Yindong Yang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yindong Yang has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
- Alexander McLean
Department of Materials Science and Engineering, University of Toronto, Toronto, ON M5S 3E4, Canada
4 shared publications - Baijun Yan
State Key Laboratory of Advanced Metallurgy, Department of Physical Chemistry of Metallurgy, School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
1 shared publication - Chuanhua Xu
Sinosteel Maanshan General Institute of Mining Research Co., Ltd., Maanshan 243000, China
1 shared publication - Daqiang Cang
School of Energy and Environmental Engineering, University of Science and Technology Beijing, Beijing 100083, China
1 shared publication - Dejian Pei
State Key Laboratory of Metal Mining Safety and Disaster Prevention and Control, National Engineering Research Center for Efficient Recycling of Metallic Mineral Resources, Sinosteel Maanshan General Institute of Mining Research Co., Ltd., Ma’anshan 243000, China
1 shared publication - Guifang Zhang
Faculty of Metallurgical and Energy Engineering, Kunming University of Science and Technology, Kunming, P.R. China
1 shared publication
Latest Publications
- Open Access
Effect of Phase Composition on Leaching Behavior and Mechanical Properties of Ceramics from Ferrochrome Slag and Tundish Slag
Ferrochrome slag (FS) and tundish slag (TS) are two typical slags containing high contents of Cr2O3 (3.88 wt.%) and MnO (18.69 wt.%), respectively. In this study, batches of ceramics were prepared from FS and TS, and their Cr/Mn leaching behaviors, mechanical properties and microstructures were investigated. Results showed that ceramics with 80 wt.% FS or 85 wt.% TS had acceptable properties. By controlling its composition and sintering temperature, pyroxene or spinel phases could become the main crystalline phases of the fired ceramics containing either of the two slags. For both slag series, pyroxene phases contributed to higher bending strengths, whereas spinel phases led to lower Cr/Mn leaching rates. Both ceramic containing 20 wt.% FS and ceramic containing 85 wt.% TS had the main crystals of pyroxene phases and possessed the highest bending strengths (FS20: 114.52 MPa and TS85: 124.61 MPa). However, both ceramic containing 80 wt.% FS and ceramic containing 25 wt.% TS with main crystals from the spinel phases had the lowest Cr/Mn leaching rates (FS80: Cr 0.05% and TS25: Mn 0.43%). Therefore, optimum designs for the compositions of ceramics from different slags were achieved by changing the proportions of pyroxene and spinel phases to obtain a balance between the high strengths of materials and the stable retention of heavy metal ions. This study provides an important basis for long-term research on the large-scale reuse of heavy metal-containing slags in the ceramic industry.
Open AccessEffect of Phase Composition on Leaching Behavior and Mechanical Properties of Ceramics from Ferrochrome Slag and Tundish Slag
Ferrochrome slag (FS) and tundish slag (TS) are two typical slags containing high contents of Cr2O3 (3.88 wt.%) and MnO (18.69 wt.%), respectively. In this study, batches of ceramics were prepared from FS and TS, and their Cr/Mn leaching behaviors, mechanical properties and microstructures were investigated. Results showed that ceramics with 80 wt.% FS or 85 wt.% TS had acceptable properties. By controlling its composition and sintering temperature, pyroxene or spinel phases could become the main crystalline phases of the fired ceramics containing either of the two slags. For both slag series, pyroxene phases contributed to higher bending strengths, whereas spinel phases led to lower Cr/Mn leaching rates. Both ceramic containing 20 wt.% FS and ceramic containing 85 wt.% TS had the main crystals of pyroxene phases and possessed the highest bending strengths (FS20: 114.52 MPa and TS85: 124.61 MPa). However, both ceramic containing 80 wt.% FS and ceramic containing 25 wt.% TS with main crystals from the spinel phases had the lowest Cr/Mn leaching rates (FS80: Cr 0.05% and TS25: Mn 0.43%). Therefore, optimum designs for the compositions of ceramics from different slags were achieved by changing the proportions of pyroxene and spinel phases to obtain a balance between the high strengths of materials and the stable retention of heavy metal ions. This study provides an important basis for long-term research on the large-scale reuse of heavy metal-containing slags in the ceramic industry.
- Open Access
Kinetic Aspects of Phosphorus Removal from Electromagnetically Levitated 600 MPa Steel Droplets
A kinetic model was developed to study the dephosphorization of 600 MPa steel droplets under electromagnetic levitation conditions. The relationships which were derived from the model between dephosphorization and the influence of temperature and gas flow rate were in good agreement with experimental data. Both temperature and gas flow rate were conducive to the evaporation of phosphorus, with the effect of temperature having a greater influence than that of the gas velocity. The results show that the rate-controlling step for the dephosphorization process was diffusion within the gas phase. This work aims to provide a theoretical basis for process optimization during the dephosphorization of 600 MPa steel.
Open AccessKinetic Aspects of Phosphorus Removal from Electromagnetically Levitated 600 MPa Steel Droplets
A kinetic model was developed to study the dephosphorization of 600 MPa steel droplets under electromagnetic levitation conditions. The relationships which were derived from the model between dephosphorization and the influence of temperature and gas flow rate were in good agreement with experimental data. Both temperature and gas flow rate were conducive to the evaporation of phosphorus, with the effect of temperature having a greater influence than that of the gas velocity. The results show that the rate-controlling step for the dephosphorization process was diffusion within the gas phase. This work aims to provide a theoretical basis for process optimization during the dephosphorization of 600 MPa steel.
- Open Access
A New Method for Plasticization of Inclusions in Saw-Wire Steel by NaF Addition
In this study, a new method is proposed for the plasticization of inclusions by taking advantage of the behavior of alkali metals in lowering the inclusion melting point. A series of experiments with NaF additions to molten steel were carried out using a carbon tube furnace followed by simulated rolling tests using the solidified ingots and characterization of inclusions with the help of automated scanning electron microscopy. Compositional changes of the steel and evolution of gaseous species were evaluated using thermodynamic software FactSage 7.2 (ThermFact Inc., Montreal, QC, Canada). Based on this approach, NaF/steel/inclusion interactions and the effects of NaF addition on the melting point, size and deformability of inclusions were clarified. The modification of MnO-SiO2 inclusions by NaF also promoted the removal of inclusions and improved the cleanliness of steel. The results show that with the addition of NaF, the melting point of inclusions is greatly reduced, the deformability is improved, and the removal of inclusions is enhanced, all of which indicates a good prospect for industrial application.
Open AccessA New Method for Plasticization of Inclusions in Saw-Wire Steel by NaF Addition
In this study, a new method is proposed for the plasticization of inclusions by taking advantage of the behavior of alkali metals in lowering the inclusion melting point. A series of experiments with NaF additions to molten steel were carried out using a carbon tube furnace followed by simulated rolling tests using the solidified ingots and characterization of inclusions with the help of automated scanning electron microscopy. Compositional changes of the steel and evolution of gaseous species were evaluated using thermodynamic software FactSage 7.2 (ThermFact Inc., Montreal, QC, Canada). Based on this approach, NaF/steel/inclusion interactions and the effects of NaF addition on the melting point, size and deformability of inclusions were clarified. The modification of MnO-SiO2 inclusions by NaF also promoted the removal of inclusions and improved the cleanliness of steel. The results show that with the addition of NaF, the melting point of inclusions is greatly reduced, the deformability is improved, and the removal of inclusions is enhanced, all of which indicates a good prospect for industrial application.
- Open Access
Effect of Cooling Rate on AlN Precipitation in FeCrAl Stainless Steel During Solidification
The effect of cooling rate on the evolution of AlN inclusions precipitated during solidification in FeCrAl stainless steel was investigated using an experimental study and thermodynamic and kinetic calculations. The number and size of AlN inclusions precipitated under different cooling rates were examined with the feature function of the field-emission scanning electron microscope. A model combining micro-segregation and the diffusion-controlled growth model was set up to determine the mechanism of AlN particle growth. The results showed that AlN precipitates in the mushy zone. The size of AlN particles decreases and the number of AlN particles increases with increasing cooling rate, whereas the volume fraction is essentially unchanged. The AlN particles grow during solidification after the content of solutes in molten steel has exceeded the concentration in equilibrium with AlN. The nitrogen content varies significantly with the cooling rate during solidification. Increasing the cooling rate and reducing the nitrogen content in the molten steel can reduce the AlN particle size in FeCrAl alloys as the growth time decreases.
Open AccessEffect of Cooling Rate on AlN Precipitation in FeCrAl Stainless Steel During Solidification
The effect of cooling rate on the evolution of AlN inclusions precipitated during solidification in FeCrAl stainless steel was investigated using an experimental study and thermodynamic and kinetic calculations. The number and size of AlN inclusions precipitated under different cooling rates were examined with the feature function of the field-emission scanning electron microscope. A model combining micro-segregation and the diffusion-controlled growth model was set up to determine the mechanism of AlN particle growth. The results showed that AlN precipitates in the mushy zone. The size of AlN particles decreases and the number of AlN particles increases with increasing cooling rate, whereas the volume fraction is essentially unchanged. The AlN particles grow during solidification after the content of solutes in molten steel has exceeded the concentration in equilibrium with AlN. The nitrogen content varies significantly with the cooling rate during solidification. Increasing the cooling rate and reducing the nitrogen content in the molten steel can reduce the AlN particle size in FeCrAl alloys as the growth time decreases.