Hiroyuki Suzuki
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Hiroyuki Suzuki has a total of 52 co-authors. Here are the top co-authors by number of shared publications:
Matahiro Komuro
Advanced Research Laboratory 1 , Hitachi Ltd., 7-1-1 Omika, Hitachi, Ibaraki 319-1292, Japan
5 shared publicationsYuichi Satsu
Advanced Research Laboratory 1 , Hitachi Ltd., 7-1-1 Omika, Hitachi, Ibaraki 319-1292, Japan
4 shared publicationsYorihiko Tsunoda
3 shared publicationsAkira Nambu
2 shared publicationsEiji Kita
Institute of Applied Physics, University of Tsukuba, Tsukuba, Ibaraki 305-8573
2 shared publicationsKay Kohn
Advanced Research Institute for Science and Engineering, Waseda University, Tokyo 169-8555
2 shared publications
Latest Publications
- Open Access
- 1 March 2020
- Published by AIP Publishing in AIP Advances
- Vol. 10 (3) , 035223
Crystal structures and electron-density distributions of Y(Fe, M)12 (M = Si, Ti, V, Cr, Mo, and W) determined by Rietveld and MEM analyses
The crystal structures of Y(Fe, M)12 (where M = Si, Ti, V, Cr, Mo, and W) were investigated by Rietveld analyses, and electron-density distributions were estimated by the maximum entropy method. There were no substituting elements to distort the lattice similarly. While the sites arranged selectively according to the element did not move necessarily, the distance between two atoms in the 8i site (an iron dumbbell) could change freely. Electron-density distributions revealed isolated iron dumbbells and a bonding network between Y, 8f, and 8j sites. Moreover, the connection in an iron dumbbell was much stronger than any other connection. As the substituting amount of the tungsten element increases, the electron density at interstitial positions increases. However, the high electron density disappears by over-substitution. It was suggested that the network of 22-hedrons, which configured the Y, 8f, and 8j sites, correlates with the thermal stability of the ThMn12 structure.
- 1 March 2020
- Published by AIP Publishing in AIP Advances
- Vol. 10 (3) , 035223
Open AccessCrystal structures and electron-density distributions of Y(Fe, M)12 (M = Si, Ti, V, Cr, Mo, and W) determined by Rietveld and MEM analyses
The crystal structures of Y(Fe, M)12 (where M = Si, Ti, V, Cr, Mo, and W) were investigated by Rietveld analyses, and electron-density distributions were estimated by the maximum entropy method. There were no substituting elements to distort the lattice similarly. While the sites arranged selectively according to the element did not move necessarily, the distance between two atoms in the 8i site (an iron dumbbell) could change freely. Electron-density distributions revealed isolated iron dumbbells and a bonding network between Y, 8f, and 8j sites. Moreover, the connection in an iron dumbbell was much stronger than any other connection. As the substituting amount of the tungsten element increases, the electron density at interstitial positions increases. However, the high electron density disappears by over-substitution. It was suggested that the network of 22-hedrons, which configured the Y, 8f, and 8j sites, correlates with the thermal stability of the ThMn12 structure.
- 30 January 2020
- Published by Elsevier in Intermetallics
- Vol. 119, 106713
Structural analysis and magnetic properties of lattice distortions from hexagonal to tetragonal systems in non-equilibrium Y–Fe alloys
- 30 January 2020
- Published by Elsevier in Intermetallics
- Vol. 119, 106713
Structural analysis and magnetic properties of lattice distortions from hexagonal to tetragonal systems in non-equilibrium Y–Fe alloys
- 30 October 2019
- Published by American Physical Society (APS) in Physical Review B
- Vol. 100 (14) , 144443
X-ray magnetic circular dichroism and neutron diffraction measurements of the magnetic moment of titanium inThe magnetic moment of titanium in was evaluated directly with x-ray magnetic circular dichroism, and magnitude of titanium's magnetic moment was identified with powder neutron Rietveld analysis. It was demonstrated experimentally that titanium in has a magnetic moment of about , and that magnetic moment of titanium couples antiferromagnetically to those of the host elements (iron and cobalt) at room temperature. From first-principles calculation, the magnitude of titanium's magnetic moment could be explained by Friedel's concept of the virtual bound state and reverse spin extended to the neighboring iron sites.- 30 October 2019
- Published by American Physical Society (APS) in Physical Review B
- Vol. 100 (14) , 144443
X-ray magnetic circular dichroism and neutron diffraction measurements of the magnetic moment of titanium inThe magnetic moment of titanium in was evaluated directly with x-ray magnetic circular dichroism, and magnitude of titanium's magnetic moment was identified with powder neutron Rietveld analysis. It was demonstrated experimentally that titanium in has a magnetic moment of about , and that magnetic moment of titanium couples antiferromagnetically to those of the host elements (iron and cobalt) at room temperature. From first-principles calculation, the magnitude of titanium's magnetic moment could be explained by Friedel's concept of the virtual bound state and reverse spin extended to the neighboring iron sites.- Open Access
- 9 January 2017
- Published by AIP Publishing in AIP Advances
- Vol. 7 (5)
Metastable phase YFe12 fabricated by rapid quenching method
A nonmagnetic Y element was selected to focus on an Fe lattice, and experiments to produce for high magnetization compounds by rapid quenching method were performed. The structure is mainly generated at a roll velocity of around 20 m/s, and the structure is mainly generated at a higher roll velocity. The structure can be changed to the structure by annealing, but at 1000°C, the convergent is decomposed into d- and -Fe. It was pointed out that has a small number of disordered parts of the Fe-dumbbell substituted into the Y site. It was clear that the magnetic moment of each site in are much larger than that of each site in . The magnetization of was estimated to be 1.66 T at liq. temperature. The Curie temperatures of the convergent structures have a maximum value of 212°C in the target composition range of .- 9 January 2017
- Published by AIP Publishing in AIP Advances
- Vol. 7 (5)
Open AccessMetastable phase YFe12 fabricated by rapid quenching method
A nonmagnetic Y element was selected to focus on an Fe lattice, and experiments to produce for high magnetization compounds by rapid quenching method were performed. The structure is mainly generated at a roll velocity of around 20 m/s, and the structure is mainly generated at a higher roll velocity. The structure can be changed to the structure by annealing, but at 1000°C, the convergent is decomposed into d- and -Fe. It was pointed out that has a small number of disordered parts of the Fe-dumbbell substituted into the Y site. It was clear that the magnetic moment of each site in are much larger than that of each site in . The magnetization of was estimated to be 1.66 T at liq. temperature. The Curie temperatures of the convergent structures have a maximum value of 212°C in the target composition range of . - 1 April 2011
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 109 (7) , 07A746
Magnetization reversal mechanism of a sintered Nd-Fe-B magnet with Dy segregation
The magnetization reversal mechanism of a sintered Nd-Fe-B magnet with Dy segregation near grain boundaries (GB) was studied using spin polarized scanning electron spectroscopy and magnetization measurements. More fine magnetic domains near GB were found in the magnet with Dy segregation than in the magnet without treatment. Magnetic modifications near the GB had no effect on the magnetization development. The domain wall motion of a quasihard magnetic component in the magnet with Dy segregation was suppressed in comparison with those in the magnet without treatment; this could also be confirmed in the different behaviors of asymmetry components toward a magnetic field direction between both magnets. From analyzing the probability of rotating magnetization near the GB, the magnetization reversal of the magnet with Dy segregation was more difficult to produce than those of the magnet without treatment.
- 1 April 2011
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 109 (7) , 07A746
Magnetization reversal mechanism of a sintered Nd-Fe-B magnet with Dy segregation
The magnetization reversal mechanism of a sintered Nd-Fe-B magnet with Dy segregation near grain boundaries (GB) was studied using spin polarized scanning electron spectroscopy and magnetization measurements. More fine magnetic domains near GB were found in the magnet with Dy segregation than in the magnet without treatment. Magnetic modifications near the GB had no effect on the magnetization development. The domain wall motion of a quasihard magnetic component in the magnet with Dy segregation was suppressed in comparison with those in the magnet without treatment; this could also be confirmed in the different behaviors of asymmetry components toward a magnetic field direction between both magnets. From analyzing the probability of rotating magnetization near the GB, the magnetization reversal of the magnet with Dy segregation was more difficult to produce than those of the magnet without treatment.
- 28 February 2011
- Published by Wiley
- p. 365-373
Development of High Coercivity Nd‐Fe‐B Permanent Magnets
- 28 February 2011
- Published by Wiley
- p. 365-373
Development of High Coercivity Nd‐Fe‐B Permanent Magnets
- 9 August 2010
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 46 (11) , 3831-3833
Increase of Coercivity and Composition Distribution in Fluoride-Diffused NdFeB Sintered Magnets Treated by Fluoride Solutions
Rare-earth and fluorine were diffused along grain boundaries in NdFeB sintered magnets during heat treatment after rare-earth fluoride liquid coating. In the case of Dy fluoride coating, the coercivity for NdFeB sintered magnets with a thickness of 1 mm after the diffusion was increased from 0.80 MA/m to 1.13 MA/m (41%) with remanence reduction of 0.6%. Segregations for Dy atoms near the grain boundaries and fluorine atoms at the grain boundary were found by TEM observations. The increase of coercivity per the weight of the rare-earth fluorides has a correlation with the anisotropy field of the RE2Fe14B (RE is rare-earth elements). Furthermore, the Dy quantity required for the observed increase of coercivity can be reduced to 1/3 compared to the previous NdFeB sintered magnets using the fluoride coating and diffusion process.
- 9 August 2010
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 46 (11) , 3831-3833
Increase of Coercivity and Composition Distribution in Fluoride-Diffused NdFeB Sintered Magnets Treated by Fluoride Solutions
Rare-earth and fluorine were diffused along grain boundaries in NdFeB sintered magnets during heat treatment after rare-earth fluoride liquid coating. In the case of Dy fluoride coating, the coercivity for NdFeB sintered magnets with a thickness of 1 mm after the diffusion was increased from 0.80 MA/m to 1.13 MA/m (41%) with remanence reduction of 0.6%. Segregations for Dy atoms near the grain boundaries and fluorine atoms at the grain boundary were found by TEM observations. The increase of coercivity per the weight of the rare-earth fluorides has a correlation with the anisotropy field of the RE2Fe14B (RE is rare-earth elements). Furthermore, the Dy quantity required for the observed increase of coercivity can be reduced to 1/3 compared to the previous NdFeB sintered magnets using the fluoride coating and diffusion process.
- 12 July 2010
- Published by AIP Publishing in Applied Physics Letters
- Vol. 97 (2) , 022510
Magnetic microstructures of neodymium in Nd2Fe14B permanent magnet by hard x-ray magnetic-circular dichroism using focused x-ray beam
Magnetic microstructures of neodymium (Nd) in a Nd–Fe–B magnet were investigated by the hard x-ray magnetic circular dichroism (HXMCD) with a focused synchrotron circular-polarized beam . Magnetic domain and Nd concentration were simultaneously acquired by measuring Nd HXMCD and intensity. The magnetic momentum of Nd was high for microdomains but was nearly zero at Nd-rich precipitates. This clearly indicates the magnetic momentum distributions are well correlated with the local concentration of Nd. Our experiments demonstrate the feasibility of studying magnetic microstructures by HXMCD mapping, which thus enables a discussion of the bulk magnetic behavior of Nd–Fe–B magnets.- 12 July 2010
- Published by AIP Publishing in Applied Physics Letters
- Vol. 97 (2) , 022510
Magnetic microstructures of neodymium in Nd2Fe14B permanent magnet by hard x-ray magnetic-circular dichroism using focused x-ray beam
Magnetic microstructures of neodymium (Nd) in a Nd–Fe–B magnet were investigated by the hard x-ray magnetic circular dichroism (HXMCD) with a focused synchrotron circular-polarized beam . Magnetic domain and Nd concentration were simultaneously acquired by measuring Nd HXMCD and intensity. The magnetic momentum of Nd was high for microdomains but was nearly zero at Nd-rich precipitates. This clearly indicates the magnetic momentum distributions are well correlated with the local concentration of Nd. Our experiments demonstrate the feasibility of studying magnetic microstructures by HXMCD mapping, which thus enables a discussion of the bulk magnetic behavior of Nd–Fe–B magnets.- 12 January 2010
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 638-642, 1357-1361
Microstructure and Magnetic Properties of NdFeB Magnets Using Fluorides Nano-Coated Process
Nd2Fe14B magnets could be sintered using terbium fluoride coated Nd2Fe14B powders. Fluorine atoms were segregated at the triple junctions and grain boundary after sintering and aging process. NdOF with fcc structure was grown at the triple junction. Terbium atoms were also distributed near grain boundaries by interdiffusion between the fluoride and Nd2Fe14B. No fluorine atoms were detected in Nd2Fe14B phase. The coercivity for 0.5wt% terbium fluoride coated magnet showed 1.23 MA/m which was 1.2 times higher than that for non-coated magnet with 1.04MA/m. The distribution of terbium and fluorine atoms increases the coercivity without reduction of remanence.
- 12 January 2010
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 638-642, 1357-1361
Microstructure and Magnetic Properties of NdFeB Magnets Using Fluorides Nano-Coated Process
Nd2Fe14B magnets could be sintered using terbium fluoride coated Nd2Fe14B powders. Fluorine atoms were segregated at the triple junctions and grain boundary after sintering and aging process. NdOF with fcc structure was grown at the triple junction. Terbium atoms were also distributed near grain boundaries by interdiffusion between the fluoride and Nd2Fe14B. No fluorine atoms were detected in Nd2Fe14B phase. The coercivity for 0.5wt% terbium fluoride coated magnet showed 1.23 MA/m which was 1.2 times higher than that for non-coated magnet with 1.04MA/m. The distribution of terbium and fluorine atoms increases the coercivity without reduction of remanence.
- 16 March 2009
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 105 (7) , 07A734
Magnetic properties of a Nd–Fe–B sintered magnet with Dy segregation
The magnetic properties and microstructures of a Nd–Fe–B sintered magnet with Dy segregation obtained by applying a fluoride-solution technique were studied using transmission electron microscopy and micromagnetic analysis. By applying fluorides in comparison with weight of the magnet and heating the magnet, coercivity increased by about 1.3 times from 1.1 to 1.4 T at 298 K while retaining remanence. Dy segregated within about 250 nm from the grain surfaces and coercivity was controlled by the area near the grain boundaries. Furthermore, we estimated that the range for reducing the magnetic anisotropy field near the grain boundaries was one or two unit cells by applying micromagnetic analysis to the magnet, which may indicate larger coercivity with less Dy.- 16 March 2009
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 105 (7) , 07A734
Magnetic properties of a Nd–Fe–B sintered magnet with Dy segregation
The magnetic properties and microstructures of a Nd–Fe–B sintered magnet with Dy segregation obtained by applying a fluoride-solution technique were studied using transmission electron microscopy and micromagnetic analysis. By applying fluorides in comparison with weight of the magnet and heating the magnet, coercivity increased by about 1.3 times from 1.1 to 1.4 T at 298 K while retaining remanence. Dy segregated within about 250 nm from the grain surfaces and coercivity was controlled by the area near the grain boundaries. Furthermore, we estimated that the range for reducing the magnetic anisotropy field near the grain boundaries was one or two unit cells by applying micromagnetic analysis to the magnet, which may indicate larger coercivity with less Dy.