Elina Huttunen-Saarivirta
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Elina Huttunen-Saarivirta has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
M. Schütze
Karl Winnacker Inst DECHEMA eV, D-60486 Frankfurt, Germany
3 shared publicationsV. Rohr
Karl Winnacker Inst DECHEMA eV, D-60486 Frankfurt, Germany
3 shared publicationsF.H. Stott
Univ Manchester, Sch Mat, Ctr Corros & Protect, Manchester M60 1QD, Lancs, England
2 shared publicationsH. Paajanen
Finnish Air Force, Air Materiel Command, Aircraft Technologies Office, P.O. Box 210, FI-33101 Tampere (Finland)
2 shared publications- Jari Kokkonen
Tampere University of Technology
2 shared publications T Tiainen
Institute of Materials Science, Tampere University of Technology, PO Box 589, FIN-33101 Tampere, Finland
2 shared publications
Latest Publications
- 26 May 2010
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 20 (2) , 298-305
Oxidation of Uncoated and Aluminized 9-12% Cr Boiler Steels at 550-650 °C
- 26 May 2010
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 20 (2) , 298-305
Oxidation of Uncoated and Aluminized 9-12% Cr Boiler Steels at 550-650 °C
- 1 January 2010
- Published by Elsevier in Tribology International
- Vol. 43 (1-2) , 161-170
Erosion-oxidation of uncoated, aluminized and chromized-aluminized 9Cr–1Mo steels under fluidized-bed conditions at 550–700 °C
- 1 January 2010
- Published by Elsevier in Tribology International
- Vol. 43 (1-2) , 161-170
Erosion-oxidation of uncoated, aluminized and chromized-aluminized 9Cr–1Mo steels under fluidized-bed conditions at 550–700 °C
- 27 February 2009
- Published by Wiley in Materials and Corrosion
- Vol. 60 (3) , 173-191
Corrosion behaviour of aircraft coating systems in acetate‐ and formate‐based de‐icing chemicals
Corrosion behaviour of four coating systems, which are commonly used in aircraft components; namely cadmium‐coated and subsequently chromate‐treated steel AISI 4340, aluminium‐coated steel AISI 4340, anodised aluminium alloy 7075‐T6 and chromate‐treated aluminium alloy 7075‐T6, were investigated in six commercial acetate‐ and formate‐based de‐icing chemicals. The results show that the aluminium‐coated steel specimens experience least corrosion among the four coating systems; no corrosion is detected in potassium acetate‐based de‐icing chemicals (Safeway KA HOT, Safegrip and Safegrip+), although some corrosion is observed in the other three chemicals (Safeway SD, Safeway SF and Meltium). In contrast, the coatings in the other three coating systems are damaged in all six de‐icing chemicals. The thickness of the coating does not necessarily predict how well the coating will protect the substrate; the thickest coating, several tens of micrometres, is apparent on the cadmium‐ and chromate‐coated steel specimens, while only a few micrometres thin aluminium coating on the steel substrate is the only coating system that can survive the corrosion tests in some of the de‐icing chemicals. Comparison of the results from the two test methods used in this research, polarisation measurements and chemical exposure tests, shows that, for each coating system, the extent of corrosion, as evaluated on the basis of weight changes calculated from corrosion current density values and those experienced during chemical exposure tests, is different: the weight changes that materialise during exposure tests are, at least, from one to two orders of magnitude higher than those predicted by calculations. In this paper, these observations are discussed and explanations for them are presented.
- 27 February 2009
- Published by Wiley in Materials and Corrosion
- Vol. 60 (3) , 173-191
Corrosion behaviour of aircraft coating systems in acetate‐ and formate‐based de‐icing chemicals
Corrosion behaviour of four coating systems, which are commonly used in aircraft components; namely cadmium‐coated and subsequently chromate‐treated steel AISI 4340, aluminium‐coated steel AISI 4340, anodised aluminium alloy 7075‐T6 and chromate‐treated aluminium alloy 7075‐T6, were investigated in six commercial acetate‐ and formate‐based de‐icing chemicals. The results show that the aluminium‐coated steel specimens experience least corrosion among the four coating systems; no corrosion is detected in potassium acetate‐based de‐icing chemicals (Safeway KA HOT, Safegrip and Safegrip+), although some corrosion is observed in the other three chemicals (Safeway SD, Safeway SF and Meltium). In contrast, the coatings in the other three coating systems are damaged in all six de‐icing chemicals. The thickness of the coating does not necessarily predict how well the coating will protect the substrate; the thickest coating, several tens of micrometres, is apparent on the cadmium‐ and chromate‐coated steel specimens, while only a few micrometres thin aluminium coating on the steel substrate is the only coating system that can survive the corrosion tests in some of the de‐icing chemicals. Comparison of the results from the two test methods used in this research, polarisation measurements and chemical exposure tests, shows that, for each coating system, the extent of corrosion, as evaluated on the basis of weight changes calculated from corrosion current density values and those experienced during chemical exposure tests, is different: the weight changes that materialise during exposure tests are, at least, from one to two orders of magnitude higher than those predicted by calculations. In this paper, these observations are discussed and explanations for them are presented.
- 21 June 2007
- Published by Springer Nature in Oxidation of Metals
- Vol. 68 (3-4) , 113-132
Erosion–Oxidation Behavior of Chromized–Aluminized 9% Chromium Steel under Fluidized-Bed Conditions at Elevated Temperature
- 21 June 2007
- Published by Springer Nature in Oxidation of Metals
- Vol. 68 (3-4) , 113-132
Erosion–Oxidation Behavior of Chromized–Aluminized 9% Chromium Steel under Fluidized-Bed Conditions at Elevated Temperature
- 30 September 2003
- Published by Elsevier in Intermetallics
- Vol. 11 (9) , 879-891
Influence of Cr alloying on the microstructure of thermally sprayed quasicrystalline Al–Cu–Fe coatings
- 30 September 2003
- Published by Elsevier in Intermetallics
- Vol. 11 (9) , 879-891
Influence of Cr alloying on the microstructure of thermally sprayed quasicrystalline Al–Cu–Fe coatings
- 22 July 2002
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 336 (1-2) , 52-58
Microstructural study of the initiation and formation of immersion tin coating on copper
- 22 July 2002
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 336 (1-2) , 52-58
Microstructural study of the initiation and formation of immersion tin coating on copper
- 8 March 2002
- Published by Elsevier in Applied Surface Science
- Vol. 191 (1-4) , 106-117
Characterising the quality of chemical tin coatings on copper by electrochemical current noise method
- 8 March 2002
- Published by Elsevier in Applied Surface Science
- Vol. 191 (1-4) , 106-117
Characterising the quality of chemical tin coatings on copper by electrochemical current noise method