Samar Al-Saleh
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Samar Al-Saleh has a total of 66 co-authors. Here are the top co-authors by number of shared publications:
- Fahim Vohra
Department of Prosthetic Dental Sciences, College of Dentistry, King Saud University, Riyadh, 11545, Saudi Arabia
13 shared publications - Tariq Abduljabbar
Department of Prosthetic Dental Sciences, College of Dentistry, King Saud University, Riyadh, 11545, Saudi Arabia
13 shared publications - Eman Mohammed AlHamdan
Department of Prosthetic Dental Sciences, College of Dentistry, King Saud University, P.O.Box 21069, Riyadh 11475, Saudi Arabia
7 shared publications - Abdulaziz S. Alqahtani
Department of Prosthetic Dental Sciences, College of Dentistry, King Saud University, Riyadh 11545, Saudi Arabia
4 shared publications - Ebtissam Mohammed Al-Madi
Department of Restorative Dental Sciences, Endodontic Division, College of Dentistry, King Saud University, Riyadh 11432, Saudi Arabia
4 shared publications - Imran Farooq
University of Toronto, Canada
4 shared publications
Latest Publications
- Open Access
Marginal Misfit of 3D-Printed (Selective Laser Sintered), CAD-CAM and Lost Wax Technique Cobalt Chromium Copings with Shoulder and Chamfer Finish Lines: An In-Vitro Study
Background and Objectives: The aim was to compare the Misfit of 3D-Printed, Selective laser melting (SLM), milled (Computer aided design-Computer aided manufacture CAD-CAM) and Lost wax technique (LWT) fabricated Cobalt chromium (CoCr) alloy copings on shoulder (SH), radial shoulder (R-SH) and chamfer (CH) finish line configuration. Materials and Methods: Ninety resin, second maxillary premolar teeth were prepared for metal-ceramic crowns, equally divided into (n = 30) SH, R-SH and CH margin preparations. For each preparation design (SH, R-SH and CH), CoCr copings were prepared using SLM, CAD-CAM and LWT. This resulted in nine study groups with 10 CoCr copings each. The marginal misfit of specimens was assessed with a high-resolution digital microscope. Misfit was evaluated in vertical and horizontal dimensions in μm. Data were analyzed using ANOVA and a post hoc multiple comparisons test. Results: For vertical misfit, the highest was observed in SLM samples with chamfer margin (167.96 ± 24.1), and the least was shown by CAD-CAM samples with radial shoulder (58.8 ± 12.53). CAD-CAM and shoulder margins showed the least vertical misfit. For horizontal misfit, the maximum was observed in SLM samples with shoulder margin (137.94 ± 37.85) and the least by LWT samples with chamfer (89.38 ± 14.81). Chamfer margins and LWT samples showed the least horizontal misfit among the group samples. Fabrication technique and finish line design play a critical role in reducing the marginal misfit of CoCr copings. Conclusions: For vertical misfit, SLM copings showed poor outcomes compared to CAD-CAM specimens, however comparable outcomes to Cast specimens. SLM copings showed comparable horizontal misfit outcomes to CAD-CAM specimens and low misfit compared to Cast copings, respectively. Vertical misfit was low with shoulder margins, and horizontal misfit was better with chamfer marginal configuration.
Open AccessMarginal Misfit of 3D-Printed (Selective Laser Sintered), CAD-CAM and Lost Wax Technique Cobalt Chromium Copings with Shoulder and Chamfer Finish Lines: An In-Vitro Study
Background and Objectives: The aim was to compare the Misfit of 3D-Printed, Selective laser melting (SLM), milled (Computer aided design-Computer aided manufacture CAD-CAM) and Lost wax technique (LWT) fabricated Cobalt chromium (CoCr) alloy copings on shoulder (SH), radial shoulder (R-SH) and chamfer (CH) finish line configuration. Materials and Methods: Ninety resin, second maxillary premolar teeth were prepared for metal-ceramic crowns, equally divided into (n = 30) SH, R-SH and CH margin preparations. For each preparation design (SH, R-SH and CH), CoCr copings were prepared using SLM, CAD-CAM and LWT. This resulted in nine study groups with 10 CoCr copings each. The marginal misfit of specimens was assessed with a high-resolution digital microscope. Misfit was evaluated in vertical and horizontal dimensions in μm. Data were analyzed using ANOVA and a post hoc multiple comparisons test. Results: For vertical misfit, the highest was observed in SLM samples with chamfer margin (167.96 ± 24.1), and the least was shown by CAD-CAM samples with radial shoulder (58.8 ± 12.53). CAD-CAM and shoulder margins showed the least vertical misfit. For horizontal misfit, the maximum was observed in SLM samples with shoulder margin (137.94 ± 37.85) and the least by LWT samples with chamfer (89.38 ± 14.81). Chamfer margins and LWT samples showed the least horizontal misfit among the group samples. Fabrication technique and finish line design play a critical role in reducing the marginal misfit of CoCr copings. Conclusions: For vertical misfit, SLM copings showed poor outcomes compared to CAD-CAM specimens, however comparable outcomes to Cast specimens. SLM copings showed comparable horizontal misfit outcomes to CAD-CAM specimens and low misfit compared to Cast copings, respectively. Vertical misfit was low with shoulder margins, and horizontal misfit was better with chamfer marginal configuration.
- Open Access
Strength of Fiber Posts with Experimental TiO2 and ZrO2 Particle Bonding—An SEM, EDX, Rheometric and Push-Out Strength Study
The present study aimed to prepare experimental adhesives (EAs): 5 wt.% titanium dioxide (TiO2) adhesive; and 5 wt.% zirconium oxide (ZrO2) adhesive; and analyze their impact on bond integrity of fiber posts to root dentin, and viscosity. The EA was composed of: bisphenol A glycol dimethacrylate (BisGMA); triethylene glycol dimethacrylate (TEGDMA); 2-hydroxyethyl methacrylate (HEMA); and ethyl 4-dimethylamino benzoate and camphorquinone. TiO2 and ZrO2 particles were individually incorporated into the EA at 5 wt.%, to form two groups (5% TiO2 and 5% ZrO2). The adhesives, with particles, were characterized using scanning electron microscopy (SEM) and energy-dispersive X-ray (EDX) spectroscopy. The bonded interface was evaluated for adhesive–dentin penetration at the interface, using SEM. The study adhesive groups (EA, 5% TiO2 and 5% ZrO2) were analyzed for rheology and push-out bond strength of the fiber post to root dentin. Data were analyzed using analysis of variance and post hoc comparison. Both TiO2 and ZrO2 particles had irregular, non-uniform shapes. The EDX mapping showed the elemental presence of Ti (TiO2), Zr (ZrO2) and oxygen in formulated adhesives. The 5% TiO2 and 5% ZrO2 adhesives showed a decrease in viscosity, compared with the EA. Bond strength among the 5% TiO2 and 5% ZrO2 adhesives was statistically comparable (p > 0.05), but higher than the control group (10.57 ± 1.45 MPa) (p < 0.05). Reinforcement of the experimental dentin adhesive with 5% TiO2 or 5% ZrO2 increased the push-out bond strength of the fiber post to root dentin, in comparison with the EA. Particle-incorporated adhesives (5% TiO2 and 5% ZrO2) displayed decreased viscosity, compared with the EA (without particles).
Open AccessStrength of Fiber Posts with Experimental TiO2 and ZrO2 Particle Bonding—An SEM, EDX, Rheometric and Push-Out Strength Study
The present study aimed to prepare experimental adhesives (EAs): 5 wt.% titanium dioxide (TiO2) adhesive; and 5 wt.% zirconium oxide (ZrO2) adhesive; and analyze their impact on bond integrity of fiber posts to root dentin, and viscosity. The EA was composed of: bisphenol A glycol dimethacrylate (BisGMA); triethylene glycol dimethacrylate (TEGDMA); 2-hydroxyethyl methacrylate (HEMA); and ethyl 4-dimethylamino benzoate and camphorquinone. TiO2 and ZrO2 particles were individually incorporated into the EA at 5 wt.%, to form two groups (5% TiO2 and 5% ZrO2). The adhesives, with particles, were characterized using scanning electron microscopy (SEM) and energy-dispersive X-ray (EDX) spectroscopy. The bonded interface was evaluated for adhesive–dentin penetration at the interface, using SEM. The study adhesive groups (EA, 5% TiO2 and 5% ZrO2) were analyzed for rheology and push-out bond strength of the fiber post to root dentin. Data were analyzed using analysis of variance and post hoc comparison. Both TiO2 and ZrO2 particles had irregular, non-uniform shapes. The EDX mapping showed the elemental presence of Ti (TiO2), Zr (ZrO2) and oxygen in formulated adhesives. The 5% TiO2 and 5% ZrO2 adhesives showed a decrease in viscosity, compared with the EA. Bond strength among the 5% TiO2 and 5% ZrO2 adhesives was statistically comparable (p > 0.05), but higher than the control group (10.57 ± 1.45 MPa) (p < 0.05). Reinforcement of the experimental dentin adhesive with 5% TiO2 or 5% ZrO2 increased the push-out bond strength of the fiber post to root dentin, in comparison with the EA. Particle-incorporated adhesives (5% TiO2 and 5% ZrO2) displayed decreased viscosity, compared with the EA (without particles).
- Open Access
Polymer-Based Bioactive Luting Agents for Cementation of All-Ceramic Crowns: An SEM, EDX, Microleakage, Fracture Strength, and Color Stability Study
The aim of the study was to compare microleakage and fracture loads of all ceramic crowns luted with conventional polymer resins and polymeric bioactive cements and to assess the color stability of polymeric bioactive cements. Seventy-five extracted premolar teeth were tested for fracture loads and microleakage in all-ceramic crowns cemented with two types of polymeric bioactive cements and resin cements. In addition, the degree of color change for each cement with coffee was assessed. Thirty maxillary premolar teeth for fracture loads and thirty mandibular premolar teeth for microleakage were prepared; standardized teeth preparations were performed by a single experienced operator. All prepared specimens were randomly distributed to three groups (n = 20) based on the type of cement, Group 1: resin cement (Multilink N); Group 2: polymeric bioactive cement (ACTIVA); Group 3: polymeric bioactive cement (Ceramir). The cementation procedures for all cements (Multilink, ACTIVA, and Ceramir) were performed according to the manufacturers’ instructions. All specimens were aged using thermocycling for 30,000 cycles (5–55 °C, dwell time 30 s). These specimens were tested using the universal testing machine for fracture strength and with a micro-CT for microleakage. For the color stability evaluation, the cement specimens were immersed in coffee and evaluated with a spectrometer. Results: The highest and lowest means for fracture loads were observed in resin cements (49.5 ± 8.85) and Ceramir (39.8 ± 9.16), respectively. Ceramir (2.563 ± 0.71) showed the highest microleakage compared to resin (0.70 ± 0.75) and ACTIVA (0.61 ± 0.56). ACTIVA cements showed comparable fracture loads, microleakage, and stain resistance compared to resin cements.
Open AccessPolymer-Based Bioactive Luting Agents for Cementation of All-Ceramic Crowns: An SEM, EDX, Microleakage, Fracture Strength, and Color Stability Study
The aim of the study was to compare microleakage and fracture loads of all ceramic crowns luted with conventional polymer resins and polymeric bioactive cements and to assess the color stability of polymeric bioactive cements. Seventy-five extracted premolar teeth were tested for fracture loads and microleakage in all-ceramic crowns cemented with two types of polymeric bioactive cements and resin cements. In addition, the degree of color change for each cement with coffee was assessed. Thirty maxillary premolar teeth for fracture loads and thirty mandibular premolar teeth for microleakage were prepared; standardized teeth preparations were performed by a single experienced operator. All prepared specimens were randomly distributed to three groups (n = 20) based on the type of cement, Group 1: resin cement (Multilink N); Group 2: polymeric bioactive cement (ACTIVA); Group 3: polymeric bioactive cement (Ceramir). The cementation procedures for all cements (Multilink, ACTIVA, and Ceramir) were performed according to the manufacturers’ instructions. All specimens were aged using thermocycling for 30,000 cycles (5–55 °C, dwell time 30 s). These specimens were tested using the universal testing machine for fracture strength and with a micro-CT for microleakage. For the color stability evaluation, the cement specimens were immersed in coffee and evaluated with a spectrometer. Results: The highest and lowest means for fracture loads were observed in resin cements (49.5 ± 8.85) and Ceramir (39.8 ± 9.16), respectively. Ceramir (2.563 ± 0.71) showed the highest microleakage compared to resin (0.70 ± 0.75) and ACTIVA (0.61 ± 0.56). ACTIVA cements showed comparable fracture loads, microleakage, and stain resistance compared to resin cements.
- 1 December 2021
- Published by Elsevier in Photodiagnosis and Photodynamic Therapy
- Vol. 36, 102601
Effectiveness of synthetic and natural photosensitizers and different chemical disinfectants on the contaminated metal crown
- 1 December 2021
- Published by Elsevier in Photodiagnosis and Photodynamic Therapy
- Vol. 36, 102601
Effectiveness of synthetic and natural photosensitizers and different chemical disinfectants on the contaminated metal crown
- Open Access
Influence of TiO2 and ZrO2 Nanoparticles on Adhesive Bond Strength and Viscosity of Dentin Polymer: A Physical and Chemical Evaluation
The present study aimed to formulate an experimental adhesive (EA) and reinforce it with 5 wt.% titanium dioxide (TiO2) or zirconium oxide (ZrO2) to yield 5% TiO2 and 5% ZrO2 adhesives, respectively, and then analyze the impact of this reinforcement on various mechanical properties of the adhesives. The EA contained a blend of monomers such as bisphenol A glycol dimethacrylate (BisGMA), triethylene glycol dimethacrylate (TEGDMA), 2-hydroxyethyl methacrylate (HEMA), and ethyl 4-dimethylamino benzoate and camphorquinone. The EA included ethyl 4-dimethylamino benzoate and camphorquinone photo-initiators, and diphenyliodonium hexafluorophosphate (DPIHP) was also included to act as an electron initiator. The TiO2 and ZrO2 nanoparticles were incorporated into the EA post-synthesis. To characterize the filler nanoparticles, scanning electron microscopy (SEM) and line-energy dispersive X-ray (EDX) spectroscopy were performed. The adhesives were characterized by analyzing their rheological properties, shear-bond strength (SBS), and interfacial failure types. Further, the resin–dentin interface was also analyzed via SEM. The TiO2 nanoparticles were spherically shaped on the SEM micrographs, while the ZrO2 nanoparticles were seen as non-uniformly shaped agglomerates. The EDX mapping demonstrated the presence of Ti and oxygen for TiO2 and Zr and oxygen for the ZrO2 nanoparticles. Both 5% TiO2 and 5% ZrO2 adhesives revealed decreased viscosity as compared with the EA. The 5% TiO2 adhesive demonstrated higher SBS values for both non-thermocycled (NTC) and thermocycled samples (NTC: 25.35 ± 1.53, TC: 23.89 ± 1.95 MPa), followed by the 5% ZrO2 adhesive group (NTC: 23.10 ± 2.22, TC: 20.72 ± 1.32 MPa). The bulk of the failures (>70%) were of adhesive type in all groups. The SEM analysis of the resin–dentin interface revealed the development of a hybrid layer and resin tags (of variable depth) for the EA and 5% TiO2 groups. However, for the 5% ZrO2 group, the hybrid layer and resin tag establishment appeared compromised. Reinforcement of the EA with TiO2 or ZrO2 caused an increase in the adhesive’s SBS (with the 5% TiO2 group demonstrating the highest values) in comparison with the EA (without nanoparticles). However, both nanoparticle-containing adhesives revealed decreased viscosity compared with the EA (without nanoparticles). Further studies investigating the impact of diverse filler concentrations on the properties of adhesives are suggested.
Open AccessInfluence of TiO2 and ZrO2 Nanoparticles on Adhesive Bond Strength and Viscosity of Dentin Polymer: A Physical and Chemical Evaluation
The present study aimed to formulate an experimental adhesive (EA) and reinforce it with 5 wt.% titanium dioxide (TiO2) or zirconium oxide (ZrO2) to yield 5% TiO2 and 5% ZrO2 adhesives, respectively, and then analyze the impact of this reinforcement on various mechanical properties of the adhesives. The EA contained a blend of monomers such as bisphenol A glycol dimethacrylate (BisGMA), triethylene glycol dimethacrylate (TEGDMA), 2-hydroxyethyl methacrylate (HEMA), and ethyl 4-dimethylamino benzoate and camphorquinone. The EA included ethyl 4-dimethylamino benzoate and camphorquinone photo-initiators, and diphenyliodonium hexafluorophosphate (DPIHP) was also included to act as an electron initiator. The TiO2 and ZrO2 nanoparticles were incorporated into the EA post-synthesis. To characterize the filler nanoparticles, scanning electron microscopy (SEM) and line-energy dispersive X-ray (EDX) spectroscopy were performed. The adhesives were characterized by analyzing their rheological properties, shear-bond strength (SBS), and interfacial failure types. Further, the resin–dentin interface was also analyzed via SEM. The TiO2 nanoparticles were spherically shaped on the SEM micrographs, while the ZrO2 nanoparticles were seen as non-uniformly shaped agglomerates. The EDX mapping demonstrated the presence of Ti and oxygen for TiO2 and Zr and oxygen for the ZrO2 nanoparticles. Both 5% TiO2 and 5% ZrO2 adhesives revealed decreased viscosity as compared with the EA. The 5% TiO2 adhesive demonstrated higher SBS values for both non-thermocycled (NTC) and thermocycled samples (NTC: 25.35 ± 1.53, TC: 23.89 ± 1.95 MPa), followed by the 5% ZrO2 adhesive group (NTC: 23.10 ± 2.22, TC: 20.72 ± 1.32 MPa). The bulk of the failures (>70%) were of adhesive type in all groups. The SEM analysis of the resin–dentin interface revealed the development of a hybrid layer and resin tags (of variable depth) for the EA and 5% TiO2 groups. However, for the 5% ZrO2 group, the hybrid layer and resin tag establishment appeared compromised. Reinforcement of the EA with TiO2 or ZrO2 caused an increase in the adhesive’s SBS (with the 5% TiO2 group demonstrating the highest values) in comparison with the EA (without nanoparticles). However, both nanoparticle-containing adhesives revealed decreased viscosity compared with the EA (without nanoparticles). Further studies investigating the impact of diverse filler concentrations on the properties of adhesives are suggested.
- Open Access
- 28 October 2021
- Published by MDPI AG in Applied Sciences
- Vol. 11 (21) , 10108
Evaluation of Smart Chromatic Technology for a Single-Shade Dental Polymer Resin: An In Vitro Study
The aim of the study was to assess the color matching ability and color stability of a single-shade resin-based composite (Omnichroma—OM) in comparison to a conventional dental composite. One hundred and sixty lower molar acrylic teeth in four different shades (B1, B2, A3, and C3) were prepared with class I cavities. Eighty teeth were divided into two groups based on the two resin composite materials (OM and Filtek Z-350 (FT)) for cavity restoration. Three groups were included in the color matching assessment, namely Gp 1-FT, Gp 2-OM-light cured (C), and Gp 3-OM-uncured (UC) groups. The color assessment was performed prior to cavity restoration and after cavity filling and before and after light curing to detect color matching. The 80 remaining teeth were restored with OM (n = 40) and FT (n = 40); half (n = 40) were submerged in coffee and the other half (n = 40) were submerged in cola for 2 weeks. The color stability was assessed by calculating material color (spectrophotometry) changes (∆E) before and after staining in immersion medium. The means and standard deviations of the ∆E values relating to color matching and color stability (stain resistance) among the study groups were analyzed using ANOVA and Tukey’s post hoc test. FT showed significantly better color matching (lower ΔE) in comparison to OM-UC specimens for shades B1, B2, and A3 (p < 0.01). Regarding the color stability in cola, the FT samples showed significantly lower ΔE values (indicating better color stability) compared to OM samples for all four shades (p < 0.01). The ΔE values of OM and FT samples in coffee were comparable (p > 0.01), showing comparable color stability. The color matching ability of the single-shade resin composite (OM) was influenced by the tooth color. The conventional resin composite showed better color matching than the single-shade composite (OM). The color stability of the single-shade resin composite (OM) was dependent on the staining medium. The OM composite showed more compromised color stability than the conventional resin composite in cola and comparable color stability to conventional resin composite in coffee.
- 28 October 2021
- Published by MDPI AG in Applied Sciences
- Vol. 11 (21) , 10108
Open AccessEvaluation of Smart Chromatic Technology for a Single-Shade Dental Polymer Resin: An In Vitro Study
The aim of the study was to assess the color matching ability and color stability of a single-shade resin-based composite (Omnichroma—OM) in comparison to a conventional dental composite. One hundred and sixty lower molar acrylic teeth in four different shades (B1, B2, A3, and C3) were prepared with class I cavities. Eighty teeth were divided into two groups based on the two resin composite materials (OM and Filtek Z-350 (FT)) for cavity restoration. Three groups were included in the color matching assessment, namely Gp 1-FT, Gp 2-OM-light cured (C), and Gp 3-OM-uncured (UC) groups. The color assessment was performed prior to cavity restoration and after cavity filling and before and after light curing to detect color matching. The 80 remaining teeth were restored with OM (n = 40) and FT (n = 40); half (n = 40) were submerged in coffee and the other half (n = 40) were submerged in cola for 2 weeks. The color stability was assessed by calculating material color (spectrophotometry) changes (∆E) before and after staining in immersion medium. The means and standard deviations of the ∆E values relating to color matching and color stability (stain resistance) among the study groups were analyzed using ANOVA and Tukey’s post hoc test. FT showed significantly better color matching (lower ΔE) in comparison to OM-UC specimens for shades B1, B2, and A3 (p < 0.01). Regarding the color stability in cola, the FT samples showed significantly lower ΔE values (indicating better color stability) compared to OM samples for all four shades (p < 0.01). The ΔE values of OM and FT samples in coffee were comparable (p > 0.01), showing comparable color stability. The color matching ability of the single-shade resin composite (OM) was influenced by the tooth color. The conventional resin composite showed better color matching than the single-shade composite (OM). The color stability of the single-shade resin composite (OM) was dependent on the staining medium. The OM composite showed more compromised color stability than the conventional resin composite in cola and comparable color stability to conventional resin composite in coffee.
- Open Access
- 8 September 2021
- Published by MDPI AG in Applied Sciences
- Vol. 11 (18) , 8328
Comparison of Marginal Integrity and Surface Roughness of Selective Laser Melting, CAD-CAM and Digital Light Processing Manufactured Co-Cr Alloy Copings
The purpose of the present study was to evaluate the influence of fabrication techniques on the surface micro-roughness (Ra) and marginal misfit of cobalt chromium (CoCr) copings. A mandibular first molar was prepared for a metal ceramic crown. Forty metal copings were prepared and divided into groups (n = 10). Group 1, Casting-Lost wax technique (Cast-LWT), Group 2, CAD-CAM, Group 3, Selective laser melting (SLM), and Group 4, Digital light processing-Cast (DLP-Cast). Ra was measured using laser profilometry and marginal misfit was analyzed with Micro-CT. Analysis of variance (ANOVA), Tukey multiple comparison, and correlation coefficient tests were applied (p < 0.05). SLM technique showed the highest Ra (2.251 ± 0.310 μm) and the Cast-LWT group presented the lowest Ra (1.055 ± 0.184 μm). CAD-CAM copings showed statistically lower Ra compared with SLM samples (p = 0.028), but comparable Ra to DLP-Cast (p > 0.05). CoCr copings fabricated from the DLP-Cast technique demonstrated the highest marginal misfit (147.746 ± 30.306 μm) and the lowest misfit was established by SLM copings (27.193 ± 8.519 μm). The SLM technique displayed lower marginal misfit than DLP-Cast and CAD-CAM (p = 0.001), but comparable misfit to Cast-LWT copings. Ra influenced the marginal misfit in CAD-CAM, SLM, and DLP-Cast technique-fabricated copings. (p < 0.01). Marginal misfit and Ra of CoCr copings are contingent on the different fabrication techniques.
- 8 September 2021
- Published by MDPI AG in Applied Sciences
- Vol. 11 (18) , 8328
Open AccessComparison of Marginal Integrity and Surface Roughness of Selective Laser Melting, CAD-CAM and Digital Light Processing Manufactured Co-Cr Alloy Copings
The purpose of the present study was to evaluate the influence of fabrication techniques on the surface micro-roughness (Ra) and marginal misfit of cobalt chromium (CoCr) copings. A mandibular first molar was prepared for a metal ceramic crown. Forty metal copings were prepared and divided into groups (n = 10). Group 1, Casting-Lost wax technique (Cast-LWT), Group 2, CAD-CAM, Group 3, Selective laser melting (SLM), and Group 4, Digital light processing-Cast (DLP-Cast). Ra was measured using laser profilometry and marginal misfit was analyzed with Micro-CT. Analysis of variance (ANOVA), Tukey multiple comparison, and correlation coefficient tests were applied (p < 0.05). SLM technique showed the highest Ra (2.251 ± 0.310 μm) and the Cast-LWT group presented the lowest Ra (1.055 ± 0.184 μm). CAD-CAM copings showed statistically lower Ra compared with SLM samples (p = 0.028), but comparable Ra to DLP-Cast (p > 0.05). CoCr copings fabricated from the DLP-Cast technique demonstrated the highest marginal misfit (147.746 ± 30.306 μm) and the lowest misfit was established by SLM copings (27.193 ± 8.519 μm). The SLM technique displayed lower marginal misfit than DLP-Cast and CAD-CAM (p = 0.001), but comparable misfit to Cast-LWT copings. Ra influenced the marginal misfit in CAD-CAM, SLM, and DLP-Cast technique-fabricated copings. (p < 0.01). Marginal misfit and Ra of CoCr copings are contingent on the different fabrication techniques.
- Open Access
Application of β-Tricalcium Phosphate in Adhesive Dentin Bonding
The study aimed at synthesizing β-tricalcium phosphate (β-TCP) nanoparticles and comparing the mechanical properties and dentin interaction of two adhesives: experimental adhesive (EA) and EA with 5 wt.% β-TCP nanoparticles (β-TCP-5%). These filler nanoparticles were synthesized and then characterized with scanning electron microscopy (SEM) and micro-Raman spectroscopy. The β-TCP nanoparticles were incorporated in the adhesives to form two groups: gp-1: EA (control) and gp-2: β-TCP-5%. These adhesives were characterized by SEM, energy-dispersive X-ray (EDX) spectroscopy and were also assessed for their micro-tensile bond strength (μTBS) with (TC) and without thermocycling (NTC). Fourier Transform Infrared (FTIR) spectroscopy was performed to evaluate the degree of conversion (DC) of two adhesives. The β-TCP filler was seen as irregularly shaped agglomerates on SEM. The micro-Raman spectra revealed characteristic peaks associated with β-TCP nanoparticles. Both adhesives presented suitable dentin interaction, which was demonstrated by the formation of resin tags of variable depths. The EDX analysis verified the existence of calcium (Ca) and phosphate (P) for the β-TCP-5% group. The greatest μTBS values were shown by β-TCP-5% group samples when they were non-thermocycled (NTC) (β-TCP-5%-NTC: 34.11 ± 3.46) followed by the thermocycled (TC) samples of the same group (β-TCP-5%-TC: 30.38 ± 3.66), compared with the EA group. Although the DC presented by β-TCP-5% group was comparable to the EA group, it was still lower. The addition of β-TCP nanoparticles in the adhesive improved its μTBS and resulted in a suitable dentin interaction, seen in the form of hybrid layer and resin tag formation. Nonetheless, a decreased DC was observed for the β-TCP-5% adhesive. Future studies probing the effect of different filler concentrations on various properties of the adhesive are warranted.
Open AccessApplication of β-Tricalcium Phosphate in Adhesive Dentin Bonding
The study aimed at synthesizing β-tricalcium phosphate (β-TCP) nanoparticles and comparing the mechanical properties and dentin interaction of two adhesives: experimental adhesive (EA) and EA with 5 wt.% β-TCP nanoparticles (β-TCP-5%). These filler nanoparticles were synthesized and then characterized with scanning electron microscopy (SEM) and micro-Raman spectroscopy. The β-TCP nanoparticles were incorporated in the adhesives to form two groups: gp-1: EA (control) and gp-2: β-TCP-5%. These adhesives were characterized by SEM, energy-dispersive X-ray (EDX) spectroscopy and were also assessed for their micro-tensile bond strength (μTBS) with (TC) and without thermocycling (NTC). Fourier Transform Infrared (FTIR) spectroscopy was performed to evaluate the degree of conversion (DC) of two adhesives. The β-TCP filler was seen as irregularly shaped agglomerates on SEM. The micro-Raman spectra revealed characteristic peaks associated with β-TCP nanoparticles. Both adhesives presented suitable dentin interaction, which was demonstrated by the formation of resin tags of variable depths. The EDX analysis verified the existence of calcium (Ca) and phosphate (P) for the β-TCP-5% group. The greatest μTBS values were shown by β-TCP-5% group samples when they were non-thermocycled (NTC) (β-TCP-5%-NTC: 34.11 ± 3.46) followed by the thermocycled (TC) samples of the same group (β-TCP-5%-TC: 30.38 ± 3.66), compared with the EA group. Although the DC presented by β-TCP-5% group was comparable to the EA group, it was still lower. The addition of β-TCP nanoparticles in the adhesive improved its μTBS and resulted in a suitable dentin interaction, seen in the form of hybrid layer and resin tag formation. Nonetheless, a decreased DC was observed for the β-TCP-5% adhesive. Future studies probing the effect of different filler concentrations on various properties of the adhesive are warranted.