Hong-Song Zhang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Hong-Song Zhang has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
Gang Li
Henan Institute of Engineering
2 shared publicationsKun Sun
Department of Physics and Electronics Chuxiong University Chuxiong 675000 China
2 shared publicationsLing Liu
School of Materials Science and Engineering Beijing Institute of Technology Beijing 100081 China
2 shared publicationsQiang Xu
School of Materials Science and Engineering Beijing Institute of Technology Beijing 100081 China
2 shared publicationsFu-Chi Wang
Beijing Institute of Technology
1 shared publicationFuchi Wang
School of Materials Science and Engineering Beijing Institute of Technology Beijing 100081 China
1 shared publication
Latest Publications
- Open Access
- 28 July 2016
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 5 (3) , 244-252
Ce1−x Sm x O2−x/2—A novel type of ceramic material for thermal barrier coatings
In this study, Ce1−x Sm x O2−x/2 ceramics were synthesized by sol–gel route and solid state sintering method. The phase structure was analyzed by X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, and Raman spectroscopy. The morphologies of the synthesized powders and the corresponding bulk samples were observed using scanning electron microscopy (SEM). Their thermal diffusivities and thermal expansion coefficients were measured by the laser-flash method and the pushing-rod method, respectively. Results show that pure Ce1−x Sm x O2−x/2 powders with single fluorite structure are synthesized successfully, and their microstructures of the corresponding bulk samples are very dense. With the increase of Sm2O3 content, their thermal expansion coefficients decrease due to the higher electro-negativity of Sm3+ ions as compared with that of Ce4+ ions. Their thermal conductivities at 1000 °C lie in the range of 1.62–2.02 W/(m·K) due to the phonon scattering caused by the substituted atoms and oxygen vacancies. The Ce1−x Sm x O2−x/2 ceramics can be used as ceramic candidates for novel thermal barrier coatings (TBCs).
- 28 July 2016
- Published by Tsinghua University Press in Journal of Advanced Ceramics
- Vol. 5 (3) , 244-252
Open AccessCe1−x Sm x O2−x/2—A novel type of ceramic material for thermal barrier coatings
In this study, Ce1−x Sm x O2−x/2 ceramics were synthesized by sol–gel route and solid state sintering method. The phase structure was analyzed by X-ray diffraction (XRD), Fourier transform infrared (FTIR) spectroscopy, and Raman spectroscopy. The morphologies of the synthesized powders and the corresponding bulk samples were observed using scanning electron microscopy (SEM). Their thermal diffusivities and thermal expansion coefficients were measured by the laser-flash method and the pushing-rod method, respectively. Results show that pure Ce1−x Sm x O2−x/2 powders with single fluorite structure are synthesized successfully, and their microstructures of the corresponding bulk samples are very dense. With the increase of Sm2O3 content, their thermal expansion coefficients decrease due to the higher electro-negativity of Sm3+ ions as compared with that of Ce4+ ions. Their thermal conductivities at 1000 °C lie in the range of 1.62–2.02 W/(m·K) due to the phonon scattering caused by the substituted atoms and oxygen vacancies. The Ce1−x Sm x O2−x/2 ceramics can be used as ceramic candidates for novel thermal barrier coatings (TBCs).
- Open Access
- 23 July 2015
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 24 (9) , 3394-3399
Thermal Conductivities and Thermal Expansion Coefficients of (Sm0.5Gd0.5)2(Ce1−x Zr x )2O7 Ceramics
- 23 July 2015
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 24 (9) , 3394-3399
Open AccessThermal Conductivities and Thermal Expansion Coefficients of (Sm0.5Gd0.5)2(Ce1−x Zr x )2O7 Ceramics
- 21 February 2013
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 11 (2) , 350-358
Preparation, Characterization, and Thermophysical Properties of (La 0.95 Sr 0.05 ) 2 Ce 2 O 6.95 Ceramic for Thermal Barrier Coatings
The La 2 Ce 2 O 7 powder doped with Sr was synthesized by sol‐gel method in this study and its dense bulk samples were also prepared by pressureless‐sintered at 1600°C for 10 h. Its phase composition, microstructure, and thermophysical property were investigated. Results reveal that pure (La 0.95 Sr 0.05 ) 2 Ce 2 O 6.95 with single fluorite structure was successfully synthesized. Microstructure of bulk sample is dense. Its thermal expansion coefficient is higher than that of Y 2 O 3 ‐stabilized ZrO 2 ( YSZ ) and its thermal conductivity is lower than that of YSZ . These results show that (La 0.95 Sr 0.05 ) 2 Ce 2 O 6.95 ceramic can be explored as the candidate material for thermal barrier coatings.
- 21 February 2013
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 11 (2) , 350-358
Preparation, Characterization, and Thermophysical Properties of (La 0.95 Sr 0.05 ) 2 Ce 2 O 6.95 Ceramic for Thermal Barrier Coatings
The La 2 Ce 2 O 7 powder doped with Sr was synthesized by sol‐gel method in this study and its dense bulk samples were also prepared by pressureless‐sintered at 1600°C for 10 h. Its phase composition, microstructure, and thermophysical property were investigated. Results reveal that pure (La 0.95 Sr 0.05 ) 2 Ce 2 O 6.95 with single fluorite structure was successfully synthesized. Microstructure of bulk sample is dense. Its thermal expansion coefficient is higher than that of Y 2 O 3 ‐stabilized ZrO 2 ( YSZ ) and its thermal conductivity is lower than that of YSZ . These results show that (La 0.95 Sr 0.05 ) 2 Ce 2 O 6.95 ceramic can be explored as the candidate material for thermal barrier coatings.
- 24 May 2009
- Published by Wiley in Rare Metals
- Vol. 28 (3) , 226-230
Thermophysical properties of Sm 2 (Zr 1− x Ce x ) 2 O 7 ceramics
Sm 2 (Zr 1− x Ce x ) 2 O 7 ( x = 0.1, 0.2, and 0.3) ceramics were prepared by solid reaction method at 1600°C for 10 h using Sm 2 O 3 , ZrO 2 , and CeO 2 as starting reactants. The phase compositions, microstructures, thermal expansion coefficients, and partial thermal conductivities of these materials were investigated. X‐ray diffraction (XRD) results reveal that Sm 2 (Zr 0.9 Ce 0.1 ) 2 O 7 with pyrochlore structure and Sm 2 (Zr 1− x Ce x ) 2 O 7 ( x = 0.2 and 0.3) with fluorite structure were synthesized, and scanning electrical microscopy (SEM) images show that the microstructures of these products are very dense. The linear thermal expansion coefficients increase with increasing temperature in the temperature range from ambient to 1200°C, and the thermal expansion coefficients increase with increasing content of doped CeO 2 . The thermal conductivities of Sm 2 (Zr 0.8 Ce 0.2 ) 2 O 7 and Sm 2 (Zr 0.7 Ce 0.3 ) 2 O 7 decrease gradually with an increase in temperature. These results show that the synthesized ceramic materials can be explored as novel prospective candidate materials for use in new thermal barrier coating systems in the future.
- 24 May 2009
- Published by Wiley in Rare Metals
- Vol. 28 (3) , 226-230
Thermophysical properties of Sm 2 (Zr 1− x Ce x ) 2 O 7 ceramics
Sm 2 (Zr 1− x Ce x ) 2 O 7 ( x = 0.1, 0.2, and 0.3) ceramics were prepared by solid reaction method at 1600°C for 10 h using Sm 2 O 3 , ZrO 2 , and CeO 2 as starting reactants. The phase compositions, microstructures, thermal expansion coefficients, and partial thermal conductivities of these materials were investigated. X‐ray diffraction (XRD) results reveal that Sm 2 (Zr 0.9 Ce 0.1 ) 2 O 7 with pyrochlore structure and Sm 2 (Zr 1− x Ce x ) 2 O 7 ( x = 0.2 and 0.3) with fluorite structure were synthesized, and scanning electrical microscopy (SEM) images show that the microstructures of these products are very dense. The linear thermal expansion coefficients increase with increasing temperature in the temperature range from ambient to 1200°C, and the thermal expansion coefficients increase with increasing content of doped CeO 2 . The thermal conductivities of Sm 2 (Zr 0.8 Ce 0.2 ) 2 O 7 and Sm 2 (Zr 0.7 Ce 0.3 ) 2 O 7 decrease gradually with an increase in temperature. These results show that the synthesized ceramic materials can be explored as novel prospective candidate materials for use in new thermal barrier coating systems in the future.
- 29 January 2009
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 18 (8) , 1140-1143
Preparation and Thermal Conductivity of Sm2(Zr0.6Ce0.4)2O7 Ceramic
- 29 January 2009
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 18 (8) , 1140-1143
Preparation and Thermal Conductivity of Sm2(Zr0.6Ce0.4)2O7 Ceramic