Maxim E. Doroshenko
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Maxim E. Doroshenko has a total of 73 co-authors. Here are the top co-authors by number of shared publications:
V V Osiko
Prokhorov General Physics Institute, Russian Academy of Sciences, Vavilov str., 38, Moscow 119991 Russia
7 shared publicationsV. V. Osiko
General Physics Institute of Russian Academy of Sciences, Vavilov Str. 38, Moscow 119991, Russia
5 shared publicationsA G Papashvili
Prokhorov General Physics Institute, Russian Academy of Sciences, Vavilov str., 38, Moscow 119991, Russia
4 shared publicationsA N Nakladov
Prokhorov General Physics Institute, Russian Academy of Sciences, Vavilov str., 38, Moscow 119991, Russia
4 shared publications- Adam Říha
Czech Technical University in Prague (Czech Republic)
4 shared publications - Michal Jelínek
Czech Technical University in Prague, Faculty of Nuclear Sciences and Physical Engineering, Prague, Czech Republic
4 shared publications
Latest Publications
- Open Access
- 19 February 2025
- Published by Springer Nature in Applied Physics B
- Vol. 131 (3) , 1-8
Comparison of temperature dependence of Fe:ZnSe laser output properties under semi-longitudinal excitation by 2.94 and $\sim$4.04 ${\upmu }$m radiationThe temperature dependence of the laser output properties of the Fe:ZnSe single crystal was compared under its excitation by 2.94 $${\upmu }$$ m Q-switched Er:YAG laser radiation and by $$\sim$$ 4.04 $${\upmu }$$ m gain-switched second Fe:ZnSe laser radiation within the same semi-longitudinal configuration. A non-selective laser cavity consisted of a flat highly reflective mirror at $$\sim$$ 4–5 $${\upmu }$$ m and a concave (r = 200 mm) output coupler with a reflectivity of 88% at $$\sim$$ 3.9 $$-$$ 5.3 $${\upmu }$$ m. To keep the energy at both excitation wavelengths the same of $$\sim$$ 9.4 mJ, a special filters were used for attenuation of 2.94 $${\upmu }$$ m radiation. The output energy almost doubled since the angle between pumping and generated laser radiation was reduced from $$\sim$$ 20 $$^{\circ }$$ to $$\sim$$ 12 $$^{\circ }$$ . The generated laser oscillation wavelength was shifted by $$\sim$$ 100 nm in the case of $$\sim$$ 4.04 $${\upmu }$$ m compared to excitation by 2.94 $${\upmu }$$ m radiation. The maximum laser output energy of $$\sim$$ 1.7 mJ under 2.94 $${\upmu }$$ m excitation was obtained at 78 K. However, at $$\sim$$ 4.04 $${\upmu }$$ m pumping, the maximum of $$\sim$$ 0.5 mJ was obtained at 260 K. The efficiency at 2.94 $${\upmu }$$ m excitation decreased from $$\sim$$ 33% at 78 K to $$\sim$$ 12% at 340 K. At $$\sim$$ 4.04 $${\upmu }$$ m radiation excitation, the efficiency increased from the laser threshold at 120 K to its maximum of $$\sim$$ 9% at 260 K.- 19 February 2025
- Published by Springer Nature in Applied Physics B
- Vol. 131 (3) , 1-8
Open AccessComparison of temperature dependence of Fe:ZnSe laser output properties under semi-longitudinal excitation by 2.94 and $\sim$4.04 ${\upmu }$m radiationThe temperature dependence of the laser output properties of the Fe:ZnSe single crystal was compared under its excitation by 2.94 $${\upmu }$$ m Q-switched Er:YAG laser radiation and by $$\sim$$ 4.04 $${\upmu }$$ m gain-switched second Fe:ZnSe laser radiation within the same semi-longitudinal configuration. A non-selective laser cavity consisted of a flat highly reflective mirror at $$\sim$$ 4–5 $${\upmu }$$ m and a concave (r = 200 mm) output coupler with a reflectivity of 88% at $$\sim$$ 3.9 $$-$$ 5.3 $${\upmu }$$ m. To keep the energy at both excitation wavelengths the same of $$\sim$$ 9.4 mJ, a special filters were used for attenuation of 2.94 $${\upmu }$$ m radiation. The output energy almost doubled since the angle between pumping and generated laser radiation was reduced from $$\sim$$ 20 $$^{\circ }$$ to $$\sim$$ 12 $$^{\circ }$$ . The generated laser oscillation wavelength was shifted by $$\sim$$ 100 nm in the case of $$\sim$$ 4.04 $${\upmu }$$ m compared to excitation by 2.94 $${\upmu }$$ m radiation. The maximum laser output energy of $$\sim$$ 1.7 mJ under 2.94 $${\upmu }$$ m excitation was obtained at 78 K. However, at $$\sim$$ 4.04 $${\upmu }$$ m pumping, the maximum of $$\sim$$ 0.5 mJ was obtained at 260 K. The efficiency at 2.94 $${\upmu }$$ m excitation decreased from $$\sim$$ 33% at 78 K to $$\sim$$ 12% at 340 K. At $$\sim$$ 4.04 $${\upmu }$$ m radiation excitation, the efficiency increased from the laser threshold at 120 K to its maximum of $$\sim$$ 9% at 260 K. - Open Access
- 18 December 2023
- Published by American Chemical Society (ACS) in ChemRxiv
Spectroscopy of yttrium scandate doped with ytterbium ion
The spectral-kinetic properties of Yb3+ optical centers in YScO3 crystal fiber were studied using selective laser spectroscopy. Various spectral characteristics of the Yb3+ optical centers were determined, including homogeneous and inhomogeneous broadening values, Stark level splitting, and the lifetime of Yb3+ ion optical centers. Three distinct types of Yb3+ optical centers were identified. The first optical center, with a lifetime of III77K = 4.05 ms, was formed due to the substitution of Y3+ for Yb3+ ions in the local site of С3i. The other two Yb3+ optical centers, with lifetimes of I77K = 1.0 ms (СII2(Y3+) center) and II77K = 0.620 ms (СII2(Sc3+)), respectively, were formed as a result of the substitution of Y3+ and Sc3+ for Yb3+ in the local site of C2.
- 18 December 2023
- Published by American Chemical Society (ACS) in ChemRxiv
Open AccessSpectroscopy of yttrium scandate doped with ytterbium ion
The spectral-kinetic properties of Yb3+ optical centers in YScO3 crystal fiber were studied using selective laser spectroscopy. Various spectral characteristics of the Yb3+ optical centers were determined, including homogeneous and inhomogeneous broadening values, Stark level splitting, and the lifetime of Yb3+ ion optical centers. Three distinct types of Yb3+ optical centers were identified. The first optical center, with a lifetime of III77K = 4.05 ms, was formed due to the substitution of Y3+ for Yb3+ ions in the local site of С3i. The other two Yb3+ optical centers, with lifetimes of I77K = 1.0 ms (СII2(Y3+) center) and II77K = 0.620 ms (СII2(Sc3+)), respectively, were formed as a result of the substitution of Y3+ and Sc3+ for Yb3+ in the local site of C2.
- 1 January 2023
- Published by Ioffe Institute Russian Academy of Sciences in Оптика и спектроскопия
- Vol. 131 (4) , 460
Формирование Cr-=SUP=-2+-=/SUP=--Fe-=SUP=-2+-=/SUP=- кластеров в кристалле Zn-=SUB=-1-x-=/SUB=-Mn-=SUB=-x-=/SUB=-Se
Spectroscopic properties of Cr2+ and Fe2+ ions in Zn1-xMnxSe solid solution with Mn content x=0.05 and x=0.3 at low (77K) temperature are investigated and their difference for crystals doped only by chromium ions and co-doped by chromium and iron ions is demonstrated. This difference is attributed to formation of Cr2+ - Fe2+ clusters in co-doped crystals.
- 1 January 2023
- Published by Ioffe Institute Russian Academy of Sciences in Оптика и спектроскопия
- Vol. 131 (4) , 460
Формирование Cr-=SUP=-2+-=/SUP=--Fe-=SUP=-2+-=/SUP=- кластеров в кристалле Zn-=SUB=-1-x-=/SUB=-Mn-=SUB=-x-=/SUB=-Se
Spectroscopic properties of Cr2+ and Fe2+ ions in Zn1-xMnxSe solid solution with Mn content x=0.05 and x=0.3 at low (77K) temperature are investigated and their difference for crystals doped only by chromium ions and co-doped by chromium and iron ions is demonstrated. This difference is attributed to formation of Cr2+ - Fe2+ clusters in co-doped crystals.
- Open Access
Mid-Infrared Laser Generation of Zn1−xMnxSe and Zn1−xMgxSe (x ≈ 0.3) Single Crystals Co-Doped by Cr2+ and Fe2+ Ions—Comparison of Different Excitation Wavelengths
Two different mid-infrared (mid-IR) solid-state crystalline laser active media of Cr, Fe:ZnMnSe and Cr, Fe:ZnMgSe with similar amounts of manganese or magnesium ions of x ≈ 0.3 were investigated at cryogenic temperatures for three different excitation wavelengths: Q-switched Er:YLF laser at the wavelength of 1.73 m, Q-switched Er:YAG laser at 2.94 m, and the gain-switched Fe:ZnSe laser operated at a liquid nitrogen temperature of 78 K at ∼4.05 m. The temperature dependence of spectral and laser characteristics was measured. Depending on the excitation wavelength and the selected output coupler, both laser systems were able to generate radiation by Cr or by Fe ions under direct excitation or indirectly by the Cr→ Fe energy transfer mechanism. Laser generation of Fe ions in Cr, Fe:ZnMnSe and Cr, Fe:ZnMgSe (x ≈ 0.3) crystals at the wavelengths of ∼4.4 and ∼4.8 m at a temperature of 78 K was achieved, respectively. The excitation of Fe ions in both samples by direct 2.94 m as well as ∼4.05 m radiation or indirectly via the Cr→ Fe ions’ energy transfer-based mechanism by 1.73 m radiation was demonstrated. Based on the obtained results, the possibility of developing novel coherent laser systems in mid-IR regions (∼2.3–2.5 and ∼4.4–4.9 m) based on AB matrices was presented.Open AccessMid-Infrared Laser Generation of Zn1−xMnxSe and Zn1−xMgxSe (x ≈ 0.3) Single Crystals Co-Doped by Cr2+ and Fe2+ Ions—Comparison of Different Excitation Wavelengths
Two different mid-infrared (mid-IR) solid-state crystalline laser active media of Cr, Fe:ZnMnSe and Cr, Fe:ZnMgSe with similar amounts of manganese or magnesium ions of x ≈ 0.3 were investigated at cryogenic temperatures for three different excitation wavelengths: Q-switched Er:YLF laser at the wavelength of 1.73 m, Q-switched Er:YAG laser at 2.94 m, and the gain-switched Fe:ZnSe laser operated at a liquid nitrogen temperature of 78 K at ∼4.05 m. The temperature dependence of spectral and laser characteristics was measured. Depending on the excitation wavelength and the selected output coupler, both laser systems were able to generate radiation by Cr or by Fe ions under direct excitation or indirectly by the Cr→ Fe energy transfer mechanism. Laser generation of Fe ions in Cr, Fe:ZnMnSe and Cr, Fe:ZnMgSe (x ≈ 0.3) crystals at the wavelengths of ∼4.4 and ∼4.8 m at a temperature of 78 K was achieved, respectively. The excitation of Fe ions in both samples by direct 2.94 m as well as ∼4.05 m radiation or indirectly via the Cr→ Fe ions’ energy transfer-based mechanism by 1.73 m radiation was demonstrated. Based on the obtained results, the possibility of developing novel coherent laser systems in mid-IR regions (∼2.3–2.5 and ∼4.4–4.9 m) based on AB matrices was presented. - 23 May 2019
- Published by Optica Publishing Group in Optics Letters
- Vol. 44 (11) , 2724-2727
Mid-IR (44 μm) Zn1−xMnxSe:Cr2+,Fe2+ (x = 03) laser pumped by 17 μm laser using Cr2+-Fe2+ energy transfer
This Letter determines the ions energy transfer process parameters in the () crystal and demonstrates a dipole-dipole type of the ions nonradiative energy transfer. The intracavity pumping as well as pumping through energy transfer in the , () crystal under 1735 nm excitation by an YLF:Er laser was realized in a temperature range of 78 up to 150 K for the first time, to the best of our knowledge. Output pulse energy up to 20 μJ at under 5.5 mJ of 1735 nm absorbed pump energy was obtained for the ions energy transfer mode.- 23 May 2019
- Published by Optica Publishing Group in Optics Letters
- Vol. 44 (11) , 2724-2727
Mid-IR (44 μm) Zn1−xMnxSe:Cr2+,Fe2+ (x = 03) laser pumped by 17 μm laser using Cr2+-Fe2+ energy transfer
This Letter determines the ions energy transfer process parameters in the () crystal and demonstrates a dipole-dipole type of the ions nonradiative energy transfer. The intracavity pumping as well as pumping through energy transfer in the , () crystal under 1735 nm excitation by an YLF:Er laser was realized in a temperature range of 78 up to 150 K for the first time, to the best of our knowledge. Output pulse energy up to 20 μJ at under 5.5 mJ of 1735 nm absorbed pump energy was obtained for the ions energy transfer mode.- 25 March 2019
- Published by Optica Publishing Group in Optics Letters
- Vol. 44 (7) , 1686-1689
Influence of the pumping wavelength on laser properties of Fe2+ ions in ZnSe crystal
active laser crystal properties at different excitation wavelengths (2.94 and 4.1 μm) were investigated, and noticeable variations of the fluorescence spectra shape and their maxima positions, as well as changes in decay times, were observed. A stepwise shift of the laser oscillation wavelength from 4.7 μm at 2.94 μm pumping to 4.95 μm at 4.1 μm pumping was achieved at room temperature.- 25 March 2019
- Published by Optica Publishing Group in Optics Letters
- Vol. 44 (7) , 1686-1689
Influence of the pumping wavelength on laser properties of Fe2+ ions in ZnSe crystal
active laser crystal properties at different excitation wavelengths (2.94 and 4.1 μm) were investigated, and noticeable variations of the fluorescence spectra shape and their maxima positions, as well as changes in decay times, were observed. A stepwise shift of the laser oscillation wavelength from 4.7 μm at 2.94 μm pumping to 4.95 μm at 4.1 μm pumping was achieved at room temperature.- 4 June 2018
- Published by Optica Publishing Group in Optical Materials Express
- Vol. 8 (7) , 1708-1722
Spectral and lasing characteristics of Fe:Cd1-xMnxTe (x = 01 – 076) crystals in the temperature range 77 to 300 K
The spectroscopic and laser properties of Fe:Cd1-xMnxTe with a various amount of manganese Mn (x = 0.1, 0.52, 0.68, and 0.76) were investigated in a broad temperature range from 77 to 300 K. The increase of Mn content in the Fe:Cd1-xMnxTe crystals was shown to result in an almost similar long-wavelength shift of absorption, fluorescence, and laser output spectra of about ~20 nm per each 10% of manganese. Laser generation was achieved in all crystals with the output energies up to 5.7 μJ. The central oscillation wavelength can be set by temperature as well as manganese content in the range 4950 up to 5650 nm.
- 4 June 2018
- Published by Optica Publishing Group in Optical Materials Express
- Vol. 8 (7) , 1708-1722
Spectral and lasing characteristics of Fe:Cd1-xMnxTe (x = 01 – 076) crystals in the temperature range 77 to 300 K
The spectroscopic and laser properties of Fe:Cd1-xMnxTe with a various amount of manganese Mn (x = 0.1, 0.52, 0.68, and 0.76) were investigated in a broad temperature range from 77 to 300 K. The increase of Mn content in the Fe:Cd1-xMnxTe crystals was shown to result in an almost similar long-wavelength shift of absorption, fluorescence, and laser output spectra of about ~20 nm per each 10% of manganese. Laser generation was achieved in all crystals with the output energies up to 5.7 μJ. The central oscillation wavelength can be set by temperature as well as manganese content in the range 4950 up to 5650 nm.
- 5 January 2017
- Published by IOP Publishing in Laser Physics Letters
- Vol. 14 (2) , 025801
Cd1−xMnxTe (x = 0.1–0.78) crystals doped with Fe2+ions: spectroscopic properties and laser oscillations at 4.95–5.27µm at low temperature
Spectroscopic and laser properties of Fe2+-doped Cd1−x Mn x Te solid solutions in a wide range of Mn concentration (x = 0.1–0.78) are investigated under excitation by a cryogenically cooled ZnSe:Fe2+ laser (λ = 4080 nm) and by a PbGa2S4:Dy3+ laser (λ = 4335 nm). To our best knowledge, lasing of Fe2+ ions in CdMnTe crystals is demonstrated for the first time. The laser worked in a nonselective cavity at 77 K within the 4950–5270 nm spectral range depending on the Mn concentration x.
- 5 January 2017
- Published by IOP Publishing in Laser Physics Letters
- Vol. 14 (2) , 025801
Cd1−xMnxTe (x = 0.1–0.78) crystals doped with Fe2+ions: spectroscopic properties and laser oscillations at 4.95–5.27µm at low temperature
Spectroscopic and laser properties of Fe2+-doped Cd1−x Mn x Te solid solutions in a wide range of Mn concentration (x = 0.1–0.78) are investigated under excitation by a cryogenically cooled ZnSe:Fe2+ laser (λ = 4080 nm) and by a PbGa2S4:Dy3+ laser (λ = 4335 nm). To our best knowledge, lasing of Fe2+ ions in CdMnTe crystals is demonstrated for the first time. The laser worked in a nonselective cavity at 77 K within the 4950–5270 nm spectral range depending on the Mn concentration x.
- 1 January 2017
- Published by Pleiades Publishing Ltd in Optics and Spectroscopy
- Vol. 122 (1) , 128-132
Formation of new Tm3+ tetragonal symmetry optical centers in CaF2 hot-formed laser ceramics
By means of time-resolved site-selective spectroscopy the formation of new Tm3+ optical centers with modified local environment and presumably tetragonal local symmetry in CaF2 hot-formed laser quality ceramics is observed. The spectroscopic properties of these new Tm3+ optical centers are investigated and shown to differ strongly from that for regular tetragonal optical centers.
- 1 January 2017
- Published by Pleiades Publishing Ltd in Optics and Spectroscopy
- Vol. 122 (1) , 128-132
Formation of new Tm3+ tetragonal symmetry optical centers in CaF2 hot-formed laser ceramics
By means of time-resolved site-selective spectroscopy the formation of new Tm3+ optical centers with modified local environment and presumably tetragonal local symmetry in CaF2 hot-formed laser quality ceramics is observed. The spectroscopic properties of these new Tm3+ optical centers are investigated and shown to differ strongly from that for regular tetragonal optical centers.