Can‐Pei Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Can‐Pei Liu has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
Gang Zhong
College of Chemistry and Materials Science, Fujian Key Laboratory of Polymer Science, Fujian Provincial Key Laboratory of Advanced Materials Oriented Chemical Engineering Fujian Normal University Fuzhou China
2 shared publicationsAlain Luigi Lanzon
College of Chemistry and Materials Science, Fujian Key Laboratory of Polymer Science, Fujian Provincial Key Laboratory of Advanced Materials Oriented Chemical Engineering Fujian Normal University Fuzhou China
1 shared publicationHua Gui Zhang
College of Chemistry and Materials Science, Fujian Key Laboratory of Polymer Science, Fujian Provincial Key Laboratory of Advanced Materials Oriented Chemical Engineering Fujian Normal University Fuzhou China
1 shared publicationHuagui Zhang
College of Chemistry and Materials Science, Fujian Key Laboratory of Polymer Science, Fujian Provincial Key Laboratory of Advanced Materials Oriented Chemical Engineering Fujian Normal University Fuzhou China
1 shared publicationJingwei Lin
Department of Thoracic Surgery First Affiliated Hospital of Fujian Medical University Fuzhou China
1 shared publicationJin‐Huo Lin
College of Chemistry and Materials, Fujian Normal University, 350007 Fuzhou, Fujian, China
1 shared publication
Latest Publications
- 24 April 2021
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 109 (11) , 1817-1835
Biological compatibility, thermal and in vitro simulated degradation for poly(p‐dioxanone)/poly(lactide‐co‐glycolide)/poly(ethylene succinate‐co‐glycolide)
Bio‐absorbable polymers are widely desired to be applied and used as biomaterials for surgery hemostatic and medical tissue engineering devices. Ring‐opening copolymerization reaction was applied to synthesize poly(ethylene succinate‐co‐glycolide) (PES‐b‐PGA). Stannous octoate was used as a catalyst whereas poly(ethylene succinate) was used as a macro‐initiator to react with glycolide. PES‐b‐PGA was then used as a compatibilizer to prepare the blend biomaterial of PPDO/PLGA/PES‐b‐PGA by melt blending poly(p‐dioxanone) (PPDO) with poly(lactide‐co‐glycolide) (PLGA). This would enhance the interactions of the inter‐molecular chains and intra‐molecular segments thus improving the compatibility. To obtain the biomaterial of PPDO/PLGA/PES‐b‐PGA with a regulated and controlled degradation and/or hydrolysis period, various ratios of PPDO, PLGA, and PES‐b‐PGA was blended. Behaviors of the thermal and in vitro simulated degradation, biological compatibility, cytotoxicity and subcutaneous implantation of PPDO/PLGA/PES‐b‐PGA were investigated. The results show that the in vitro hydrolytic degradation cycle is consistent with the wound healing time and that the biomaterial has slight cytotoxicity and it will do good to the cell proliferation, with 1 grade of cytotoxicity and the relative growth rate being the range from 92.5% to 96.2%. The implantation of the biomaterial into the rabbits' ears will not adversely affect the wound healing and the tissues surrounding the implanted sites. Therefore, the biomaterial has good biocompatibility and potential applications in medical tissue engineering devices.
- 24 April 2021
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 109 (11) , 1817-1835
Biological compatibility, thermal and in vitro simulated degradation for poly(p‐dioxanone)/poly(lactide‐co‐glycolide)/poly(ethylene succinate‐co‐glycolide)
Bio‐absorbable polymers are widely desired to be applied and used as biomaterials for surgery hemostatic and medical tissue engineering devices. Ring‐opening copolymerization reaction was applied to synthesize poly(ethylene succinate‐co‐glycolide) (PES‐b‐PGA). Stannous octoate was used as a catalyst whereas poly(ethylene succinate) was used as a macro‐initiator to react with glycolide. PES‐b‐PGA was then used as a compatibilizer to prepare the blend biomaterial of PPDO/PLGA/PES‐b‐PGA by melt blending poly(p‐dioxanone) (PPDO) with poly(lactide‐co‐glycolide) (PLGA). This would enhance the interactions of the inter‐molecular chains and intra‐molecular segments thus improving the compatibility. To obtain the biomaterial of PPDO/PLGA/PES‐b‐PGA with a regulated and controlled degradation and/or hydrolysis period, various ratios of PPDO, PLGA, and PES‐b‐PGA was blended. Behaviors of the thermal and in vitro simulated degradation, biological compatibility, cytotoxicity and subcutaneous implantation of PPDO/PLGA/PES‐b‐PGA were investigated. The results show that the in vitro hydrolytic degradation cycle is consistent with the wound healing time and that the biomaterial has slight cytotoxicity and it will do good to the cell proliferation, with 1 grade of cytotoxicity and the relative growth rate being the range from 92.5% to 96.2%. The implantation of the biomaterial into the rabbits' ears will not adversely affect the wound healing and the tissues surrounding the implanted sites. Therefore, the biomaterial has good biocompatibility and potential applications in medical tissue engineering devices.
- 2 October 2020
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 138 (9)
DOPO‐based curing flame retardant of epoxy composite material for char formation and intumescent flame retardance
Phosphorus‐containing flame retardant (HBAEA‐DOPO) for epoxy resin was synthesized by addition reaction of 9,10‐dihydro‐9‐oxa‐10‐phosphaphenanthrene‐10‐oxide (DOPO) with bis[2‐(4‐hydroxybenzylideneamino)ethyl]amine (HBAEA) that was synthesized via 4‐hydroxybenzaldehyde with diethylenetriamine. HBAEA‐DOPO was mixed with 4,4′‐diaminodiphenyl sulfone to co‐cure the epoxy resin of diglycidyl ether bisphenol A. The silane modified nano‐silica (nano‐SiO2) was used to reinforce the epoxy resin. Thermal stability and dynamic mechanical properties of the cured epoxy materials were studied with the use of thermogravimetric analysis and dynamic mechanical thermal analysis. Flame retardance and burning behavior were evaluated by the limiting oxygen index (LOI), vertical burning test, and the cone calorimetry. The cured epoxy materials have excellent thermal stability, and the temperatures at the maximum weight loss rate are over 384.0°C. The characteristic temperature corresponding to 5.00 wt% of thermal decomposition reaches 341.5°C as 1.00 wt% of phosphorus content is loaded. Flame retardant grade meets the V‐0 level. The fire residue mass gradually increases with HBAEA‐DOPO and nano‐SiO2. The characteristics of high flame retardance and smoke suppression of HBAEA‐DOPO and nano‐SiO2 on the cured epoxy composites have been demonstrated to be related to char formation and intumescent flame retardance in the condensed phase.
- 2 October 2020
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 138 (9)
DOPO‐based curing flame retardant of epoxy composite material for char formation and intumescent flame retardance
Phosphorus‐containing flame retardant (HBAEA‐DOPO) for epoxy resin was synthesized by addition reaction of 9,10‐dihydro‐9‐oxa‐10‐phosphaphenanthrene‐10‐oxide (DOPO) with bis[2‐(4‐hydroxybenzylideneamino)ethyl]amine (HBAEA) that was synthesized via 4‐hydroxybenzaldehyde with diethylenetriamine. HBAEA‐DOPO was mixed with 4,4′‐diaminodiphenyl sulfone to co‐cure the epoxy resin of diglycidyl ether bisphenol A. The silane modified nano‐silica (nano‐SiO2) was used to reinforce the epoxy resin. Thermal stability and dynamic mechanical properties of the cured epoxy materials were studied with the use of thermogravimetric analysis and dynamic mechanical thermal analysis. Flame retardance and burning behavior were evaluated by the limiting oxygen index (LOI), vertical burning test, and the cone calorimetry. The cured epoxy materials have excellent thermal stability, and the temperatures at the maximum weight loss rate are over 384.0°C. The characteristic temperature corresponding to 5.00 wt% of thermal decomposition reaches 341.5°C as 1.00 wt% of phosphorus content is loaded. Flame retardant grade meets the V‐0 level. The fire residue mass gradually increases with HBAEA‐DOPO and nano‐SiO2. The characteristics of high flame retardance and smoke suppression of HBAEA‐DOPO and nano‐SiO2 on the cured epoxy composites have been demonstrated to be related to char formation and intumescent flame retardance in the condensed phase.
- 1 March 2013
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 129 (6) , 3629-3639
Preparation, property characterization and UV‐converting application of poly(conjugated azomethine‐urethane)/hydroxyl polyacrylate resin
A functional polyurethane coating with ultraviolet (UV) rays converting ability of changing higher energy UV rays into lower ones was prepared from poly(conjugated azomethine‐urethane) (CAUP) reacting with hydroxyl polyacrylate resin (HPAR). As an oligomeric isocyanate, CAUP was prepared in a reaction of toluene‐2,4‐diisocyanate with N,N′‐bis(4‐hydroxyl‐3‐methoxybenzylidene)‐o, m or p‐diaminobenzene that was synthesized from vanillin and o‐phenylenediamine or m‐phenylenediamine or p‐phenylenediamine. Fourier transform infrared spectroscopy, 1H‐NMR, UV–vis, and fluorescence spectra were used to characterize those synthesized products and HPAR/CAUP films. UV‐converting abilities of HPAR/CAUP films had been demonstrated by natural exposure to ageing and the fluorescence emission spectra of HPAR/CAUP films and CAUP solutions. Red‐shift phenomena in the fluorescence emission spectra were due to molecule aggregations and stacks caused by intramolecular and intermolecular interactions such as hydrogen bonding effects. Dynamic mechanical thermal analysis and thermogravimetric analysis techniques were employed to study their mechanical and thermal properties of HPAR/CAUP films. The films exhibited excellent mechanical properties and owned high glass transition temperatures over 97.0°C, and their maximum thermal degradation temperatures were about 176.0°C. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013
- 1 March 2013
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 129 (6) , 3629-3639
Preparation, property characterization and UV‐converting application of poly(conjugated azomethine‐urethane)/hydroxyl polyacrylate resin
A functional polyurethane coating with ultraviolet (UV) rays converting ability of changing higher energy UV rays into lower ones was prepared from poly(conjugated azomethine‐urethane) (CAUP) reacting with hydroxyl polyacrylate resin (HPAR). As an oligomeric isocyanate, CAUP was prepared in a reaction of toluene‐2,4‐diisocyanate with N,N′‐bis(4‐hydroxyl‐3‐methoxybenzylidene)‐o, m or p‐diaminobenzene that was synthesized from vanillin and o‐phenylenediamine or m‐phenylenediamine or p‐phenylenediamine. Fourier transform infrared spectroscopy, 1H‐NMR, UV–vis, and fluorescence spectra were used to characterize those synthesized products and HPAR/CAUP films. UV‐converting abilities of HPAR/CAUP films had been demonstrated by natural exposure to ageing and the fluorescence emission spectra of HPAR/CAUP films and CAUP solutions. Red‐shift phenomena in the fluorescence emission spectra were due to molecule aggregations and stacks caused by intramolecular and intermolecular interactions such as hydrogen bonding effects. Dynamic mechanical thermal analysis and thermogravimetric analysis techniques were employed to study their mechanical and thermal properties of HPAR/CAUP films. The films exhibited excellent mechanical properties and owned high glass transition temperatures over 97.0°C, and their maximum thermal degradation temperatures were about 176.0°C. © 2013 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013
- 3 July 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 106 (2) , 897-908
Kinetic study on cross‐linking and blowing behavior of EVA/EPDM/CPE high elasticity material
Blend of ethylene‐vinyl acetate copolymer (EVA), ethylene‐propylene‐diene terpolymer rubber (EPDM), and chlorinated polyethylene (CPE) filled with talc was cross‐linked with dicumyl peroxide and blown simultaneously with azodicarbonamide for preparation of high elasticity material by injecting, cross‐linking, and blowing process. It had excellent mechanical properties and elasticity. It was found that mechanical properties were a function of cross‐linking and blowing temperature and time and formula. A good cross‐linking and blowing temperature was in the range of 440–450 K and the optimum temperature and time were 448 K and 360 s, respectively. Kinetics of both cross‐linking and blowing reactions were investigated by closed nonrotor torque rheometer. The results showed that both cross‐linking and blowing reactions were first order. The activation energy of the cross‐linking reaction was higher than that of the blowing reaction. With increasing of EDPM content, the activation energy of the cross‐linking reaction reduced whereas it increased for the blowing reaction. The gas cell morphology was characterized by scanning electron microscopy (SEM). The results of SEM and mechanical property analyses showed that the morphology and mechanical properties were improved by incorporating CPE. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2007
- 3 July 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 106 (2) , 897-908
Kinetic study on cross‐linking and blowing behavior of EVA/EPDM/CPE high elasticity material
Blend of ethylene‐vinyl acetate copolymer (EVA), ethylene‐propylene‐diene terpolymer rubber (EPDM), and chlorinated polyethylene (CPE) filled with talc was cross‐linked with dicumyl peroxide and blown simultaneously with azodicarbonamide for preparation of high elasticity material by injecting, cross‐linking, and blowing process. It had excellent mechanical properties and elasticity. It was found that mechanical properties were a function of cross‐linking and blowing temperature and time and formula. A good cross‐linking and blowing temperature was in the range of 440–450 K and the optimum temperature and time were 448 K and 360 s, respectively. Kinetics of both cross‐linking and blowing reactions were investigated by closed nonrotor torque rheometer. The results showed that both cross‐linking and blowing reactions were first order. The activation energy of the cross‐linking reaction was higher than that of the blowing reaction. With increasing of EDPM content, the activation energy of the cross‐linking reaction reduced whereas it increased for the blowing reaction. The gas cell morphology was characterized by scanning electron microscopy (SEM). The results of SEM and mechanical property analyses showed that the morphology and mechanical properties were improved by incorporating CPE. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2007
- 26 January 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 104 (2) , 1271-1278
Gloss and degradation of hydroxyl polyacrylic resin/hexamethylene‐1,6‐diisocyanate coatings under ultraviolet and natural‐exposure aging
Reactive coatings of hydroxyl polyacrylic resin (HPAR) with hexamethylene‐1,6‐diisocyanate were carried out under accelerated 313‐nm ultraviolet (UV) aging for 2000 h and under natural exposure in Lhasa, Tibet, for 24 months. With UV irradiation and exposure time, the gloss changes in coatings with HPAR containing 3.0% or less hydroxyl groups decreased exponentially, whereas the gloss decay of coatings with HPAR containing over 4.5% hydroxyl groups decreased linearly. During 254‐nm UV aging, the gloss changes in coatings with HPAR containing 1.4% or less hydroxyl groups decreased as a Gaussian function. The weather resistance of a coating was correlated to the HPAR, UV irradiation, temperature, and humidity. Scanning electron microscopy indicated that there were degradation reactions and that some substance was lost in the matrix polymer during accelerated UV aging; then, uneven surfaces appeared and caused decreased gloss. Accelerated UV aging was faster than natural‐exposure aging, and the aging velocity of 254‐nm UV was 3–5 times faster than that of 313‐nm UV. Through the changes in the gloss, the aging tolerance of a coating could be monitored, and its aging resistance could also be predicted. The dynamic mechanical thermal analysis results showed that the coatings had good properties. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 104: 1271–1278, 2007
- 26 January 2007
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 104 (2) , 1271-1278
Gloss and degradation of hydroxyl polyacrylic resin/hexamethylene‐1,6‐diisocyanate coatings under ultraviolet and natural‐exposure aging
Reactive coatings of hydroxyl polyacrylic resin (HPAR) with hexamethylene‐1,6‐diisocyanate were carried out under accelerated 313‐nm ultraviolet (UV) aging for 2000 h and under natural exposure in Lhasa, Tibet, for 24 months. With UV irradiation and exposure time, the gloss changes in coatings with HPAR containing 3.0% or less hydroxyl groups decreased exponentially, whereas the gloss decay of coatings with HPAR containing over 4.5% hydroxyl groups decreased linearly. During 254‐nm UV aging, the gloss changes in coatings with HPAR containing 1.4% or less hydroxyl groups decreased as a Gaussian function. The weather resistance of a coating was correlated to the HPAR, UV irradiation, temperature, and humidity. Scanning electron microscopy indicated that there were degradation reactions and that some substance was lost in the matrix polymer during accelerated UV aging; then, uneven surfaces appeared and caused decreased gloss. Accelerated UV aging was faster than natural‐exposure aging, and the aging velocity of 254‐nm UV was 3–5 times faster than that of 313‐nm UV. Through the changes in the gloss, the aging tolerance of a coating could be monitored, and its aging resistance could also be predicted. The dynamic mechanical thermal analysis results showed that the coatings had good properties. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 104: 1271–1278, 2007