  • Open Access

    Biomimetic Deposition of Zn-Doped Calcium Phosphate Coatings on Surface-Activated Ti6Al4V for Multifunctional Implant Interfaces

    by Yaimi Martín-Santana, Yadira González-Carranza, Leonel Díaz-Tato, Arturo Juárez-Hernández, Edgar Omar García-Sánchez, Myriam Angélica De La Garza-Ramos, Edén Amaral Rodríguez-Castellanos, Marco Antonio Loudovic Hernández-Rodríguez

    The design of implant surfaces that support bone integration while limiting bacterial colonization remains a central challenge in biomaterials science and engineering. In this work, zinc-doped biomimetic calcium phosphate (CaP-Zn) coatings were fabricated on Ti6Al4V through surface activation followed by deposition in supersaturated simulated body fluid (SBF). Acid and alkali–calcium treatments produced a porous, calcium-rich interface that enabled the uniform formation of apatite-like CaP layers. Zinc incorporation was achieved without suppressing the formation of CaP phases and led to systematic changes in coating microstructure and surface chemistry. Spectroscopic and structural analyses indicated Zn incorporation within the CaP matrix, consistent with partial Ca2+ substitution and its association with poorly crystalline domains. These features promoted controlled ionic release and localized dissolution–reprecipitation behavior. Antibacterial testing against Streptococcus mutans revealed a clear Zn-dependent reduction in bacterial viability, while cytocompatibility remained within acceptable limits at moderate Zn levels. Finally, the coatings combine intrinsic bioactivity with ion-mediated antibacterial functionality, offering a multifunctional surface strategy for advanced titanium-based implants.


  • Open Access

    Evolution of Microstructure, Hardness, and Wear Behavior of Medium-Entropy CuNiSiCrCoTiNbx Alloy

    by Denis Ariel Avila-Salgado, Arturo Juárez-Hernández, Nelson Javier Izaguirre-Bonilla, Jonathan Muñoz Tabora, José Luis Camacho-Martínez

    Medium-entropy alloys (MEAs) allow the formation of different phases, generally in a solid-solution state, and compounds that favor obtaining alloys with properties superior to those of conventional alloys. In this study, medium-entropy CuNiSiCrCoTiNbx alloys were fabricated via melting in a vacuum induction furnace. The influence of the Nb addition (X = 0, 0.5 and 1 wt%) alloying elements on the microstructure, hardness, and wear resistance of the CuNiSiCrCoTiNb0 (M1), CuNiSiCrCoTiNb0.5 (M2), and CuNiCoCrSiTiNb1 (M3) alloys were explored using X-ray diffraction (XRD), scanning electron microscopy (SEM), and a ball-on-disc tribometer, respectively. In general, the results indicated that the incorporation of Nb alloying element promoted the evolution of the microstructure, increased the hardness, and improvement of the wear resistance. The XRD and SEM findings demonstrate that higher Nb addition and aging heat treatment (AT) modification mainly favored the formation of dendritic regions and the precipitation of the Co2Nb, Cr3Si, and Ni2Si phases, which promoted the refinement and strengthening of the microstructure. Significant increases in hardness were recorded: 11.95% increased, promoted by the addition of Nb before (E1) and after (E2, E3, and E4) the heat treatments. The maximum hardness values recorded were 92 ± 0.11 (AC) and 103 ± 0.5 HRB (AT-60 min) for the M3 alloy. The increase in hardness caused by Nb addition and aging heat treatments contributed to the dry sliding wear resistance response, decreasing material loss by 20%. This was related to the high concentration of precipitated phases rich in CoNb, CrSi, and NiSi with high hardness. Finally, the M3 alloy aged for 60 min exhibited the best specific wear rate behavior, with a material loss of 1.29 mm3. The commercial Cu-Be C17510 alloy experienced a maximum hardness of 83.47 Hardness Rockwell B, HRB, and a high wear rate of 3.34 mm3.


  • Process parameters effect and porosity reduction on AlSi10Mg parts manufactured by selective laser melting

    by July Andrea Taborda Rios, Patricia Zambrano-Robledo, Juan Daniel Trejos Taborda, Johan Andrés Gómez Espinoza, Catalina Jaramillo Isaza, Arturo Juárez-Hernández


  • Effect of laser surface texturing and boriding on the tribocorrosion resistance of an ASTM F-1537 cobalt alloy

    by C.A. Cuao-Moreu, I. Campos-Silva, A.M. Delgado-Brito, E.O. Garcia-Sanchez, A. Juarez-Hernandez, Jose M. Diabb-Zavala, M.A.L. Hernandez-Rodriguez


  • Open Access

    Effects of Nb Additions and Heat Treatments on the Microstructure, Hardness and Wear Resistance of CuNiCrSiCoTiNbx High-Entropy Alloys

    by Denis Ariel Avila-Salgado, Arturo Juárez-Hernández, María Lara Banda, Arnoldo Bedolla-Jacuinde, Francisco V. Guerra

    In this research, a set of CuNiCrSiCoTi (H-0Nb), CuNiCrSiCoTiNb0.5 (H-0.5Nb) and CuNiCrSiCoTiNb1 (H-1Nb) high-entropy alloys (HEAs) were melted in a vacuum induction furnace. The effects of Nb additions on the microstructure, hardness, and wear behavior of these HEAs (compared with a CuBe commercial alloy) in the as-cast (AC) condition, and after solution (SHT) and aging (AT) heat treatments, were investigated using X-ray diffraction, optical microscopy, and electron microscopy. A ball-on-disc configuration tribometer was used to study wear behavior. XRD and SEM results showed that an increase in Nb additions and modification by heat treatment (HT) favored the formation of BCC and FCC crystal structures (CS), dendritic regions, and the precipitation of phases that promoted microstructure refinement during solidification. Increases in hardness of HEA systems were recorded after heat treatment and Nb additions. Maximum hardness values were recorded for the H-1Nb alloy with measured increases from 107.53 HRB (AC) to 112.98 HRB, and from 1104 HV to 1230 HV (aged for 60 min). However, the increase in hardness caused by Nb additions did not contribute to wear resistance response. This can be attributed to a high distribution of precipitated phases rich in high-hardness NiSiTi and CrSi. Finally, the H-0Nb alloy exhibited the best wear resistance behavior in the aged condition of 30 min, with a material loss of 0.92 mm3.


  • Open Access

    Strengthening Properties and Wear Resistance of the Cu-xNi-yCo-Cr-Si Alloy by Varying Ni/Co and Zr Addition

    by Denis Ariel Avila-Salgado, Arturo Juárez-Hernández, José Cabral-Miramontes, José Luis Camacho-Martínez

    This work examines the effect of nickel (Ni) and cobalt (Co) concentrations on wear resistance behavior of Cu-xNi-yCo-Cr-Si (x = 8−9 wt%, y = 1−2 wt%) and the zirconium (Zr) addition, in order to obtain an alloy with similar or better properties than the C17510 alloy. In this study, hardness and wear resistance mechanism behavior were associated with the microstructure evolution of these alloys with different aging strengthening conditions. Different heat treatments (HT) were applied to three alloys Cu-8Ni-2Co-1.6Cr-2Si wt% (L1), Cu-8.5Ni-1.5Co-1.6Cr-2Si wt% (L2) and Cu-9Ni-1Co-1.6Cr-2Si-0.18Fe-0.3Zr wt% (L3), the properties obtained were compared with C17510 alloy. Specimens were characterized by different metallographic techniques; the microstructural characterization was made with scanning electron microscopy (SEM) and revealed regions of dendritic morphologies. The solidification sequence is primary Cu dendrites and some phases in the interdendritic regions. The solution heat treatment decreased (ST) the Hardness Rockwell B (HRB) and wear rate resistance, and there was an increase with the first aging heat treatment (HT1) for each alloy. The most outstanding combination of properties was found for Cu-8.5Ni-1.5Co-1.6Cr-2Si wt% alloy (L2C3) with 100 ± 1 HRB and specific wear rate resistance of 1.2 × 10−4 mm3/Nm, after the first aging heat treatment.


  • Open Access

    Influence of B and Nb Additions and Heat Treatments on the Mechanical Properties of Cu-Ni-Co-Cr-Si Alloy for High Pressure Die Casting Applications

    by Denis Ariel Avila-Salgado, Arturo Juárez-Hernández, Fermín Medina-Ortíz, María Lara Banda, Marco Antonio Loudovic Hernández-Rodríguez

    During the high pressure die casting process (HPDC), it is necessary to develop new designs and alloys for the copper plungers. In this research, two alloys Cu-9Ni-1Co-1.6Cr-2Si-1.3Fe-0.25B wt.% (A1) and Cu-9Ni-1Co-1.6Cr-2Si-0.1Fe-0.2Nb wt.% (A2) under different heat treatments (HT) were studied. Optical microscopy technique was applied to reveal the regions of dendritic morphology, also lower Secondary Dendrite Arm Spacing (SDAS); and different grain orientations. The results reveal that the solidification sequence is primary Cu dendrites and secondary intermetallics; heat treatments increase the redistribution of alloying elements in the interdendritic regions. During the heat treatments, some precipitates were found in the grain boundary after aging heat treatments for both alloys, which were determined by X-ray diffraction. Hardness test HRB presented a decrease with the solution heat treatment and an increase with the aging heat treatments proposed for both alloys. Finally, the wear resistances for both alloys were compared with a commercial alloy C17530, with decreased A1 with B additions having the best result in the as-cast condition 4.07 × 10−4 mm3/Nm, while for A2 with Nb additions wear resistance increased, with the best result in the one with aging heat treatment 1.69 × 10−4 mm3/Nm while for the C17530 alloy this was 2.74 × 10−4 mm3/Nm.