Aiman Mukhtar
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Aiman Mukhtar has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Tahir Mehmood
The State Key Laboratory of Refractories and Metallurgy, Hubei Province Key Laboratory of Systems Science in Metallurgical Process, International Research Institute for Steel Technology, Wuhan University of Science and Technology, Wuhan, P. R. China
2 shared publications - Babar Shahzad Khan
Department of Physics, Government College Women University, Sialkot, Pakistan
1 shared publication - Kaiming Wu
Collaborative Innovation Center for Advanced Steels, Wuhan University of Science and Technology, Wuhan 430081, China
1 shared publication - Liyuan Gu
School of Nuclear Technology and Chemistry & Biology Hubei University of Science and Technology Xianning People's Republic of China
1 shared publication - Shike Hu
Research and Development Center for Non-Powered Nuclear Technology, Hubei University of Science and Technology, Xianning 437000, China
1 shared publication T. Mehmood
Wuhan University of Science and Technology, Wuhan, P. R. China
1 shared publication
Latest Publications
- Open Access
Fe/Mn Multilayer Nanowires as High-Performance T1-T2 Dual Modal MRI Contrast Agents
A lot of nanomaterials are using T1-T2 dual mode magnetic resonance (MR) contrast agents (CAs), but multilayer nanowire (NW) with iron (Fe) and manganese (Mn) as T1-T2 dual modal CAs has not been reported yet. Herein, we synthesized a Fe/Mn multilayer NW with an adjustable Fe layer, as T1-T2 dual-mode CAs. The relaxation performance of Fe/Mn multilayer NW was studied at 1.5 T. Results show that, when the length of the Fe layer is about 10 nm and the Mn is about 5 nm, the r1 value (21.8 mM−1s−1) and r2 value (74.8 mM−1s−1) of the Fe/Mn multilayer NW are higher than that of Mn NW (3.7 mM−1s−1) and Fe NW (59.3 mM−1s−1), respectively. We predict that our Fe/Mn multilayer NW could be used as T1-T2 dual mode MRI CAs in the near future.
Open AccessFe/Mn Multilayer Nanowires as High-Performance T1-T2 Dual Modal MRI Contrast Agents
A lot of nanomaterials are using T1-T2 dual mode magnetic resonance (MR) contrast agents (CAs), but multilayer nanowire (NW) with iron (Fe) and manganese (Mn) as T1-T2 dual modal CAs has not been reported yet. Herein, we synthesized a Fe/Mn multilayer NW with an adjustable Fe layer, as T1-T2 dual-mode CAs. The relaxation performance of Fe/Mn multilayer NW was studied at 1.5 T. Results show that, when the length of the Fe layer is about 10 nm and the Mn is about 5 nm, the r1 value (21.8 mM−1s−1) and r2 value (74.8 mM−1s−1) of the Fe/Mn multilayer NW are higher than that of Mn NW (3.7 mM−1s−1) and Fe NW (59.3 mM−1s−1), respectively. We predict that our Fe/Mn multilayer NW could be used as T1-T2 dual mode MRI CAs in the near future.
- Open Access
- 6 June 2017
- Published by Science Publishing Group in American Journal of Electromagnetics and Applications
- Vol. 5 (1) , 1-6
Electrodeposition of Single Crystalline Co 56.48 Ni 43.52 Alloy Nanowires in AAO Template
Single crystalline cobalt nickel (Co-Ni) alloy nanowires are successfully fabricated using direct current (DC) electrodeposition with in the nanopore of highly ordered anodized aluminum oxide (AAO) template. SEM studies show that the average diameter of the alloy nanowires is approximately equal to 50 nm which corresponds to the pore size of the AAO template. Energy-dispersive X-ray (EDX) analysis confirmed that the Co-Ni alloy nanowires are deposited with 56.48:43.52 atomic ratios. We believe that at high potential the current density of Co nanowires is higher than depositing Ni nanowires which are clear by polarization curves, so content of Co increases in deposited Co 56.48 Ni 43.52 alloy nanowires. Single crystalline Co 56.48 Ni 43.52 alloys can be useful in future to compose and synthesize other metal nanostructures via template-based electrodeposition.
- 6 June 2017
- Published by Science Publishing Group in American Journal of Electromagnetics and Applications
- Vol. 5 (1) , 1-6
Open AccessElectrodeposition of Single Crystalline Co 56.48 Ni 43.52 Alloy Nanowires in AAO Template
Single crystalline cobalt nickel (Co-Ni) alloy nanowires are successfully fabricated using direct current (DC) electrodeposition with in the nanopore of highly ordered anodized aluminum oxide (AAO) template. SEM studies show that the average diameter of the alloy nanowires is approximately equal to 50 nm which corresponds to the pore size of the AAO template. Energy-dispersive X-ray (EDX) analysis confirmed that the Co-Ni alloy nanowires are deposited with 56.48:43.52 atomic ratios. We believe that at high potential the current density of Co nanowires is higher than depositing Ni nanowires which are clear by polarization curves, so content of Co increases in deposited Co 56.48 Ni 43.52 alloy nanowires. Single crystalline Co 56.48 Ni 43.52 alloys can be useful in future to compose and synthesize other metal nanostructures via template-based electrodeposition.
- Open Access
- 10 February 2017
- Published by Science Publishing Group in Modern Chemistry
- Vol. 5 (1) , 1-6
Silver and Copper Microstructures: The Workfunction’s Effect
To understand the growth mechanism of Ag and Cu nanowires we have studied the effect of workfunction on the metal nanowire growth by XRD, SEM and Potentiostat. Under the same potential and overpotential, the metal with a smaller workfunction has a higher current density, i.e. current density for Ag is higher than of Cu nanowires. Likewise metals, the plane with smaller workfunction grows faster than with the larger workfunction, thus the preferential growth plane is (220) for both metals. We argued that the current arises from electrons tunneling from metal surface to hydrated metal and hydrogen ions. The metal with a smaller workfunction has a thinner barrier for tunneling, thus leading to a higher current density. It is found that deposition method have no such effect on the structure of deposited nanowires.
- 10 February 2017
- Published by Science Publishing Group in Modern Chemistry
- Vol. 5 (1) , 1-6
Open AccessSilver and Copper Microstructures: The Workfunction’s Effect
To understand the growth mechanism of Ag and Cu nanowires we have studied the effect of workfunction on the metal nanowire growth by XRD, SEM and Potentiostat. Under the same potential and overpotential, the metal with a smaller workfunction has a higher current density, i.e. current density for Ag is higher than of Cu nanowires. Likewise metals, the plane with smaller workfunction grows faster than with the larger workfunction, thus the preferential growth plane is (220) for both metals. We argued that the current arises from electrons tunneling from metal surface to hydrated metal and hydrogen ions. The metal with a smaller workfunction has a thinner barrier for tunneling, thus leading to a higher current density. It is found that deposition method have no such effect on the structure of deposited nanowires.
- Open Access
- 31 December 2016
- Published by Pakistan Atomic Energy Commission in The Nucleus
- Vol. 53 (4) , 260-263
Effect of Deposition Temperature and Electrolytic Cell Concentration on Phase Transformation at Nanoscale
The coexistence of both hcp and fcc phases for Co nanowires was studied in this work. Both hcp and fcc Co nanowires with diameter of ~ 50nm were successfully prepared by adjusting the deposition parameters. The systematic results show the effect of electrolytic cell with different cobalt sulfate concentration and different deposition temperatures with same pH and potential for the formation of (fcc and hcp) Co nanowires. The fabricated nanowires were characterized by X-ray diffraction, and the morphology of the electrodeposited nanowires was explored by scanning electron microscope.
- 31 December 2016
- Published by Pakistan Atomic Energy Commission in The Nucleus
- Vol. 53 (4) , 260-263
Open AccessEffect of Deposition Temperature and Electrolytic Cell Concentration on Phase Transformation at Nanoscale
The coexistence of both hcp and fcc phases for Co nanowires was studied in this work. Both hcp and fcc Co nanowires with diameter of ~ 50nm were successfully prepared by adjusting the deposition parameters. The systematic results show the effect of electrolytic cell with different cobalt sulfate concentration and different deposition temperatures with same pH and potential for the formation of (fcc and hcp) Co nanowires. The fabricated nanowires were characterized by X-ray diffraction, and the morphology of the electrodeposited nanowires was explored by scanning electron microscope.