Jun Hyub Park
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Jun Hyub Park has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
H.‐J. Lee
Nano Mechanics Team, Korea Institute of Machinery & Materials, Taejon 305‐343, Korea
3 shared publicationsY.‐H. Huh
Korea Research Institute of Standards and Science, Yusong‐gu, Daejeon, South Korea
3 shared publicationsY.‐J. Kim
Korea university, Anam‐dong Seongbuk‐Gu, Seoul 136‐701, South Korea
3 shared publicationsHyeon-Chang Choi
Department of Mechatronics Engineering, College of Engineering, Tongmyong University, Busan, Korea
2 shared publicationsB.‐I. Choi
Nano Mechanics Team, Korea Institute of Machinery & Materials, Taejon 305‐343, Korea
1 shared publicationH.Y. Kim
Nanofab Center, 53‐3 Eoeun‐dong Yuseong‐gu Daejeon, 305‐806, South Korea
1 shared publication
Latest Publications
- Open Access
- 3 May 2011
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 42 (5) , 478-484
Tensile test of lead zirconate titanate (PZT)/Platinum (Pt) thin film
This paper presents the results of tensile tests for lead zirconate titanate (PZT)/Platinum (Pt) thin films of 2.15 μm thickness in atmospheric air at room temperature. An axial loading tester developed by the authors was used for the tests. The tester was equipped with a load cell with a maximum capacity of 0.5 N and a non‐contact position measuring system based on the principle of capacitance micrometry. Furthermore, the tester was equipped with a CCD (charge‐coupled device) system for measuring the displacement of the gage length. Specimens with three different widths (50, 100 and 150 μm) were fabricated to study the size (width of specimen) effects. The elastic moduli of the specimens with 50, 100 and 150 μm width were 72.8 ± 3.7, 75.0 ± 1.3, 73.3 ± 1.8 GPa, respectively. In addition, the ultimate tensile strength of the specimens with 50, 100 and 150 μm width were 263.4 ± 21.1, 238.6 ± 4.5, 221.1 ± 13.9 MPa, respectively. It was observed that the width of specimen has little effect on the elastic modulus of PZT/Pt thin films but has an effect on the ultimate tensile strength of PZT/Pt thin films and the ultimate tensile strength decreases as the width increases. It was assumed that the scatter in the ultimate tensile strength of 50 μm width was attributed to delamination of PZT/Pt layers before the fracture in the tensile test. The 0.2% offset yield strength could not be measured because the PZT/Pt thin film is very brittle.
- 3 May 2011
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 42 (5) , 478-484
Open AccessTensile test of lead zirconate titanate (PZT)/Platinum (Pt) thin film
This paper presents the results of tensile tests for lead zirconate titanate (PZT)/Platinum (Pt) thin films of 2.15 μm thickness in atmospheric air at room temperature. An axial loading tester developed by the authors was used for the tests. The tester was equipped with a load cell with a maximum capacity of 0.5 N and a non‐contact position measuring system based on the principle of capacitance micrometry. Furthermore, the tester was equipped with a CCD (charge‐coupled device) system for measuring the displacement of the gage length. Specimens with three different widths (50, 100 and 150 μm) were fabricated to study the size (width of specimen) effects. The elastic moduli of the specimens with 50, 100 and 150 μm width were 72.8 ± 3.7, 75.0 ± 1.3, 73.3 ± 1.8 GPa, respectively. In addition, the ultimate tensile strength of the specimens with 50, 100 and 150 μm width were 263.4 ± 21.1, 238.6 ± 4.5, 221.1 ± 13.9 MPa, respectively. It was observed that the width of specimen has little effect on the elastic modulus of PZT/Pt thin films but has an effect on the ultimate tensile strength of PZT/Pt thin films and the ultimate tensile strength decreases as the width increases. It was assumed that the scatter in the ultimate tensile strength of 50 μm width was attributed to delamination of PZT/Pt layers before the fracture in the tensile test. The 0.2% offset yield strength could not be measured because the PZT/Pt thin film is very brittle.
- 1 May 2010
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 41 (5) , 391-397
Optimal design of rear chassis components for lightweight automobile using design of experiment
- 1 May 2010
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 41 (5) , 391-397
Optimal design of rear chassis components for lightweight automobile using design of experiment
- 23 March 2009
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 40 (3) , 187-191
A study on the fatigue behaviour of electro‐plated NiCo thin film for probe tip applications
In this study, fatigue tests were performed for NiCo alloy which is commonly used in probe tips of test machines of semiconductors. The smooth specimens were fabricated by MEMS process including electro‐plating process on a single‐side polished 6 inches (100) silicon wafer. The NiCo thin film consists of about 66.2 % Ni and 33.8 % Co. The specimen is 2000 μm long, 9 μm thick and 100 μm wide. The tests were performed using a novel test procedure, a structure of the specimen is easy to manipulate, align and grip a thin‐film and a test machine proposed by the authors. The closed‐loop feedback control of the magnetic‐electric actuator allowed load‐controlled and high cycle fatigue tests with 5 Hz frequency, in ambient environment and with a stress ratio of R = 0.1. The fatigue strength coefficient and exponent were 1324 MPa and ‐0.0558, respectively. In a fatigue test of thin film, it is difficult to perform the fatigue test at R = ‐1. However, the result of the fatigue test at R = ‐1 should be required when fatigue life prediction is performed under variable loading. Therefore, in this study, the modified Goodman method, Gerber method and Soderberg method were considered to investigate which method is most reasonable when mean stress is considered.
- 23 March 2009
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 40 (3) , 187-191
A study on the fatigue behaviour of electro‐plated NiCo thin film for probe tip applications
In this study, fatigue tests were performed for NiCo alloy which is commonly used in probe tips of test machines of semiconductors. The smooth specimens were fabricated by MEMS process including electro‐plating process on a single‐side polished 6 inches (100) silicon wafer. The NiCo thin film consists of about 66.2 % Ni and 33.8 % Co. The specimen is 2000 μm long, 9 μm thick and 100 μm wide. The tests were performed using a novel test procedure, a structure of the specimen is easy to manipulate, align and grip a thin‐film and a test machine proposed by the authors. The closed‐loop feedback control of the magnetic‐electric actuator allowed load‐controlled and high cycle fatigue tests with 5 Hz frequency, in ambient environment and with a stress ratio of R = 0.1. The fatigue strength coefficient and exponent were 1324 MPa and ‐0.0558, respectively. In a fatigue test of thin film, it is difficult to perform the fatigue test at R = ‐1. However, the result of the fatigue test at R = ‐1 should be required when fatigue life prediction is performed under variable loading. Therefore, in this study, the modified Goodman method, Gerber method and Soderberg method were considered to investigate which method is most reasonable when mean stress is considered.
- 1 August 2008
- Published by Springer Nature in Acta Mechanica Solida Sinica
- Vol. 21 (4) , 318-326
Effect of Fabrication on High Cycle Fatigue Properties of Copper Thin Films
- 1 August 2008
- Published by Springer Nature in Acta Mechanica Solida Sinica
- Vol. 21 (4) , 318-326
Effect of Fabrication on High Cycle Fatigue Properties of Copper Thin Films
- 21 February 2008
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 39 (2) , 187-192
Tensile and high cycle fatigue test of copper thin film
This paper presents the results of tensile and high cycle fatigue tests for copper thin film. Copper films coated by Sn are often used in various electro devices. Especially, when the film is used in tape carrier package (TCP), the film is repeatedly exposed to mechanical or(and) thermal stresses which results often in the failure of the component. Therefore, to guarantee the reliability of the electrical devices using a film, tensile and fatigue characteristics of the film are important. In this study, to obtain the tensile and fatigue characteristics of the film, the specimen was fabricated by an etching process to make a smooth specimen of 2000 μm width, 8000 μm length and 15.26 μm thickness. The tensile and high cycle fatigue tests were performed with the specimen using the test machine developed by the authors. These specimens had measured values of Young's modulus (72 GPa) and a 0.2 % offset yield and an ultimate strength of 358 MPa and 462 MPa, respectively. A closed‐loop feedback control of the magnetic‐electric actuator allowed load‐controlled fatigue tests with 20 Hz frequency, in ambient environment and at two levels of mean stresses. The fatigue strength coefficient and exponent at 0.5 times of the ultimate tensile strength were 431 MPa and ‐0.0843, respectively. The fatigue strength coefficient and exponent at 0.6 times of the ultimate tensile strength were 371 MPa and ‐0.0923, respectively. The Goodman method is recommended when the fatigue life of thin film with mean stress will be estimated. The fatigue strength coefficient and exponent of copper thin film modified using Goodman method were 910 MPa and ‐0.0896, respectively.
- 21 February 2008
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 39 (2) , 187-192
Tensile and high cycle fatigue test of copper thin film
This paper presents the results of tensile and high cycle fatigue tests for copper thin film. Copper films coated by Sn are often used in various electro devices. Especially, when the film is used in tape carrier package (TCP), the film is repeatedly exposed to mechanical or(and) thermal stresses which results often in the failure of the component. Therefore, to guarantee the reliability of the electrical devices using a film, tensile and fatigue characteristics of the film are important. In this study, to obtain the tensile and fatigue characteristics of the film, the specimen was fabricated by an etching process to make a smooth specimen of 2000 μm width, 8000 μm length and 15.26 μm thickness. The tensile and high cycle fatigue tests were performed with the specimen using the test machine developed by the authors. These specimens had measured values of Young's modulus (72 GPa) and a 0.2 % offset yield and an ultimate strength of 358 MPa and 462 MPa, respectively. A closed‐loop feedback control of the magnetic‐electric actuator allowed load‐controlled fatigue tests with 20 Hz frequency, in ambient environment and at two levels of mean stresses. The fatigue strength coefficient and exponent at 0.5 times of the ultimate tensile strength were 431 MPa and ‐0.0843, respectively. The fatigue strength coefficient and exponent at 0.6 times of the ultimate tensile strength were 371 MPa and ‐0.0923, respectively. The Goodman method is recommended when the fatigue life of thin film with mean stress will be estimated. The fatigue strength coefficient and exponent of copper thin film modified using Goodman method were 910 MPa and ‐0.0896, respectively.
- 28 June 2005
- Published by Springer Nature in Microsystem Technologies
- Vol. 11 (8) , 925-932
FEM analysis of multilayered MEMS device under thermal and residual stress
- 28 June 2005
- Published by Springer Nature in Microsystem Technologies
- Vol. 11 (8) , 925-932
FEM analysis of multilayered MEMS device under thermal and residual stress
- 1 May 2005
- Published by Springer Nature in Journal of Mechanical Science and Technology
- Vol. 19 (5) , 1065-1071
Prediction of residual stress distribution in multi-stacked thin film by curvature measurement and iterative FEA
- 1 May 2005
- Published by Springer Nature in Journal of Mechanical Science and Technology
- Vol. 19 (5) , 1065-1071
Prediction of residual stress distribution in multi-stacked thin film by curvature measurement and iterative FEA
- 1 January 2005
- Published by Springer Nature in Microsystem Technologies
- Vol. 11 (1) , 16-22
Investigation to minimize heater burnout in thermal thin film print heads
- 1 January 2005
- Published by Springer Nature in Microsystem Technologies
- Vol. 11 (1) , 16-22
Investigation to minimize heater burnout in thermal thin film print heads
- 1 April 2003
- Published by ASME International in Journal of Engineering Materials and Technology
- Vol. 125 (2) , 208-214
New Estimation Method of Fatigue Properties of Aluminum Alloys
A new method on estimating fatigue properties from simple tensile data was proposed for aluminum alloys. The method is based on experimental strain-life curves. An optimization technique was used to get the best fatigue properties. The four-point correlation method, the universal slopes method, Mitchell’s method, the modified universal slopes method, the uniform material law by Ba¨umel and Seeger, the modified four-point correlation method by Ong and a new method proposed in this work were evaluated in a quantitative manner. Mitchell’s method, the uniform materials law and the new method give good life predictions for aluminum alloys. In particular, the new method provided the best results.
- 1 April 2003
- Published by ASME International in Journal of Engineering Materials and Technology
- Vol. 125 (2) , 208-214
New Estimation Method of Fatigue Properties of Aluminum Alloys
A new method on estimating fatigue properties from simple tensile data was proposed for aluminum alloys. The method is based on experimental strain-life curves. An optimization technique was used to get the best fatigue properties. The four-point correlation method, the universal slopes method, Mitchell’s method, the modified universal slopes method, the uniform material law by Ba¨umel and Seeger, the modified four-point correlation method by Ong and a new method proposed in this work were evaluated in a quantitative manner. Mitchell’s method, the uniform materials law and the new method give good life predictions for aluminum alloys. In particular, the new method provided the best results.