resulted from corrosion kinetics being greatly accelerated by decreasing the pH and increasing the temperature. Due to the chemical dissolution of TiO₂ through soluble fluoride complexes, the presence of fluoride ions significantly reduced passivity and in-creased corrosion current densities by more than an order of magnitude. A bilayer pas-sive structure with a compact inner barrier layer and a porous outer layer was identified by EIS analysis. The integrity of this structure gradually decreased as the fluoride con-centration and acidity increased. Over time, passive film degradation predominated in fluoride-free seawater, whereas prolonged immersion encouraged partial re-passivation in fluoride-containing media. Overall, the findings highlight the potential and constraints of β-TZNT alloy for advanced marine and offshore applications by offering new mecha-nistic insights into the synergistic effects of fluoride ions and environmental parameters on corrosion performance.
- 7 January 2026
- Published by MDPI AG in Preprints.org
Open AccessElectrochemical Stability of Passive Films on β-TiZrTaNb Alloy in Seawater-Based Electrolytes: Influence of Fluoride, pH, and Scan Rate
The corrosion behavior and passive-film stability of a β-TiZrNbTa (β-TZNT) alloy were thoroughly examined in artificial seawater (ASW), with a focus on the effects of pH, temperature, immersion time, fluoride ion concentration, and potential scan rate. In addi-tion to electrochemical methods such as open-circuit potential (OCP), potentiodynamic polarization (PDP), and electrochemical impedance spectroscopy (EIS), scanning elec-tron microscopy (SEM) and X-ray diffraction (XRD) were used for surface characteriza-tion. The establishment of a stable and efficient passive layer enriched with Zr-, Nb-, and Ta-oxides was responsible for the β-TZNT alloy's superior corrosion resistance in fluo-ride-free ASW when compared to commercially pure titanium. Reduced passive-film re-sistance resulted from corrosion kinetics being greatly accelerated by decreasing the pH and increasing the temperature. Due to the chemical dissolution of TiO₂ through soluble fluoride complexes, the presence of fluoride ions significantly reduced passivity and in-creased corrosion current densities by more than an order of magnitude. A bilayer pas-sive structure with a compact inner barrier layer and a porous outer layer was identified by EIS analysis. The integrity of this structure gradually decreased as the fluoride con-centration and acidity increased. Over time, passive film degradation predominated in fluoride-free seawater, whereas prolonged immersion encouraged partial re-passivation in fluoride-containing media. Overall, the findings highlight the potential and constraints of β-TZNT alloy for advanced marine and offshore applications by offering new mecha-nistic insights into the synergistic effects of fluoride ions and environmental parameters on corrosion performance.
- 12 December 2025
- Published by American Chemical Society (ACS) in Industrial & Engineering Chemistry Research
- Vol. 64 (51) , 24501-24515
Perovskite-Based MnSn(OH) 6 Nanocubes Coupled with 2D Chalcogenide Cu 3 SnS 4 Nanosheets for Electrocatalytic Methanol Oxidation
- 12 December 2025
- Published by American Chemical Society (ACS) in Industrial & Engineering Chemistry Research
- Vol. 64 (51) , 24501-24515
Perovskite-Based MnSn(OH) 6 Nanocubes Coupled with 2D Chalcogenide Cu 3 SnS 4 Nanosheets for Electrocatalytic Methanol Oxidation
- Open Access
- 4 December 2025
- Published by Springer Nature in Scientific Reports
- Vol. 15 (1)
Multifaceted insights of experimental, surface, and computational investigations for a synthesized pyrazolyl derivative inhibitor for carbon steel corrosion in an acidic environment
For sustainable corrosion protection, this study introduces newly synthesized pyrazolyl- N -acetylthiocarbohydrazone ( PTH ) as a highly efficient and environmentally friendly inhibitor for carbon steel (CS) in an aggressive 1.0 M HCl solution. A comprehensive evaluation of PTH inhibition performance was conducted through chemical weight loss and electrochemical techniques, involving potentiodynamic polarization ( PDP ) and electrochemical impedance spectroscopy ( EIS ), which demonstrated a significant reduction in CS corrosion. PDP and EIS reinforced these findings, confirming the robust protective nature of PTH with an inhibition potency of 96%. The mitigation power of the PTH can be explained by its adsorption onto the CS surface, which followed the Langmuir adsorption model. The inhibitor exhibited exceptional stability and efficiency across varying temperature conditions and various immersion times using EIS, reinforcing its reliability in harsh acidic media, with a mitigation capacity of 97.16% at 50 °C and 97.3% after 24 h. The morphology of the CS surface was examined using SEM /EDX (Scanning Electron Microscopy), AFM (Atomic Force Microscopy), and XPS (X-ray Photoelectron Spectroscopy), exhibiting the PTH adsorption over CS , which was also proved and elucidated employing theoretical quantum investigations as density functional theory and Monte Carlo simulations.
- 4 December 2025
- Published by Springer Nature in Scientific Reports
- Vol. 15 (1)
Open AccessMultifaceted insights of experimental, surface, and computational investigations for a synthesized pyrazolyl derivative inhibitor for carbon steel corrosion in an acidic environment
For sustainable corrosion protection, this study introduces newly synthesized pyrazolyl- N -acetylthiocarbohydrazone ( PTH ) as a highly efficient and environmentally friendly inhibitor for carbon steel (CS) in an aggressive 1.0 M HCl solution. A comprehensive evaluation of PTH inhibition performance was conducted through chemical weight loss and electrochemical techniques, involving potentiodynamic polarization ( PDP ) and electrochemical impedance spectroscopy ( EIS ), which demonstrated a significant reduction in CS corrosion. PDP and EIS reinforced these findings, confirming the robust protective nature of PTH with an inhibition potency of 96%. The mitigation power of the PTH can be explained by its adsorption onto the CS surface, which followed the Langmuir adsorption model. The inhibitor exhibited exceptional stability and efficiency across varying temperature conditions and various immersion times using EIS, reinforcing its reliability in harsh acidic media, with a mitigation capacity of 97.16% at 50 °C and 97.3% after 24 h. The morphology of the CS surface was examined using SEM /EDX (Scanning Electron Microscopy), AFM (Atomic Force Microscopy), and XPS (X-ray Photoelectron Spectroscopy), exhibiting the PTH adsorption over CS , which was also proved and elucidated employing theoretical quantum investigations as density functional theory and Monte Carlo simulations.