Selim H. Kusefoglu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Selim H. Kusefoglu has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Gökhan Çaylı
Department of Chemistry and Polymer Research Center, Boğaziçi University, Istanbul, Turkey
6 shared publications Tarik Eren
Department of Chemistry and Polymer Research Center, Boğaziçi University, Bebek, Istanbul 34342, Turkey
5 shared publicationsCem Öztürk
Department of Chemistry and Polymer Research Center, Boğaziçi University, Bebek, Istanbul 34342, Turkey
4 shared publicationsE. Taylan
Department of Chemistry and Polymer Research Center, Boğaziçi University, Bebek, Istanbul, Turkey 34342
2 shared publications- Hüseyin Esen
Department of Chemistry and Polymer Research Center, Boğaziçi University, Bebek, Istanbul, 34342, Turkey
2 shared publications Richard Wool
Center of Composite Materials, University of Delaware, Newark, Delaware 19716
2 shared publications
Latest Publications
- 4 November 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 124 (4) , 3229-3235
Chain extension reactions of unsaturated polyesters with bis(2‐oxazoline)s
Two different bisoxazolines, 2,2′‐(1,3‐phenylene) bis(2‐oxazoline) (1,3‐PBO) and 2,2′‐bis(2‐oxazoline) (BO) were investigated as chain extenders for short chain unsaturated polyesters (UPEs). These extenders reacted readily with carboxyl ends of unsaturated polyesters, leading to rapid molecular weight increase through coupling of oligomeric chains. Commercially available unsaturated polyesters commonly have molecular weights around 1500, usually reached after a 20‐h polyesterification reaction. When bisoxazolines were reacted with short UPE chains obtained at the 6th hour of a commercial polyesterification reaction, the molecular weight of UPE reached 1500 within 5–30 min, which provides economies and prevents the glycol loss and yellowing which are associated with extended reaction times. Styrene solubility, gel time, and thermal and mechanical properties of the chain extended polyesters remained comparable to the commercial UPE, with 8–10 min of gel time and a storage modulus about 3000 MPa. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012
- 4 November 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 124 (4) , 3229-3235
Chain extension reactions of unsaturated polyesters with bis(2‐oxazoline)s
Two different bisoxazolines, 2,2′‐(1,3‐phenylene) bis(2‐oxazoline) (1,3‐PBO) and 2,2′‐bis(2‐oxazoline) (BO) were investigated as chain extenders for short chain unsaturated polyesters (UPEs). These extenders reacted readily with carboxyl ends of unsaturated polyesters, leading to rapid molecular weight increase through coupling of oligomeric chains. Commercially available unsaturated polyesters commonly have molecular weights around 1500, usually reached after a 20‐h polyesterification reaction. When bisoxazolines were reacted with short UPE chains obtained at the 6th hour of a commercial polyesterification reaction, the molecular weight of UPE reached 1500 within 5–30 min, which provides economies and prevents the glycol loss and yellowing which are associated with extended reaction times. Styrene solubility, gel time, and thermal and mechanical properties of the chain extended polyesters remained comparable to the commercial UPE, with 8–10 min of gel time and a storage modulus about 3000 MPa. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012
- 30 March 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 121 (5) , 2976-2984
New polymers from epoxidized soybean oil with pyridine derivatives
In this study 4‐methylpyridine (4MP), 4‐vinylpyridine (4VP) and poly(4‐vinylpyridine) (P4VP) were separately reacted with epoxidized soybean oil triglycerides (ESO) to give plant oil based thermoset polymers. The addition reaction of pyridine with epoxide followed by a rearrangement results in formation of pyridone units and these were polymerized via a Diels–Alder reaction. DMA, DSC, TGA and IR spectroscopy were used for the characterization of the products. 4MP‐ESO, P4VP‐ESO and P4VP‐ESO‐in situ polymers were crosslinked yielding rigid infusible polymers. Glass transition temperatures (Tg) of 4MP‐ESO and P4VP‐ESO‐in situ were found as −10.5 and 70.5 (32.3 as shoulder) °C respectively, by DMA analysis. Storage moduli of 4MP‐ESO and P4VP‐ESO‐in situ at 25°C were 13.7 and 187.2 MPa, respectively. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 30 March 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 121 (5) , 2976-2984
New polymers from epoxidized soybean oil with pyridine derivatives
In this study 4‐methylpyridine (4MP), 4‐vinylpyridine (4VP) and poly(4‐vinylpyridine) (P4VP) were separately reacted with epoxidized soybean oil triglycerides (ESO) to give plant oil based thermoset polymers. The addition reaction of pyridine with epoxide followed by a rearrangement results in formation of pyridone units and these were polymerized via a Diels–Alder reaction. DMA, DSC, TGA and IR spectroscopy were used for the characterization of the products. 4MP‐ESO, P4VP‐ESO and P4VP‐ESO‐in situ polymers were crosslinked yielding rigid infusible polymers. Glass transition temperatures (Tg) of 4MP‐ESO and P4VP‐ESO‐in situ were found as −10.5 and 70.5 (32.3 as shoulder) °C respectively, by DMA analysis. Storage moduli of 4MP‐ESO and P4VP‐ESO‐in situ at 25°C were 13.7 and 187.2 MPa, respectively. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 1 December 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 120 (3) , 1707-1712
Polymerization of acrylated epoxidized soybean oil with phenol furfural resins via repeated forward and retro diels–alder reactions
In this work, the Diels–Alder reaction between the acrylate groups of acrylated epoxidized soybean oil and the furan rings of p‐tertiary butyl phenol furfural resin (TBPF) is described. The reaction was carried out at 110°C in presence of FeCl3 catalyst, and tough polymers were obtained in 1 h. Surprisingly, samples that were heated and cooled 5, 10, and 20 times to 140°C and room temperature had better mechanical properties than samples that were kept at 140°C for the same total duration. This unexpected behavior is attributed to a series of forward and retro Diels–Alder reactions between the functional groups. To prove this hypothesis, a model reaction between TBPF and n‐butyl acrylate was studied. At 100°C, 1H‐nuclear magnetic resonance signals of the furan ring protons disappeared, only to reappear at 140°C. Thermogravimetric analysis of the adduct showed a weight loss at 140–150°C, which was in quantitative agreement with the amount of butyl acrylate. Infrared analysis showed that furan rings were not completely consumed by extended heating at 110°C. After five heating and cooling cycles of much shorter duration at 140°C, the furan absorption in the infrared disappeared. The storage modulus of acrylated epoxidized soybean oil‐TBPF samples after 20 heating cycles was 1.15 GPa. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 1 December 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 120 (3) , 1707-1712
Polymerization of acrylated epoxidized soybean oil with phenol furfural resins via repeated forward and retro diels–alder reactions
In this work, the Diels–Alder reaction between the acrylate groups of acrylated epoxidized soybean oil and the furan rings of p‐tertiary butyl phenol furfural resin (TBPF) is described. The reaction was carried out at 110°C in presence of FeCl3 catalyst, and tough polymers were obtained in 1 h. Surprisingly, samples that were heated and cooled 5, 10, and 20 times to 140°C and room temperature had better mechanical properties than samples that were kept at 140°C for the same total duration. This unexpected behavior is attributed to a series of forward and retro Diels–Alder reactions between the functional groups. To prove this hypothesis, a model reaction between TBPF and n‐butyl acrylate was studied. At 100°C, 1H‐nuclear magnetic resonance signals of the furan ring protons disappeared, only to reappear at 140°C. Thermogravimetric analysis of the adduct showed a weight loss at 140–150°C, which was in quantitative agreement with the amount of butyl acrylate. Infrared analysis showed that furan rings were not completely consumed by extended heating at 110°C. After five heating and cooling cycles of much shorter duration at 140°C, the furan absorption in the infrared disappeared. The storage modulus of acrylated epoxidized soybean oil‐TBPF samples after 20 heating cycles was 1.15 GPa. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 11 October 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 120 (1) , 116-123
Polymerization of epoxidized soybean oil with maleinized polybutadiene
- 11 October 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 120 (1) , 116-123
Polymerization of epoxidized soybean oil with maleinized polybutadiene
- 1 September 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 119 (4) , 2431-2438
Oleophilic modification of poly(vinyl alcohol) films by functionalized soybean oil triglycerides
- 1 September 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 119 (4) , 2431-2438
Oleophilic modification of poly(vinyl alcohol) films by functionalized soybean oil triglycerides
- 30 July 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 119 (2) , 1102-1110
Blocked isocyanates and isocyanated soybean oil as new chain extenders for unsaturated polyesters
Two different blocked isocyanates, diphenylmethane–bis‐4,4′‐ethyleneurea and diphenylmethane–bis‐4,4′‐carbamoil–ϵ‐caprolactam, and isocyanated soybean oil were used as chain extenders for low‐molecular‐weight unsaturated polyesters. Oligomeric polyesters (molecular weight = 600–700), taken from a manufacturing process in the sixth hour of a 16‐h polyesterification reaction, were reacted with these chain extenders, and the desired chain lengths (molecular weight = 1000–1500) were obtained in a very short time through the reaction of the chain extenders with the polyester end groups. The increase in the molecular weight was monitored with gel permeation chromatography. The obtained polymers were characterized with Fourier transform infrared and 1H‐NMR and with styrene solubility and gel time measurements. After dilution with styrene, the polyesters were cured with a radical initiator. The thermal and mechanical properties of the cured polyesters were examined with dynamic mechanical analysis and thermogravimetric analysis tests and then compared to those of a commercially available reference unsaturated polyester. The results show that unsaturated polyesters can be chain‐extended with these compounds to shorten the polyesterification time substantially without alterations of the styrene solubility or gel time of the polyesters. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 30 July 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 119 (2) , 1102-1110
Blocked isocyanates and isocyanated soybean oil as new chain extenders for unsaturated polyesters
Two different blocked isocyanates, diphenylmethane–bis‐4,4′‐ethyleneurea and diphenylmethane–bis‐4,4′‐carbamoil–ϵ‐caprolactam, and isocyanated soybean oil were used as chain extenders for low‐molecular‐weight unsaturated polyesters. Oligomeric polyesters (molecular weight = 600–700), taken from a manufacturing process in the sixth hour of a 16‐h polyesterification reaction, were reacted with these chain extenders, and the desired chain lengths (molecular weight = 1000–1500) were obtained in a very short time through the reaction of the chain extenders with the polyester end groups. The increase in the molecular weight was monitored with gel permeation chromatography. The obtained polymers were characterized with Fourier transform infrared and 1H‐NMR and with styrene solubility and gel time measurements. After dilution with styrene, the polyesters were cured with a radical initiator. The thermal and mechanical properties of the cured polyesters were examined with dynamic mechanical analysis and thermogravimetric analysis tests and then compared to those of a commercially available reference unsaturated polyester. The results show that unsaturated polyesters can be chain‐extended with these compounds to shorten the polyesterification time substantially without alterations of the styrene solubility or gel time of the polyesters. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 14 July 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 118 (6) , 3311-3317
Polymerization of epoxidized soybean oil with maleinized soybean oil and maleic anhydride grafted polypropylene mixtures
In this study, maleinized soybean oil triglycerides (SOMA) were reacted with epoxidized soybean oil triglycerides (ESO) to give plant oil‐based thermoset polymers. To increase fracture toughness of the product, different amounts of SOMA was replaced by maleic anhydride grafted polypropylene (MMPP) (Epolene E43, maleate content 2.9%, Mn = 3900 and Polybond 3200, maleate content 1%, Mn = 1,10,000). The improvement in mechanical properties was monitored. The characterizations of the products were done by DMA, DSC, TGA, and IR spectroscopy. ESO‐SOMA and ESO‐SOMA‐MMPP polymers are crosslinked rigid infusible polymers. ESO‐SOMA‐MMPP(E43) and ESO‐SOMA‐MMPP(PB3200) showed a phase change at 146 and 169°C, respectively, probably due to the melting transition of the MMPP backbone. Storage moduli of the two polymers at 35°C were 54.6 and 246.1 MPa, respectively. Storage moduli and the impact strength of the polymers increased with MMPP content and with MMPP molecular weight. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 14 July 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 118 (6) , 3311-3317
Polymerization of epoxidized soybean oil with maleinized soybean oil and maleic anhydride grafted polypropylene mixtures
In this study, maleinized soybean oil triglycerides (SOMA) were reacted with epoxidized soybean oil triglycerides (ESO) to give plant oil‐based thermoset polymers. To increase fracture toughness of the product, different amounts of SOMA was replaced by maleic anhydride grafted polypropylene (MMPP) (Epolene E43, maleate content 2.9%, Mn = 3900 and Polybond 3200, maleate content 1%, Mn = 1,10,000). The improvement in mechanical properties was monitored. The characterizations of the products were done by DMA, DSC, TGA, and IR spectroscopy. ESO‐SOMA and ESO‐SOMA‐MMPP polymers are crosslinked rigid infusible polymers. ESO‐SOMA‐MMPP(E43) and ESO‐SOMA‐MMPP(PB3200) showed a phase change at 146 and 169°C, respectively, probably due to the melting transition of the MMPP backbone. Storage moduli of the two polymers at 35°C were 54.6 and 246.1 MPa, respectively. Storage moduli and the impact strength of the polymers increased with MMPP content and with MMPP molecular weight. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 26 May 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 118 (2) , 849-856
Polymerization of linseed oil with phenolic resins
In this study, linseed oil was directly polymerized with different oil soluble resoles. p‐Ethyl (PEP), p‐tertiary butyl (PTB), p‐tertiary octyl (PTO), and p‐phenyl (PPP) phenols were separately reacted with formaldehyde to give linseed oil soluble resoles. These were then reacted with linseed oil to give transparent rubbery polymers. A model reaction was performed with methyl oleate and PTB phenol resole to clarify the reaction mechanism. Reaction products were characterized with 1H‐NMR and IR techniques. Spectral examination of the model reaction showed that polymerization reaction proceeded via ene reaction of the quinone methide formed at the end group of the resole with the allylic positions of the fatty ester. Rubbery polymers were obtained with linseed oil using 10 to 40% of the different resoles. Hard, load bearing and tough materials were obtained at 40% phenolic resin loading. Mechanical properties of the materials were characterized by dynamic mechanical analyzer (DMA) and stress–strain tests. The best mechanical and thermal properties were obtained with PEP resole which showed a storage modulus of 350 MPa and a tan δ peak at 65°C. Storage moduli of 275, 250, and 30 were obtained for PPP, PTB, and PTO resoles‐linseed oil polymers, respectively. At the same phenolic resin loading, elongation at break and swelling ratios in CH2Cl2 increased with the longer alkyl substitution on the resole resins. The highest thermal stability was observed by PEP resole–linseed oil polymer which has a 5% weight loss temperature of 340°C as determined by TGA. The lowest thermal stability was observed for PTB resole‐linseed oil polymer at 220°C. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 26 May 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 118 (2) , 849-856
Polymerization of linseed oil with phenolic resins
In this study, linseed oil was directly polymerized with different oil soluble resoles. p‐Ethyl (PEP), p‐tertiary butyl (PTB), p‐tertiary octyl (PTO), and p‐phenyl (PPP) phenols were separately reacted with formaldehyde to give linseed oil soluble resoles. These were then reacted with linseed oil to give transparent rubbery polymers. A model reaction was performed with methyl oleate and PTB phenol resole to clarify the reaction mechanism. Reaction products were characterized with 1H‐NMR and IR techniques. Spectral examination of the model reaction showed that polymerization reaction proceeded via ene reaction of the quinone methide formed at the end group of the resole with the allylic positions of the fatty ester. Rubbery polymers were obtained with linseed oil using 10 to 40% of the different resoles. Hard, load bearing and tough materials were obtained at 40% phenolic resin loading. Mechanical properties of the materials were characterized by dynamic mechanical analyzer (DMA) and stress–strain tests. The best mechanical and thermal properties were obtained with PEP resole which showed a storage modulus of 350 MPa and a tan δ peak at 65°C. Storage moduli of 275, 250, and 30 were obtained for PPP, PTB, and PTO resoles‐linseed oil polymers, respectively. At the same phenolic resin loading, elongation at break and swelling ratios in CH2Cl2 increased with the longer alkyl substitution on the resole resins. The highest thermal stability was observed by PEP resole–linseed oil polymer which has a 5% weight loss temperature of 340°C as determined by TGA. The lowest thermal stability was observed for PTB resole‐linseed oil polymer at 220°C. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 14 January 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 116 (4) , 2433-2440
A simple one‐step synthesis and polymerization of plant oil triglyceride iodo isocyanates
In this study, a novel and simple route for the synthesis of the iodine isocyanate (INCO) adduct of soybean oil triglycerides is described. Soybean oil iodo isocyanate (ISONCO) was synthesized by the reaction of iodine isocyanate and soybean oil at room temperature. ISONCO was then polymerized with polyols, such as, castor oil, pentamethylene glycol, and glycerol to give the corresponding polyurethanes and with polyamines, such as, ethylene diamine, hexamethylene diamine, and triethylene tetramine to give corresponding polyureas. The structures of the monomer and the polymers were determined by FTIR and 1H‐NMR analyses. Thermal properties of the polymers were determined by DSC and TGA. Thermal degradation of the polyurethanes started at 150°C. Stability of the polyureas was higher than polyurethanes. Almost all polymers showed a Tg around −50°C. The mechanical properties of the polymers were determined by tensile tests. Among the polymers synthesized, castor oil polyurethane showed the highest elongation at break and the lowest tensile strength of 140 KPa. The highest tensile strength of 900 KPa was observed in the pentamethylene glycol polyurethanes. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 14 January 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 116 (4) , 2433-2440
A simple one‐step synthesis and polymerization of plant oil triglyceride iodo isocyanates
In this study, a novel and simple route for the synthesis of the iodine isocyanate (INCO) adduct of soybean oil triglycerides is described. Soybean oil iodo isocyanate (ISONCO) was synthesized by the reaction of iodine isocyanate and soybean oil at room temperature. ISONCO was then polymerized with polyols, such as, castor oil, pentamethylene glycol, and glycerol to give the corresponding polyurethanes and with polyamines, such as, ethylene diamine, hexamethylene diamine, and triethylene tetramine to give corresponding polyureas. The structures of the monomer and the polymers were determined by FTIR and 1H‐NMR analyses. Thermal properties of the polymers were determined by DSC and TGA. Thermal degradation of the polyurethanes started at 150°C. Stability of the polyureas was higher than polyurethanes. Almost all polymers showed a Tg around −50°C. The mechanical properties of the polymers were determined by tensile tests. Among the polymers synthesized, castor oil polyurethane showed the highest elongation at break and the lowest tensile strength of 140 KPa. The highest tensile strength of 900 KPa was observed in the pentamethylene glycol polyurethanes. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 1 December 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 116 (1) , 355-365
New polymers from plant oil derivatives and styrene‐maleic anhydride copolymers
- 1 December 2009
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 116 (1) , 355-365
New polymers from plant oil derivatives and styrene‐maleic anhydride copolymers