Zongshen Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Zongshen Wang has a total of 51 co-authors. Here are the top co-authors by number of shared publications:
- Shan Gao
School of Materials Science and Engineering, Guangdong Ocean University, Yangjiang 529500, China
4 shared publications Yanjin Guan
Key Laboratory for Liquid-Solid Structural Evolution and Processing of Materials (Ministry of Education), Shandong University, Jinan, People’s Republic of China
4 shared publications- Hongyu Zheng
Shandong University of Technology
3 shared publications Lihua Zhu
School of Mechanical Engineering, Shandong University of Technology, Zibo, People’s Republic of China
3 shared publications- Lihua Zhu
Shandong University
3 shared publications - Harry M. Ngwangwa
Department of Mechanical Engineering, School of Engineering, College of Engineering Science and Technology, University of South Africa, Johannesburg 1709, South Africa
2 shared publications
Latest Publications
- Open Access
Effect of Heat Treatment on Microstructure and Corrosion Resistance of Al-Si-Mg-Zr-Cu-Sc Alloy
Aluminum–silicon (Al-Si) alloys are widely used in aerospace, automotive manufacturing, power electronics, marine engineering and other fields due to their excellent physical properties. However, their corrosion resistance is insufficient in harsh service environments. In this study, a variety of characterization methods were adopted, including scanning electron microscopy (SEM), X-ray diffraction (XRD), electrochemical measurements (electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization), immersion corrosion tests, and scanning vibrating electrode technique (SVET). The results show that the appropriate heat treatment regime can significantly enhance the corrosion resistance of the alloy, while improper aging parameters will aggravate the corrosion tendency. The optimal heat treatment regime is solution treatment at 500 °C for 4 h followed by aging at 200 °C for 48 h. Under this condition, the corrosion current density (icorr) is as low as 79.30 μA/cm2, and the low-frequency impedance modulus and phase angle in EIS tests are optimal. The as-extruded alloy exhibits severe localized corrosion, while the heat-treated alloy transforms into mild and uniform corrosion. The underlying mechanism is that heat treatment induces the formation of uniformly distributed nanoscale Mg2Si and Al3(Sc,Zr) precipitates, which synergistically improve the corrosion resistance of the alloy by weakening micro-galvanic coupling and facilitating the formation of a stable passive film.
Open AccessEffect of Heat Treatment on Microstructure and Corrosion Resistance of Al-Si-Mg-Zr-Cu-Sc Alloy
Aluminum–silicon (Al-Si) alloys are widely used in aerospace, automotive manufacturing, power electronics, marine engineering and other fields due to their excellent physical properties. However, their corrosion resistance is insufficient in harsh service environments. In this study, a variety of characterization methods were adopted, including scanning electron microscopy (SEM), X-ray diffraction (XRD), electrochemical measurements (electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization), immersion corrosion tests, and scanning vibrating electrode technique (SVET). The results show that the appropriate heat treatment regime can significantly enhance the corrosion resistance of the alloy, while improper aging parameters will aggravate the corrosion tendency. The optimal heat treatment regime is solution treatment at 500 °C for 4 h followed by aging at 200 °C for 48 h. Under this condition, the corrosion current density (icorr) is as low as 79.30 μA/cm2, and the low-frequency impedance modulus and phase angle in EIS tests are optimal. The as-extruded alloy exhibits severe localized corrosion, while the heat-treated alloy transforms into mild and uniform corrosion. The underlying mechanism is that heat treatment induces the formation of uniformly distributed nanoscale Mg2Si and Al3(Sc,Zr) precipitates, which synergistically improve the corrosion resistance of the alloy by weakening micro-galvanic coupling and facilitating the formation of a stable passive film.
- Open Access
Microstructure Evolution and Wear Resistance of TiC-Reinforced H13 Alloy Coatings Fabricated by Laser Cladding on H13 Steel
With the growing demand for high-performance die materials under harsh service conditions, the development of composite coatings with enhanced hardness and wear resistance has attracted significant attention. In this study, homogeneous laser cladding was employed to fabricate H13 alloy coatings reinforced with varying TiC contents (0, 10, 20, and 30 in wt.%) on H13 steel, which minimizes compositional segregation and ensures strong metallurgical bonding. TiC particles acted as heterogeneous nucleation sites during solidification, refining the microstructure and enhancing phase stability. The coatings consisted of initial TiC residues, newly formed primary and eutectic TiC, as well as austenite and martensite phases. With increasing TiC addition, TiC morphology evolved from fine particles to complex fishbone-like and polygonal structures. The coating containing 30% TiC achieved the highest hardness of 1095.9 HV0.5, approximately five times that of the as-annealed H13 steel substrate while the 20% TiC coating exhibited optimal high-temperature wear resistance. Under the sliding conditions at 600 °C, the friction coefficient decreased from 0.467 for the substrate to 0.367 for the 20% TiC coating, accompanied by a remarkable reduction in wear rate from 27.45 × 10−4 mm3 N−1 m−1 to 4.32 × 10−4 mm3 N−1 m−1. The superior performance was attributed to the multiscale TiC reinforcement mechanism: initial TiC promoted grain refinement and strong interfacial bonding, in situ formed primary TiC induced lattice distortion and dislocation strengthening, and eutectic TiC reinforced grain boundaries, jointly enhancing hardness, thermal stability, and wear resistance.
Open AccessMicrostructure Evolution and Wear Resistance of TiC-Reinforced H13 Alloy Coatings Fabricated by Laser Cladding on H13 Steel
With the growing demand for high-performance die materials under harsh service conditions, the development of composite coatings with enhanced hardness and wear resistance has attracted significant attention. In this study, homogeneous laser cladding was employed to fabricate H13 alloy coatings reinforced with varying TiC contents (0, 10, 20, and 30 in wt.%) on H13 steel, which minimizes compositional segregation and ensures strong metallurgical bonding. TiC particles acted as heterogeneous nucleation sites during solidification, refining the microstructure and enhancing phase stability. The coatings consisted of initial TiC residues, newly formed primary and eutectic TiC, as well as austenite and martensite phases. With increasing TiC addition, TiC morphology evolved from fine particles to complex fishbone-like and polygonal structures. The coating containing 30% TiC achieved the highest hardness of 1095.9 HV0.5, approximately five times that of the as-annealed H13 steel substrate while the 20% TiC coating exhibited optimal high-temperature wear resistance. Under the sliding conditions at 600 °C, the friction coefficient decreased from 0.467 for the substrate to 0.367 for the 20% TiC coating, accompanied by a remarkable reduction in wear rate from 27.45 × 10−4 mm3 N−1 m−1 to 4.32 × 10−4 mm3 N−1 m−1. The superior performance was attributed to the multiscale TiC reinforcement mechanism: initial TiC promoted grain refinement and strong interfacial bonding, in situ formed primary TiC induced lattice distortion and dislocation strengthening, and eutectic TiC reinforced grain boundaries, jointly enhancing hardness, thermal stability, and wear resistance.
- Open Access
Corrosion Resistance of AZ31 Magnesium Alloy Processed by Femtosecond Laser Shock Peening
The present study investigates the impact of femtosecond laser shock peening (FLSP) on the corrosion resistance of an AZ31 magnesium alloy. The alloy was subjected to irradiation with varying pulse energies in an air environment, and subsequent modifications in surface properties were characterized. Surface wettability, assessed by contact angle measurements, indicated enhanced hydrophobicity following FLSP, especially at higher pulse energies. Corrosion behavior after immersion with various durations was assessed in a 3.5% NaCl solution using electrochemical polarization curves and electrochemical impedance spectroscopy, applying a three-electrode system. The results revealed that FLSP significantly augmented corrosion resistance; the most notable effects were observed at higher pulse energies. SEM/EDS analysis post-corrosion revealed a transition from localized to more uniform corrosion, accompanied by reduced pit size and density. XRD and XPS confirmed the formation of a protective Mg(OH)2 layer, which exhibited greater stability and uniformity at higher laser energies. The study concluded that FLSP represented an effective approach for enhancing the corrosion resistance of the AZ31 magnesium alloy, with potential applications in improving the longevity of magnesium alloy components in industrial settings.
Open AccessCorrosion Resistance of AZ31 Magnesium Alloy Processed by Femtosecond Laser Shock Peening
The present study investigates the impact of femtosecond laser shock peening (FLSP) on the corrosion resistance of an AZ31 magnesium alloy. The alloy was subjected to irradiation with varying pulse energies in an air environment, and subsequent modifications in surface properties were characterized. Surface wettability, assessed by contact angle measurements, indicated enhanced hydrophobicity following FLSP, especially at higher pulse energies. Corrosion behavior after immersion with various durations was assessed in a 3.5% NaCl solution using electrochemical polarization curves and electrochemical impedance spectroscopy, applying a three-electrode system. The results revealed that FLSP significantly augmented corrosion resistance; the most notable effects were observed at higher pulse energies. SEM/EDS analysis post-corrosion revealed a transition from localized to more uniform corrosion, accompanied by reduced pit size and density. XRD and XPS confirmed the formation of a protective Mg(OH)2 layer, which exhibited greater stability and uniformity at higher laser energies. The study concluded that FLSP represented an effective approach for enhancing the corrosion resistance of the AZ31 magnesium alloy, with potential applications in improving the longevity of magnesium alloy components in industrial settings.
- Open Access
Surface Integrity and Corrosion Resistance of Additively Manufactured AZ91 Mg Alloys Post-Processed by Laser Shock Peening
Mg alloys show great potential in biomedical fields due to superior biocompatibility and biodegradability. Additive manufacturing (AM) provides opportunities in fabricating metallic implants with complex geometries while inherent defects during AM limit its further applications. In this work, laser shock peening (LSP) was employed as a post-processing technique to tailor the surface integrity and corrosion resistance of additively manufactured AZ91 Mg alloy by selective laser melting (SLM). The surface morphology, microstructure and porosity, surface hardness and residual stress, and corrosion resistance of the SLMed alloy before and after LSP were examined. The results show that a gradient structure is formed along the depth direction after LSP and high-density dislocations and high-fraction low-angle grain boundaries are induced. The porosity is gradually reduced in number and size and the highest density of 1.794 g/cm3 is obtained after two impacts of LSP. The surface hardness and residual compressive stress both increase with LSP number and the highest values of 135.26 HV and 40.13 MPa after four impacts, respectively. All of the SLMed alloy samples show improved corrosion resistance after LSP. This work provides a promising route for enhancing the performance of additively manufactured Mg alloys through laser materials surface modification.
Open AccessSurface Integrity and Corrosion Resistance of Additively Manufactured AZ91 Mg Alloys Post-Processed by Laser Shock Peening
Mg alloys show great potential in biomedical fields due to superior biocompatibility and biodegradability. Additive manufacturing (AM) provides opportunities in fabricating metallic implants with complex geometries while inherent defects during AM limit its further applications. In this work, laser shock peening (LSP) was employed as a post-processing technique to tailor the surface integrity and corrosion resistance of additively manufactured AZ91 Mg alloy by selective laser melting (SLM). The surface morphology, microstructure and porosity, surface hardness and residual stress, and corrosion resistance of the SLMed alloy before and after LSP were examined. The results show that a gradient structure is formed along the depth direction after LSP and high-density dislocations and high-fraction low-angle grain boundaries are induced. The porosity is gradually reduced in number and size and the highest density of 1.794 g/cm3 is obtained after two impacts of LSP. The surface hardness and residual compressive stress both increase with LSP number and the highest values of 135.26 HV and 40.13 MPa after four impacts, respectively. All of the SLMed alloy samples show improved corrosion resistance after LSP. This work provides a promising route for enhancing the performance of additively manufactured Mg alloys through laser materials surface modification.
- 30 April 2022
- Published by Springer Nature in Journal of Mechanical Science and Technology
- Vol. 36 (5) , 2277-2286
Research on metal flow law of micro-riblets based on multi-pass rolling
- 30 April 2022
- Published by Springer Nature in Journal of Mechanical Science and Technology
- Vol. 36 (5) , 2277-2286
Research on metal flow law of micro-riblets based on multi-pass rolling
- 27 October 2020
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 29 (11) , 7693-7709
Influence of Surface Nanocrystallization and Partial Amorphization Induced by Ultrasonic Shot Peening on Surface Properties of 7075 Aluminum Alloy
- 27 October 2020
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 29 (11) , 7693-7709
Influence of Surface Nanocrystallization and Partial Amorphization Induced by Ultrasonic Shot Peening on Surface Properties of 7075 Aluminum Alloy
- 26 October 2020
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 29 (11) , 7662-7677
Warm Tensile Deformation and Fracture Behavior of AZ31 Magnesium Alloy Sheets Processed by Constrained Groove Pressing
- 26 October 2020
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 29 (11) , 7662-7677
Warm Tensile Deformation and Fracture Behavior of AZ31 Magnesium Alloy Sheets Processed by Constrained Groove Pressing
- 22 August 2020
- Published by Wiley in Advanced Engineering Materials
- Vol. 23 (1)
Microstructure and Mechanical Properties of a Two‐Phase Mg–Li Alloy Processed By Constrained Groove Pressing
Constrained groove pressing (CGP), as a novel severe plastic deformation method, is applied to a two‐phase Mg–Li alloy at room temperature, 373 K, 423 K, and 473 K. The microstructural evolution and mechanical properties of Mg–Li alloy sheets during CGP are investigated. The optimum mechanical properties are achieved at 373 K after two passes. The tensile strength and yield strength are 157 MPa and 145 MPa, respectively, with a moderate elongation to failure of 12.4%, and the average micro‐hardness is about 63 HV. At 373 K, high‐density dislocations induced by CGP are preserved to enhance the strength and microhardness. The cross‐orientation procedure improves the deformation homogeneity and results in strength increase and ductility recovery at later stages. Increasing temperature weakens the homogeneity improvement and grain refinement with strain accumulation. The β‐Li phase is refined faster than α‐Mg phase, and grain sizes about 1 μm are observed in β‐Li phase. Dynamic recrystallization (DRX) first occurs in the soft and ductile β‐Li phase at 423 K. The grain refinement induced by DRX in β‐Li phase is counteracted by grain coarsening in α‐Mg phase, which causes no obvious enhancement of mechanical properties at higher temperatures of 423 K and 473 K.
- 22 August 2020
- Published by Wiley in Advanced Engineering Materials
- Vol. 23 (1)
Microstructure and Mechanical Properties of a Two‐Phase Mg–Li Alloy Processed By Constrained Groove Pressing
Constrained groove pressing (CGP), as a novel severe plastic deformation method, is applied to a two‐phase Mg–Li alloy at room temperature, 373 K, 423 K, and 473 K. The microstructural evolution and mechanical properties of Mg–Li alloy sheets during CGP are investigated. The optimum mechanical properties are achieved at 373 K after two passes. The tensile strength and yield strength are 157 MPa and 145 MPa, respectively, with a moderate elongation to failure of 12.4%, and the average micro‐hardness is about 63 HV. At 373 K, high‐density dislocations induced by CGP are preserved to enhance the strength and microhardness. The cross‐orientation procedure improves the deformation homogeneity and results in strength increase and ductility recovery at later stages. Increasing temperature weakens the homogeneity improvement and grain refinement with strain accumulation. The β‐Li phase is refined faster than α‐Mg phase, and grain sizes about 1 μm are observed in β‐Li phase. Dynamic recrystallization (DRX) first occurs in the soft and ductile β‐Li phase at 423 K. The grain refinement induced by DRX in β‐Li phase is counteracted by grain coarsening in α‐Mg phase, which causes no obvious enhancement of mechanical properties at higher temperatures of 423 K and 473 K.
- 11 February 2020
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 29 (2) , 819-831
Influence of Nanocrystalline–Amorphous Composite Layer on Tensile Properties of Pure Titanium
- 11 February 2020
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 29 (2) , 819-831
Influence of Nanocrystalline–Amorphous Composite Layer on Tensile Properties of Pure Titanium
- Open Access
The Fracture Behavior and Thermal Stability of Commercially Pure Nickel Sheets Processed by Constrained Groove Pressing
Constrained groove pressing (CGP) is one of the most promising severe plastic deformation (SPD) techniques suitable for producing ultra-fine grained (UFG) sheet or plane metallic materials with unique physical, chemical, and mechanical properties. However, the heavily deformed sheets are usually with high strength but low ductility due to work hardening and micro-cracking, and the UFG microstructure and high strength are unstable especially when exposed to high temperatures. Thus, in this work, CGP was conducted on commercially pure nickel sheets and, firstly, the fracture mechanism of the processed sheets was examined. Then, the annealing behavior of CGP nickel sheets was investigated in detail to explore their thermal stability and improve their ductility. The results showed that significant grain refinement and strength improvement of the nickel sheets were achieved with great loss of ductility. The fracture surface morphology of the sheet sample exhibited typical characteristics of fatigue fracture, and inhomogeneous strain distribution and work hardening determined the micro-crack initiation position and propagation direction. The CGP sheets by one and two passes showed high thermal stability up to 650 and 600 °C, respectively, owing to different stored internal stresses and accumulated energy. In both cases, obvious recovery of elongation to failure from 12.7% and 10.6% to 29.3% and 27.3% were achieved by CGP with post-deformation annealing treatment, respectively, with acceptable drop of strength.
Open AccessThe Fracture Behavior and Thermal Stability of Commercially Pure Nickel Sheets Processed by Constrained Groove Pressing
Constrained groove pressing (CGP) is one of the most promising severe plastic deformation (SPD) techniques suitable for producing ultra-fine grained (UFG) sheet or plane metallic materials with unique physical, chemical, and mechanical properties. However, the heavily deformed sheets are usually with high strength but low ductility due to work hardening and micro-cracking, and the UFG microstructure and high strength are unstable especially when exposed to high temperatures. Thus, in this work, CGP was conducted on commercially pure nickel sheets and, firstly, the fracture mechanism of the processed sheets was examined. Then, the annealing behavior of CGP nickel sheets was investigated in detail to explore their thermal stability and improve their ductility. The results showed that significant grain refinement and strength improvement of the nickel sheets were achieved with great loss of ductility. The fracture surface morphology of the sheet sample exhibited typical characteristics of fatigue fracture, and inhomogeneous strain distribution and work hardening determined the micro-crack initiation position and propagation direction. The CGP sheets by one and two passes showed high thermal stability up to 650 and 600 °C, respectively, owing to different stored internal stresses and accumulated energy. In both cases, obvious recovery of elongation to failure from 12.7% and 10.6% to 29.3% and 27.3% were achieved by CGP with post-deformation annealing treatment, respectively, with acceptable drop of strength.