Miaomiao Ma
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Miaomiao Ma has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
Aleksei La Rue
Department of Electrical Engineering, Colorado School of Mines, Golden, Colorado 80401, USA
1 shared publicationAzzam N. Mansour
Naval Surface Warfare Center, Carderock Division, West Bethesda, Maryland 20817-5700, United States of America
1 shared publication- Charlotte Michele Thomas
University of Colorado, Boulder
1 shared publication - Christopher E. Hendricks
Naval Surface Warfare Center Carderock Division, Bethesda, Maryland 20817, USA
1 shared publication - Christopher E. Hendricks
Naval Surface Warfare Center, Carderock Division, West Bethesda, Maryland 20817-5700, United States of America
1 shared publication - Chunmei Ban
Paul M. Rady Department of Mechanical Engineering College of Engineering and Applied Science University of Colorado Boulder Boulder Colorado USA
1 shared publication
Latest Publications
- Open Access
- 10 November 2026
- Published by Wiley in Small Structures
- Vol. 7 (11)
Dual‐Function Ammonium Treatment for Robust Prussian White Cathodes
Prussian White (PW, Na2Mn[Fe(CN)6]) is a promising low‐cost cathode material for sodium‐ion batteries, yet its performance is limited by structural degradation associated with phase transitions, vacancy defects, and sensitivity to moisture. Here, a low‐cost postsynthesis NH 4 + doping strategy is introduced to simultaneously enhance the structural integrity and environmental stability of the material. NH 4 + is incorporated into PW following a neutral aqueous coprecipitation reaction, inducing a stable monoclinic structure distinct from the moisture‐dependent monoclinic phase observed in pristine PW. This structural stabilization facilitates reversible Na + intercalation/deintercalation while mitigating detrimental water interactions. Consequently, NH 4 + ‐doped PW (PW–NH 4 ) exhibits improved capacity retention, reduced polarization, and enhanced rate capability compared with pristine PW. Postmortem spectroscopy confirms that NH 4 + remains within the structure after 200 cycles, supporting its persistent role in stabilizing the framework during cycling. Furthermore, PW–NH 4 demonstrates significantly improved tolerance to atmospheric rehydration. These findings show that NH 4 + is a dual‐function dopant that structurally stabilizes PW and suppresses water‐induced degradation, offering a safe and scalable route to robust cathode materials for sodium‐ion batteries.
- 10 November 2026
- Published by Wiley in Small Structures
- Vol. 7 (11)
Open AccessDual‐Function Ammonium Treatment for Robust Prussian White Cathodes
Prussian White (PW, Na2Mn[Fe(CN)6]) is a promising low‐cost cathode material for sodium‐ion batteries, yet its performance is limited by structural degradation associated with phase transitions, vacancy defects, and sensitivity to moisture. Here, a low‐cost postsynthesis NH 4 + doping strategy is introduced to simultaneously enhance the structural integrity and environmental stability of the material. NH 4 + is incorporated into PW following a neutral aqueous coprecipitation reaction, inducing a stable monoclinic structure distinct from the moisture‐dependent monoclinic phase observed in pristine PW. This structural stabilization facilitates reversible Na + intercalation/deintercalation while mitigating detrimental water interactions. Consequently, NH 4 + ‐doped PW (PW–NH 4 ) exhibits improved capacity retention, reduced polarization, and enhanced rate capability compared with pristine PW. Postmortem spectroscopy confirms that NH 4 + remains within the structure after 200 cycles, supporting its persistent role in stabilizing the framework during cycling. Furthermore, PW–NH 4 demonstrates significantly improved tolerance to atmospheric rehydration. These findings show that NH 4 + is a dual‐function dopant that structurally stabilizes PW and suppresses water‐induced degradation, offering a safe and scalable route to robust cathode materials for sodium‐ion batteries.
- 20 April 2021
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 168 (5) , 050519
Interpretation and Modelling of the Electrochemical Impedance of LiFePO 4 /Li 4 Ti 5 O 12 Batteries
In this work, a comprehensive equivalent circuit model (ECM) was developed for the a commercial 26650 LiFePO 4 /Li 4 Ti 5 O 12 cell in which the main processes at the anode and cathode electrodes and their contributions to the full-cell impedance were investigated and quantified separately. To unambiguously separate the anode and cathode processes, EIS spectra from Li 4 Ti 5 O 12 /Li and LiFePO 4 /Li half cells were modeled at different state of charge (SOC) and SOC history and the fit results were used to develop the full-cell ECM. The distribution of relaxation times (DRT) analysis was used in all cases to better resolve the frequencies of the processes, and thereby help their accurate identification. The LiFePO 4 /Li 4 Ti 5 O 12 -cell impedance was found to be significantly dependant on the SOC history, i.e. it changes slightly only at low SOCs during charge, whereas, it changes significantly during discharge. The SOC-dependence of the full-cell impedance was found to be mainly due to the decrease of the LiFePO 4 electrode’s charge transfer resistance with SOC increase. While Li 4 Ti 5 O 12 electrode processes did not show a significant change with SOC history, it was revealed that the SOC-histoty dependence of the LiFePO 4 /Li 4 Ti 5 O 12 full cell was also mainly due to the variation of charge transfer frequency and resistance of LiFePO 4 electrode.
- 20 April 2021
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 168 (5) , 050519
Interpretation and Modelling of the Electrochemical Impedance of LiFePO 4 /Li 4 Ti 5 O 12 Batteries
In this work, a comprehensive equivalent circuit model (ECM) was developed for the a commercial 26650 LiFePO 4 /Li 4 Ti 5 O 12 cell in which the main processes at the anode and cathode electrodes and their contributions to the full-cell impedance were investigated and quantified separately. To unambiguously separate the anode and cathode processes, EIS spectra from Li 4 Ti 5 O 12 /Li and LiFePO 4 /Li half cells were modeled at different state of charge (SOC) and SOC history and the fit results were used to develop the full-cell ECM. The distribution of relaxation times (DRT) analysis was used in all cases to better resolve the frequencies of the processes, and thereby help their accurate identification. The LiFePO 4 /Li 4 Ti 5 O 12 -cell impedance was found to be significantly dependant on the SOC history, i.e. it changes slightly only at low SOCs during charge, whereas, it changes significantly during discharge. The SOC-dependence of the full-cell impedance was found to be mainly due to the decrease of the LiFePO 4 electrode’s charge transfer resistance with SOC increase. While Li 4 Ti 5 O 12 electrode processes did not show a significant change with SOC history, it was revealed that the SOC-histoty dependence of the LiFePO 4 /Li 4 Ti 5 O 12 full cell was also mainly due to the variation of charge transfer frequency and resistance of LiFePO 4 electrode.
- Open Access
- 8 January 2020
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 167 (11) , 110549
Characterization of Li Diffusion and Solid Electrolyte Interface for Li4Ti5O12 Electrode Cycled with an Organosilicon Additive Electrolyte
The use of lithium titanate (Li4Ti5O12, LTO) for the negative electrode in lithium ion batteries has attracted enormous attention owing to its fast charging capability, high power, safe operating voltage window and stable structure (“zero strain”) during cycling. Researchers have investigated the formation of the solid electrolyte interface (SEI) of the LTO electrode, which prevents gassing issue and leads to longer cycle life. In this study, the solid-state diffusion property of LTO at room temperature was characterized using AC impedance spectroscopy at different states of charge (SOC) during charge and discharge to reveal the dependency of the lithium diffusion coefficient on SOC. Meanwhile the formation and growth of the solid electrolyte interface (SEI) on the LTO electrode using an electrolyte containing Silatronix OS3® additive were investigated using X-ray photoelectron spectroscopy (XPS). The composition of the SEI and its evolution due to cycling with the OS3® additive was compared to that with a commercial electrolyte. Half-cell coin cells of LTO vs lithium metal were formed and cycled at room temperature for over 200 cycles, where the resistance increase, as measured by impedance spectroscopy, is correlated to the SEI growth. Electrode samples were analyzed in the pristine state, after formation, and after 200 cycles. XPS results showed that a thin layer of SEI is formed during the first two formation cycles and the composition of the SEI on the surface of the LTO electrode varied with increasing cycle number. Based on the escape depths of Ti 3 s and Ti 2p regions, the SEI after formation is thicker than 5.5 nm but is less than 7.0 nm for both the OS3® and A7 electrolytes. Based on Ar-ion depth profiling, the SEI thickness in terms of the equivalent thickness of SiO2 after 200 cycles in coin cell configuration is estimated to be near 14 nm for both the OS3® and A7 electrolytes. A much higher fluorine content (F 1s peak) was found in the SEI formed with the OS3® electrolyte than the SEI formed with the commercial A7 electrolyte.
- 8 January 2020
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 167 (11) , 110549
Open AccessCharacterization of Li Diffusion and Solid Electrolyte Interface for Li4Ti5O12 Electrode Cycled with an Organosilicon Additive Electrolyte
The use of lithium titanate (Li4Ti5O12, LTO) for the negative electrode in lithium ion batteries has attracted enormous attention owing to its fast charging capability, high power, safe operating voltage window and stable structure (“zero strain”) during cycling. Researchers have investigated the formation of the solid electrolyte interface (SEI) of the LTO electrode, which prevents gassing issue and leads to longer cycle life. In this study, the solid-state diffusion property of LTO at room temperature was characterized using AC impedance spectroscopy at different states of charge (SOC) during charge and discharge to reveal the dependency of the lithium diffusion coefficient on SOC. Meanwhile the formation and growth of the solid electrolyte interface (SEI) on the LTO electrode using an electrolyte containing Silatronix OS3® additive were investigated using X-ray photoelectron spectroscopy (XPS). The composition of the SEI and its evolution due to cycling with the OS3® additive was compared to that with a commercial electrolyte. Half-cell coin cells of LTO vs lithium metal were formed and cycled at room temperature for over 200 cycles, where the resistance increase, as measured by impedance spectroscopy, is correlated to the SEI growth. Electrode samples were analyzed in the pristine state, after formation, and after 200 cycles. XPS results showed that a thin layer of SEI is formed during the first two formation cycles and the composition of the SEI on the surface of the LTO electrode varied with increasing cycle number. Based on the escape depths of Ti 3 s and Ti 2p regions, the SEI after formation is thicker than 5.5 nm but is less than 7.0 nm for both the OS3® and A7 electrolytes. Based on Ar-ion depth profiling, the SEI thickness in terms of the equivalent thickness of SiO2 after 200 cycles in coin cell configuration is estimated to be near 14 nm for both the OS3® and A7 electrolytes. A much higher fluorine content (F 1s peak) was found in the SEI formed with the OS3® electrolyte than the SEI formed with the commercial A7 electrolyte.
- 3 December 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 166 (16) , A4041-A4046
State-of-Charge Estimation of LiFePO4–Li4Ti5O12Batteries using History-Dependent Complex-Impedance
The present paper seeks to extract, analyze, and interpret the electrochemical impedance spectra of a LiFePO4-Li4Ti5O12 battery to supplement state-of-charge estimation. A particular challenge in determining the state-of-charge of a LiFePO4-Li4Ti5O12 cell is that the open-circuit voltage is flat over a large range of states of charge. Because the voltage in standard batteries is typically used to inform state-of-charge estimation, a different corrective factor needs to be determined for this cell chemistry. Instead of using the battery voltage, the present study uses the battery’s dynamic response to assist state of charge estimation. The present work includes at least three novel contributions: 1) the electrochemical impedance of the LiFePO4-Li4Ti5O12 cell is shown to be strongly history dependent, 2) a novel system-identification technique is implemented to extract the EIS in-situ, and 3) a signature electrochemical impedance spectra attribute is identified that is a strong function of battery state of charge.
- 3 December 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 166 (16) , A4041-A4046
State-of-Charge Estimation of LiFePO4–Li4Ti5O12Batteries using History-Dependent Complex-Impedance
The present paper seeks to extract, analyze, and interpret the electrochemical impedance spectra of a LiFePO4-Li4Ti5O12 battery to supplement state-of-charge estimation. A particular challenge in determining the state-of-charge of a LiFePO4-Li4Ti5O12 cell is that the open-circuit voltage is flat over a large range of states of charge. Because the voltage in standard batteries is typically used to inform state-of-charge estimation, a different corrective factor needs to be determined for this cell chemistry. Instead of using the battery voltage, the present study uses the battery’s dynamic response to assist state of charge estimation. The present work includes at least three novel contributions: 1) the electrochemical impedance of the LiFePO4-Li4Ti5O12 cell is shown to be strongly history dependent, 2) a novel system-identification technique is implemented to extract the EIS in-situ, and 3) a signature electrochemical impedance spectra attribute is identified that is a strong function of battery state of charge.