  • Effect of pH on the Optical, Structural, Morphological, and Photocatalytic Properties of CdS Thin Films Prepared by Chemical Bath Deposition

    by Sozan A. Haji, Raghad Y. Mohammed

    Cadmium sulfide (CdS) thin films were deposited by chemical bath deposition (CBD) using cadmium acetate as the cadmium source, thiourea as the sulfur source, ammonium acetate as a buffering agent, and ammonium hydroxide as a complexing agent and pH controller. The bath pH was adjusted to 7, 8, 9, and 10 using NH₄OH solution at 80°C for 30 min; no film formation occurred at pH 6, establishing pH 7–10 as the viable deposition window for this system. X‐ray diffraction (XRD) data revealed that the films at pH 7 and 10 are amorphous, whereas films at pH 8 and 9 exhibit mixed cubic zinc blende and hexagonal wurtzite crystal structures. The morphological analysis showed that the average particle sizes increased from 22.35 to 38.8 nm with increasing bath pH from 7 to 9, and decreased at pH 10 to 25.69. The optical bandgap decreased from 2.39 to 2.26 then to 2.18 eV for pH 7, 8, and 9, respectively, consistent with the increase in crystallite size and reduced quantum confinement, before reverting to 2.32 eV at pH 10, alongside a corresponding decrease in film thickness. Photocatalytic degradation of methyl orange (MO) dye under UV irradiation (254 nm, 25 W) demonstrated the highest mean efficiency of 25.31% ± 2.35% ( k = 0.0048 ± 0.0005 min −1 ) at pH 8, based on triplicate testing, attributed to its optimal crystallinity, surface morphology, and favorable bandgap of 2.26 eV. The pH 8 film also retained approximately 90.5% of its initial photocatalytic activity after three reuse cycles, confirming good stability. Unlike previous studies that examine these properties in isolation, this work provides an integrated structural, optical, morphological, compositional, and photocatalytic investigation of pH‐dependent CBD‐grown CdS thin films, further supported by reusability testing and triplicate reproducibility validation across four pH conditions.

  • Open Access

    Green synthesis of a manganese (oxyhydr) oxide nanocomposite, utilizing Eriobotrya japonica leaf extract for adsorbing methyl blue dye from water

    by Honar Salah Ahmed, Raghad Yousif Mohammed

    Green synthesis of manganese (oxyhydr) oxide nanocomposite using Eriobotrya japonica leaf extract shows high efficiency for methyl blue dye removal from aqueous solution via chemisorption-driven adsorption.


  • Eco‐Friendly Synthesis of CdO Photocatalyst: Tuning Structural, Morphological, and Optical Characteristics via Calcination Temperature

    by Salim A. Miraeez, Raghad Y. Mohammed

    The resistance of azo dyes to degradation in wastewater, together with the limitations of conventional treatment technologies and the limited availability of green‐synthesized cadmium oxide nanoparticles (CdO NPs) with tunable properties, represents a major environmental concern. To address these issues, CdO NPs were synthesized at various calcination temperatures (300°C–500°C) through a simple and cost‐effective method using Ficus carica leaf extract as a reducing, capping, and stabilizing agent. Structural analyses revealed a calcination‐induced phase transition from cadmium hydroxide (Cd(OH) 2 ) to crystalline CdO accompanied by a reduction in surface ‐OH groups, which can influence the surface properties and photocatalytic activity of the nanoparticles. The photocatalytic activity of CdO NPs, assessed via methyl orange degradation. The sample calcined at 500°C exhibited the highest efficiency, achieving 41% degradation in the absence of H 2 O 2 , which markedly increased to 95% upon H 2 O 2 addition. Furthermore, the reusability test over 5 cycles showed only a minimal decrease in photocatalytic activity, demonstrating the stability of the CdO NPs.

  • Open Access

    INVESTIGATION THE IMPACT OF DIFFERENT ANNEALING TEMPERATURES ON STRUCTURAL AND OPTICAL PROPERTIES OF BI-DOPED GETE (BI: 5 %) THIN FILMS FABRICATED BY PVD TECHNIQUE)

    by Shayma M. Ahmed, Azhen H. Jarjes, Ahmed F. Abdulrahman, Raghad Y. Mohammed

    The impact of different annealing temperatures on the Bi-doped GeTe thin films were investigated. The thin films have been prepared by using physical vapor deposition techniques (PVD). The Bismuth (Bi) is doped GeTe with ratio of 5%. Different characterizations techniques have been used to study the different properties of thin films with several annealing temperatures. It has been found that the film thickness decreases as the annealing temperature increases. The XRD patterns show that as-deposited and annealed Bi-doped GeTe films at 150°C,200°C, and 250°C were fully amorphous, while the film annealed at 100 °C was crystalline. FESEM image shows that the structure is amorphous with no grain appearing for the crystallite GeTe compound. Whereas the annealed thin films at 100°C are well-appeared crystallites of GeTe with an average size of (110.64 nm). The thin films are annealed at (150, 200, and 250)°C which reveals that the crystallite or grain is increased. An increase in the annealing temperature has been found to cause a significant shift in the absorption edge toward an extended wavelength and an overall reduction in transmittance. At a wavelength of 1100 nm, the transmittance dropped from 65.25% for as-deposited thin films to 32.57% for annealed thin films at 250 °C. Furthermore, when the annealing temperature rises from 100°C to 250°C, the optical band gap reduces from 0.95 eV to 0.42 eV.

  • Open Access

    Effect of Annealing Time on Structure, Morphology, and Optical Properties of Nanostructured CdO Thin Films Prepared by CBD Technique

    by Khalid Ridha Kadhim, Raghad Y. Mohammed

    Nanostructured cadmium oxide (CdO) thin films were deposited onto glass substrates using the chemical bath deposition (CBD) technique. Different deposition parameters such as deposition time, bath temperature, pH, and CdSO4 concentration have been considered to specify the optimum conditions to obtain uniform and well-adherent thin films. The thin films prepared under these optimum conditions were annealed for different times (20, 40, and 60 min) at 300 °C, where no previous studies had been done to study the effect of annealing time. The XRD analysis showed that the as-deposited film is Cd(OH)2 with a hexagonal phase. While all the annealed films are CdO with a cubic phase. The crystallite size increases with the annealing time. However, the strain, dislocation density, and the number of crystallites were found to be decreased with annealing time. SEM images of annealed films showed a spherical nanoparticle with an average of particle size 80–46 nm. EDX analysis revealed that the ratio of cadmium to oxygen increases with increasing the annealing time to 40 min. The optical characterization shows that the transmittance is in the range of 63–73% and the energy gap is in the range of 2.61–2.56 eV. It has been found that the transmittance increased and the energy gap decreased with the annealing time. The prepared CdO films can be used in photodegradation applications to remove pollutants from water.


  • Open Access

    The Effect of Deposition Parameters on Morphological and Optical Properties of Cu2S Thin Films Grown by Chemical Bath Deposition Technique

    by Honar S. Ahmed, Raghad Y. Mohammed

    The chemical bath deposition technique has been used for the deposition of Cu2S thin films on glass substrates. The thickness of deposited thin films strongly depends on the deposition parameters. The present study revealed that the thickness increased from 185 to 281 nm as deposition time increased and from 183 to 291 nm as bath temperature increased. In addition, the thickness increased from 257 to 303 nm with the increment of precursors concentration and from 185 to 297 nm as the pH value increased. However, the thickness decreased from 299 to 234 nm with the increment of precursors concentration. The morphology of Cu2S thin films remarkably changed as the deposition parameters varied. The increase in deposition time, bath temperature, and CuSO4.5H2O concentration leads to the increase in particle sizes, homogeneity, compactness of the thin films, and the number of clusters, and agglomeration, while the increase in thiourea concentration leads to the decrease in particle sizes and quality of films. Optical results demonstrated that the transmission of thin films rapidly increased in the UV–VIS region at (λ = 350–500 nm) until it reached its maximum peak at (λ = 600–650 nm) in the visible region, then it decreased in the NIR region. The high absorption was obtained in the UV–VIS region at (λ = 350–500 nm) before it decreased to its minimum value in the visible region, and then increased in the NIR region. The energy bandgap of thin films effectively depends on the deposition parameters. It decreased with the increasing deposition time (3.01–2.95 eV), bath temperature (3.04–2.63 eV), CuSO4.5H2O concentration (3.1–2.6 eV), and pH value (3.14–2.75 eV), except for thiourea concentration, while it decreased with the increasing thiourea concentration (2.79–3.09 eV).


  • Open Access

    Effects of Deposition Time And PH on The Characterization of Chemically Synthesized Composite Nano-Wires of Cu2S Thin Films

    by Honar S. Ahmed, Raghad Y. Mohammed, Mohammed Hussein Khalil

    The chemical bath deposition technique (CBD) had used for depositing Cu2S thin films on the glass substrates. It found that thickness and deposition rate were significantly dependent on deposition parameters (deposition time and pH value). XRD data indicates that at different deposition times and pH values are given amorphous structure except for the deposited thin film of (8hours) and, pH of (10.4) the structure was crystalline. The morphology of the deposited thin films remarkably changed as the deposition time increased. Optical transmittance measurements illustrate that transmission of the thin films decreases from 93.27% for a deposition time of 4 hours to 81.73 for deposition time of 10 hours and, the maximum transmission rate of the films is 95.21 % with pH=8.4 and decreases to 28.39 % with pH=11.4. Also, optical studies revealed that Cu2S thin film with direct energy bandgap decreased from 3.04 to 2.78 eV as deposition time increased and from 3.09 to 2.32 eV as pH increased.


  • Open Access

    Annealing Effect on the Structure and Optical Properties of CBD-ZnS Thin Films for Windscreen Coating

    by Raghad Y. Mohammed

    Zinc sulfide (ZnS) thin films were prepared and synthesized by the chemical bath deposition (CBD) technique on microscopic glass substrates using stoichiometric amounts of the precursor materials (ZnSO4·7H2O, NH4OH, and CS(NH2)2). Structural, morphological, compositional, and optical characterization of the films were studied. The obtained thin films were found to exhibit polycrystalline possessions. The effect of annealing temperature on the crystallographic structure and optical bandgap of ZnS thin films were both examined. The grain size and unit cell volume were both found to be increased. In addition, the strain, dislocation density, and the number of crystallites were found to be decreased with annealing temperature at 300 °C. However, the annealed sample was perceived to have more Zn content than S. The optical characterization reveals that the transmittance was around 76% of the as-deposited thin film and had been decreased to ~50% with the increasing of the annealing temperature. At the same time, the bandgap energy of the as-deposited film was 3.98 eV and was found to be decreased to 3.93 eV after annealing.