  • Open Access

    Effect of Thermal Ageing on Changes in Modulus of Elasticity E Measured by Ultrasound, Bending Test and EBSD

    by Jana Vesela, Petr Beneš, David Bricín

    The materials used in VVER nuclear power plants are subject to thermal ageing in operation, among other degradation mechanisms. The aim of the experiment was to verify the effect of thermal ageing on the change of ultrasound velocity on the extracted parts of main circulation piping and pressurizer surge line made of austenitic steels. Two steel conditions were evaluated, as received and thermally aged. The research was carried out on samples made from non-operated pipelines and samples from pipelines after 28 years of operation. The samples were subjected to thermal ageing at 450 °C in an atmospheric furnace with a specified exposure time to simulate extended operation of the component for 60 years, where 1 year of operation means 10 months at 100 %-unit power and 2 months in shutdown. The samples were subjected to ultrasonic property measurements and the longitudinal and transverse wave velocities obtained are further used to calculate the Poisson's constant and elastic modulus E of the material. To verify the ultrasonic measurements, the samples were also subjected to mechanical tests to verify the changes in the mechanical properties in terms of elastic behaviour of the selected steels when subjected to a static 3-point flexural test and Electron backscatter diffraction analysis (EBSD). Ultrasound speed Thermal ageing Elastic modulus E Tree-point flexural test Elastic stiffness coefficient


  • Open Access

    Quality verification of Cold spray protection of the weld root

    by J Veselá, P Mareš, Z Špirit, J Brom

    Cold spray technology (CS) as an advanced surface treatment can also be applied in the field of energy. Depending on the type of spraying, the coating itself plays the role of protecting the surface from corrosion, abrasion and other operational influences. In the case of dissimilar metal welds (DMW), it can play the role of protection against stress corrosion cracking (SCC). The thickness of the applied spray can range from tens of microns to units of mm. The quality of NiCr and Ni protective coatings made by CS technology was tested by means of non-destructive (NDT) and destructive (DT) testing. NDT focused on measuring the attenuation of the ultrasonic signal, measuring the thickness of the applied coatings and the adhesion to the base material using pulsed echo (PEUT) and phased array (PAUT) ultrasonic testing techniques. Evaluation of the microstructure, porosity and corrosion stability of CS coatings before and after the salt spray test was performed metallographically.

  • Replicas Application in Non-Destructive Testing

    by Jana Veselá, Pavel Zahrádka, Jan Matějíček

    Abstra c t The use of replication kits has recently become an integral part of the field of non-destructive testing (NDT). Classical surface NDT methods are thus advantageously supplemented by surface prints in selected places of the inspected material. Replicate kits are set to be the fingerprint surface structure requiring no special surface preparation prior to collection of replicas and are intended for the 3D measurement of the dimensions of surface defects. Replicas are then evaluated using a 3D optical profilometer with optical or laser-optical lenses.

  • Evaluation of Steam Turbine Blades Surface Cracks Detectability by Nondestructive Methods

    by Jana Veselá, Pavel MareŠ, Pavel Zahradka, Jan Patera

    This article describes methods suitable for crack detection on low pressure steam turbine blades, not including the blade root. These cracks, which are initiated in the corrosion pitting, can cause serious damage to the steam turbine blade leading to its breakaway. Therefore, the detection of these cracks on the early stages of blade fracture is very important. Several methods for detecting of surface cracks (ultrasonic Rayleigh waves, eddy current with flexible array probe, etc.) has been tested on artificial flaws, which were manufactured into turbine blades. The comparison of all these methods is described as well as the evaluation of their advantages and disadvantages. Simulations of ultrasonic testing are also presented in this article.


  • Internal oxide thickness measurement by ultrasonic method

    by Jana Vesela, Pavel Mareš, Roman Janura

    Long-term exposition of re-heater and super-heater tubes in fossil-fired steam boilers at high temperature causes the growth of the iron oxide scale (magnetite) on the both internal and external tube surfaces. The presence of the internal oxide scale on the water side of the tube acts as a thermal insulator reduces heat transfer through the tube wall. Persistent overheating of the tube wall is a crucial issue, which leads to a metallurgical failure of the tube. The oxide scales react as a thermal insulator on the water side and reduce the heat transfer through the tube wall. Relatively thin oxide scale contributes to a reduction of boiler efficiency and causes persistent overheating of the tube wall. The growth of internal oxide scale is a time- and temperature-dependent process with a negative impact on the remaining creep-to-rupture life.