Thulasinath Raman Venkatesan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Thulasinath Raman Venkatesan has a total of 32 co-authors. Here are the top co-authors by number of shared publications:
- Dorina Maria Opris
Laboratory for Functional Polymers, Swiss Federal Laboratories for Materials Science and Technology Empa, Ueberlandstr. 129, CH-8600 Dübendorf, Switzerland
9 shared publications - Frank Nüesch
Laboratory for Functional Polymers, Swiss Federal Laboratories for Materials Science and Technology Empa, Ueberlandstr. 129, CH-8600 Dübendorf, Switzerland
6 shared publications Reimund Gerhard
Institute of Physics and Astronomy, University of Potsdam, Karl-Liebknecht-Strasse 24-25, 14476 Potsdam, Germany
5 shared publications- Reimund Gerhard
Institute of Physics and Astronomy Faculty of Science University of Potsdam 14476 Potsdam‐Golm Germany
4 shared publications Cansu Zeytun Karaman
Functional Polymers, Empa, Swiss Federal Laboratories for Materials Science and Technology (EMPA), 8600 Duebendorf, Switzerland
3 shared publicationsJohannes von Szczepanski
Functional Polymers, Empa, Swiss Federal Laboratories for Materials Science and Technology (EMPA), 8600 Duebendorf, Switzerland
3 shared publications
Latest Publications
- Open Access
- 18 September 2026
- Published by Wiley in Advanced Energy and Sustainability Research
- Vol. 7 (9) , e70271
Modulation of Thermal and Dielectric Properties in Poly(acrylonitrile‐ co ‐vinyl ether)s via Alkyl Side‐Chain Length Variation
The chemical structure of a polymer matrix fundamentally governs its macroscopic thermal, mechanical, and dielectric performance. High dielectric permittivity () polymers are essential for transducers, and introducing strongly polar nitrile groups effectively elevates . However, standard nitrile polymers face key trade‐offs: polyacrylonitrile features a high glass transition temperature () that inhibits dipolar polarization at room temperature (RT), while copolymerizing acrylonitrile (AN) with butadiene yields materials prone to aging. Copolymerizing AN with vinyl ethers (VE) offers a promising solution, yet the influence of lateral alkyl substituents on these systems has not been systematically studied. Herein, we synthesized a series of poly(AN‐ co ‐VE) copolymers with varying alkyl side‐chain lengths and, by systematically tuning the VE side‐chain length, macrostructural behavior was tailored from rigid plastics to soft elastomers. The resulting copolymers exhibited values spanning 5–45 °C and RT values between 3.7 and 13.7 (at 1 Hz). Blending with lithium bis(trifluoromethanesulfonyl)imide yielded an ionic conductivity of 4.4 × 10 − 7 S/cm at 60 °C. Furthermore, a representative crosslinked formulation demonstrated a high dielectric breakdown strength exceeding 100 V/μm, tensile strains up to 200%, and shape‐memory behavior.
- 18 September 2026
- Published by Wiley in Advanced Energy and Sustainability Research
- Vol. 7 (9) , e70271
Open AccessModulation of Thermal and Dielectric Properties in Poly(acrylonitrile‐ co ‐vinyl ether)s via Alkyl Side‐Chain Length Variation
The chemical structure of a polymer matrix fundamentally governs its macroscopic thermal, mechanical, and dielectric performance. High dielectric permittivity () polymers are essential for transducers, and introducing strongly polar nitrile groups effectively elevates . However, standard nitrile polymers face key trade‐offs: polyacrylonitrile features a high glass transition temperature () that inhibits dipolar polarization at room temperature (RT), while copolymerizing acrylonitrile (AN) with butadiene yields materials prone to aging. Copolymerizing AN with vinyl ethers (VE) offers a promising solution, yet the influence of lateral alkyl substituents on these systems has not been systematically studied. Herein, we synthesized a series of poly(AN‐ co ‐VE) copolymers with varying alkyl side‐chain lengths and, by systematically tuning the VE side‐chain length, macrostructural behavior was tailored from rigid plastics to soft elastomers. The resulting copolymers exhibited values spanning 5–45 °C and RT values between 3.7 and 13.7 (at 1 Hz). Blending with lithium bis(trifluoromethanesulfonyl)imide yielded an ionic conductivity of 4.4 × 10 − 7 S/cm at 60 °C. Furthermore, a representative crosslinked formulation demonstrated a high dielectric breakdown strength exceeding 100 V/μm, tensile strains up to 200%, and shape‐memory behavior.
- Open Access
- 4 May 2026
- Published by Royal Society of Chemistry (RSC) in Materials Horizons
- Vol. 13 (13) , 6553-6568
Synthesis and pyroelectric response of disperse red 1 functionalized silicones: cyclic monomer, homopolymer, and block copolymer derivatives
Pyroelectric materials enable the direct conversion of thermal fluctuations into electrical energy, offering a promising approach to waste heat recovery. While pyroelectric polymers are highly valued for their scalable synthesis, mechanical flexibility, and tunable properties, the field is currently dominated by poly(vinylidene fluoride) (PVDF)-based materials, which present environmental and processing challenges. To develop fluorine-free alternatives and elucidate the influence of molecular architecture on thermal-to-electrical conversion, we synthesized a series of siloxane-based materials functionalized with Disperse Red 1 (DR1) moieties, including a cyclic siloxane monomer, a homopolysiloxane, and a block copolysiloxane. Differential scanning calorimetry confirms the semicrystalline nature of these siloxanes, with glass transitions (Tg) near room temperature and melting temperatures of about 80 °C. Notably, even unpoled samples exhibit a measurable pyroelectric response at elevated temperatures. The pyroelectric response at low temperatures is significantly enhanced by poling the crystalline domains in an electric field above the melting transitions (Tm). Among the synthesized materials, the homopolymer exhibited the highest pyroelectric response (0.66 µC m−2 K−1 at 60 °C). While this value is significantly lower than the typical values for PVDF (>20 µC m−2 K−1), it should be noted that the processing and poling steps differ substantially. Under similar conditions, the PVDF value was only twice that of the homopolymer. Even more interesting, in an unpoled sample, the homopolymer shows a response similar to that of the poled sample, while PVDF shows almost no response. The superior response for the unpoled sample is attributed to the synergistic effects of DR1 self-ordering and secondary pyroelectricity—the strain-induced changes in dipole density resulting from thermal expansion. These findings provide a framework for designing high-performance, silicone-based pyroelectric transducers through precise structural control.
- 4 May 2026
- Published by Royal Society of Chemistry (RSC) in Materials Horizons
- Vol. 13 (13) , 6553-6568
Open AccessSynthesis and pyroelectric response of disperse red 1 functionalized silicones: cyclic monomer, homopolymer, and block copolymer derivatives
Pyroelectric materials enable the direct conversion of thermal fluctuations into electrical energy, offering a promising approach to waste heat recovery. While pyroelectric polymers are highly valued for their scalable synthesis, mechanical flexibility, and tunable properties, the field is currently dominated by poly(vinylidene fluoride) (PVDF)-based materials, which present environmental and processing challenges. To develop fluorine-free alternatives and elucidate the influence of molecular architecture on thermal-to-electrical conversion, we synthesized a series of siloxane-based materials functionalized with Disperse Red 1 (DR1) moieties, including a cyclic siloxane monomer, a homopolysiloxane, and a block copolysiloxane. Differential scanning calorimetry confirms the semicrystalline nature of these siloxanes, with glass transitions (Tg) near room temperature and melting temperatures of about 80 °C. Notably, even unpoled samples exhibit a measurable pyroelectric response at elevated temperatures. The pyroelectric response at low temperatures is significantly enhanced by poling the crystalline domains in an electric field above the melting transitions (Tm). Among the synthesized materials, the homopolymer exhibited the highest pyroelectric response (0.66 µC m−2 K−1 at 60 °C). While this value is significantly lower than the typical values for PVDF (>20 µC m−2 K−1), it should be noted that the processing and poling steps differ substantially. Under similar conditions, the PVDF value was only twice that of the homopolymer. Even more interesting, in an unpoled sample, the homopolymer shows a response similar to that of the poled sample, while PVDF shows almost no response. The superior response for the unpoled sample is attributed to the synergistic effects of DR1 self-ordering and secondary pyroelectricity—the strain-induced changes in dipole density resulting from thermal expansion. These findings provide a framework for designing high-performance, silicone-based pyroelectric transducers through precise structural control.
- Open Access
- 1 April 2026
- Published by Royal Society of Chemistry (RSC) in Materials Horizons
- Vol. 13 (11) , 5502-5514
Electrically responsive multilayer soft actuators using a solvent-free high dielectric permittivity polysiloxane ink
Multilayer soft dielectric elastomer actuators (DEAs) consist of stacked elastic capacitors that convert electrical energy into mechanical work.
- 1 April 2026
- Published by Royal Society of Chemistry (RSC) in Materials Horizons
- Vol. 13 (11) , 5502-5514
Open AccessElectrically responsive multilayer soft actuators using a solvent-free high dielectric permittivity polysiloxane ink
Multilayer soft dielectric elastomer actuators (DEAs) consist of stacked elastic capacitors that convert electrical energy into mechanical work.
- Open Access
- 20 June 2025
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry C
- Vol. 13 (31) , 15886-15896
High dielectric permittivity sulfonyl-modified polysiloxanes as a dielectric for soft actuators
High-permittivity elastomers were made by grafting sulfolane groups onto polysiloxane. Tuned polarity, thin films, and UV cross-linking yielded DEAs with 7.2% lateral strain at 14 V μm−1, enabling reliable low-voltage soft stack actuators.
- 20 June 2025
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry C
- Vol. 13 (31) , 15886-15896
Open AccessHigh dielectric permittivity sulfonyl-modified polysiloxanes as a dielectric for soft actuators
High-permittivity elastomers were made by grafting sulfolane groups onto polysiloxane. Tuned polarity, thin films, and UV cross-linking yielded DEAs with 7.2% lateral strain at 14 V μm−1, enabling reliable low-voltage soft stack actuators.
- Open Access
- 17 June 2025
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 17 (26) , 38504-38514
Single-Layer and Stack Dielectric Elastomer Actuators Using Polysiloxanes Modified with Ethylsulfonyl Groups
Dielectric elastomer actuators (DEAs) are soft transducers well-suited to precise motion applications in robotics and prosthetics. However, low dielectric permittivity or very soft elastomers result in a high operating voltage or low force output. These issues can be mitigated using high dielectric permittivity elastomers in a stack actuator. To optimize electromechanical performance, we synthesized high-permittivity polysiloxanes with varying ratios of ethyl sulfonyl thioether and butane thioether groups. The best material exhibited a dielectric permittivity of 16.2 at 10 kHz and 25 °C, a low conductivity of 1.8 × 10-10 S cm-1, and a large lateral actuation strain of 13% at a low electric field of 8.2 V μm-1 (1 Hz, 900 V), whereas state-of-the-art nitrile- and methyl sulfonyl-functionalized polysiloxane required electric fields exceeding 20 V μm-1 for the same actuation. A stack of five single-layer actuators using this material as the dielectric exhibited a thickness strain of 4.5% at a low electric field of 14.5 V μm-1 (1 Hz, 1600 V). The stack actuator showed stable performance at 1200 V over various frequencies, including 5 and 10 Hz, and maintained a reversible actuation over 4000 cycles at 1 Hz.
- 17 June 2025
- Published by American Chemical Society (ACS) in ACS Applied Materials & Interfaces
- Vol. 17 (26) , 38504-38514
Open AccessSingle-Layer and Stack Dielectric Elastomer Actuators Using Polysiloxanes Modified with Ethylsulfonyl Groups
Dielectric elastomer actuators (DEAs) are soft transducers well-suited to precise motion applications in robotics and prosthetics. However, low dielectric permittivity or very soft elastomers result in a high operating voltage or low force output. These issues can be mitigated using high dielectric permittivity elastomers in a stack actuator. To optimize electromechanical performance, we synthesized high-permittivity polysiloxanes with varying ratios of ethyl sulfonyl thioether and butane thioether groups. The best material exhibited a dielectric permittivity of 16.2 at 10 kHz and 25 °C, a low conductivity of 1.8 × 10-10 S cm-1, and a large lateral actuation strain of 13% at a low electric field of 8.2 V μm-1 (1 Hz, 900 V), whereas state-of-the-art nitrile- and methyl sulfonyl-functionalized polysiloxane required electric fields exceeding 20 V μm-1 for the same actuation. A stack of five single-layer actuators using this material as the dielectric exhibited a thickness strain of 4.5% at a low electric field of 14.5 V μm-1 (1 Hz, 1600 V). The stack actuator showed stable performance at 1200 V over various frequencies, including 5 and 10 Hz, and maintained a reversible actuation over 4000 cycles at 1 Hz.
- Open Access
- 21 April 2025
- Published by Royal Society of Chemistry (RSC) in Materials Horizons
- Vol. 12 (14) , 5287-5301
Pushing the boundaries of dielectric permittivity in polysiloxanes: polar dipole modifications enable amorphous pyroelectric polymers
A polysiloxane containing nitroaniline has a permittivity of 35 at 40 °C. Its TiO 2 composite has two T g s for the polymer in bulk and interface. Poling of this composite leads to a material with a pyroelectric coefficient of 3.4 μC m −2 K −1 at 30 °C.
- 21 April 2025
- Published by Royal Society of Chemistry (RSC) in Materials Horizons
- Vol. 12 (14) , 5287-5301
Open AccessPushing the boundaries of dielectric permittivity in polysiloxanes: polar dipole modifications enable amorphous pyroelectric polymers
A polysiloxane containing nitroaniline has a permittivity of 35 at 40 °C. Its TiO 2 composite has two T g s for the polymer in bulk and interface. Poling of this composite leads to a material with a pyroelectric coefficient of 3.4 μC m −2 K −1 at 30 °C.
- Open Access
- 10 December 2024
- Published by Elsevier in Composites Part B: Engineering
- Vol. 293
Ferroelectric elastomers of functionalized polar fillers in polydimethylsiloxane with improved dielectric and ferroelectric properties
- 10 December 2024
- Published by Elsevier in Composites Part B: Engineering
- Vol. 293
Open AccessFerroelectric elastomers of functionalized polar fillers in polydimethylsiloxane with improved dielectric and ferroelectric properties
- Open Access
- 27 November 2024
- Published by Royal Society of Chemistry (RSC) in Polymer Chemistry
- Vol. 16 (2) , 204-216
Spiropyran-based supramolecular elastomers with tuneable mechanical properties and switchable dielectric permittivity
Functionalization of poly(dimethylsiloxane- co -3-aminopropylmethylsiloxane) with an epoxy-modified spiropyran using a ZnCl 2 catalyst yields materials with tunable solubility, mechanical and thermal properties, and switchable dielectric permittivity.
- 27 November 2024
- Published by Royal Society of Chemistry (RSC) in Polymer Chemistry
- Vol. 16 (2) , 204-216
Open AccessSpiropyran-based supramolecular elastomers with tuneable mechanical properties and switchable dielectric permittivity
Functionalization of poly(dimethylsiloxane- co -3-aminopropylmethylsiloxane) with an epoxy-modified spiropyran using a ZnCl 2 catalyst yields materials with tunable solubility, mechanical and thermal properties, and switchable dielectric permittivity.
- Open Access
- 11 July 2024
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry C
- Vol. 12 (33) , 12825-12834
A polyphosphazene elastomer containing 2,2,2-trifluoroethoxy groups as a dielectric in electrically responsive soft actuators
Dielectric elastomer actuators based on polyphosphazenes modified with trifluoroethoxy groups exhibit a dielectric permittivity two times higher than polydimethylsiloxanes (PDMS), excellent elasticity, and a high dielectric breakdown field.
- 11 July 2024
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry C
- Vol. 12 (33) , 12825-12834
Open AccessA polyphosphazene elastomer containing 2,2,2-trifluoroethoxy groups as a dielectric in electrically responsive soft actuators
Dielectric elastomer actuators based on polyphosphazenes modified with trifluoroethoxy groups exhibit a dielectric permittivity two times higher than polydimethylsiloxanes (PDMS), excellent elasticity, and a high dielectric breakdown field.
- Open Access
- 16 May 2024
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry C
- Vol. 12 (23) , 8408-8417
Pyroelectricity in poled all-organic polar polynorbornene/polydimethylsiloxane-based stretchable electrets
Pyroelectricity in a recently developed all-organic composite electret with a polar polynorbornene-based filler and polydimethylsiloxane (PDMS) matrix has been studied with the help of thermal and dielectric techniques. Measurement of the pyroelectric p coefficient using a quasi-static periodic temperature variation at RT shows a non-linear dependence with the applied poling field, which is uncharacteristic of amorphous materials. Dielectric relaxation spectroscopy (DRS) and the thermally stimulated depolarization current (TSDC) technique reveal that this behaviour can be attributed to Maxwell–Wagner interface (MWI) polarization that occurs at the filler–matrix interface. These charges released during the onset of dipolar α and β relaxations of the filler particles contribute majorly to the observed pyroelectricity at RT. The saturation of both MWI TSDC shoulders and spontaneous polarization at higher electric fields correlates with the p coefficient value reaching a plateau at these applied fields. A maximum p coefficient of 0.54 μC m−2 K−1 is calculated for a poling field of 30 V μm−1.
- 16 May 2024
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry C
- Vol. 12 (23) , 8408-8417
Open AccessPyroelectricity in poled all-organic polar polynorbornene/polydimethylsiloxane-based stretchable electrets
Pyroelectricity in a recently developed all-organic composite electret with a polar polynorbornene-based filler and polydimethylsiloxane (PDMS) matrix has been studied with the help of thermal and dielectric techniques. Measurement of the pyroelectric p coefficient using a quasi-static periodic temperature variation at RT shows a non-linear dependence with the applied poling field, which is uncharacteristic of amorphous materials. Dielectric relaxation spectroscopy (DRS) and the thermally stimulated depolarization current (TSDC) technique reveal that this behaviour can be attributed to Maxwell–Wagner interface (MWI) polarization that occurs at the filler–matrix interface. These charges released during the onset of dipolar α and β relaxations of the filler particles contribute majorly to the observed pyroelectricity at RT. The saturation of both MWI TSDC shoulders and spontaneous polarization at higher electric fields correlates with the p coefficient value reaching a plateau at these applied fields. A maximum p coefficient of 0.54 μC m−2 K−1 is calculated for a poling field of 30 V μm−1.