Sheng-Yang Lee
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Sheng-Yang Lee has a total of 38 co-authors. Here are the top co-authors by number of shared publications:
Haw-Ming Huang
3 shared publicationsY.‐H. Shih
Dental Department of Wan-Fang Hospital, Taipei, Taiwan
3 shared publicationsC.‐T. Lin
Graduate Institute of Oral Rehabilitation Sciences
2 shared publicationsChe-Tong Lin
2 shared publicationsD.‐R. Dong
School of Dentistry, National Defense Medical Center, and §Wan-Fan Hospital, Taipei, Taiwan, R.O.C.
2 shared publicationsH. Tseng
Graduate Institute of Medical Sciences, Taipei, Taiwan
2 shared publications
Latest Publications
- 1 September 2001
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 28 (9) , 805-813
Effects of surface treatments on bond strength of glass‐infiltrated ceramic
The purpose of this study was to evaluate the effects of various surface treatments on the bond strength at the In‐Ceram/resin composite interface. Ninety‐eight In‐Ceram specimens were divided into seven groups and exposed to various surface treatments as follows: (A) control (B) saliva contamination (C) saliva contamination plus aluminum oxide sandblasting (D) glove powder contamination (E) glove powder contamination plus aluminum oxide sandblasting (F) rough aluminum oxide sandblasting and (G) excess glass infiltration. A resin composite cylinder was cemented to each In‐Ceram specimen with Panavia 21 resin luting cement. Half of the cemented specimens in each group were stored in water for 24 h, and the other half were stored in water for 2 weeks and then were thermo‐cycled for 2000 cycles. Shear bond strengths (SBS) of seven specimens in each subgroup were determined and analysed using analysis of variance (ANOVA) and Tukey HSD test as well as Student‘s t‐test. Scanning electronic microscopy was used to identify the type of bond failure. Shear bond strength was significantly decreased by saliva and glove powder contaminations (P < 0·05). Sandblasting treatment did not improve the saliva‐contaminated specimens. However, the glove powder plus sandblasting group showed no significant difference in SBS compared with the control group. There was no significant difference in SBS between the excess glass‐infiltrating group and the control group. The SBS was significantly decreased by rough aluminum oxide sandblasting (P < 0·05). The SBS values of groups without thermocycling were significantly greater than those of groups with thermocycling (P < 0·05). There were no significant differences among SBS values of the seven groups with thermocycling. Combined cohesive and adhesive bond failures were seen in every group. Various surface treatments or contaminants may significantly influence the bond strength of In‐Ceram restorative in clinical use.
- 1 September 2001
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 28 (9) , 805-813
Effects of surface treatments on bond strength of glass‐infiltrated ceramic
The purpose of this study was to evaluate the effects of various surface treatments on the bond strength at the In‐Ceram/resin composite interface. Ninety‐eight In‐Ceram specimens were divided into seven groups and exposed to various surface treatments as follows: (A) control (B) saliva contamination (C) saliva contamination plus aluminum oxide sandblasting (D) glove powder contamination (E) glove powder contamination plus aluminum oxide sandblasting (F) rough aluminum oxide sandblasting and (G) excess glass infiltration. A resin composite cylinder was cemented to each In‐Ceram specimen with Panavia 21 resin luting cement. Half of the cemented specimens in each group were stored in water for 24 h, and the other half were stored in water for 2 weeks and then were thermo‐cycled for 2000 cycles. Shear bond strengths (SBS) of seven specimens in each subgroup were determined and analysed using analysis of variance (ANOVA) and Tukey HSD test as well as Student‘s t‐test. Scanning electronic microscopy was used to identify the type of bond failure. Shear bond strength was significantly decreased by saliva and glove powder contaminations (P < 0·05). Sandblasting treatment did not improve the saliva‐contaminated specimens. However, the glove powder plus sandblasting group showed no significant difference in SBS compared with the control group. There was no significant difference in SBS between the excess glass‐infiltrating group and the control group. The SBS was significantly decreased by rough aluminum oxide sandblasting (P < 0·05). The SBS values of groups without thermocycling were significantly greater than those of groups with thermocycling (P < 0·05). There were no significant differences among SBS values of the seven groups with thermocycling. Combined cohesive and adhesive bond failures were seen in every group. Various surface treatments or contaminants may significantly influence the bond strength of In‐Ceram restorative in clinical use.
- 1 July 2001
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 28 (7) , 658-667
Flexural behaviour of post‐cured composites at oral‐simulating temperatures
Post‐curing treatments have been known to improve the mechanical stability of visible light‐cured composites. After individual post‐curing treatment, the flexural strength (FS) of four commercial direct/indirect placement composite materials which differ greatly in composition [oligocarbonate dimethacrylate (OCDMA)‐based Conquest C & B (CQT), Bisphenol‐A glycidyl dimethacrylate (BisGMA)‐based Charisma, urethane dimethacrylate (UDMA)‐based Concept (CCT), and BisGMA/UDMA‐based Dentacolor] was evaluated under water in the temperature range of 12–50 °C. A control series was tested in air at room temperature (25 ± 1 °C). Data were analysed using ANOVA and Duncan’s test. Flexural strengths overall decreased (20–40%, P < 0·01) with increasing temperatures except with Conquest C & B. Surprisingly, higher FS values were found in wet conditions than in dry conditions at 25 °C. UDMA‐based materials much more easily undergo softening in water and by temperature change than do BisGMA‐ or OCDMA‐based materials. Post‐cured composites can be significantly affected by exposure to oral environments. Different composition determines the degree of influence.
- 1 July 2001
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 28 (7) , 658-667
Flexural behaviour of post‐cured composites at oral‐simulating temperatures
Post‐curing treatments have been known to improve the mechanical stability of visible light‐cured composites. After individual post‐curing treatment, the flexural strength (FS) of four commercial direct/indirect placement composite materials which differ greatly in composition [oligocarbonate dimethacrylate (OCDMA)‐based Conquest C & B (CQT), Bisphenol‐A glycidyl dimethacrylate (BisGMA)‐based Charisma, urethane dimethacrylate (UDMA)‐based Concept (CCT), and BisGMA/UDMA‐based Dentacolor] was evaluated under water in the temperature range of 12–50 °C. A control series was tested in air at room temperature (25 ± 1 °C). Data were analysed using ANOVA and Duncan’s test. Flexural strengths overall decreased (20–40%, P < 0·01) with increasing temperatures except with Conquest C & B. Surprisingly, higher FS values were found in wet conditions than in dry conditions at 25 °C. UDMA‐based materials much more easily undergo softening in water and by temperature change than do BisGMA‐ or OCDMA‐based materials. Post‐cured composites can be significantly affected by exposure to oral environments. Different composition determines the degree of influence.
- 1 January 2001
- Published by Elsevier in Biomaterials
- Vol. 22 (2) , 113-123
Thermo-debonding mechanisms in dentin bonding systems using finite element analysis
- 1 January 2001
- Published by Elsevier in Biomaterials
- Vol. 22 (2) , 113-123
Thermo-debonding mechanisms in dentin bonding systems using finite element analysis
- 1 December 2000
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 27 (12) , 1047-1053
Effect of temperature and flux concentration on soldering of base metal
The present study used the acoustic emission (AE) technique to evaluate interactions among soldering temperature, flux treatment, and the resultant ultimate tensile strength (UTS). Scanning electron microscopy (SEM) was used to examine fracture surfaces of the solder joints. Specimens were cast from removable partial denture alloy and then placed in a jig with a gap distance of 1.0 mm. A high-frequency soldering machine with an optical pyrometer was used for soldering at 1150 degrees C and 1200 degrees C, respectively. The flux concentrations were 67% and 75%. The soldered specimens were subjected to tensile test at a crosshead speed of 0.05 mm/min. During testing, acoustic emissions in the frequency range of 100--1200 kHz were collected, filtered, recorded, and processed by a sensing device. The results were analysed by ANOVA and Tukey LSD test. UTS at different temperatures showed no significant difference according to either mechanical or acoustic results. But in the 1200 degrees C group, the UTSs and AE counts showed significant differences (P<0.05) at both flux concentrations. SEM showed that the 1200C group had better dendritic crystal structure than did the 1150 degrees C group. In the 1200 degrees C group specimens with 67% flux had fewer flux inclusion bodies and dendritic crystals than did specimens with 75% flux. The 75% flux subgroup produced high-amplitude (60--70 dB) acoustic signals within the elastic deformation zone, while the 67% flux subgroup produced similar signals within the plastic deformation zone, either beyond the 0.2% yield point or before fracture.
- 1 December 2000
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 27 (12) , 1047-1053
Effect of temperature and flux concentration on soldering of base metal
The present study used the acoustic emission (AE) technique to evaluate interactions among soldering temperature, flux treatment, and the resultant ultimate tensile strength (UTS). Scanning electron microscopy (SEM) was used to examine fracture surfaces of the solder joints. Specimens were cast from removable partial denture alloy and then placed in a jig with a gap distance of 1.0 mm. A high-frequency soldering machine with an optical pyrometer was used for soldering at 1150 degrees C and 1200 degrees C, respectively. The flux concentrations were 67% and 75%. The soldered specimens were subjected to tensile test at a crosshead speed of 0.05 mm/min. During testing, acoustic emissions in the frequency range of 100--1200 kHz were collected, filtered, recorded, and processed by a sensing device. The results were analysed by ANOVA and Tukey LSD test. UTS at different temperatures showed no significant difference according to either mechanical or acoustic results. But in the 1200 degrees C group, the UTSs and AE counts showed significant differences (P<0.05) at both flux concentrations. SEM showed that the 1200C group had better dendritic crystal structure than did the 1150 degrees C group. In the 1200 degrees C group specimens with 67% flux had fewer flux inclusion bodies and dendritic crystals than did specimens with 75% flux. The 75% flux subgroup produced high-amplitude (60--70 dB) acoustic signals within the elastic deformation zone, while the 67% flux subgroup produced similar signals within the plastic deformation zone, either beyond the 0.2% yield point or before fracture.
- 1 November 2000
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 27 (11) , 919-926
Influence of silanization and filler fraction on aged dental composites
The effect of silanization and filler fraction on the mechnical properties of aged dental composites was investigated. Experimental composites (75/25 Bis‐GMA/TEGDMA resin reinforced with 0, 12·6, 30·0, and 56·5 vol% 8 μm silanized/unsilanized BaSiO6) were fabricated into 4·7 mm diameter×2·2 mm thick discs and 3·5 mm diameter×7·3 mm thick discs for diametral tensile and compressive tests, respectively. The effect of immersion in 75% ethanol at 37 °C for 0–30 days on the diametral tensile strength (DTS) and compressive strength (CS) of the samples was evaluated and analysed by anova and Tukey LSD test. The fracture interface between filler and resin matrix was then examined by scanning electron microscope. Results and subsequent statistical evidence from DTS (18·6±7·6 MPa, silanized versus 11·7±2·6 MPa, unsilanized) and CS (85·1±29·7 MPa, silanized versus 56·0±11·3 MPa, unsilanized) strongly implies that silanization may greatly enhance the mechanical properties of the resin composites. Furthermore, it also shows that both DTS and CS increased proportionally as the filler fraction of the composites increased. However, in the unsilanized groups, DTS decreased (up to 40%) as the filler fraction increased, and CS showed no relevance to the filler fraction at all. As for the influence of aging, it was found that both DTS and CS showed a significant decrease after immersion in 75% ethanol, and silanization heavily correlated with the filler fraction of aged‐resin composites. Microscopic examination of the fractured samples showed that failure primarily occurred within the resin matrix per se for silanized composites and adjacent to the filler particles for unsilanized composites. All the evidence points to the conclusion that mechanical properties of aged‐resin composites can be greatly influenced by silanization and the filler fraction.
- 1 November 2000
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 27 (11) , 919-926
Influence of silanization and filler fraction on aged dental composites
The effect of silanization and filler fraction on the mechnical properties of aged dental composites was investigated. Experimental composites (75/25 Bis‐GMA/TEGDMA resin reinforced with 0, 12·6, 30·0, and 56·5 vol% 8 μm silanized/unsilanized BaSiO6) were fabricated into 4·7 mm diameter×2·2 mm thick discs and 3·5 mm diameter×7·3 mm thick discs for diametral tensile and compressive tests, respectively. The effect of immersion in 75% ethanol at 37 °C for 0–30 days on the diametral tensile strength (DTS) and compressive strength (CS) of the samples was evaluated and analysed by anova and Tukey LSD test. The fracture interface between filler and resin matrix was then examined by scanning electron microscope. Results and subsequent statistical evidence from DTS (18·6±7·6 MPa, silanized versus 11·7±2·6 MPa, unsilanized) and CS (85·1±29·7 MPa, silanized versus 56·0±11·3 MPa, unsilanized) strongly implies that silanization may greatly enhance the mechanical properties of the resin composites. Furthermore, it also shows that both DTS and CS increased proportionally as the filler fraction of the composites increased. However, in the unsilanized groups, DTS decreased (up to 40%) as the filler fraction increased, and CS showed no relevance to the filler fraction at all. As for the influence of aging, it was found that both DTS and CS showed a significant decrease after immersion in 75% ethanol, and silanization heavily correlated with the filler fraction of aged‐resin composites. Microscopic examination of the fractured samples showed that failure primarily occurred within the resin matrix per se for silanized composites and adjacent to the filler particles for unsilanized composites. All the evidence points to the conclusion that mechanical properties of aged‐resin composites can be greatly influenced by silanization and the filler fraction.
- 1 September 2000
- Published by Elsevier in Oral Surgery Oral Medicine Oral Pathology Oral Radiology and Endodontology
- Vol. 90 (3) , 285-291
Assessing the implant/bone interface by using natural frequency analysis
- 1 September 2000
- Published by Elsevier in Oral Surgery Oral Medicine Oral Pathology Oral Radiology and Endodontology
- Vol. 90 (3) , 285-291
Assessing the implant/bone interface by using natural frequency analysis
- 3 May 2000
- Published by Elsevier in Biomaterials
- Vol. 21 (13) , 1399-1408
Laser-induced acoustic emissions in experimental dental composites.
- 3 May 2000
- Published by Elsevier in Biomaterials
- Vol. 21 (13) , 1399-1408
Laser-induced acoustic emissions in experimental dental composites.
- 1 May 2000
- Published by Springer Nature in Medical & Biological Engineering & Computing
- Vol. 38 (3) , 253-259
Finite element analysis of brain contusion: An indirect impact study
The mechanism of brain contusion has been investigated using a series of three-dimensional (3D) finite element analyses. A head injury model was used to simulate forward and backward rotation around the upper cervical vertebra. Intracranial pressure and shear stress responses were calculated and compared. The results obtained with this model support the predictions of cavitation theory that a pressure gradient develops in the brain during indirect impact. Contrecoup pressure-time histories in the parasagittal plane demonstrated that an indirect impact induced a smaller intracranial pressure (−53.7 kPa for backward rotation, and −65.5 kPa for forward rotation) than that caused by a direct impact. In addition, negative pressures induced by indirect impact to the head were not high enough to form cavitation bubbles, which can damage the brain tissue. Simulations predicted that a decrease in skull deformation had a large effect in reducing the intracranial pressure. However, the areas of high shear stress concentration were consistent with those of clinical observations. The findings of this study suggest that shear strain theory appears to better account for the clinical findings in head injury when the head is subjected to an indirect impact.
- 1 May 2000
- Published by Springer Nature in Medical & Biological Engineering & Computing
- Vol. 38 (3) , 253-259
Finite element analysis of brain contusion: An indirect impact study
The mechanism of brain contusion has been investigated using a series of three-dimensional (3D) finite element analyses. A head injury model was used to simulate forward and backward rotation around the upper cervical vertebra. Intracranial pressure and shear stress responses were calculated and compared. The results obtained with this model support the predictions of cavitation theory that a pressure gradient develops in the brain during indirect impact. Contrecoup pressure-time histories in the parasagittal plane demonstrated that an indirect impact induced a smaller intracranial pressure (−53.7 kPa for backward rotation, and −65.5 kPa for forward rotation) than that caused by a direct impact. In addition, negative pressures induced by indirect impact to the head were not high enough to form cavitation bubbles, which can damage the brain tissue. Simulations predicted that a decrease in skull deformation had a large effect in reducing the intracranial pressure. However, the areas of high shear stress concentration were consistent with those of clinical observations. The findings of this study suggest that shear strain theory appears to better account for the clinical findings in head injury when the head is subjected to an indirect impact.
- 1 April 2000
- Published by Wiley in Journal of Periodontology
- Vol. 71 (4) , 632-640
In Vivo and In Vitro Natural Frequency Analysis of Periodontal Conditions: An Innovative Method
Background: When measuring periodontal disease, various types of equipment for making objective measurements of tooth mobility have been proposed. However, these devices and methodology are insufficient in terms of reliability. An innovative method using vibrational theories to assess the periodontal attachment level of natural teeth is presented in this study.Methods: Modal testing technique, a non‐destructive and time‐saving method, was used for non‐invasive and quantitative measurement of the natural frequencies of the upper central incisor in vivo and in vitro. A finite element model was established, and modal testing experiments were simulated to assess the relationship between bone level and teeth.Results: The first dominant natural frequency of healthy human upper central incisors ranges from 710 Hz to 3,360 Hz, with an average of 1,701 ± 679 Hz. Both in vitro experiment and finite element simulation showed that lowering of the attachment level causes a significant decrease in the natural frequencies, and a strong relationship (r = ‐0.99, P Conclusions: Our results suggested that natural frequency is an important parameter for assessing the periodontal condition and that the modal testing technique is a useful supplemental method for assessing the attachment conditions of the periodontium. J Periodontol 2000;71:632‐640.
- 1 April 2000
- Published by Wiley in Journal of Periodontology
- Vol. 71 (4) , 632-640
In Vivo and In Vitro Natural Frequency Analysis of Periodontal Conditions: An Innovative Method
Background: When measuring periodontal disease, various types of equipment for making objective measurements of tooth mobility have been proposed. However, these devices and methodology are insufficient in terms of reliability. An innovative method using vibrational theories to assess the periodontal attachment level of natural teeth is presented in this study.Methods: Modal testing technique, a non‐destructive and time‐saving method, was used for non‐invasive and quantitative measurement of the natural frequencies of the upper central incisor in vivo and in vitro. A finite element model was established, and modal testing experiments were simulated to assess the relationship between bone level and teeth.Results: The first dominant natural frequency of healthy human upper central incisors ranges from 710 Hz to 3,360 Hz, with an average of 1,701 ± 679 Hz. Both in vitro experiment and finite element simulation showed that lowering of the attachment level causes a significant decrease in the natural frequencies, and a strong relationship (r = ‐0.99, P Conclusions: Our results suggested that natural frequency is an important parameter for assessing the periodontal condition and that the modal testing technique is a useful supplemental method for assessing the attachment conditions of the periodontium. J Periodontol 2000;71:632‐640.
- 1 March 2000
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 27 (3) , 190-198
Degradation of repaired denture base materials in simulated oral fluid
This in vitro study evaluates the degradation of repaired denture bases upon immersion in a simulated oral fluid. Denture base materials (Luciton 199®), after being repaired by Repair Material® and Triad®, using three different joint surface designs (butt, round and 45 ° bevel), were immersed onto 99·5 vol.% ethanol/water solution (with similar solubility parameter) for various amounts of time (0–72 h). The flexural loads of the six combination of groups were measured by the three‐point bending tests using a universal testing machine. Acoustic emission (AE) during sample fracturing were processed using the MISTRA 2001 system. The fracture pattern and surface details of the interface were examined with a scanning electronic microscope (SEM). Data were analysed using three‐way anova and Tukey LSD tests. SEM micrographs of the fracture interface were used to differentiate the fracture mode. The flexural loads (2·72±0·51 Kgf) of the round joint specimens were significantly higher (PP<0·05) than those (1·59±0·40 Kgf) of specimens repaired with Repair Material®. Significant progressive reduction of the flexural load and/or AE signals of the specimens was noted in proportion to the length of time of the immersion in the simulated oral fluid. Mechanical strength of a denture base repaired with a round joint design and light‐cured material is significantly higher after immersion in simulated oral fluid.
- 1 March 2000
- Published by Wiley in Journal of Oral Rehabilitation
- Vol. 27 (3) , 190-198
Degradation of repaired denture base materials in simulated oral fluid
This in vitro study evaluates the degradation of repaired denture bases upon immersion in a simulated oral fluid. Denture base materials (Luciton 199®), after being repaired by Repair Material® and Triad®, using three different joint surface designs (butt, round and 45 ° bevel), were immersed onto 99·5 vol.% ethanol/water solution (with similar solubility parameter) for various amounts of time (0–72 h). The flexural loads of the six combination of groups were measured by the three‐point bending tests using a universal testing machine. Acoustic emission (AE) during sample fracturing were processed using the MISTRA 2001 system. The fracture pattern and surface details of the interface were examined with a scanning electronic microscope (SEM). Data were analysed using three‐way anova and Tukey LSD tests. SEM micrographs of the fracture interface were used to differentiate the fracture mode. The flexural loads (2·72±0·51 Kgf) of the round joint specimens were significantly higher (PP<0·05) than those (1·59±0·40 Kgf) of specimens repaired with Repair Material®. Significant progressive reduction of the flexural load and/or AE signals of the specimens was noted in proportion to the length of time of the immersion in the simulated oral fluid. Mechanical strength of a denture base repaired with a round joint design and light‐cured material is significantly higher after immersion in simulated oral fluid.