Roby Gauthier
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Roby Gauthier has a total of 49 co-authors. Here are the top co-authors by number of shared publications:
- Jeff R. Dahn
Dalhousie University
5 shared publications - Jay. F. Whitacre
Carnegie Mellon University, Dept of Material Science and Engineering
4 shared publications - David Scott Hall
Department of Energy and Petroleum Engineering, University of Stavanger, Kristine Bonnevies vei 22, Stavanger 4021, Norway
3 shared publications Hongyi Lin
Department of Mechanical Engineering
3 shared publicationsChanho Jeong
Hyundai
2 shared publications- Eugene Jeong
Carnegie Mellon University
2 shared publications
Latest Publications
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02  (40) , 1960
Multi-Modal Chemical Analysis of Fuel Cell Electrode Ionomer Binder
Heavy-duty trucks account for most freight movement in the US and consequently contribute a large share of transportation emissions. Efforts to eliminate tailpipe emissions have focused on electrifying these vehicles through proton exchange membrane fuel cells (PEMFCs). While the scalability of PEMFCs makes them an attractive candidate for heavy-duty applications, further improvements in electrode durability are needed to achieve total cost of ownership targets to be commercially competitive. One challenge with understanding PEMFC lifetime is quantifying the extent of degradation to the the polymer electrolyte binder (commonly referred to as the ionomer) in the catalyst layers of the electrodes. The ionomer is needed for the mechanical structure and proton conductivity of the electrodes. However, the ionomer also negatively influences catalyst performance by restricting local oxygen transport at the catalyst and its catalyst adsorbtion that reduces activity. While the degradation of PEMFC membrane has been extensively studied, analysis of ionomer within the electrode is challenging due to the low total mass of material present. Typical methods for membrane degradation analysis, such as fluoride emission measurement, are frustrated by the need to distinguish degradation products of the catalyst layer ionomer from the membrane. In the present work, we assess a variety of postmortem chemical analysis techniques for their relevance to measuring catalyst layer ionomer degradation. We report methods of separating catalyst layer ionomer from the membrane in a membrane electrode assembly (MEA), and measurement conditions for a range of analytical techniques including nuclear magnetic resonance (NMR), Raman spectroscopy, and x-ray photoelectron spectroscopy (XPS). We also describe the results of fabricating a simulated degraded MEA through ex-situ treatment of the electrode on the decal backing layer prior to transfer to the membrane and compare the cell performance with MEAs which have been left untreated, and which have undergone open-circuit voltage degradation conditions. We evaluate the effectiveness and sensitivity of each characterization approach and identify potential directions for developing a postmortem MEA ionomer degradation assessment protocol.
- 24 November 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-02  (40) , 1960
Multi-Modal Chemical Analysis of Fuel Cell Electrode Ionomer Binder
Heavy-duty trucks account for most freight movement in the US and consequently contribute a large share of transportation emissions. Efforts to eliminate tailpipe emissions have focused on electrifying these vehicles through proton exchange membrane fuel cells (PEMFCs). While the scalability of PEMFCs makes them an attractive candidate for heavy-duty applications, further improvements in electrode durability are needed to achieve total cost of ownership targets to be commercially competitive. One challenge with understanding PEMFC lifetime is quantifying the extent of degradation to the the polymer electrolyte binder (commonly referred to as the ionomer) in the catalyst layers of the electrodes. The ionomer is needed for the mechanical structure and proton conductivity of the electrodes. However, the ionomer also negatively influences catalyst performance by restricting local oxygen transport at the catalyst and its catalyst adsorbtion that reduces activity. While the degradation of PEMFC membrane has been extensively studied, analysis of ionomer within the electrode is challenging due to the low total mass of material present. Typical methods for membrane degradation analysis, such as fluoride emission measurement, are frustrated by the need to distinguish degradation products of the catalyst layer ionomer from the membrane. In the present work, we assess a variety of postmortem chemical analysis techniques for their relevance to measuring catalyst layer ionomer degradation. We report methods of separating catalyst layer ionomer from the membrane in a membrane electrode assembly (MEA), and measurement conditions for a range of analytical techniques including nuclear magnetic resonance (NMR), Raman spectroscopy, and x-ray photoelectron spectroscopy (XPS). We also describe the results of fabricating a simulated degraded MEA through ex-situ treatment of the electrode on the decal backing layer prior to transfer to the membrane and compare the cell performance with MEAs which have been left untreated, and which have undergone open-circuit voltage degradation conditions. We evaluate the effectiveness and sensitivity of each characterization approach and identify potential directions for developing a postmortem MEA ionomer degradation assessment protocol.
- Open Access
- 3 November 2025
- Published by American Chemical Society (ACS) in Chemistry of Materials
- Vol. 37  (22) , 9057-9071
Formation Accelerated Side-Reactions Test: A Technique to Study Anode Passivation during Lithium-Ion Cell Formation
- 3 November 2025
- Published by American Chemical Society (ACS) in Chemistry of Materials
- Vol. 37  (22) , 9057-9071
Open AccessFormation Accelerated Side-Reactions Test: A Technique to Study Anode Passivation during Lithium-Ion Cell Formation
- Open Access
- 20 August 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 657
Nuclear magnetic resonance spectroscopy and differential capacity analysis as tools to study electrolyte consumption during the formation cycle of Li-ion pouch cells
- 20 August 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 657
Open AccessNuclear magnetic resonance spectroscopy and differential capacity analysis as tools to study electrolyte consumption during the formation cycle of Li-ion pouch cells
- 11 July 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-01  (40) , 2097
Development of Characterization Techniques to Study Chemical and Ionomer Degradation in Proton-Exchange Membrane Fuel Cells
We here show the characterization techniques we have developed to study the chemical degradation of proton-exchange membrane fuel cells with a focus on perfluoro sulfonic acid (PFSA) ionomer (e.g., Nafion) degradation in the catalyst layers. The study of catalyst layer ionomer degradation is particularly challenging because of the low amount of PFSA mass in the electrode and its adsorption to complex catalyst particles. Furthermore, effluent water and MEA analysis are often overwhelmed by the signal coming from the PFSA membrane. An additional challenge is the lack of specific accelerated stress tests for the ionomer in the electrode. Here we present methods of targeting the electrode ionomer in accelerated stress tests (ASTs) and separating out the electrode ionomer in chemical analyses. Quantitative nuclear magnetic resonance (qNMR) and fluoride ion selective electrode (ISE) measurements, among other techniques, were selected to study those degradations. We will discuss the spin relaxation of fluorine atoms in the ionomer, accurate post-processing of 19F NMR data, the calculation of the equivalent weight (EW), and other important considerations for accurate qNMR and ISE measurements.
- 11 July 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-01  (40) , 2097
Development of Characterization Techniques to Study Chemical and Ionomer Degradation in Proton-Exchange Membrane Fuel Cells
We here show the characterization techniques we have developed to study the chemical degradation of proton-exchange membrane fuel cells with a focus on perfluoro sulfonic acid (PFSA) ionomer (e.g., Nafion) degradation in the catalyst layers. The study of catalyst layer ionomer degradation is particularly challenging because of the low amount of PFSA mass in the electrode and its adsorption to complex catalyst particles. Furthermore, effluent water and MEA analysis are often overwhelmed by the signal coming from the PFSA membrane. An additional challenge is the lack of specific accelerated stress tests for the ionomer in the electrode. Here we present methods of targeting the electrode ionomer in accelerated stress tests (ASTs) and separating out the electrode ionomer in chemical analyses. Quantitative nuclear magnetic resonance (qNMR) and fluoride ion selective electrode (ISE) measurements, among other techniques, were selected to study those degradations. We will discuss the spin relaxation of fluorine atoms in the ionomer, accurate post-processing of 19F NMR data, the calculation of the equivalent weight (EW), and other important considerations for accurate qNMR and ISE measurements.
- 11 July 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-01  (5) , 532
Low Salt Concentration and Temperature during Formation as a Tool to Characterize the Passivation of the Anode Solid Electrolyte Interface
This study developed an accelerated stress test using low salt concentration and low formation temperatures to study the degree of passivation of the solid electrolyte interface (SEI) for different electrolyte formulations in lithium-ion pouch cells. Using differential capacity analysis, we can characterize the degree of passivation of additives under various conditions by looking at the degree of linear carbonate reduction. Using this technique, we observe that an electrolyte containing fluoroethylene carbonate or a mixture of vinylene carbonate and ethylene sulfate as additives passivates better than an electrolyte containing only vinylene carbonate as an additive, consistent with long-term cycling performance. This technique also allowed us to discover that additive-free electrolytes that contain low-viscosity solvents, such as methyl acetate, passivate the anode better by acting as graphite exfoliation inhibitors. We hope that the developed technique can be used to accelerate the discovery of new high-performance electrolytes.
- 11 July 2025
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2025-01  (5) , 532
Low Salt Concentration and Temperature during Formation as a Tool to Characterize the Passivation of the Anode Solid Electrolyte Interface
This study developed an accelerated stress test using low salt concentration and low formation temperatures to study the degree of passivation of the solid electrolyte interface (SEI) for different electrolyte formulations in lithium-ion pouch cells. Using differential capacity analysis, we can characterize the degree of passivation of additives under various conditions by looking at the degree of linear carbonate reduction. Using this technique, we observe that an electrolyte containing fluoroethylene carbonate or a mixture of vinylene carbonate and ethylene sulfate as additives passivates better than an electrolyte containing only vinylene carbonate as an additive, consistent with long-term cycling performance. This technique also allowed us to discover that additive-free electrolytes that contain low-viscosity solvents, such as methyl acetate, passivate the anode better by acting as graphite exfoliation inhibitors. We hope that the developed technique can be used to accelerate the discovery of new high-performance electrolytes.
- Open Access
- 14 January 2025
- Published by American Chemical Society (ACS) in ChemRxiv
Formation Accelerated Stress Test (FAST): A New Technique to Study Anode Passivation in Lithium-ion Cells using Differential Capacity, Low Salt Concentration and Low Temperature.
This study investigates the formation and properties of the solid electrolyte interface (SEI) in lithium-ion batteries under varying salt concentrations (0.4M, 0.8M, 1.2M) and low formation temperatures. This method was used as a formation accelerated stress test (FAST) to evaluate the impact of different solvent blends and additives on anode passivation using the reduction rate of ethyl methyl carbonate (EMC) seen in the differential capacity of cells containing them as a performance metric. Electrolytes containing a mixture of vinylene carbonate and ethylene sulfate showed superior passivation, while a 3:7 mixture of fluoroethylene carbonate and ethyl methyl carbonate proved to be the most effective at passivating. Furthermore, the low-viscosity solvents methyl acetate and acetonitrile significantly enhanced SEI passivation during formation at the anode due to lower graphite exfoliation. We also show that the differential capacity data correlate with long-term cycling performance for some of the chemistry studied here. These results provide valuable insights for the efficient design of a new formation accelerated stress test (FAST) that could accelerate the discovery of high-performance electrolytes through rapid monitoring of SEI passivation during formation.
- 14 January 2025
- Published by American Chemical Society (ACS) in ChemRxiv
Open AccessFormation Accelerated Stress Test (FAST): A New Technique to Study Anode Passivation in Lithium-ion Cells using Differential Capacity, Low Salt Concentration and Low Temperature.
This study investigates the formation and properties of the solid electrolyte interface (SEI) in lithium-ion batteries under varying salt concentrations (0.4M, 0.8M, 1.2M) and low formation temperatures. This method was used as a formation accelerated stress test (FAST) to evaluate the impact of different solvent blends and additives on anode passivation using the reduction rate of ethyl methyl carbonate (EMC) seen in the differential capacity of cells containing them as a performance metric. Electrolytes containing a mixture of vinylene carbonate and ethylene sulfate showed superior passivation, while a 3:7 mixture of fluoroethylene carbonate and ethyl methyl carbonate proved to be the most effective at passivating. Furthermore, the low-viscosity solvents methyl acetate and acetonitrile significantly enhanced SEI passivation during formation at the anode due to lower graphite exfoliation. We also show that the differential capacity data correlate with long-term cycling performance for some of the chemistry studied here. These results provide valuable insights for the efficient design of a new formation accelerated stress test (FAST) that could accelerate the discovery of high-performance electrolytes through rapid monitoring of SEI passivation during formation.
- 22 November 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-02  (4) , 497
Cluster Analysis of Cell Health and Characterization of Lithium and Active Material Loss in a Large Format LiFePO4 Hybrid Vehicle Battery Pack
Currently, the second-life Li-ion battery (LIB) landscape lacks a widely accepted safety standard for determining the viability of retired batteries for reuse.1 While the impact of abusive conditions on battery failures, such as toxic gas releases, fires, and explosions, has been studied extensively, the understanding of how aging affects the likelihood of thermal runaway under normal use conditions remains limited. This knowledge gap underscores the critical need for a deeper understanding of material degradation throughout the LIB lifecycle and its direct safety implications. In response, researchers are exploring advanced characterization methods to deconvolve and identify degradation behaviors, typically using lab-aged cells. These methods, which range from non-destructive evaluation to post-mortem analyses, have revealed various degradation modes (such as active material loss and Li inventory loss) and mechanisms (including Li plating, SEI growth and decomposition, transition metal dissolution, and particle cracking).2 However, the variability of these degradation modes in real-world battery packs remains poorly understood, making it challenging to estimate the likelihood of thermal runaway. A precise statistical understanding of these degradation mechanisms is essential for developing robust safety standards and maximizing the economic benefits of reusing LIBs. In this work, we apply differential voltage analysis to assess the statistical distribution of active material loss in a retired 1,536-cell hybrid-vehicle battery pack (see Ref. 3 for pack details).3 Initially, we measured the capacity and ohmic resistance of 1,500 cells (98% of the pack) using galvanostatic cycling at a rate of 1C (Fig. 1A-D). We then implemented k-medoids clustering to categorize the cells based on their capacity and resistance (Fig. 1E). The representative medoid cell from each cluster was then selected for further analysis at a slower C/10 cycling rate to gather dV/dQ data. Using open-source software provided by Dahn et al.,4 we fit the measured dV/dQ curves to reference curves collected from a LiFePO4 cathode vs. Li/Li+ and a graphite anode vs. Li/Li+ half-cells (the latter was provided by with the dV/dQ software). The fitting process yields 4 parameters: mG (active mass of the graphite anode), mLFP (active mass of the LFP cathode), 𝛿 LFP (LFP cathode slippage), and 𝛿 G (graphite anode slippage). Active material loss and slippage are then calculated relative to an uncycled cell with mG = 8.1 g and mLFP = 13 g. Fig. 1 summarizes the SOH of 1,500 cells (A-C), the cell categories and representative cells determined via k-medoid clustering (D), the dV/dQ curve-fitting method (E), and example dV/dQ curve-fitting results for 2 cells (F). The cell capacities (nominally 2.3 to 2.5 Ah) ranged from 0.0 to 2.2 Ah and their direct-current internal resistances (DCIR), which started at 10 mΩ when newly manufactured, ranged from 30 to 1000 mΩ. For two example cells (Fig. 1F), a -24% and +22% difference in % initial capacity (PIC) and DCIR, respectively, corresponded to a 150% increase in active graphite loss, a 99% increase in active LFP loss and a 6.7% difference in slippage (where 𝛿 = 𝛿 G - 𝛿 LFP ). In this presentation, we will expand on these initial results and will summarize our findings on the distribution of capacity, resistance, active material loss, and Li inventory loss across the entire pack. References Christensen, P. A., Mrozik, W. & Wise, M. S. A Study on the Safety of Second-Life Batteries in Battery Energy Storage Systems. UK BEIS/OPSS Report (2021). Li, A. G., West, A. C. & Preindl, M. Applied Energy 316, 119030 (2022). DOI: 10.1016/j.apenergy.2022.119030. Ramirez-Meyers, K., Rawn, B. & Whitacre, J. F. J. Energy Storage 59, 106472 (2023). DOI: 10.1016/j.est.2022.106472. Dahn, H. M., Smith, A. J., Burns, J. C., Stevens, D. A. & Dahn, J. R. J. Electrochem. Soc. 159, A1405–A1409 (2012). DOI: 10.1149/2.013209jes. Figure 1: A-D summarize the SOH of 1,500 cells. A) Charge and discharge curves, V(Q), at a 1C rate (that is, current = 2.0 A). B and D) Capacity and DCIR distributions. C) K-medoids clustering using z-scores (normalized capacity and DCIR values) shows representative cells as medoids of each cluster. E) An example of fitting measured dV/dQ (black) to dV/dQ calculated from the LFP cathode (blue) and graphite anode (purple) references. F) Comparative example of electrode mass and slippage calculations obtained from dV/dQ analysis. * = outliers are exclud ed. DCIR = direct-current internal resistance. LAM = Loss of active material. LFP = LiFePO4. PIC = Percent of initial capacity. Z-score = (Value – Mean)/Standard Deviation. Figure 1
- 22 November 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-02  (4) , 497
Cluster Analysis of Cell Health and Characterization of Lithium and Active Material Loss in a Large Format LiFePO4 Hybrid Vehicle Battery Pack
Currently, the second-life Li-ion battery (LIB) landscape lacks a widely accepted safety standard for determining the viability of retired batteries for reuse.1 While the impact of abusive conditions on battery failures, such as toxic gas releases, fires, and explosions, has been studied extensively, the understanding of how aging affects the likelihood of thermal runaway under normal use conditions remains limited. This knowledge gap underscores the critical need for a deeper understanding of material degradation throughout the LIB lifecycle and its direct safety implications. In response, researchers are exploring advanced characterization methods to deconvolve and identify degradation behaviors, typically using lab-aged cells. These methods, which range from non-destructive evaluation to post-mortem analyses, have revealed various degradation modes (such as active material loss and Li inventory loss) and mechanisms (including Li plating, SEI growth and decomposition, transition metal dissolution, and particle cracking).2 However, the variability of these degradation modes in real-world battery packs remains poorly understood, making it challenging to estimate the likelihood of thermal runaway. A precise statistical understanding of these degradation mechanisms is essential for developing robust safety standards and maximizing the economic benefits of reusing LIBs. In this work, we apply differential voltage analysis to assess the statistical distribution of active material loss in a retired 1,536-cell hybrid-vehicle battery pack (see Ref. 3 for pack details).3 Initially, we measured the capacity and ohmic resistance of 1,500 cells (98% of the pack) using galvanostatic cycling at a rate of 1C (Fig. 1A-D). We then implemented k-medoids clustering to categorize the cells based on their capacity and resistance (Fig. 1E). The representative medoid cell from each cluster was then selected for further analysis at a slower C/10 cycling rate to gather dV/dQ data. Using open-source software provided by Dahn et al.,4 we fit the measured dV/dQ curves to reference curves collected from a LiFePO4 cathode vs. Li/Li+ and a graphite anode vs. Li/Li+ half-cells (the latter was provided by with the dV/dQ software). The fitting process yields 4 parameters: mG (active mass of the graphite anode), mLFP (active mass of the LFP cathode), 𝛿 LFP (LFP cathode slippage), and 𝛿 G (graphite anode slippage). Active material loss and slippage are then calculated relative to an uncycled cell with mG = 8.1 g and mLFP = 13 g. Fig. 1 summarizes the SOH of 1,500 cells (A-C), the cell categories and representative cells determined via k-medoid clustering (D), the dV/dQ curve-fitting method (E), and example dV/dQ curve-fitting results for 2 cells (F). The cell capacities (nominally 2.3 to 2.5 Ah) ranged from 0.0 to 2.2 Ah and their direct-current internal resistances (DCIR), which started at 10 mΩ when newly manufactured, ranged from 30 to 1000 mΩ. For two example cells (Fig. 1F), a -24% and +22% difference in % initial capacity (PIC) and DCIR, respectively, corresponded to a 150% increase in active graphite loss, a 99% increase in active LFP loss and a 6.7% difference in slippage (where 𝛿 = 𝛿 G - 𝛿 LFP ). In this presentation, we will expand on these initial results and will summarize our findings on the distribution of capacity, resistance, active material loss, and Li inventory loss across the entire pack. References Christensen, P. A., Mrozik, W. & Wise, M. S. A Study on the Safety of Second-Life Batteries in Battery Energy Storage Systems. UK BEIS/OPSS Report (2021). Li, A. G., West, A. C. & Preindl, M. Applied Energy 316, 119030 (2022). DOI: 10.1016/j.apenergy.2022.119030. Ramirez-Meyers, K., Rawn, B. & Whitacre, J. F. J. Energy Storage 59, 106472 (2023). DOI: 10.1016/j.est.2022.106472. Dahn, H. M., Smith, A. J., Burns, J. C., Stevens, D. A. & Dahn, J. R. J. Electrochem. Soc. 159, A1405–A1409 (2012). DOI: 10.1149/2.013209jes. Figure 1: A-D summarize the SOH of 1,500 cells. A) Charge and discharge curves, V(Q), at a 1C rate (that is, current = 2.0 A). B and D) Capacity and DCIR distributions. C) K-medoids clustering using z-scores (normalized capacity and DCIR values) shows representative cells as medoids of each cluster. E) An example of fitting measured dV/dQ (black) to dV/dQ calculated from the LFP cathode (blue) and graphite anode (purple) references. F) Comparative example of electrode mass and slippage calculations obtained from dV/dQ analysis. * = outliers are exclud ed. DCIR = direct-current internal resistance. LAM = Loss of active material. LFP = LiFePO4. PIC = Percent of initial capacity. Z-score = (Value – Mean)/Standard Deviation. Figure 1
- 9 August 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-01  (2) , 408
A Study on the Kinetics and Structural Changes of Silicon during Ball Milling
Enhancing our understanding of the ball milling process is important to optimize silicon amorphization, a key factor in improving the performance of lithium-ion battery anodes. To improve this understanding, we quantitatively studied the kinetics of silicon amorphization during ball milling using x-ray diffraction (XRD) and electrochemical methods, among other methods. The percentage of amorphous and crystalline silicon was deduced by fitting the XRD data and electrochemical results. The resulting trend versus ball milling time was then fitted using the Avrami model. The material resulting from ball milling was further studied using scanning and transmission electron microscopy (SEM/TEM). Under extended milling times, we found that a maximum of 86% of the silicon became amorphous. Similarly, the grain size of the crystalline silicon phase could not be reduced below 6 nm. Our observations suggest that amorphization results from defects creation during ball milling. Amorphization then stops when the grain size reaches a limit where defects are no longer formed. Figure 1
- 9 August 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-01  (2) , 408
A Study on the Kinetics and Structural Changes of Silicon during Ball Milling
Enhancing our understanding of the ball milling process is important to optimize silicon amorphization, a key factor in improving the performance of lithium-ion battery anodes. To improve this understanding, we quantitatively studied the kinetics of silicon amorphization during ball milling using x-ray diffraction (XRD) and electrochemical methods, among other methods. The percentage of amorphous and crystalline silicon was deduced by fitting the XRD data and electrochemical results. The resulting trend versus ball milling time was then fitted using the Avrami model. The material resulting from ball milling was further studied using scanning and transmission electron microscopy (SEM/TEM). Under extended milling times, we found that a maximum of 86% of the silicon became amorphous. Similarly, the grain size of the crystalline silicon phase could not be reduced below 6 nm. Our observations suggest that amorphization results from defects creation during ball milling. Amorphization then stops when the grain size reaches a limit where defects are no longer formed. Figure 1
- Open Access
- 14 January 2022
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 169  (2)
How do Depth of Discharge, C-rate and Calendar Age Affect Capacity Retention, Impedance Growth, the Electrodes, and the Electrolyte in Li-Ion Cells?
Lithium-ion cells testing under different state of charge ranges, C-rates and cycling temperature have different degrees of lithium inventory loss, impedance growth and active mass loss. Here, a large matrix of polycrystalline NMC622/natural graphite Li-ion pouch cells were tested with seven different state of charge ranges (0-25, 0-50, 0-75, 0-100, 75-100, 50-100 and 25-100%), three different C-rates and at two temperatures. First, capacity fade was compared to a model developed by Deshpande and Bernardi. Second, after 2.5 years of cycling, detailed analysis by dV/dQ analysis, lithium-ion differential thermal analysis, volume expansion by Archimedes’ principle, electrode stack growth, ultrasonic transmissivity and x-ray computed tomography were undertaken. These measurements enabled us to develop a complete picture of cell aging for these cells. This then led to an empirical predictive model for cell capacity loss versus SOC range and calendar age. Although these particular cells exhibited substantial positive electrode active mass loss, this did not play a role in capacity retention because the cells were anode limited during full discharge under all the tests carried out here. However, the positive electrode mass loss was strongly coupled to positive electrode swelling and electrolyte “unwetting” that would eventually cause dramatic failure.
- 14 January 2022
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 169  (2)
Open AccessHow do Depth of Discharge, C-rate and Calendar Age Affect Capacity Retention, Impedance Growth, the Electrodes, and the Electrolyte in Li-Ion Cells?
Lithium-ion cells testing under different state of charge ranges, C-rates and cycling temperature have different degrees of lithium inventory loss, impedance growth and active mass loss. Here, a large matrix of polycrystalline NMC622/natural graphite Li-ion pouch cells were tested with seven different state of charge ranges (0-25, 0-50, 0-75, 0-100, 75-100, 50-100 and 25-100%), three different C-rates and at two temperatures. First, capacity fade was compared to a model developed by Deshpande and Bernardi. Second, after 2.5 years of cycling, detailed analysis by dV/dQ analysis, lithium-ion differential thermal analysis, volume expansion by Archimedes’ principle, electrode stack growth, ultrasonic transmissivity and x-ray computed tomography were undertaken. These measurements enabled us to develop a complete picture of cell aging for these cells. This then led to an empirical predictive model for cell capacity loss versus SOC range and calendar age. Although these particular cells exhibited substantial positive electrode active mass loss, this did not play a role in capacity retention because the cells were anode limited during full discharge under all the tests carried out here. However, the positive electrode mass loss was strongly coupled to positive electrode swelling and electrolyte “unwetting” that would eventually cause dramatic failure.
- Open Access
- 1 October 2020
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 167  (13) , 130529
Effect of Duty Cycle on the Lifetime of Single Crystal LiNi0.5Mn0.3Co0.2O2/Graphite Lithium-Ion Cells
The effects of different duty cycles, involving mixtures of charge-discharge cycling and open-circuit storage segments, on the lifetime of single crystal NMC532/graphite cells were studied. Charge-discharge cycling was performed at C/3 with open circuit storage times of 0, 12, 84, 180 h or 3 months applied at upper cutoff voltages (UCV) of 4.1, 4.2 and 4.3 V. Testing was made at 40 °C for a period of 2.5 years. Cells tested to the same UCV showed similar capacity loss and impedance growth with time, independent of the ratio between the time spent cycling or in storage. Differential voltage analysis showed that the vast majority of the capacity loss stemmed from lithium inventory loss at the negative electrode with little or no loss of active materials. The thickness of the pouch cells after testing increased with the fraction of time spent cycling and the amount of gas generated in the cells increased with fraction of time spent in storage at the UCV. These results show that cycled and stored cells age differently, even though a similar capacity fade rate was observed in the first 2.5 years of cell life, which may cause different failure modes at the end of cell life.
- 1 October 2020
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 167  (13) , 130529
Open AccessEffect of Duty Cycle on the Lifetime of Single Crystal LiNi0.5Mn0.3Co0.2O2/Graphite Lithium-Ion Cells
The effects of different duty cycles, involving mixtures of charge-discharge cycling and open-circuit storage segments, on the lifetime of single crystal NMC532/graphite cells were studied. Charge-discharge cycling was performed at C/3 with open circuit storage times of 0, 12, 84, 180 h or 3 months applied at upper cutoff voltages (UCV) of 4.1, 4.2 and 4.3 V. Testing was made at 40 °C for a period of 2.5 years. Cells tested to the same UCV showed similar capacity loss and impedance growth with time, independent of the ratio between the time spent cycling or in storage. Differential voltage analysis showed that the vast majority of the capacity loss stemmed from lithium inventory loss at the negative electrode with little or no loss of active materials. The thickness of the pouch cells after testing increased with the fraction of time spent cycling and the amount of gas generated in the cells increased with fraction of time spent in storage at the UCV. These results show that cycled and stored cells age differently, even though a similar capacity fade rate was observed in the first 2.5 years of cell life, which may cause different failure modes at the end of cell life.