O. B. Berdnik
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
O. B. Berdnik has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
I N Tsareva
Institute of Mechanical Engineering Problems of the Russian Academy of Sciences (IPM of RAS)-branch of the FIC of the Institute of Applied Physics of the Russian Academy of Sciences, 603024, Nizhny Novgorod, Russia
2 shared publicationsIrina Tsareva
Institute of Mechanical Engineering Problems of the Russian Academy of Sciences – Branch of FIC IPF RAS, Nizhny Novgorod, Russia
2 shared publicationsL A Krivina
Institute of Mechanical Engineering Problems of the Russian Academy of Sciences (IPM of RAS)-branch of the FIC of the Institute of Applied Physics of the Russian Academy of Sciences, 603024, Nizhny Novgorod, Russia
2 shared publicationsM. K. Chegurov
2 shared publications- Evgeny N. Razov
N. I. Lobachevsky Nizhny Novgorod State University, Nizhny Novgorod, Russian Federation
1 shared publication - I. N. Tsareva
Institute for Problems in Machine Building, of the Russian Academy of Sciences, Nizhny Novgorod—a Branch of the Federal Research Center A.V. Gaponov-Grekhov Institute of Applied Physics of the Russian Academy of Sciences, Nizhny Novgorod, Russia
1 shared publication
Latest Publications
- 26 August 2024
- Published by Ore and Metals Publishing House in Chernye Metally
- No. 8,p. 39-46
The influence of heat treatment modes on structure and corrosion properties of 14Kh17N2 steel
Issues of ensuring the stability of the structural state and mechanical properties are very relevant for production when processing products, assessing quality and extending service life. The article presents studies of the influence of changes in the structure resulting from the use of various heat treatment modes using the example of heat-resistant, corrosion-resistant steel 14Kh17N2, which belongs to the martensitic-ferritic class steels, containing in its structure, in addition to martensite, at least 10 % ferrite. It has the greatest corrosion resistance after hardening with high tempering. Steel 14Kh17N2 is very complex in technological terms. The presence of large quantities of δ-ferrite in the structure of this steel has a harmful effect on the course of technological processes: it worsens the deformability of steel and sharply reduces the plasticity properties (especially impact strength) when testing samples in the tangential or transverse direction, and increases the anisotropy of mechanical properties. A relationship has been established between the amount of δ-ferrite and the carbide phase precipitated at its boundaries with the mechanical properties of steel. It has been shown that with increasing quenching temperature, the amount of δ-ferrite changes slightly, and the amount of the carbide phase decreases. Corrosion tests of samples in an aqueous solution of potassium thiocyanate (KSCN) with sulfuric acid (H₂SO₄) after various heat treatment modes showed that with a decrease in the amount of chromium carbides released at the boundaries of the δ-phase, the ratio of the amount of electricity (Sk/Sa) decreases. the depth of corrosion does not depend on the amount of δ-ferrite and chromium carbides. On the surface of all samples, in the areas of the boundary between the δ-phase and tempered troostite, traces of corrosion destruction of varying depths are visible.State assignment of the Institute of Applied Physics RAS for fundamental scientific research for 2024–2026. FFUF-2024-0031. No. NIOKTR 1023032800130-3-2.3.2.
- 26 August 2024
- Published by Ore and Metals Publishing House in Chernye Metally
- No. 8,p. 39-46
The influence of heat treatment modes on structure and corrosion properties of 14Kh17N2 steel
Issues of ensuring the stability of the structural state and mechanical properties are very relevant for production when processing products, assessing quality and extending service life. The article presents studies of the influence of changes in the structure resulting from the use of various heat treatment modes using the example of heat-resistant, corrosion-resistant steel 14Kh17N2, which belongs to the martensitic-ferritic class steels, containing in its structure, in addition to martensite, at least 10 % ferrite. It has the greatest corrosion resistance after hardening with high tempering. Steel 14Kh17N2 is very complex in technological terms. The presence of large quantities of δ-ferrite in the structure of this steel has a harmful effect on the course of technological processes: it worsens the deformability of steel and sharply reduces the plasticity properties (especially impact strength) when testing samples in the tangential or transverse direction, and increases the anisotropy of mechanical properties. A relationship has been established between the amount of δ-ferrite and the carbide phase precipitated at its boundaries with the mechanical properties of steel. It has been shown that with increasing quenching temperature, the amount of δ-ferrite changes slightly, and the amount of the carbide phase decreases. Corrosion tests of samples in an aqueous solution of potassium thiocyanate (KSCN) with sulfuric acid (H₂SO₄) after various heat treatment modes showed that with a decrease in the amount of chromium carbides released at the boundaries of the δ-phase, the ratio of the amount of electricity (Sk/Sa) decreases. the depth of corrosion does not depend on the amount of δ-ferrite and chromium carbides. On the surface of all samples, in the areas of the boundary between the δ-phase and tempered troostite, traces of corrosion destruction of varying depths are visible.State assignment of the Institute of Applied Physics RAS for fundamental scientific research for 2024–2026. FFUF-2024-0031. No. NIOKTR 1023032800130-3-2.3.2.
- 26 August 2024
- Published by Ore and Metals Publishing House in Chernye Metally
- No. 8,p. 51-55
Regularities of formation of PNKh20K20Yu13 powder material intermetallic coating
An important area in the field of gas-thermal technologies is the development of heatprotective ceramic coatings for thermally loaded parts of power and aircraft engineering (combustion chambers, working and guide blades, protective plates, heat shields of gas turbines). However, the coefficient of thermal expansion and the hardness value of metal-ceramic coatings differ significantly from the metal base of the processed parts. Therefore, in order to create a smooth transition from the substrate to the working ceramic layer, a transition layer (sublayer) is first formed from multicomponent powder materials of the Ni - Cr - Co - Al - Y system. The most popular powder materials on the domestic ferrous metallurgy market are PNKh20K20Yu13 grade from different manufacturers. The properties of this domestically produced intermetallic powder material with a particle size of 40 to 80 μm were studied and tested as a initial material for plasma spraying of a heat-resistant coating. X-ray phase and microstructural analysis methods showed that the powder has an intermetallic phase composition based on the β-Ni(Me)Al phase. Under high-temperature exposure to a plasma flow, a phase transformation β → γ’ occurs in the sprayed material. Derivatographic studies showed that the phase transition occurs in the temperature range of 660–839 °C. As a result, a coating of the Ni – Cr – Co – Al – Y system is formed with a two-phase intermetallic composition (β-Ni(Me)Al + γ’-(Ni,Me)3Al), a layered microstructure of grains and a dendritic structure of spheroidal grains. The coating is characterized by low total porosity (~5 %), Vickers hardness HV = 5.5 GPa, roughness Ra = 6.5 μm. The studied coating is recommended for use both as a sublayer in two-layer heat-protective coatings and as an independent heat-resistant coating for protecting critical parts of power and aircraft engineering.The work was carried out within the framework of the state assignment of the IAP RAS for fundamental scientific research in 2024–2026. FFUF-2024-0031. No. NIOKTR 1023032800130-3-2.3.2.
- 26 August 2024
- Published by Ore and Metals Publishing House in Chernye Metally
- No. 8,p. 51-55
Regularities of formation of PNKh20K20Yu13 powder material intermetallic coating
An important area in the field of gas-thermal technologies is the development of heatprotective ceramic coatings for thermally loaded parts of power and aircraft engineering (combustion chambers, working and guide blades, protective plates, heat shields of gas turbines). However, the coefficient of thermal expansion and the hardness value of metal-ceramic coatings differ significantly from the metal base of the processed parts. Therefore, in order to create a smooth transition from the substrate to the working ceramic layer, a transition layer (sublayer) is first formed from multicomponent powder materials of the Ni - Cr - Co - Al - Y system. The most popular powder materials on the domestic ferrous metallurgy market are PNKh20K20Yu13 grade from different manufacturers. The properties of this domestically produced intermetallic powder material with a particle size of 40 to 80 μm were studied and tested as a initial material for plasma spraying of a heat-resistant coating. X-ray phase and microstructural analysis methods showed that the powder has an intermetallic phase composition based on the β-Ni(Me)Al phase. Under high-temperature exposure to a plasma flow, a phase transformation β → γ’ occurs in the sprayed material. Derivatographic studies showed that the phase transition occurs in the temperature range of 660–839 °C. As a result, a coating of the Ni – Cr – Co – Al – Y system is formed with a two-phase intermetallic composition (β-Ni(Me)Al + γ’-(Ni,Me)3Al), a layered microstructure of grains and a dendritic structure of spheroidal grains. The coating is characterized by low total porosity (~5 %), Vickers hardness HV = 5.5 GPa, roughness Ra = 6.5 μm. The studied coating is recommended for use both as a sublayer in two-layer heat-protective coatings and as an independent heat-resistant coating for protecting critical parts of power and aircraft engineering.The work was carried out within the framework of the state assignment of the IAP RAS for fundamental scientific research in 2024–2026. FFUF-2024-0031. No. NIOKTR 1023032800130-3-2.3.2.
- 1 December 2020
- Published by Allerton Press in Journal of Machinery Manufacture and Reliability
- Vol. 49 (7) , 646-651
Fracture of Blade Material under Long-Term Operation
This paper presents an analysis of changes in the mechanical properties of the EI-961Sh alloy under operation and the causes of fracture of the inlet guide
- 1 December 2020
- Published by Allerton Press in Journal of Machinery Manufacture and Reliability
- Vol. 49 (7) , 646-651
Fracture of Blade Material under Long-Term Operation
This paper presents an analysis of changes in the mechanical properties of the EI-961Sh alloy under operation and the causes of fracture of the inlet guide
- Open Access
- 1 November 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 971 (3) , 032015
The study of high-temperature stability of the heat-resisting intermetallide coating
The article presents the results of a study of the processes occurring in a heat-resistant intermetallic coating under ultrafast thermal heating by a laser beam. Workers, guide vanes and other parts of the hot tract of gas turbine engines are operated at elevated temperatures, pressures and speeds. Significantly increase the life of such parts by applying heat-resistant coatings that protect the surface from high-temperature oxidation, erosion, and softening of the base material. The plasma coating consists of an intermetallic (β-phase) compound. A pulsed-periodic laser with pulse energy E = 5, 10, 15, and 30 J was used for thermal heating. Upon heating, surface melting of the fusible phases occurred and the integrity of the surface layer of the coating was violated. By changing the parameters of laser radiation, it is possible to carry out express diagnostics and comparative tests of coatings, as well as to predict their behavior in extreme conditions.
- 1 November 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 971 (3) , 032015
Open AccessThe study of high-temperature stability of the heat-resisting intermetallide coating
The article presents the results of a study of the processes occurring in a heat-resistant intermetallic coating under ultrafast thermal heating by a laser beam. Workers, guide vanes and other parts of the hot tract of gas turbine engines are operated at elevated temperatures, pressures and speeds. Significantly increase the life of such parts by applying heat-resistant coatings that protect the surface from high-temperature oxidation, erosion, and softening of the base material. The plasma coating consists of an intermetallic (β-phase) compound. A pulsed-periodic laser with pulse energy E = 5, 10, 15, and 30 J was used for thermal heating. Upon heating, surface melting of the fusible phases occurred and the integrity of the surface layer of the coating was violated. By changing the parameters of laser radiation, it is possible to carry out express diagnostics and comparative tests of coatings, as well as to predict their behavior in extreme conditions.
- Open Access
- 1 January 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 709 (4) , 044011
Uneven degradation of the material during the operation of turdine blades
Turbine rotor blades operate under the action of centrifugal forces, which create height-varying stresses. The temperature field of the blades is also inhomogeneous, and the value of its gradient depends on the flow parameters and the geometric dimensions of the blades. In the process of manufacturing and quality control of completed turbine rotor blades, the manufacturer uses the generally accepted state standards to determine the condition during long-term operation. It is assumed that the material of the blades should be uniform all over the volume so that the manufacturer proposes analyzing mainly the blade root. In this case, mechanical tests are carried out on large samples and the results provide only averaged data on the state of the material. Life prediction based on the results of mechanical tests can lead to a mistaken overestimation of service life. This is because this approach takes into account only the state of the internal zones of the material. However, the rupture of material occurs on the surface and in the more thermally stressed parts like the trailing edge or leading edge. As a consequence, the application of this approach is unacceptable for blades with long operating time.
- 1 January 2020
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 709 (4) , 044011
Open AccessUneven degradation of the material during the operation of turdine blades
Turbine rotor blades operate under the action of centrifugal forces, which create height-varying stresses. The temperature field of the blades is also inhomogeneous, and the value of its gradient depends on the flow parameters and the geometric dimensions of the blades. In the process of manufacturing and quality control of completed turbine rotor blades, the manufacturer uses the generally accepted state standards to determine the condition during long-term operation. It is assumed that the material of the blades should be uniform all over the volume so that the manufacturer proposes analyzing mainly the blade root. In this case, mechanical tests are carried out on large samples and the results provide only averaged data on the state of the material. Life prediction based on the results of mechanical tests can lead to a mistaken overestimation of service life. This is because this approach takes into account only the state of the internal zones of the material. However, the rupture of material occurs on the surface and in the more thermally stressed parts like the trailing edge or leading edge. As a consequence, the application of this approach is unacceptable for blades with long operating time.
- Open Access
- 18 November 2019
- Published by EDP Sciences in MATEC Web of Conferences
- Vol. 298, 00035
Application of the complex parameter of strength and ductility to assess the state of the blades’ material at different periods of operation
The paper is devoted to the study of the material’s condition of guide blades made of heat-resistant nickel alloy with different operating time. It is established that the structure of the blade material and their mechanical properties are not satisfactory for further operation. To recovery the performance properties and structure of the blade material, several types of heat treatment were tested and the optimal one was chosen. The complex parameter of strength and plasticity is calculated and on its basis the estimation of degree of recovery of blade’ material after heat treatment is carried out.
- 18 November 2019
- Published by EDP Sciences in MATEC Web of Conferences
- Vol. 298, 00035
Open AccessApplication of the complex parameter of strength and ductility to assess the state of the blades’ material at different periods of operation
The paper is devoted to the study of the material’s condition of guide blades made of heat-resistant nickel alloy with different operating time. It is established that the structure of the blade material and their mechanical properties are not satisfactory for further operation. To recovery the performance properties and structure of the blade material, several types of heat treatment were tested and the optimal one was chosen. The complex parameter of strength and plasticity is calculated and on its basis the estimation of degree of recovery of blade’ material after heat treatment is carried out.
- Open Access
- 18 November 2019
- Published by EDP Sciences in MATEC Web of Conferences
- Vol. 298, 00036
The gas-dynamic antifriction coating of babbitt for bearings of the turbine rotor
The application of the anti-friction coating of babbitt on the working surface of sliding bearings is an important technological procedure necessary both for their manufacture and for their repair. To extend the service life and restore the performance of bearings, the coating is preferably applied by gas-dynamic spraying, The coating formed by this method has a low porosity, high adhesion strength and low friction coefficient.
- 18 November 2019
- Published by EDP Sciences in MATEC Web of Conferences
- Vol. 298, 00036
Open AccessThe gas-dynamic antifriction coating of babbitt for bearings of the turbine rotor
The application of the anti-friction coating of babbitt on the working surface of sliding bearings is an important technological procedure necessary both for their manufacture and for their repair. To extend the service life and restore the performance of bearings, the coating is preferably applied by gas-dynamic spraying, The coating formed by this method has a low porosity, high adhesion strength and low friction coefficient.