Huahui Chen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Huahui Chen has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
Bin Wen
School of Mechanical Engineering, Henan University of Engineering, PR China
1 shared publicationChunyang Wang
China University of Mining and Technology, Beijing, China
1 shared publicationFei Du
China University of Mining and Technology, Beijing, China
1 shared publicationFu Zhao
China University of Mining and Technology, Beijing, China
1 shared publicationHaiping Hong
South Dakota School of Mines and Technology, SD, USA
1 shared publication- Hongsong Zhang
Department of Mechanical Engineering, Henan University of Engineering, Zhengzhou, China
1 shared publication
Latest Publications
- 14 May 2021
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 52 (5) , 529-539
Formation mechanism of in‐situ V8C7 and V3B4 particles in iron matrix composites by vacuum sintering
The in‐situ V8C7‐V3B4/Fe45 composites were fabricated by vacuum sintering using ferrovanadium, carbon black and Fe45 alloy powders as raw materials. The microstructure, phase structure and hardness of sintered Fe45+x wt.% (FeV+C) composite specimens (x = 0, x = 5, x = 10, x = 15, x = 20) were investigated. The results show that the type and shape of in‐situ borides and carbides depend on the content of (FeV+C) mixed powders. When x = 5, the composite consists of α‐(Fe, Cr, V) solid solution, strip M7C3 carbides and block M2B borides. When x = 10, the V3B4 particles initiate inside the M2B borides by in‐situ precipitation, and the excess vanadium reacts with carbon to in‐situ form V8C7 particles. When x≥15, the M2B completely transform into V3B4. Furthermore, the V8C7 and V3B4 particles coarsened and tended to be spheroidal and rectangle shape respectively. The V3B4 particles coarsen possibly by contacting and merging of the small V3B4 particles. However, the V8C7 particles coarsen possibly by the Ostwald ripening. The hardness of the composites increases firstly and then decreases with the increase of (FeV+C) mixed powders. The Fe45+10 wt.% (FeV+C) composite has the highest hardness value (54.2 HRC), which is due to the fine boride and carbide reinforcement and little pore defect.
- 14 May 2021
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 52 (5) , 529-539
Formation mechanism of in‐situ V8C7 and V3B4 particles in iron matrix composites by vacuum sintering
The in‐situ V8C7‐V3B4/Fe45 composites were fabricated by vacuum sintering using ferrovanadium, carbon black and Fe45 alloy powders as raw materials. The microstructure, phase structure and hardness of sintered Fe45+x wt.% (FeV+C) composite specimens (x = 0, x = 5, x = 10, x = 15, x = 20) were investigated. The results show that the type and shape of in‐situ borides and carbides depend on the content of (FeV+C) mixed powders. When x = 5, the composite consists of α‐(Fe, Cr, V) solid solution, strip M7C3 carbides and block M2B borides. When x = 10, the V3B4 particles initiate inside the M2B borides by in‐situ precipitation, and the excess vanadium reacts with carbon to in‐situ form V8C7 particles. When x≥15, the M2B completely transform into V3B4. Furthermore, the V8C7 and V3B4 particles coarsened and tended to be spheroidal and rectangle shape respectively. The V3B4 particles coarsen possibly by contacting and merging of the small V3B4 particles. However, the V8C7 particles coarsen possibly by the Ostwald ripening. The hardness of the composites increases firstly and then decreases with the increase of (FeV+C) mixed powders. The Fe45+10 wt.% (FeV+C) composite has the highest hardness value (54.2 HRC), which is due to the fine boride and carbide reinforcement and little pore defect.
- Open Access
- 1 January 2021
- Published by National Library of Serbia in Processing and Application of Ceramics
- Vol. 15 (3) , 306-313
Thermophysical performances of (Sm1-xLux)3TaO7 (x = 0, 0.1, 0.3 and 0.5) ceramics
To optimize thermophysical performances, Sm3TaO7 was doped with Lu3+ and pressureless sintered at 1600 ?C. It was shown that Sm3+ is partly substituted by Lu3+ cations and the (Sm1-xLux)3TaO7 ceramics with a single pyrochlore structure are obtained.With increasing x value from 0 to 0.5, the band gap increases gradually from 4.677 to 4.880 eV. Owing to the enhanced phonon scattering caused by Lu3+ doping, the thermal conductivities at 800 ?C of the prepared samples are in the range of 0.95-1.44W?K?1?m?1. It was also confirmed that the phase transition is restrained effectively by substituting Sm3+ with Lu3+. Due to the reduction of crystal lattice energy and average electro-negativity difference, the thermal expansion coefficient (TEC) is heightened with increasing Lu content. TEC achieves the highest value (10.45 ? 10?6 K?1 at 1200 ?C) at the equal molar ratio between Sm3+ and Lu3+ cations (i.e. x = 0.5), which is much higher than those of 7YSZ and Sm2Zr2O7 ceramics.
- 1 January 2021
- Published by National Library of Serbia in Processing and Application of Ceramics
- Vol. 15 (3) , 306-313
Open AccessThermophysical performances of (Sm1-xLux)3TaO7 (x = 0, 0.1, 0.3 and 0.5) ceramics
To optimize thermophysical performances, Sm3TaO7 was doped with Lu3+ and pressureless sintered at 1600 ?C. It was shown that Sm3+ is partly substituted by Lu3+ cations and the (Sm1-xLux)3TaO7 ceramics with a single pyrochlore structure are obtained.With increasing x value from 0 to 0.5, the band gap increases gradually from 4.677 to 4.880 eV. Owing to the enhanced phonon scattering caused by Lu3+ doping, the thermal conductivities at 800 ?C of the prepared samples are in the range of 0.95-1.44W?K?1?m?1. It was also confirmed that the phase transition is restrained effectively by substituting Sm3+ with Lu3+. Due to the reduction of crystal lattice energy and average electro-negativity difference, the thermal expansion coefficient (TEC) is heightened with increasing Lu content. TEC achieves the highest value (10.45 ? 10?6 K?1 at 1200 ?C) at the equal molar ratio between Sm3+ and Lu3+ cations (i.e. x = 0.5), which is much higher than those of 7YSZ and Sm2Zr2O7 ceramics.