DVDmytro V. Vedel

Dmytro V. Vedel

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Dmytro V. Vedel has a total of 127 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Oxidation behavior of Ta-free high entropy (Mo, W, Ti, Nb)Si2 up to 1400 °C

    by D. Vedel, V. Sheremet, M. Gorban, M. Kovalenko, S. Teslia

  • Effect of processing route on the oxidation resistance of ultra-high-temperature (Zr, Mo)B₂ ceramics

    by Dmytro Vedel, Anton Osipov, Petro Mazur, Mykola Skoryk, Małgorzata Pomorska, Jerzy Morgiel

  • Open Access

    Optimization of production of high-entropy flux-cored welding wire

    by J. Junwen, A. V. Klapatyuk, D. V. Vedel, O. H. Pashynskaya, V. I. Kopylov, A. V. Zavdoveev, N. M. Strelenko

    Metal cored wire with a sheath opens a practical way to obtain high-entropy alloys (HEAs) in arc additive manufacturing. At the same time, the choice of the final wire diameter is mostly based on empirical rules: a decrease in diameter contributes to the densification of the powder core and stabilization of the composition, but can cause crumpling of the sheath, surface microcracks or through-hole fracture, which worsens the wire feed and the stability of the deposition process. In the work, an evaluation system based on the filling factor Kz and elongation ∆L is proposed for multi-pass drawing of HEAs powder wire. Comparison of macrogeometry, surface micromorphology and statistical indicators for the same wire at different final diameters shows that Kz changes non-monotonically with decreasing diameter, while ∆L first increases and then decreases and exhibits fracture under excessive drawing, which indicates the transition of the sheath to unstable deformation. Based on the experiments conducted, the optimal diameter of the flux-cored wire was established for such a Kz

  • Open Access

    Oxidation behavior of Ta-free high entropy (Mo, W, Ti, Nb)Si2 up to 1400 °C

    by Dmitry Vedel, Vitalii Sheremet, M. Gorban, M. Kovalenko, Sergii Teslia

    This study reports, for the first time, the oxidation behavior of Ta-free (Mo, W, Ti, Nb)Si2 in air up to 1400 ºC. The material, produced by spark-plasma sintering at 1450 ºC and 60 MPa (porosity ~4.5 %), consists of a C40-type high-entropy disilicide matrix with minor C11b (W, Mo)Si2. DSC/TGA and non-isothermal furnaces oxidation tests at 600-1400 ºC, combined XRD and SEM/EDS showed that oxidation starts at ~270 ºC without pest degradation or mass loss, the total mass gain not exceeding ~2.3 %. A four-stage mechanism was proposed. Ti and Nb oxidize preferentially, forming a silica-rich scale with rutile-type (Ti, Nb)O2, while a transient Nb-W-O phase binds W and prevents WO3 volatilization. Above 1200 ºC a continuous ~10 µm SiO2-based scale provides passive protection. Ti does not degrade oxidation resistance, and the combination of Nb, W and Ti can partly replace Ta in high-entropy disilicides.

  • High temperature oxidation resistance of medium-entropy diboride ceramics based on (Zr, Hf)B2 solid solution

    by D. V. Vedel, P. V. Mazur, Ya. V. Ilnitska, M. A. Skoryk

    High-temperature oxidation resistance of medium-entropy diboride ceramics based on (Zr, Hf)В2 solid solutions alloyed with TiВ2, NbВ2 and TaВ2 was investigated. Samples were produced by hot pressing and subjected to oxidation at 1500C in air. It is found that ceramic oxidation has a selective mechanism and depends on the individual resistance of each diboride. The addition of Ti reduces oxidation resistance due to the intense formation of a liquid phase during oxidation, which leads to the formation of a thick, heteroge¬neous scale. Alloying with NbВ2 and TaВ2 promotes the formation of thinner oxide layers, but the oxidation mechanisms differ in the case of Nb, a liquid phase is present, whereas TaВ2 forms a dense surface layer of Ta2O5, which effectively reduces oxygen diffusion. The obtained results allow us to clarify the oxidation mechanisms of medium-entropy boride ceramics and identify promising areas for their further improvement.

  • Thermal protection of aircraft at extremely high temperatures

    by I. O. Husarova, O. M. Grigoriev, D. V. Vedel, M. V. Kraiev, T. A. Manko, K. V. Kozis, G. G. Osinovyy

    А comparative analysis of heat-shielding coatings of rocket and space technology is carried out, and the prospects for the use of ultrahigh-temperature ceramics as heat-resis¬tant coatings for elements of hypersonic aircraft, in particular, nose сone and wing edges, are considered. A coating based on the ZrB2-MoSi2 ceramic system was obtained by vacuum-arc deposition on a carbon substrate. It is shown that the formed coating has a homogeneous structure, low oxygen content (< 2 mass%), and satis¬factory adhesion to the substrate, which is associated with close coefficients of thermal expansion of the compo¬nents. The technology of vacuum ion-plasma spraying of ZrB2-MoSi2 coatings is promi¬sing for increasing the temperature resistance of carbon structures under conditions of short-term thermal load in an oxidizing environment at extremely high temperatures.

  • Open Access

    THE EFFECT OF DEFECTS OF VARIOUS GENESIS ON THE PROPERTIES OF CARBON NANOTUBES

    by Halyna Mykhailova, Mykola Shevchenko, Ihor Danylenko, Mykola Skoryk, Dmitry Vedel, Vitaliy Lebed, Volodymyr Koda, Evgen Len

    We investigate how growth-related and γ-radiation-induced defects jointly control the electrical, thermoelectric, and elastic response of bulk arrays of highly defective multiwalled carbon nanotubes (MWCNTs). The MWCNT arrays were irradiated by 1.2 MeV γ-quanta in the dose range (1.63–32.8)×10¹⁶ γ/cm². Defect evolution was tracked by Raman spectroscopy (λ = 532 nm), SEM, and EDX, while the electrical conductivity and thermo-EMF (Seebeck coefficient) were measured under moderate compression, i.e., in the regime where transport is governed by percolation through intertube junctions and their tunneling or contact barriers. The dose response is nonmonotonic: conductivity increases quasi-linearly at low doses and reaches a broad maximum near 17.08×10¹⁶ γ/cm², followed by a slight decrease at 32.8×10¹⁶ γ/cm². Raman data indicate that γ-irradiation does not merely accumulate disorder: the smallest dose produces a sharp increase of the effective size of ordered sp²-regiones, consistent with deoxygenation and partial reconstruction of growth defects, whereas the intermediate dose ∼4.51×1016 γ/cm²) corresponds to the maximum spatial heterogeneity (largest line widths and scatter of the parameters throughout the sample), and the highest doses promote morphological thinning and loosening (seen by SEM). At the microscopic level, topological rearrangements of graphene layers of different genesis (growth and radiation), together with vacancy-type disorder, alter MWCNT curvature and junction geometry and thereby reshape the percolation and contact-barrier landscape that governs both conductivity and thermo-EMF. Overall, transport is controlled by the coupled evolution of intertube contacts and intratube defects under competition between partial healing and radiation damage.

  • Open Access

    Strain Rate Influence on Mechanical Behaviour of Ti-6Al-4V Reinforced with TiC or TiB Composites Produced by Sintering and Hot Isostatic Pressure on Compression

    by Judyta Sienkiewicz, Bartosz Fikus, Jacek Janiszewski, O.O. Stasyuk, Dmitry Vedel, Pavlo Markovsky

    Layered metal matrix composites were produced using the Blended Elemental Powder Metallurgy technology, followed by hot isostatic pressing (HIP). Two three-layer samples were made, consisting of a matrix based on Ti-6Al-V (wt.%) (Ti64) alloy. Each individual layer/tile was synthesized with BEPM and reinforced by 10, 20, or 40 vol. %, respectively, of TiC or TiB particles. The use of HIP effectively bonded individual MMC tiles into cohesive, dense three-layer samples, also leading to the nearly complete elimination of residual porosity. Quasi-static compression tests were performed at strain rates of 10-3 s-1 and 10-1 s-1. Dynamic tests were utilized the split Hopkinson pressure bar method, with the strain rates ranging from approximately 2500 s-1 to 4600 s-1. For MMC with TiC, these features are associated with the formation of large conglomerates of carbide phase particles both at the synthesis stage and during long-term isothermal holding under load during HIP. During compression testing, the main deformation localizes within TiC particles, leading to their crumbling and subsequent destruction of the matrix phase bridges between them. In MMC with TiB, the strengthening particles are more dispersed, and there is a simultaneous existence of relatively coarser residues of untransformed TiB2 particles and dispersed titanium monoboride particles that appeared as a result of the interaction of diboride with the titanium matrix. The enhanced resistance to destruction at higher strain rates for MMC strengthened by TiB2 and TiB is attributed to their more homogenously dispersed structure compared to MMC strengthened by TiC.

  • High-temperature properties of ZrB2–HfB2 and ZrB2–HfB2–SiC solid solutions

    by D. V. Vedel, P. V. Mazur, І. V. Kozak, А. Ye. Osipov, М. P. Brodnikovskyi

    Solid (ZrxHf1–х)B2 and (ZrxHf1–х)B2–15 vol.% SiC composites were obtained by hot pressing. It was shown that the formation of homogeneous solid solution occurs at an equimolar ratio. The coreshell structure was formed in composite with 25 and 75 at.% HfB2. In the first case, the core was pure zirconium diboride, and in the second – pure hafnium diboride. The shell composition corresponded to the chemical formula (Zr0.75Hf0.25)B2 or (Zr0.25Hf0.75)B2, respectively. The formation of an equimolar solid solution results in a 28% increase in high temperature bending strength in comparison to ZrB2–15 vol.% SiC or HfB2–15 vol.% SiC. At the same time, high oxidation resistance is observed in a solid solution close to hafnium diboride due to the formation of the (Hf0.75Zr0.25)SiO4 and HfSiO4 phases on the scale surface, which reduce the diffusion of oxygen into the material