JXJun Xiao

Jun Xiao

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Jun Xiao has a total of 21 co-authors. Here are the top co-authors by number of shared publications:

  • Q. Xu

    2 shared publications
  • Shao-Yu Qiu

    Science and Technology on Reactor Fuel and Materials Laboratory, Nuclear Power Institute of China, Chengdu 610041, China

    2 shared publications
  • Y. Chen

    2 shared publications
  • Yong Chen

    Science and Technology on Reactor Fuel and Materials Laboratory, Nuclear Power Institute of China, Chengdu 610213, China

    2 shared publications
  • Bing Tang

    Science and Technology on Reactor Fuel and Materials Laboratory, Nuclear Power Institute of China, Chengdu 610213, China

    1 shared publication
  • Guoqing Li

    Science and Technology on Reactor Fuel and Materials Laboratory, Nuclear Power Institute of China, Chengdu 610213, China

    1 shared publication

Latest Publications

  • Fatigue Crack Growth of Z2CND18-12N Austenitic Stainless Steel and Its Heat-Affected Zone in a Dissimilar Metal Weld Joint in 325°C Water

    by Jun Xiao, Ting Xiao, Guoqing Li, Bing Tang, Yuqi Zheng, Hao Wang, Yong Chen, Shaoyu Qiu

    Fatigue crack growth (FCG) in Z2CND18-12N austenitic stainless steel and its heat-affected zone (HAZ) in the Z2CND18-12N/16MND5 dissimilar metal weld joint has been investigated in room temperature air and 325°C water. The dependence of FCG rates on specimen orientation in room temperature air got somewhat evident as ΔK decreased to 13 MPa√m. However, for Z2CND18-12N steel, the influence of specimen orientation on the FCG in room temperature air and the corrosion fatigue crack growth (CFCG) in 325°C water was slight and negligible. A moderate increase in the FCG rate was observed for the Z2CND18-12N HAZ in room temperature air at a low ΔK = 13 MPa√m (near ΔK threshold), compared with its base metal. However, the CFCG rate difference between the Z2CND18-12N HAZ and its base metal was minor. The CFCG in the Z2CND18-12N in 325°C water (without the addition of H2) was consistent with a slip-oxidation-rupture mechanism and the oxide film on the corrosion fatigue crack tip mainly consisted of Fe3O4.


  • Open Access

    Corrosion Behavior and Surface Treatment of Cladding Materials Used in High-Temperature Lead-Bismuth Eutectic Alloy: A Review

    by Hao Wang, Jun Xiao, Hui Wang, Yong Chen, Xing Yin, Ning Guo

    Liquid metal fast reactors were considered to be the most promising solution to meet the enormous energy demand in the future. However, corrosion phenomenon caused by the liquid metal, especially in high-temperature lead-bismuth coolant, has greatly hindered the commercialization of the advanced Generation-IV nuclear system. This review discussed current research on the corrosion resistance of structural materials (such as EP823, T91, ODS, and authentic steels) in high-temperature liquid metal served as reactor coolants. The current corrosion resistance evaluation has proved that even for the excellent performance of EP823, the structural material selected in pressurized water reactor is not the ideal material for operation in the high-temperature lead-bismuth eutectic (LBE). Furthermore, the latest coating technologies that are expected to be applied to cladding materials for coolant system were extensively discussed, including Al-containing coatings, ceramic coatings, oxide coatings, amorphous coatings and high-entropy alloy coatings. The detailed comparison summarized the corrosion morphology and corrosion products of various coatings in LBE. This review not only provided a systematic understanding of the corrosion phenomena, but also demonstrated that coating technology is an effective method to solve the corrosion issues of the advanced next-generation reactors.


  • Technical Note: Corrosion Fatigue Crack Growth of Forged Type 316NG Austenitic Stainless Steel in 325°C Water

    by Jun Xiao, Lu Yao Chen, Jun Zhou, Shao-Yu Qiu, Yong Chen

    Forged Type 316NG austenitic stainless steel is commonly used to fabricate primary coolant pipe in advanced pressurized water reactor systems, but it is subject to corrosion fatigue cracking in primary coolant environments. In this study, the fatigue crack growth of Type 316NG austenitic stainless steel in 325°C water was investigated. The corrosion fatigue effect in 325°C water was mainly correlated to the crack growth rate and load frequency. A maximum Fen (environment corrected factor) value up to 100 was observed at f = 0.005 Hz, ΔK = 13 MPa√m. The dissolved oxygen tended to have little influence on the fatigue crack growth. The crack path was deflected and branched. Most secondary cracks tended to be initiated from grain boundaries.


  • Technical Note: Investigation of Oxide Film Formed on Alloy 690 (TT) Tubes in Alkaline Water

    by Hui Jiang, Jun Xiao

    Alloy 690 (thermally treated, TT) tubes are used for steam generator heat transfer components. It is subjected to serious corrosion problem in the heat transfer crevices. In this paper, the long-term oxidation of Alloy 690 (TT) tubes in alkaline water (264°C, 50% NaOH) was investigated. It was found the structure of the oxide film varied with exposure time. The oxide film was initially composed of an outer layer of Fe2O3 and an inner layer of Cr2O3/Ni(OH)2. As the time of exposure extended to 3,000 h, it became a monolayer of Ni(OH)2. In addition, the selective dissolution of Fe and Cr was also found and a porous metallic Ni layer was observed in the matrix/oxide film interface by scanning electron microscopy and x-ray photoelectron spectroscopy.


  • Technical Note: Frequency Dependence of Fatigue Crack Growth Rate of Alloy 690TT in High-Temperature Boron-Lithium Water

    by Jun Xiao, X. Qiu, Z.Y. Lin, Shao-Yu Qiu, Y. Chen, Q. Xu

    Alloy 690TT is a widely used material for steam generator tubes in pressurized water reactors, where it is susceptible to corrosion fatigue. In this study, the effect of loading frequency on the corrosion fatigue behavior of Alloy 690TT in boron-lithium water was investigated under small-scale yielding conditions. Along with stress ratio, the loading frequency had a significant influence on the crack path and fatigue crack growth rate. Both the corrosion fatigue crack growth rate and the environment enhancement factor were quantitatively correlated with the loading frequency in the form of exponential functions.


  • Prediction Model for Corrosion Fatigue Lives of Austenitic Stainless Steels in Pressurized Water Reactor Environments

    by J. Xiao, S.Y. Qiu, Y. Chen, Q. Xu

    A basic problem of austenitic stainless steels applied in pressurized water reactors (PWR) is degradation by corrosion fatigue. This paper proposes a prediction model (Nuclear Power Institute of China [NPIC] model) to estimate corrosion fatigue lives of austenitic stainless steels in PWR environments. The NPIC model is built on a corrosion fatigue mechanism and indicates the corrosion fatigue processes better than the ANL model proposed by Argonne National Laboratory. Both the NPIC and ANL models are somewhat conservative in their predictions.