Rishi E. Kumar
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Rishi E. Kumar has a total of 31 co-authors. Here are the top co-authors by number of shared publications:
- David P. Fenning
Aiiso Yufeng Li Family Department of Chemical and Nano Engineering, University of California, San Diego, La Jolla, CA 92093, USA
6 shared publications - Mariana I. Bertoni
Ira A. Fulton School of Engineering, Arizona State University, Tempe, AZ, USA
5 shared publications Rico Meier
3 shared publications- Guillaume Von Gastrow
Department of NanoEngineering, University of California, San Diego, CA, USA
2 shared publications Hir Gandhi
2 shared publications- Ian M. Slauch
School of Electrical, Computer and Energy Engineering, Arizona State University,Tempe,AZ,USA,85287
2 shared publications
Latest Publications
- 23 February 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 13 (3) , 365-372
Moisture Ingress and Distribution in Bifacial Silicon Photovoltaics
Water participates in multiple modes of degradation in photovoltaic (PV) modules including encapsulant yellowing, delamination, and contact corrosion. To mitigate moisture-induced degradation, we must understand the kinetics of moisture in state-of-the-art encapsulants and module architectures. In this article, we present a robust optical method to quantify water content in the front and rear side encapsulants of bifacial silicon PV modules, then use such measurements to validate a model for simulating water concentration in these modules. First, we quantify the solubility of water in four modern encapsulants: ethylene vinyl acetate and polyolefin, each with and without UV-blocking additives. Second, we use water reflectometry detection to measure the diffusion of moisture within glass-backsheet modules as a function of time and environmental condition. Third, we present a model of moisture transport in bifacial silicon PV modules and show it to be consistent with our measurements. Crucially, our methodology enables the separate evaluation of water content in the front encapsulant and the rear polymers within glass-backsheet modules. Overall, our work presents a quantitative picture of moisture in emerging module architectures and a framework to extend this approach other encapsulants and module designs.
- 23 February 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 13 (3) , 365-372
Moisture Ingress and Distribution in Bifacial Silicon Photovoltaics
Water participates in multiple modes of degradation in photovoltaic (PV) modules including encapsulant yellowing, delamination, and contact corrosion. To mitigate moisture-induced degradation, we must understand the kinetics of moisture in state-of-the-art encapsulants and module architectures. In this article, we present a robust optical method to quantify water content in the front and rear side encapsulants of bifacial silicon PV modules, then use such measurements to validate a model for simulating water concentration in these modules. First, we quantify the solubility of water in four modern encapsulants: ethylene vinyl acetate and polyolefin, each with and without UV-blocking additives. Second, we use water reflectometry detection to measure the diffusion of moisture within glass-backsheet modules as a function of time and environmental condition. Third, we present a model of moisture transport in bifacial silicon PV modules and show it to be consistent with our measurements. Crucially, our methodology enables the separate evaluation of water content in the front encapsulant and the rear polymers within glass-backsheet modules. Overall, our work presents a quantitative picture of moisture in emerging module architectures and a framework to extend this approach other encapsulants and module designs.
- Open Access
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
In-Situ Determination of Moisture- and Temperature-Driven Deflection of an Encapsulated Si Photovoltaic Cell
Module reliability and service lifetime are critical factors in improving photovoltaic system performance and reducing the levelized cost of electricity (LCOE). Soldering and lamination of the cell impart residual stresses that persist over time and superimpose additional loads during operation. This paper demonstrates the use of X-ray Topography (XRT) to image in-situ the dynamic response of a glass/backsheet mini-module upon drying at elevated temperature after saturation at humidity levels used in accelerated testing. The local water content in the encapsulant is also determined in-situ over time via Water Reflectometric Detection (WaRD), with diffusion of water in the front (glass side) and rear (backsheet side) resolved. As water diffuses out from the back of the glass/backsheet module, the cell curves towards the backsheet concomitantly. The local cell deflections (changes in cell orientation) are correlated with the dynamic loss of water in the backside encapsulant. We conclude that the observed cell deflections are the result of hygroscopic stress induced by the encapsulant upon moisture outdiffusion. Therefore, the cell experiences a continually changing stress state and curvature dependent on local humidity and temperature. Depending on cell architecture and interconnection, this “breathing” mode of the cell may affect the disconnection of cracked pieces or cause wear out and fatigue of the interconnects, especially as elevated operating temperature allows a greater amount of water into the encapsulant.
- 1 January 2022
- Published by Elsevier in SSRN Electronic Journal
Open AccessIn-Situ Determination of Moisture- and Temperature-Driven Deflection of an Encapsulated Si Photovoltaic Cell
Module reliability and service lifetime are critical factors in improving photovoltaic system performance and reducing the levelized cost of electricity (LCOE). Soldering and lamination of the cell impart residual stresses that persist over time and superimpose additional loads during operation. This paper demonstrates the use of X-ray Topography (XRT) to image in-situ the dynamic response of a glass/backsheet mini-module upon drying at elevated temperature after saturation at humidity levels used in accelerated testing. The local water content in the encapsulant is also determined in-situ over time via Water Reflectometric Detection (WaRD), with diffusion of water in the front (glass side) and rear (backsheet side) resolved. As water diffuses out from the back of the glass/backsheet module, the cell curves towards the backsheet concomitantly. The local cell deflections (changes in cell orientation) are correlated with the dynamic loss of water in the backside encapsulant. We conclude that the observed cell deflections are the result of hygroscopic stress induced by the encapsulant upon moisture outdiffusion. Therefore, the cell experiences a continually changing stress state and curvature dependent on local humidity and temperature. Depending on cell architecture and interconnection, this “breathing” mode of the cell may affect the disconnection of cracked pieces or cause wear out and fatigue of the interconnects, especially as elevated operating temperature allows a greater amount of water into the encapsulant.
- 8 November 2021
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 12 (1) , 285-292
Glass vs. Backsheet: Deconvoluting the Role of Moisture in Power Loss in Silicon Photovoltaics With Correlated Imaging During Accelerated Testing
Moisture ingress is an established issue for photovoltaic module durability. Durability studies that probe moisture effects typically evaluate performance losses at the module level, attributing global power losses to the overall humidity condition of the test environment while leaving local module behavior unknown. We leverage our recently published water reflectometry detection method and biased photoluminescence imaging to spatially correlate moisture content and cell performance over 2500 h of damp heat testing. These tests, carried out on glass–glass and glass–backsheet mini-modules at multiple temperatures and humidities, reveal two dominant modes of local cell performance loss—acute finger interruptions and cell-wide “background” series resistance increase. Finger interruptions occur earliest in glass–glass modules and at dry conditions. We do not observe any signs of contact corrosion at the front side in either module types. Still, glass–backsheet modules show a unique increase in series resistance at high humidities, suggesting a mechanism at the back contact. Overall, our results point to the humidity level of installation climate as a driving variable in selection of the bottom module layer.
- 8 November 2021
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 12 (1) , 285-292
Glass vs. Backsheet: Deconvoluting the Role of Moisture in Power Loss in Silicon Photovoltaics With Correlated Imaging During Accelerated Testing
Moisture ingress is an established issue for photovoltaic module durability. Durability studies that probe moisture effects typically evaluate performance losses at the module level, attributing global power losses to the overall humidity condition of the test environment while leaving local module behavior unknown. We leverage our recently published water reflectometry detection method and biased photoluminescence imaging to spatially correlate moisture content and cell performance over 2500 h of damp heat testing. These tests, carried out on glass–glass and glass–backsheet mini-modules at multiple temperatures and humidities, reveal two dominant modes of local cell performance loss—acute finger interruptions and cell-wide “background” series resistance increase. Finger interruptions occur earliest in glass–glass modules and at dry conditions. We do not observe any signs of contact corrosion at the front side in either module types. Still, glass–backsheet modules show a unique increase in series resistance at high humidities, suggesting a mechanism at the back contact. Overall, our results point to the humidity level of installation climate as a driving variable in selection of the bottom module layer.
- 20 June 2021
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 2101-2103
The Role of Water on the Interfacial Adhesion in Si Solar Modules
Delamination of solar module interfaces often occurs in field-tested solar modules after decades of service due to environmental stressors such as humidity. As water diffuses into the module, failure mechanisms like corrosion and delamination are significantly affected. In the presence of water, the interfaces between EVA and the cell, glass, and backsheet all experience losses of adhesion exposing the module to accelerated degradation. Understanding the relation between interfacial adhesion and water content inside PV modules can help mitigate detrimental power losses. Water content measurements via short wave infrared reflectometry combined with 180° peel tests were used to study and quantify the effect of water ingress and egress on adhesion. Changes in adhesion strength for different module interfaces are quantified, correlating spatial distribution of water content to adhesion for damp heat and dry heat exposed samples. After 1000 hours of damp heat exposure, decreases in adhesion strength of approximately 1 N/mm were noted for all interfaces.
- 20 June 2021
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 2101-2103
The Role of Water on the Interfacial Adhesion in Si Solar Modules
Delamination of solar module interfaces often occurs in field-tested solar modules after decades of service due to environmental stressors such as humidity. As water diffuses into the module, failure mechanisms like corrosion and delamination are significantly affected. In the presence of water, the interfaces between EVA and the cell, glass, and backsheet all experience losses of adhesion exposing the module to accelerated degradation. Understanding the relation between interfacial adhesion and water content inside PV modules can help mitigate detrimental power losses. Water content measurements via short wave infrared reflectometry combined with 180° peel tests were used to study and quantify the effect of water ingress and egress on adhesion. Changes in adhesion strength for different module interfaces are quantified, correlating spatial distribution of water content to adhesion for damp heat and dry heat exposed samples. After 1000 hours of damp heat exposure, decreases in adhesion strength of approximately 1 N/mm were noted for all interfaces.
- 26 February 2021
- Published by Wiley in Advanced Optical Materials
- Vol. 9 (18) , 2002221
Europium Addition Reduces Local Structural Disorder and Enhances Photoluminescent Yield in Perovskite CsPbBr3
Correlative X‐ray microscopy, including synchrotron X‐ray diffraction and fluorescence, is leveraged to understand the local role of europium as a B‐site additive in CsPbBr3 perovskite crystals. Europium addition reduces microstrain in the perovskite, despite the fact that the degree of europium incorporation into the perovskite varies locally, with a maximum loading over twice the nominal stoichiometry. The presence of europium improves photoluminescence yield and bandwidth, while shifting the emission to bluer wavelengths. Finally, europium‐containing crystals have greatly improved X‐ray hardness. The findings show promise for europium as an additive in perovskite optoelectronic devices.
- 26 February 2021
- Published by Wiley in Advanced Optical Materials
- Vol. 9 (18) , 2002221
Europium Addition Reduces Local Structural Disorder and Enhances Photoluminescent Yield in Perovskite CsPbBr3
Correlative X‐ray microscopy, including synchrotron X‐ray diffraction and fluorescence, is leveraged to understand the local role of europium as a B‐site additive in CsPbBr3 perovskite crystals. Europium addition reduces microstrain in the perovskite, despite the fact that the degree of europium incorporation into the perovskite varies locally, with a maximum loading over twice the nominal stoichiometry. The presence of europium improves photoluminescence yield and bandwidth, while shifting the emission to bluer wavelengths. Finally, europium‐containing crystals have greatly improved X‐ray hardness. The findings show promise for europium as an additive in perovskite optoelectronic devices.
- 1 October 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 9 (6) , 1748-1753
Quantitative Determination of Moisture Content in Solar Modules by Short-Wave Infrared Reflectometry
A short-wave infrared (SWIR) reflectometry method is developed to quantify the water content in solar modules in a noncontact approach. Water content has been implicated as a key factor in many module degradation pathways, including contact corrosion and yellowing. Despite these established issues, to date no robust method for quantitative in situ determination of water content in standard modules is available. The water reflectometry detection (WaRD) method provides this capability by leveraging the SWIR optical spectrum, in which water exhibits vibrational absorption bands, module components are highly transparent, and solar cell back reflectors are reflective. Here, we describe the operating principle and demonstrate measurement of moisture in encapsulated aluminum back surface field and passivated-emitter rear contact architectures over the full range of temperatures and relative humidity relevant to field operation and damp heat testing.
- 1 October 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Journal of Photovoltaics
- Vol. 9 (6) , 1748-1753
Quantitative Determination of Moisture Content in Solar Modules by Short-Wave Infrared Reflectometry
A short-wave infrared (SWIR) reflectometry method is developed to quantify the water content in solar modules in a noncontact approach. Water content has been implicated as a key factor in many module degradation pathways, including contact corrosion and yellowing. Despite these established issues, to date no robust method for quantitative in situ determination of water content in standard modules is available. The water reflectometry detection (WaRD) method provides this capability by leveraging the SWIR optical spectrum, in which water exhibits vibrational absorption bands, module components are highly transparent, and solar cell back reflectors are reflective. Here, we describe the operating principle and demonstrate measurement of moisture in encapsulated aluminum back surface field and passivated-emitter rear contact architectures over the full range of temperatures and relative humidity relevant to field operation and damp heat testing.