Paolo Bruzzaniti
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Paolo Bruzzaniti has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Luigi Calabrese
Department of Engineering, University of Messina, Contrada di Dio, Sant’Agata, 98158 Messina, Italy
4 shared publications - Antonino Valenza
Department of Engineering, University of Palermo, Viale delle Scienze, Edificio 6, 90128 Palermo, Italy
2 shared publications - Tommasso Scalici
Department of “Ingegneria Civile, Ambientale, Aerospaziale, dei Materiali”, University of Palermo, Palermo, Italy
2 shared publications - Vincenzo Fiore
Department of Engineering University of Palermo Palermo Italy
2 shared publications - Andrea Frazzica
CNR ITAE “Nicola Giordano”—Institute of Advanced Technologies for Energy, Via Salita S. Lucia Sopra Contesse 5, 98126 Messina, Italy
1 shared publication - Angela Caprì
Department of Engineering, University of Messina, Contrada di Dio, 98166 Messina, Italy
1 shared publication
Latest Publications
- 5 December 2022
- Published by Springer Nature in JOM
- Vol. 75 (2) , 537-548
Flexural Toughening of a Cementitious Mortar Reinforced with Wave-Shaped Short Plastic Fibers
- 5 December 2022
- Published by Springer Nature in JOM
- Vol. 75 (2) , 537-548
Flexural Toughening of a Cementitious Mortar Reinforced with Wave-Shaped Short Plastic Fibers
- Open Access
- 8 January 2020
- Published by MDPI AG in Applied Sciences
- Vol. 10 (2) , 453
Morphological and Structural Evaluation of Hydration/Dehydration Stages of MgSO4 Filled Composite Silicone Foam for Thermal Energy Storage Applications
Salt hydrates, such as MgSO4∙7H2O, are considered attractive materials for thermal energy storage, thanks to their high theoretical storage density. However, pure salt hydrates present some challenges in real application due to agglomeration, corrosion and swelling problems during hydration/dehydration cycles. In order to overcome these limitations, a composite material based on silicone vapor-permeable foam filled with the salt hydrate is here presented. For its characterization, a real-time in situ environmental scanning electron microscopy (ESEM) investigation was carried out in controlled temperature and humidity conditions. The specific set-up was proposed as an innovative method in order to evaluate the morphological evolution of the composite material during the hydrating and dehydrating stages of the salt. The results evidenced an effective micro-thermal stability of the material. Furthermore, dehydration thermogravimetric/differential scanning calorimetric (TG/DSC) analysis confirmed the improved reactivity of the realized composite foam compared to pure MgSO4∙7H2O.
- 8 January 2020
- Published by MDPI AG in Applied Sciences
- Vol. 10 (2) , 453
Open AccessMorphological and Structural Evaluation of Hydration/Dehydration Stages of MgSO4 Filled Composite Silicone Foam for Thermal Energy Storage Applications
Salt hydrates, such as MgSO4∙7H2O, are considered attractive materials for thermal energy storage, thanks to their high theoretical storage density. However, pure salt hydrates present some challenges in real application due to agglomeration, corrosion and swelling problems during hydration/dehydration cycles. In order to overcome these limitations, a composite material based on silicone vapor-permeable foam filled with the salt hydrate is here presented. For its characterization, a real-time in situ environmental scanning electron microscopy (ESEM) investigation was carried out in controlled temperature and humidity conditions. The specific set-up was proposed as an innovative method in order to evaluate the morphological evolution of the composite material during the hydrating and dehydrating stages of the salt. The results evidenced an effective micro-thermal stability of the material. Furthermore, dehydration thermogravimetric/differential scanning calorimetric (TG/DSC) analysis confirmed the improved reactivity of the realized composite foam compared to pure MgSO4∙7H2O.
- Open Access
Pinned Hybrid Glass-Flax Composite Laminates Aged in Salt-Fog Environment: Mechanical Durability
The aim of the present paper is to study the mechanical performance evolution of pinned hybrid glass-flax composite laminates under environment aging conditions. Hybrid glass-flax fibers/epoxy pinned laminates were exposed to salt-spray fog environmental conditions up to 60 days. With the purpose of assessing the relationship between mechanical performances and failure mechanisms at increasing aging time, single lap joints at varying joint geometry (i.e., hole diameter D and hole distance E from free edge) were characterized after 0 days (i.e., unaged samples), 30 days, and 60 days of salt-fog exposition. Based on this approach, the property–structure relationship of the composite laminates was assessed on these critical environmental conditions. In particular, a reduction of failure strength for long-aging-time-aged samples was observed in the range 20–30% compared to unaged one. Due to the natural fiber degradation in a salt-fog environment, premature catastrophic fractures mode due to shear-out and net-tension were found, related to reduced joint fracture strength. This behavior identifies that this type of joint requires a careful design in order to guarantee an effective mechanical stability of the composite hybrid joint under long-term operating conditions in an aggressive environment.
Open AccessPinned Hybrid Glass-Flax Composite Laminates Aged in Salt-Fog Environment: Mechanical Durability
The aim of the present paper is to study the mechanical performance evolution of pinned hybrid glass-flax composite laminates under environment aging conditions. Hybrid glass-flax fibers/epoxy pinned laminates were exposed to salt-spray fog environmental conditions up to 60 days. With the purpose of assessing the relationship between mechanical performances and failure mechanisms at increasing aging time, single lap joints at varying joint geometry (i.e., hole diameter D and hole distance E from free edge) were characterized after 0 days (i.e., unaged samples), 30 days, and 60 days of salt-fog exposition. Based on this approach, the property–structure relationship of the composite laminates was assessed on these critical environmental conditions. In particular, a reduction of failure strength for long-aging-time-aged samples was observed in the range 20–30% compared to unaged one. Due to the natural fiber degradation in a salt-fog environment, premature catastrophic fractures mode due to shear-out and net-tension were found, related to reduced joint fracture strength. This behavior identifies that this type of joint requires a careful design in order to guarantee an effective mechanical stability of the composite hybrid joint under long-term operating conditions in an aggressive environment.
- Open Access
An Aging Evaluation of the Bearing Performances of Glass Fiber Composite Laminate in Salt Spray Fog Environment
The aim of the present paper is to assess the bearing performance evolution of pinned, glass-composite laminates due to environmental aging in salt-spray fog tests. Glass fibers/epoxy pinned laminates were exposed for up to 60 days in salt-spraying, foggy environmental conditions (according to ASTM B117 standard). In order to evaluate the relationship between mechanical failure mode and joint stability over increasing aging time, different single lap joints, measured by the changing hole diameter (D), laminate width (W) and hole free edge distance (E), were characterized at varying aging steps. Based on this approach, the property-structure relationship of glass-fibers/epoxy laminates was assessed under these critical environmental conditions. Furthermore, an experimental 2D failure map, clustering main failure modes in the plane E/D versus W/D ratios, was generated, and its cluster variation was analyzed at each degree of aging.
Open AccessAn Aging Evaluation of the Bearing Performances of Glass Fiber Composite Laminate in Salt Spray Fog Environment
The aim of the present paper is to assess the bearing performance evolution of pinned, glass-composite laminates due to environmental aging in salt-spray fog tests. Glass fibers/epoxy pinned laminates were exposed for up to 60 days in salt-spraying, foggy environmental conditions (according to ASTM B117 standard). In order to evaluate the relationship between mechanical failure mode and joint stability over increasing aging time, different single lap joints, measured by the changing hole diameter (D), laminate width (W) and hole free edge distance (E), were characterized at varying aging steps. Based on this approach, the property-structure relationship of glass-fibers/epoxy laminates was assessed under these critical environmental conditions. Furthermore, an experimental 2D failure map, clustering main failure modes in the plane E/D versus W/D ratios, was generated, and its cluster variation was analyzed at each degree of aging.